GB/T 16270 Q620E quenched and tempered high-strength structural steel plate, −40 °C impact, SHH STEEL

Q620E QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q620E is quenched-and-tempered carbon structural plate with 620 MPa minimum yield and −40°C impact toughness. SHH STEEL supplies Q620E QT plate mill-direct for cranes, mining frames and cold-region fabrication.
Keywords
Q620E, Q620E steel plate, GB/T 16270 Q620E, Q620E QT plate, Q620E carbon steel plate, Q620E supplier, ASTM A514, GB/T 16270 QT plate
Equivalent Grades:
GB/T 16270 Q620E / EN 10025-6 S620QL (cold) / ASTM A514 Gr — Material Specification: GB/T 16270 — Delivery: QT; -40℃
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q620E QT Carbon Steel Plate GB/T 16270?

Q620E, also searched as GB/T 16270 Q620E, Q620E QT plate, Q620E carbon steel plate, Q620E steel plate and Q620E quenched and tempered plate, is the 620 MPa quality-grade-E grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 620 is the thin-plate minimum yield in MPa, and E is the quality letter for Charpy impact at −40°C.

Q620E is the grade most buyers compare with European QL plate at 620 MPa. C is 0°C. D is −20°C. E is −40°C. F is −60°C. About 90 ksi on a US drawing is the same yield number. Cold-region crane and mine-truck builders use Q620E when the member was sized at 620 MPa and the specification names −40°C. A Q620C heat tested only at 0°C cannot be stamped E.

The closest European name is EN 10025-6 S620QL. Both are about 620 MPa QT plate tested at −40°C. S620Q is 0°C and lines up with Q620C. S620QL1 is −60°C and lines up with Q620F. On the US side there is no official 90 ksi plate grade. A514 Grade Q is 100 ksi / 690 MPa QT plate, one step higher. ASTM A656 Grade 80 is 80 ksi / 550 MPa, one step lower. Dual mark only when both books are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q620E from first-line QT mills, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q620E Confirmed
Other search names Q620E QT plate, Q620E carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 620 MPa min Confirmed
Quality grade E, impact at −40°C Confirmed
US comparison A514 is 690 MPa, not a twin Comparison only
Product analysis GB/T 222 column when ordered Confirmed
Not the same letter Q620C or Q620D Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S620QL, S620Q and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade E is tighter on phosphorus and sulfur than grade C, because the impact test is at −40°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Cr, Ni, Mo or B by thickness. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q620E

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 1.70 1.78
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.013
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q620E mechanical properties, Q620E yield strength, GB/T 16270 Q620E tensile and Q620E impact −40°C.

Tensile and impact — GB/T 16270 Q620E

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 620 MPa 700–890 MPa 15% −40°C, grade E
> 50–100 mm 600 MPa 700–890 MPa 15% −40°C, grade E
> 100–150 mm 550 MPa as standard table 15% −40°C, grade E

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A typical production heat is at or above 27 J to 34 J at −40°C, depending on the ordered edition and thickness. Write the energy on the purchase order if the owner wants a number above the book minimum.

Yield steps down with thickness. A 620 MPa name on 20 mm plate is not the minimum on a 120 mm flange. 620 MPa is about 90 ksi. ASTM A514 is 100 ksi and is not this number. SHH STEEL quotes the thickness band on the offer.

Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q620C GB/T 16270 QT 620 MPa 0°C Warmer sister
Q620D GB/T 16270 QT 620 MPa −20°C Warmer sister
Q620E GB/T 16270 QT 620 MPa −40°C This page
Q620F GB/T 16270 QT 620 MPa −60°C Colder sister
Q550E GB/T 16270 QT 550 MPa −40°C Lower yield
S620Q EN 10025-6 QT 620 MPa 0°C No
S620QL EN 10025-6 QT 620 MPa −40°C Closest comparison
A514 Gr.Q ASTM A514 QT 690 MPa Different Higher yield

Equivalent Material Grades

There is no official one-to-one substitute for Q620E. What buyers compare is a 620 MPa QT plate tested at −40°C.

In the United States there is no standard 90 ksi plate grade that matches this number. A514 Grade Q is 100 ksi / 690 MPa QT structural plate, closer to Q690E than to Q620E. ASTM A656 Grade 80 is 80 ksi / 550 MPa, closer to Q550. A572 Gr.65 is only 65 ksi. SHH STEEL will not stamp A514 on a Q620E certificate unless the purchase order names both books and both tables are met.

The usual European pair is S620QL. S620Q is warmer. S620QL1 is colder. In Japan, SM570 is a welded structural grade and is well below this yield.

Designation Country / region Standard Notes
Q620E China GB/T 16270 Name on this page
Q620C / Q620D / Q620F China GB/T 16270 Other impact letters
Q550E China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi QT, higher yield
ASTM A656 Grade 80 USA ASTM A656 80 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S620QL Europe EN 10025-6 −40°C QT comparison
S620Q Europe EN 10025-6 0°C, closer to Q620C

QT Structural Service

Buyers pick Q620E when a welded frame, boom or chassis wants 620 MPa yield, QT delivery and impact at −40°C. Search phrases such as Q620E steel plate, GB/T 16270 Q620E and Q620E QT plate all point here.

It is the wrong plate for a 0°C file that can use Q620C. It is the wrong plate for a −20°C file that can use Q620D. It is the wrong plate for a −60°C arctic file. That work is Q620F. It is the wrong plate for a 100 ksi US file. That work is A514 Grade Q. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade E at 620 MPa.

Weldability

Q620E is weldable QT carbon plate. The plate has already been quenched and tempered, and the joint must keep −40°C toughness. A procedure written for S355JR is not a Q620E procedure.

Typical consumables are matching 620–690 MPa low-hydrogen electrodes or wires, qualified on a QT 620 MPa family with a −40°C impact coupon. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S620QL is the usual starting point. An A514 procedure is a higher-strength reference, not a finished WPS for this grade.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −40°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q620E is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 620 MPa yield and the −40°C impact. Exact temperatures stay on the mill process sheet.

Do not order Q620E as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q620E, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S620QL is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q620E QT carbon steel plate:

  • Thickness: commonly 8 mm – 80 mm, heavier plate to 100 mm by enquiry
  • Width: 1500 mm – 3500 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q620E follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q620E QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2
50 – 80 −0.6 +1.4
80 – 100 −0.8 +1.6

Width on 1500–3500 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q620E unless the order says so.

Supplementary Requirements

Q620E already defines 620 MPa yield, QT delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q620E. Do not write only Q620E.

Impact. Grade E is −40°C. Write a higher energy if the owner requires it.

US comparison. Write A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q620E, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Construction machinery Q620E QT booms, frames and bases
Mining equipment Q620E chassis and body plate from SHH STEEL
Cranes and port equipment Q620E webs and flanges
Cold-region fabrication Q620E members tested at −40°C
Comparison vs S620QL Q620E next to S620QL
Comparison vs S620Q Q620E next to S620Q
Comparison vs A514 Q620E next to A514 Gr.Q

Q620E is the plate for a 620 MPa QT file tested at −40°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for a 100 ksi QT member.

Supply Capability

SHH STEEL sources Q620E from first-line Chinese QT mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm, 60 mm, 80 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when plate is in yard; standard QT rolling about 35–45 days; 3.2 inspection about 45–60 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q620E that means mill-direct QT price, not a multi-layer stockist mark-up. We buy from mills that already run the 620 MPa quench-and-temper route, so the heat carries the −40°C impact without a second upgrade charge.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard heat about 35–45 days, 3.2 inspection about 45–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q620E, keep the QT route, and do not ship Q620D or A514 as Q620E. We will not change E to D to save a cold test, and we will not treat Q620E as S355. If the drawing needs −60°C, we will move the inquiry to Q620F and keep the price on the right grade.

FAQ

What is Q620E steel plate?
Q620E in GB/T 16270 is quenched-and-tempered carbon structural plate with 620 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q620E the same as Q620C?
No. Both yield at 620 MPa. Q620C is tested at 0°C. Q620E is tested at −40°C.
What is the US equivalent of Q620E?
There is no official ASTM twin at 90 ksi. A514 Grade Q is 100 ksi / 690 MPa QT plate, one step higher. A656 Grade 80 is 80 ksi, one step lower. SHH STEEL does not dual-mark A514 unless both books are met.
Is Q620E the same as S620QL?
They are the usual comparison pair: both are about 620 MPa QT plate tested at −40°C. Dual mark only when both books are fully met. S620Q is warmer. S620QL1 is colder.

Conclusion

Q620E QT carbon steel plate to GB/T 16270 is 620 MPa quenched-and-tempered structural plate with impact at −40°C. The nearest US QT comparison is ASTM A514, which is 690 MPa and is not a substitute. Whether the inquiry says Q620E, GB/T 16270 Q620E, Q620E QT plate or Q620E carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q620E chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q620E QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, QT route, cutting, UT, 3.2 inspection or a worldwide quotation.

Q620E, Q620E steel plate, GB/T 16270 Q620E, Q620E QT plate, Q620E carbon steel plate, Q620E supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X