ASTM A387/A387M Carbon Steel Plates

SHH STEEL offers ASTM A387-compliant Grade 11/12/22 chromium-molybdenum alloy steel plates. ASTM A387 specifies plates for welded boilers and pressure vessels at high temperatures. Corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!

ASTM A387 Grade 911 Class 2 9Cr-1Mo-V-W pressure vessel steel plate, SHH STEEL

ASTM A387 Grade 911 Class 2 Steel Plate | A387 Gr.911 Cl.2 9Cr-1Mo-V Vessel Plate

ASTM A387 Grade 911 Class 2 / A387 Gr.911 Cl.2 is 9Cr-1Mo-1W-V-Nb vessel plate. Tensile is 620–840 MPa and yield is 440 MPa min. SHH STEEL supplies A387GR911CL2 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 21L Class 1 low-carbon 3Cr-1Mo pressure vessel steel plate, SHH STEEL

ASTM A387 Grade 21L Class 1 Steel Plate | A387 Gr.21L Cl.1 3Cr-1Mo Vessel Plate

ASTM A387 Grade 21L Class 1 / A387 Gr.21L Cl.1 is low-carbon 3Cr-1Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR21LCL1 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 22L Class 1 low-carbon 2.25Cr-1Mo pressure vessel steel plate, SHH STEEL

ASTM A387 Grade 22L Class 1 Steel Plate | A387 Gr.22L Cl.1 2.25Cr-1Mo Vessel Plate

ASTM A387 Grade 22L Class 1 / A387 Gr.22L Cl.1 is low-carbon 2.25Cr-1Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR22LCL1 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 91 Class 2 9Cr-1Mo-V pressure vessel steel plate, CSEF Grade 91, SHH STEEL

ASTM A387 Grade 91 Class 2 Steel Plate | A387 Gr.91 Cl.2 9Cr-1Mo-V Vessel Plate

ASTM A387 Grade 91 Class 2 / A387 Gr.91 Cl.2 is 9Cr-1Mo-V-Nb pressure-vessel plate. Tensile is 585–760 MPa and yield is 415 MPa min. SHH STEEL supplies A387GR91CL2 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 9 Class 2 chromium-molybdenum pressure vessel steel plate, 9Cr-1Mo, SHH STEEL

ASTM A387 Grade 9 Class 2 Steel Plate | A387 Gr.9 Cl.2 9Cr-1Mo Vessel Plate

ASTM A387 Grade 9 Class 2 / A387 Gr.9 Cl.2 is 9Cr-1Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. SHH STEEL supplies A387GR9CL2 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 9 Class 1 chromium-molybdenum pressure vessel steel plate, 9Cr-1Mo, SHH STEEL

ASTM A387 Grade 9 Class 1 Steel Plate | A387 Gr.9 Cl.1 9Cr-1Mo Vessel Plate

ASTM A387 Grade 9 Class 1 / A387 Gr.9 Cl.1 is 9Cr-1Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR9CL1 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 5 Class 2 chromium-molybdenum pressure vessel steel plate, 5Cr-0.5Mo, SHH STEEL

ASTM A387 Grade 5 Class 2 Steel Plate | A387 Gr.5 Cl.2 5Cr-0.5Mo Vessel Plate

ASTM A387 Grade 5 Class 2 / A387 Gr.5 Cl.2 is 5Cr-0.5Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. SHH STEEL supplies A387GR5CL2 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 5 Class 1 chromium-molybdenum pressure vessel steel plate, 5Cr-0.5Mo, SHH STEEL

ASTM A387 Grade 5 Class 1 Steel Plate | A387 Gr.5 Cl.1 5Cr-0.5Mo Vessel Plate

ASTM A387 Grade 5 Class 1 / A387 Gr.5 Cl.1 is 5Cr-0.5Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR5CL1 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 21 Class 2 chromium-molybdenum pressure vessel steel plate, 3Cr-1Mo, SHH STEEL

ASTM A387 Grade 21 Class 2 Steel Plate | A387 Gr.21 Cl.2 3Cr-1Mo Vessel Plate

ASTM A387 Grade 21 Class 2 / A387 Gr.21 Cl.2 is 3Cr-1Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. SHH STEEL supplies A387GR21CL2 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 21 Class 1 chromium-molybdenum pressure vessel steel plate, 3Cr-1Mo, SHH STEEL

ASTM A387 Grade 21 Class 1 Steel Plate | A387 Gr.21 Cl.1 3Cr-1Mo Vessel Plate

ASTM A387 Grade 21 Class 1 / A387 Gr.21 Cl.1 is 3Cr-1Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR21CL1 worldwide as a global steel mill sourcing partner.
View More
ASTM A387 Grade 22 Class 2 chromium-molybdenum pressure vessel steel plate, 2.25Cr-1Mo, SHH STEEL

ASTM A387 Grade 22 Class 2 Steel Plate | A387 Gr.22 Cl.2 2.25Cr-1Mo Vessel Plate

ASTM A387 Grade 22 Class 2 / A387 Gr.22 Cl.2 is 2.25Cr-1Mo pressure-vessel plate. Tensile is 515–690 MPa and yield is 310 MPa min. SHH STEEL supplies A387GR22CL2 worldwide as a global steel mill sourcing partner. SEO Title
View More
ASTM A387 Grade 22 Class 1 chromium-molybdenum pressure vessel steel plate, 2.25Cr-1Mo, SHH STEEL

ASTM A387 Grade 22 Class 1 Steel Plate | A387 Gr.22 Cl.1 2.25Cr-1Mo Vessel Plate

ASTM A387 Grade 22 Class 1 / A387 Gr.22 Cl.1 is 2.25Cr-1Mo pressure-vessel plate. Tensile is 415–585 MPa and yield is 205 MPa min. SHH STEEL supplies A387GR22CL1 worldwide as a global steel mill sourcing partner.
View More

ASTM A387/A387M Carbon Steel Plates

Nuclear-Grade Steel Plates

SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.

Nuclear-Grade Steel Plates