ASME SB-265

Product Showcase

ASME SB-265 Titanium Alloys

SHH STEEL offers ASME SB-265-compliant Grade 2/5 titanium alloy sheets and plates. ASME SB-265 specifies pressure vessel-grade materials for chemical processing and desalination with high strength-to-weight ratio. Weldable, certified quality, competitive prices, customizable. Trust SHH STEEL!

ASME SB-265 Grade 40 Titanium Plate | Ti-3.9V-0.85Al (UNS R54407)

ASME SB-265 Grade 40 titanium plate is Ti-3.9V-0.85Al titanium alloy (UNS R54407) supplied annealed. It is specified for 655 MPa minimum tensile strength, 517 MPa yield and 15% minimum elongation. Typical uses include cold-formed medium-strength parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 35 Titanium Plate | Ti-4.5Al-2Mo-1.6V (UNS R56340)

ASME SB-265 Grade 35 titanium plate is Ti-4.5Al-2Mo-1.6V titanium alloy (UNS R56340) supplied annealed. It is specified for 895 MPa minimum tensile strength, 828 MPa yield and 5% minimum elongation. Typical uses include high-strength plate parts in the Grade 5 strength class. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 36 Titanium Plate | Ti-45Nb (UNS R58450)

ASME SB-265 Grade 36 titanium plate is Ti-45Nb titanium alloy (UNS R58450) supplied solution treated. It is specified for 450 MPa minimum tensile strength, 410–655 MPa yield and 10% minimum elongation. Typical uses include aerospace rivets and fastener blanks. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 37 Titanium Plate | Ti-1.5Al (UNS R52815)

ASME SB-265 Grade 37 titanium plate is Ti-1.5Al titanium alloy (UNS R52815) supplied annealed. It is specified for 345 MPa minimum tensile strength, 215–450 MPa yield and 20% minimum elongation. Typical uses include exhaust systems and mufflers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 38 Titanium Plate | Ti-4Al-2.5V-1.5Fe (UNS R54250)

ASME SB-265 Grade 38 titanium plate is Ti-4Al-2.5V-1.5Fe titanium alloy (UNS R54250) supplied annealed. It is specified for 895 MPa minimum tensile strength, 794 MPa yield and 10% minimum elongation. Typical uses include armour and defence plate. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 39 Titanium Plate | Ti-0.25Fe-0.4Si (UNS R53390)

ASME SB-265 Grade 39 titanium plate is Ti-0.25Fe-0.4Si titanium alloy (UNS R53390) supplied annealed. It is specified for 515 MPa minimum tensile strength, 410–620 MPa yield and 20% minimum elongation. Typical uses include automotive and motorcycle exhaust systems. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 34 Titanium Plate | Ni-Pd-Ru-Cr Titanium (UNS R53445)

ASME SB-265 Grade 34 titanium plate is Ni-Pd-Ru-Cr titanium (UNS R53445) supplied annealed. It is specified for 450 MPa minimum tensile strength, 380–550 MPa yield and 18% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 27 Titanium Plate | Grade 1 with Ru (UNS R52254)

ASME SB-265 Grade 27 titanium plate is Grade 1 with Ru titanium (UNS R52254) supplied annealed. It is specified for 240 MPa minimum tensile strength, 138–310 MPa yield and 24% minimum elongation. Typical uses include linings and cladding in crevice-prone chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 28 Titanium Plate | Ti-3Al-2.5V with Ru (UNS R56323)

ASME SB-265 Grade 28 titanium plate is Ti-3Al-2.5V with Ru titanium alloy (UNS R56323) supplied annealed. It is specified for 620 MPa minimum tensile strength, 483 MPa yield and 15% minimum elongation. Typical uses include oil and gas and geothermal equipment. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 29 Titanium Plate | Ti-6Al-4V ELI with Ru (UNS R56404)

ASME SB-265 Grade 29 titanium plate is Ti-6Al-4V ELI with Ru titanium alloy (UNS R56404) supplied annealed. It is specified for 828 MPa minimum tensile strength, 759 MPa yield and 10% minimum elongation. Typical uses include offshore drilling and production riser components. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 30 Titanium Plate | Ti-0.3Co-0.05Pd (UNS R53530)

ASME SB-265 Grade 30 titanium plate is Ti-0.3Co-0.05Pd titanium (UNS R53530) supplied annealed. It is specified for 345 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Grade 31 Titanium Plate | Ti-0.3Co-0.05Pd (UNS R53532)

ASME SB-265 Grade 31 titanium plate is Ti-0.3Co-0.05Pd titanium (UNS R53532) supplied annealed. It is specified for 450 MPa minimum tensile strength, 380–550 MPa yield and 18% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

ASME SB-265 Titanium Alloys

ASME SB-265 Grade 40 Titanium Plate | Ti-3.9V-0.85Al (UNS R54407) ASME SB-265 Grade 35 Titanium Plate | Ti-4.5Al-2Mo-1.6V (UNS R56340) ASME SB-265 Grade 36 Titanium Plate | Ti-45Nb (UNS R58450) ASME SB-265 Grade 37 Titanium Plate | Ti-1.5Al (UNS R52815)
ASME SB-265 Grade 38 Titanium Plate | Ti-4Al-2.5V-1.5Fe (UNS R54250) ASME SB-265 Grade 39 Titanium Plate | Ti-0.25Fe-0.4Si (UNS R53390) ASME SB-265 Grade 27 Titanium Plate | Grade 1 with Ru (UNS R52254) ASME SB-265 Grade 28 Titanium Plate | Ti-3Al-2.5V with Ru (UNS R56323)
ASME SB-265 Grade 29 Titanium Plate | Ti-6Al-4V ELI with Ru (UNS R56404) ASME SB-265 Grade 30 Titanium Plate | Ti-0.3Co-0.05Pd (UNS R53530) ASME SB-265 Grade 31 Titanium Plate | Ti-0.3Co-0.05Pd (UNS R53532) ASME SB-265 Grade 32 Titanium Plate | Ti-5Al-1Sn-1Zr-1V-0.8Mo (UNS R55111)
ASME SB-265 Grade 33 Titanium Plate | Ni-Pd-Ru-Cr Titanium (UNS R53442) ASME SB-265 Grade 34 Titanium Plate | Ni-Pd-Ru-Cr Titanium (UNS R53445) ASME SB-265 Grade 23 Titanium Plate | Ti-6Al-4V ELI (UNS R56407) ASME SB-265 Grade 24 Titanium Plate | Ti-6Al-4V with Pd (UNS R56405)
ASME SB-265 Grade 25 Titanium Plate | Ti-6Al-4V with Ni and Pd (UNS R56403) ASME SB-265 Grade 26 Titanium Plate | Ru-Bearing CP Titanium (UNS R52404) ASME SB-265 Grade 26H Titanium Plate | Grade 26 High Strength (UNS R52404) ASME SB-265 Grade 17 Titanium Plate | Grade 1 Lean Pd (UNS R52252)
ASME SB-265 Grade 18 Titanium Plate | Ti-3Al-2.5V with Pd (UNS R56322) ASME SB-265 Grade 19 Titanium Plate | Beta C Titanium (UNS R58640) ASME SB-265 Grade 20 Titanium Plate | Beta C with Pd (UNS R58645) ASME SB-265 Grade 21 Titanium Plate | TIMETAL 21S (UNS R58210)
ASME SB-265 Grade 13 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53413) ASME SB-265 Grade 14 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53414) ASME SB-265 Grade 15 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53415) ASME SB-265 Grade 16 Titanium Plate | Lean Pd CP Titanium (UNS R52402)
ASME SB-265 Grade 16H Titanium Plate | Grade 16 High Strength (UNS R52402) ASME SB-265 Grade 7H Titanium Plate | Grade 7 High Strength (UNS R52400) ASME SB-265 Grade 9 Titanium Plate | Ti-3Al-2.5V (UNS R56320) ASME SB-265 Grade 11 Titanium Plate | Grade 1 with Pd (UNS R52250)
ASME SB-265 Grade 12 Titanium Plate | Ti-0.3Mo-0.8Ni (UNS R53400) ASME SB-265 Grade 1 Titanium Plate | CP Titanium (UNS R50250) ASME SB-265 Grade 2 Titanium Plate | CP Titanium (UNS R50400) ASME SB-265 Grade 2H Titanium Plate | Grade 2 High Strength (UNS R50400)
ASME SB-265 Grade 3 Titanium Plate | CP Titanium (UNS R50550) ASME SB-265 Grade 4 Titanium Plate | CP Titanium (UNS R50700) ASME SB-265 Grade 5 Titanium Plate | Ti-6Al-4V (UNS R56400) ASME SB-265 Grade 6 Titanium Plate | Ti-5Al-2.5Sn (UNS R54520)
ASME SB-265 Grade 7 Titanium Plate | Ti-0.2Pd (UNS R52400)

Titanium Alloy Plates and Sheets

SHH STEEL, a premier Titanium Alloy Plates and Sheets exporter, produces and exports titanium alloy plates and sheets for aerospace, marine, and chemical industries. Our products, like Grade 2 and Grade 5 (ASTM B265), offer high strength and corrosion resistance. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Grade 5 titanium plates and custom solutions for high-performance projects.

Titanium Alloy Plates and Sheets

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X