ASME SB-265 Grade 16H titanium plate is Grade 16 high strength titanium (UNS R52402) supplied annealed. It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASME SB-265 Grade 16H titanium plate, Grade 16H titanium plate, UNS R52402 plate, Grade 16 high strength titanium plate, ASME SB-265 titanium sheet
Equivalent Grades:
UNS R52402, ASTM B265 Gr.16H, JIS Class 18 (TP345Pd), GB/T TA8
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASME SB-265 Grade 16H titanium plate?

ASME SB-265 Grade 16H titanium plate is made to ASME SB-265, the ASME Boiler and Pressure Vessel Code Section II, Part B specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R52402. Grade 16H is Grade 16 with 58 ksi (400 MPa) minimum tensile strength, intended mainly for pressure vessels.

This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Because SB-265 adopts ASTM B265, it uses the same grade numbers and UNS numbers. A grade being listed in SB-265 does not by itself mean it has allowable stresses for every Code; that depends on Section II, Part D and the Code of construction.

SHH STEEL handles Grade 16H plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASME SB-265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 16, ASME SB-265 Grade 16, ASTM B265 Grade 16H.

Material specification for ASME SB-265 Grade 16H

ASME SB-265 is the specification for titanium and titanium alloy strip, sheet and plate in ASME Boiler and Pressure Vessel Code Section II, Part B. It adopts ASTM B265 with any ASME changes noted on its cover, so the product definitions and test requirements follow the adopted B265 edition.

Ordering item ASME SB-265 basis
Specification ASME SB-265 in the BPVC Section II, Part B edition named by the Code of construction
Grade / UNS Grade 16H, Grade 16 High Strength, UNS R52402
Product forms Plate over 0.187 in (4.75 mm) and over 10 in (254 mm) wide; sheet and strip 0.187 in (4.75 mm) and under
Condition Annealed
Code use Allowable stresses, if any, come from Section II, Part D for the Code and edition being used
Certificate Manufacturer’s report certifying SB-265; add ASTM B265 if dual certification is needed
Marking Specification number, grade, heat number, manufacturer’s identification and nominal thickness

The ASME edition referenced by a design may lag the newest ASTM B265 edition. If the plate will be stamped or used for Code construction, state SB-265, the Section II edition and any Code Case on the order, and confirm that the grade is accepted for the intended Code before design is fixed.

Chemical composition of ASME SB-265 Grade 16H (UNS R52402)

Single values are maximums; ranges are shown where an element is added. Titanium is the remainder. The product analysis column applies to check analysis on finished product.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.08 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.25 +0.03
Palladium (Pd) 0.04–0.08 ±0.005
Other elements, each 0.1 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

The heat is analysed for the listed elements and hydrogen is reported on the final product. Residual elements need not be reported unless they exceed the each or total limits. Because SB-265 adopts B265, the limits match the ASTM grade in the adopted edition.

Mechanical properties of ASME SB-265 Grade 16H

The values below are the requirements for Grade 16H plate in the annealed condition.

Property Requirement
Tensile strength, min 58 ksi (400 MPa)
Yield strength, 0.2% offset 40–65 ksi (275–450 MPa)
Elongation in 2 in or 50 mm, min 20%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 2T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 2.5T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail the grade even if it is strong. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASME SB-265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Annealed
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

The grade is supplied annealed and is not strengthened by heat treatment. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 16H titanium plate

Grade 16H is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.

  • Use trailing shields and back purging until the metal cools below about 400 °C
  • Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
  • Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
  • Check weld colour and reject heavily discoloured welds

Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.

For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 16H titanium plate

Typical uses of Grade 16H plate include:

  • Equipment handling hot chloride brines where crevice corrosion is a risk
  • Reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid
  • Flue gas desulfurisation and chemical process heat exchangers
  • Gasket faces, flange areas and crevice-prone parts of titanium equipment

Plate certified as 16H may also be certified as Grade 16. The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.

When selecting Grade 16H, compare it with Grade 7, Grade 7H, Grade 11. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 16H with other ASME SB-265 grades

The grades below are the closest neighbours of Grade 16H in ASME SB-265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 7 (R52400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% Pd-bearing Grade 2 for crevice and reducing-acid service
Grade 7H (R52400) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 7 with higher guaranteed tensile
Grade 11 (R52250) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Pd-bearing Grade 1
Grade 16 (R52402) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% Lean-Pd Grade 2
Grade 16H (R52402) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 16 with higher guaranteed tensile
Grade 17 (R52252) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Lean-Pd Grade 1
Grade 26 (R52404) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% Ru-bearing Grade 2
Grade 26H (R52404) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 26 with higher guaranteed tensile
Grade 27 (R52254) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Ru-bearing Grade 1

The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.

ASME SB-265 Grade 16H equivalent grades

The designations below are commonly compared with ASME SB-265 Grade 16H. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASME SB-265 Grade 16H
ASTM B265 Grade 16 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
ASME SB-265 Grade 16 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
ASTM B265 Grade 16H ASTM specification adopted by SB-265; same grade requirements
JIS H4600 Class 18 (TP345Pd) Close equivalent; JIS strength range and tests differ
GB/T 3621 TA8 Close equivalent; confirm grade name and limits in the ordered edition
UNS R52402 Same unified number as ASTM Grade 16

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 16H titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to ASME SB-265 and the Section II edition you name, and can arrange dual SB-265 / B265 certification
  • Certificates are checked against the Grade 16H chemistry and tensile limits before shipment
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASME SB-265 Grade 16H plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASME SB-265 Grade 16H (UNS R52402), Section II edition; add ASTM B265 if dual certification
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What is the difference between ASME SB-265 Grade 16H and ASTM B265 Grade 16H?
SB-265 adopts B265, so chemistry and tensile requirements normally match the adopted edition. SB-265 is the document cited by ASME Code construction; B265 is the ASTM industrial specification. Dual certification covers both.
What is the tensile strength of ASME SB-265 Grade 16H titanium plate?
The requirement is 58 ksi (400 MPa) minimum. The 0.2% proof or yield strength is 40–65 ksi (275–450 MPa). Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is Grade 16H mainly used for?
Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk, reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid and flue gas desulfurisation and chemical process heat exchangers. Plate certified as 16H may also be certified as Grade 16.
Does SB-265 use the same plate, sheet and strip definitions as B265?
Yes. Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide; thinner product is sheet if 24 in (610 mm) or more wide, otherwise strip.
What should I send for a quotation?
Send ASME SB-265 Grade 16H, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for ASME SB-265 Grade 16H titanium plate

ASME SB-265 Grade 16H is Grade 16 high strength titanium, UNS R52402, specified for 58 ksi (400 MPa) minimum tensile strength, 40–65 ksi (275–450 MPa) yield or proof strength and 20% minimum elongation in the annealed condition. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk and reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASME SB-265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response