SA-1017/SA-1017M Carbon Steel Plates

ASME SA-1017/SA-1017M is identical with ASTM A1017/A1017M. It covers chromium-molybdenum-tungsten pressure-vessel plates for elevated-temperature boilers and vessels. Grades are 23, 911, 92 and 122. Grade 911 was moved here from A387. General requirements follow SA-20. SHH STEEL supplies SA-1017 / A1017 mill-direct from China origin. Search names: SA1017, SA-1017, SA1017M, SA-1017 Gr.911, P911, P92, T23.

ASME SA-1017 Grade 122 chromium-molybdenum-tungsten pressure vessel steel plate, 12Cr-0.4Mo-2W, SHH STEEL

ASME SA1017 Grade 122 Steel Plate | SA-1017 Gr.122 12Cr-2W Vessel Plate

ASME SA-1017 Grade 122 / SA1017 Gr.122 is 12Cr-0.40Mo-2.00W vessel plate, identical with A1017 Grade 122. Tensile is 620 MPa min and yield is 400 MPa min. SHH STEEL supplies SA1017GR122 worldwide as a global steel mill sourcing partner.
View More
ASME SA-1017 Grade 23 chromium-molybdenum-tungsten pressure vessel steel plate, 2.25Cr-0.2Mo-1.6W, SHH STEEL

ASME SA1017 Grade 23 Steel Plate | SA-1017 Gr.23 2.25Cr-1.6W Vessel Plate

ASME SA-1017 Grade 23 / SA1017 Gr.23 is 2.25Cr-0.20Mo-1.60W vessel plate, identical with A1017 Grade 23. Tensile is 510–690 MPa and yield is 400 MPa min. SHH STEEL supplies SA1017GR23 worldwide as a global steel mill sourcing partner.
View More
ASME SA-1017 Grade 92 chromium-molybdenum-tungsten pressure vessel steel plate, 9Cr-0.45Mo-1.75W, SHH STEEL

ASME SA1017 Grade 92 Steel Plate | SA-1017 Gr.92 9Cr-1.75W Vessel Plate

ASME SA-1017 Grade 92 / SA1017 Gr.92 is 9Cr-0.45Mo-1.75W vessel plate, identical with A1017 Grade 92. Tensile is 620–840 MPa and yield is 440 MPa min. SHH STEEL supplies SA1017GR92 worldwide as a global steel mill sourcing partner.
View More
ASME SA-1017 Grade 911 chromium-molybdenum-tungsten pressure vessel steel plate, 9Cr-1Mo-1W, SHH STEEL

ASME SA1017 Grade 911 Steel Plate | SA-1017 Gr.911 9Cr-1Mo-W Vessel Plate

ASME SA-1017 Grade 911 / SA1017 Gr.911 is 9Cr-1Mo-1W-V-Nb vessel plate, identical with A1017 Grade 911. Tensile is 620–840 MPa and yield is 440 MPa min. SHH STEEL supplies SA1017GR911 worldwide as a global steel mill sourcing partner.
View More

Nuclear-Grade Steel Plates

SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.