ASME SA736/SA736M Carbon Steel Plates

SHH STEEL supplies ASME SA736 / ASTM A736 low-carbon age-hardening nickel-copper-chromium-molybdenum-niobium alloy steel plates as China steel mill-Direct Supply. Plates are intended for welded pressure vessels and piping components, typically supplied as Grade A, Class 3 in quenched and precipitation heat-treated condition. Competitive mill price, cut-to-size service, fast delivery and full MTCs.

ASME SA736 Grade C Class 3 age-hardening vessel plate, Q+PHT, TS 95–115 ksi, SHH STEEL

ASME SA736 Grade C Class 3 Steel Plate | SA736 Gr.C Cl.3 Age-Hardening Vessel Plate

ASME SA736 Grade C Class 3 / ASME SA736 GR.C CL.3 is low-carbon age-hardening Ni-Cu-Mn-Mo-Nb plate under older ASME SA-736/SA-736M listings. Class 3 is the thickness-stepped Grade C line, 585 MPa yield on the thin band. Current ASTM A736 lists Grade A Class 3 only. SHH STEEL supplies SA736 Gr.C Cl.3 mill-direct against the edition named on the order, with 3.1 or 3.2 certificates.
View More
ASME SA736 Grade C Class 1 age-hardening Ni-Cu-Mn-Mo-Nb plate, ≤20 mm, TS 100–120 ksi, SHH STEEL

ASME SA736 Grade C Class 1 Steel Plate | SA736 Gr.C Cl.1 Age-Hardening Vessel Plate

ASME SA736 Grade C Class 1 / ASME SA736 GR.C CL.1 is low-carbon age-hardening Ni-Cu-Mn-Mo-Nb plate under older ASME SA-736/SA-736M listings. Class 1 is the high thin-plate line, typically to 20 mm, 620 MPa yield. Current ASTM A736 lists Grade A Class 3 only. SHH STEEL supplies SA736 Gr.C Cl.1 mill-direct against the edition named on the order, with 3.1 or 3.2 certificates.
View More
ASME SA736 Grade A Class 2 age-hardening vessel plate, normalized + PHT, SHH STEEL

ASME SA736 Grade A Class 2 Steel Plate | SA736 Gr.A Cl.2 Age-Hardening Vessel Plate

ASME SA736 Grade A Class 2 / ASME SA736 GR.A CL.2 is low-carbon age-hardening Ni-Cu-Cr-Mo-Nb plate under ASME SA-736/SA-736M. Class 2 is the mid-strength line that continues through thicker plate. Current ASTM A736 lists Grade A Class 3 only. SHH STEEL supplies SA736 Gr.A Cl.2 mill-direct against the edition named on the order, with 3.1 or 3.2 certificates.
View More
ASME SA736 Grade A Class 1 age-hardening vessel plate, as-rolled + PHT, ≤20 mm, TS 90–110 ksi, SHH STEEL

ASME SA736 Grade A Class 1 Steel Plate | SA736 Gr.A Cl.1 Age-Hardening Vessel Plate

ASME SA736 Grade A Class 1 / ASME SA736 GR.A CL.1 is low-carbon age-hardening Ni-Cu-Cr-Mo-Nb plate under ASME SA-736/SA-736M. Class 1 is the high-strength thin-plate line, typically to 20 mm. Current ASTM A736 lists Grade A Class 3 only. SHH STEEL supplies SA736 Gr.A Cl.1 mill-direct against the edition named on the order, with 3.1 or 3.2 certificates.
View More
ASME SA736 Grade A Class 3 age-hardening Ni-Cu-Cr-Mo-Nb vessel plate, Q+PHT, SHH STEEL

ASME SA736 Grade A Class 3 Steel Plate | SA736 Gr.A Cl.3 Age-Hardening Vessel Plate

ASME SA736 Grade A Class 3 / ASME SA736 GR.A CL.3 is low-carbon age-hardening Ni-Cu-Cr-Mo-Nb plate under ASME SA-736/SA-736M. Current ASTM A736 lists Grade A Class 3 only. Quenched and precipitation heat treated. SHH STEEL supplies SA736 Gr.A Cl.3 mill-direct with 3.1 or 3.2 certificates.
View More

Nuclear-Grade Steel Plates

SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.

Nuclear-Grade Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X