ASTM A588 Grade A high-strength low-alloy weathering steel plate, 50 ksi yield, SHH STEEL

ASTM A588 Grade A Steel Plate | A588 Gr.A Weathering Steel supplier

ASTM A588 Grade A / A588 Gr.A is 50 ksi weathering structural plate for bridges and outdoor frames. Yield 345 MPa to 100 mm, Cu-Cr-V chemistry, unpainted patina service. SHH STEEL supplies A588GRA worldwide.
Keywords
ASTM A588 Grade A, A588 Gr.A, A588GRA, A588-A, A588 Gr A, weathering steel plate, A588 Grade A supplier, 50ksi weathering steel
Equivalent Grades:
ASTM A588 Gr A / EN 10025-5 S355J2W (near) / JIS SMA490AW / GB Q355NH — Material Specification: ASTM A588 / A588M — Delivery: As-rolled + age (AR), or TMCP; weathering (Corten-type)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Weathering Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is ASTM A588 Grade A Steel?

ASTM A588 Grade A, also searched as A588 Gr.A, A588GRA, A588-A, A588 Gr A, ASTM A588 Gr.A and A588 Grade A 50ksi, is the most specified grade in ASTM A588/A588M. That book covers high-strength low-alloy structural steel plates, shapes and bars with atmospheric corrosion resistance for welded, riveted or bolted construction. The main use is welded bridges and buildings where weight saving or unpainted durability matters.

The current book lists three grades: A, B and K. This page is Grade A. Grade B uses a different Cu-Cr-Ni-V window. Grade K uses niobium instead of vanadium. Mechanical properties follow the same thickness table. Do not treat A588 as ASTM A572 Grade 50 unless the file does not need weathering. Do not treat A588 as ASTM A36. A36 has no 50 ksi yield and no Cu-Cr patina system. Do not treat A588 as a pressure-vessel plate. That work sits on ASTM A516 or pressure vessel steel plates.

Buyers also type Corten A, Corten B and A242. Corten A and Corten B are trademark names. ASTM A242 is a different weathering book. Dual mark only when both chemistries and both mechanical tables are met. European comparisons are EN 10025-5 S355J0W and EN 10025-5 S355J2W.

A588 Grade A develops a stable oxide film in wet-dry outdoor air. That film is why shops leave bridges, towers and facades unpainted. The book asks for an atmospheric corrosion-resistance index of 6.0 or higher by ASTM G101 on heat analysis. Indoor wet service, standing water and marine splash still need coating review. Weathering steel is not stainless steel.

General requirements follow A6/A6M. Steel is produced to fine-grain practice. Thickness in the book goes to 8 in / 200 mm. To 100 mm the minimum yield is 50 ksi / 345 MPa and the minimum tensile is 70 ksi / 485 MPa. Over 100 mm the yield name drops. Density is 7.85 g/cm³.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We source A588 Gr.A from first-line Chinese mills, print heat analysis, record the G101 index when requested, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America.

Related category pages: weathering steel plates, structural steel plates, EN 10025-5 and high strength low alloy plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book ASTM A588/A588M Grade A Confirmed
Other search names A588 Gr.A, A588GRA, A588-A, A588 Gr A Covered
Steel type HSLA weathering structural plate Confirmed
Grain practice Fine grain Confirmed
General requirements A6 / A6M Confirmed
Yield to 100 mm 50 ksi / 345 MPa min Confirmed
Tensile to 100 mm 70 ksi / 485 MPa min Confirmed
Corrosion index G101 ≥ 6.0 on heat analysis When ordered
Max thickness in book 8 in / 200 mm Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

Sister grades in the same book are Grade B and Grade K. Nearby pages that buyers compare, but must not swap blindly, include Corten A, Corten B, EN 10025-5 S355J2W and A572 Gr.50.

Chemical Composition

Grade A is the vanadium-bearing Cu-Cr grade. Heat analysis is the mill table. Product analysis, when ordered, follows A6 product tolerances on that heat.

Heat Analysis — ASTM A588 Grade A

Element Heat analysis (%)
Carbon (C), max 0.19
Manganese (Mn) 0.80 – 1.25
Phosphorus (P), max 0.030
Sulfur (S), max 0.030
Silicon (Si) 0.30 – 0.65
Nickel (Ni), max 0.40
Chromium (Cr) 0.40 – 0.65
Copper (Cu) 0.25 – 0.40
Vanadium (V) 0.02 – 0.10

For each 0.01% carbon below the 0.19% max, manganese may rise 0.06%, up to 1.50% Mn. Grade B allows 0.20% C, 0.75–1.35% Mn, 0.15–0.50% Si and 0.20–0.40% Cu. Grade K drops vanadium and adds niobium 0.005–0.05%. If the purchase order writes product analysis, SHH STEEL prints heat plus A6 product checks.

Do not treat this chemistry as A572 Gr.50. A572-50 has no mandatory Cu-Cr weathering window. Do not treat it as S355JR. S355JR is ordinary structural steel.

Mechanical Properties

Buyers search A588 Gr.A mechanical properties, A588GRA yield, A588 Grade A 50ksi and A588-A tensile.

Tensile Properties — ASTM A588 plates and bars

Thickness Tensile min Yield min Elongation 8 in min Elongation 2 in min
≤ 4 in / 100 mm 70 ksi / 485 MPa 50 ksi / 345 MPa 18% 21%
Over 4 in to 5 in / 100–125 mm 67 ksi / 460 MPa 46 ksi / 315 MPa — 21%
Over 5 in to 8 in / 125–200 mm 63 ksi / 435 MPa 42 ksi / 290 MPa — 21%

Structural shapes keep 50 ksi yield and 70 ksi tensile at all listed thicknesses. Grade A, Grade B and Grade K share this table. The grade letter does not change the yield name.

Impact is not automatic. Bridge work that needs Charpy values must write temperature, joules and orientation. A709 Grade 50W is the bridge-book twin when the file is an AASHTO bridge, not a building frame.

Density is 7.85 g/cm³. Typical hardness after rolling sits around 130–180 HBW. Hardness is not a Table 2 limit.

Material Comparison

Grade Book Yield to 100 mm Weathering Swap?
A588 Grade A A588/A588M 345 MPa Yes, V grade This page
A588 Grade B A588/A588M 345 MPa Yes Chemistry only
A588 Grade K A588/A588M 345 MPa Yes, Nb grade Chemistry only
A572 Gr.50 A572 345 MPa No No
A36 A36 250 MPa No No
Corten A Trademark ~355 MPa class Yes Comparison only
S355J2W EN 10025-5 355 MPa Yes Comparison only
S355J2WP EN 10025-5 355 MPa P weathering Comparison only

Equivalent Material Grades

There is no official one-to-one worldwide twin for A588 Gr.A. What buyers compare is a 345 MPa weathering plate with Cu-Cr-V.

In the United States the sister grades are A588 Grade B and Grade K. Bridge files often rewrite the same chemistry as A709 Grade 50W. Corten A and Corten B are the trademark names purchasing departments still type. ASTM A242 is a thinner-product weathering book, not a free substitute.

In Europe compare S355J0W, S355J2W and S355K2W. Phosphorus weathering grades S355J0WP and S355J2WP are a different chemistry family. See EN 10025-5 and weathering steel plates.

In China compare GB/T 4171 Q355GNH or Q355NH. Q355GNH is the closer weathering talk. Dual mark only when both books are fully met. In Japan shops compare JIS G3125 SPA-H for thin product, not for 40–80 mm bridge plate.

Designation Country / region Standard Notes
A588 Gr.A / A588GRA USA ASTM A588/A588M Name on this page
A588 Grade B USA A588/A588M Sister chemistry
A588 Grade K USA A588/A588M Nb sister
A709 Grade 50W USA A709 Bridge-book twin
Corten A Trademark — Common search name
Corten B Trademark — Common search name
S355J2W Europe EN 10025-5 Fine-grain weathering
S355J0W Europe EN 10025-5 0 °C weathering
Q355GNH China GB/T 4171 Weathering comparison

Weathering Structural Service

Buyers pick A588 Gr.A when a bridge, tower, hopper, facade or unpainted frame wants 50 ksi yield and a patina instead of a full paint system. Search phrases such as A588GRA, A588 Grade A, A588-A and A588 Gr A 50ksi all point here.

It is the wrong plate for a pressure vessel. That work is A516 Grade 70 or A662 Grade B. It is the wrong plate for a painted 50 ksi building that does not need copper and chromium. That work is A572 Gr.50. It is the wrong plate for a 70 ksi HPS bridge girder. That work is A709 HPS 70W. It is the wrong plate for stainless cladding. That work sits on stainless steel sheets and plates.

Unpainted A588 needs wet-dry cycles. Standing water, buried faces, and constant spray do not form a stable film. SHH STEEL will say that on the quotation when the drawing shows a tank floor or a splash zone.

Weldability

ASTM A588 Grade A is weldable HSLA plate. Treat welding as structural production welding, not as ordinary A36 shop practice.

Typical consumables are matching weathering wires or E8018-C3 / E80C-G type electrodes qualified on a 50 ksi weathering family. If the fillet will be painted and the file allows it, some shops use E7018 and accept a color mismatch at the toe. A procedure written for A572 Gr.50 may miss the copper and chromium effect on the HAZ color. A procedure written for S355JR is not a weathering procedure.

Preheat follows thickness and hydrogen control. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, CEV and the G101 index for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for A588 Gr.A is as-rolled or normalized when the mill route or the purchase order asks for it.

A588 is not a QT vessel book. Do not order it as SA517 or A514. Normalizing, when used, is typically 880–920 °C, soaked through, then air cooled. Fine-grain practice is part of manufacture.

If the fabricator hot-forms outside the mill window, a new normalize or a controlled cool may be required. Simulated PWHT is uncommon on weathering bridges and only applies when the order writes it.

The certificate lists ASTM A588 Grade A; heat number; heat analysis; tensile by thickness band; fine-grain practice; G101 index when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for A588 Gr.A weathering steel plate:

  • Thickness: commonly 6 mm – 100 mm, heavier plate to 200 mm by enquiry
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size girders, flanges and facade panels are available. Browse more sizes on weathering steel plates, structural steel plates and the products index.

Tolerances

Dimensional limits for ASTM A588 Grade A follow A6 / A6M unless the purchase order names another table.

Typical A6 thickness tolerance idea for A588 Gr.A

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
6 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2
50 – 80 −0.6 +1.4
80 – 100 −0.8 +1.6

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows A6 unless a tighter class is written. SHH STEEL will not assume a zero-minus extra on A588GRA unless the order says so.

Supplementary Requirements

Grade A already defines chemistry and the 50 ksi table to 100 mm. Extra items still have to be written on the purchase order.

Book name. Write ASTM A588 Grade A. Write A709 Grade 50W if the file is a bridge to AASHTO.

Impact details. Write temperature, joules, location and orientation.

Product analysis. Write it if the file needs A6 product checks.

G101 index. Write it if the owner wants the corrosion index on the certificate.

Through-thickness / Z-test. When needed on thick flanges.

NDE. UT to the named class.

Shot blast and primer. Only when the plate will not stay bare. Bare weathering plate is usually shipped with mill scale or a light blast, not a full paint system.

Identification and stamping. Heat number, A588 Grade A, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Bridges A588 Gr.A / A588GRA girders and flanges
Buildings Unpainted frames and facade panels from SHH STEEL
Towers and poles Weathering lattice and shafts
Hoppers and wagons Bare weathering plate
Comparison vs Corten A A588GRA next to Corten A
Comparison vs S355J2W A588GRA next to S355J2W
Comparison vs A572-50 A588GRA next to A572 Gr.50

A588 Grade A is the plate for a file that wants 50 ksi yield and a patina. It is the wrong plate for a painted warehouse that can use A36 or S355JR. It is the wrong plate for a QT 100 ksi member. That work sits on A514 Grade Q or A709 HPS 100W.

Supply Capability

SHH STEEL sources ASTM A588 Grade A from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, TISCO (Taiyuan), Jiuquan (JISCO) and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point. Dual marking to A709 Grade 50W or GB/T 4171 Q355GNH is available only when both books are met.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard rolling about 30–45 days; normalized or 3.2 inspection about 45–60 days.

Why Choose SHH STEEL

Experience on this grade is simple: print A588 Grade A, keep Cu 0.25–0.40% and V 0.02–0.10% on heat analysis, and do not ship A572-50 as weathering plate. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) will not drop copper to save alloy, will not mark Grade B chemistry as Grade A, and will not treat A588 as A36.

We keep the book on the order. A588GRA is not A572 Gr.50. A588 Grade A is not Corten A unless the trademark chemistry is also met. A588 Grade A is not S355J2W unless both books are on the certificate. If the drawing is a bridge to AASHTO, we will ask whether the stamp should read A709 Grade 50W.

FAQ

What is ASTM A588 Grade A steel plate?
ASTM A588 Grade A, also searched as A588 Gr.A, A588GRA and A588-A, is 50 ksi weathering structural plate. To 100 mm the yield is 345 MPa and the tensile is 485 MPa minimum. Copper, chromium and vanadium form the patina. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is A588 Grade A the same as Corten A?
No. Corten A is a trademark. Chemistry and thickness tables are close, not identical. Dual mark only when both requirements are met.
What is the difference between A588 Grade A and Grade B?
Strength tables are the same. Grade A uses 0.19% max carbon, 0.30–0.65% silicon, 0.25–0.40% copper and 0.02–0.10% vanadium. Grade B opens carbon to 0.20% and uses a different Mn-Si-Cu window.
What is the difference between A588 Grade A and A572 Grade 50?
Both yield at 345 MPa to 100 mm. A572 Gr.50 is not a weathering grade. A588 Grade A has mandatory copper and chromium.
Does A588GRA need painting?
Not for normal wet-dry outdoor air. Standing water, marine splash and buried faces still need a coating review.
What is the Chinese equivalent of A588 Grade A?
Buyers compare GB/T 4171 Q355GNH or Q355NH. It is a comparison, not an automatic substitute.
What is the delivery time for A588 Grade A?
Ex-stock about 5–7 days when plate is in yard. Standard rolling about 30–45 days. Normalized or 3.2 inspection about 45–60 days.
Can SHH STEEL issue EN 10204 3.2 for A588GRA?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS or the inspector named on the order.

Conclusion

ASTM A588 Grade A Steel Plate is 50 ksi weathering structural plate for bridges, towers and unpainted frames, with 345 MPa yield to 100 mm and Cu-Cr-V chemistry. Whether the inquiry says ASTM A588 Grade A, A588 Gr.A, A588GRA, A588-A, A588 Gr A or A588 Grade A 50ksi, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with Grade A chemistry, heat analysis, A6 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies ASTM A588 Grade A / A588 Gr.A Weathering Steel to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, dual A709 50W marking, cutting, blast, 3.2 inspection or a worldwide quotation.

ASTM A588 Grade A Steel Plate, A588 Gr.A, A588GRA, weathering steel plate, A588 Grade A supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X