ASME SB-265 Grade 29 Titanium Plate | Ti-6Al-4V ELI with Ru (UNS R56404)
What is ASME SB-265 Grade 29 titanium plate?
ASME SB-265 Grade 29 titanium plate is made to ASME SB-265, the ASME Boiler and Pressure Vessel Code Section II, Part B specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R56404. Grade 29 is Grade 23 (Ti-6Al-4V ELI) with 0.08–0.14% ruthenium. It is used where high strength, toughness and resistance to sour brines are all required, for example in offshore riser and drilling equipment.
This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.
Its typical density of about 4.43 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Because SB-265 adopts ASTM B265, it uses the same grade numbers and UNS numbers. A grade being listed in SB-265 does not by itself mean it has allowable stresses for every Code; that depends on Section II, Part D and the Code of construction.
SHH STEEL handles Grade 29 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASME SB-265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 29, ASTM B265 Grade 23.
Material specification for ASME SB-265 Grade 29
ASME SB-265 is the specification for titanium and titanium alloy strip, sheet and plate in ASME Boiler and Pressure Vessel Code Section II, Part B. It adopts ASTM B265 with any ASME changes noted on its cover, so the product definitions and test requirements follow the adopted B265 edition.
| Ordering item | ASME SB-265 basis |
|---|---|
| Specification | ASME SB-265 in the BPVC Section II, Part B edition named by the Code of construction |
| Grade / UNS | Grade 29, Ti-6Al-4V ELI with Ru, UNS R56404 |
| Product forms | Plate over 0.187 in (4.75 mm) and over 10 in (254 mm) wide; sheet and strip 0.187 in (4.75 mm) and under |
| Condition | Annealed |
| Code use | Allowable stresses, if any, come from Section II, Part D for the Code and edition being used |
| Certificate | Manufacturer’s report certifying SB-265; add ASTM B265 if dual certification is needed |
| Marking | Specification number, grade, heat number, manufacturer’s identification and nominal thickness |
The ASME edition referenced by a design may lag the newest ASTM B265 edition. If the plate will be stamped or used for Code construction, state SB-265, the Section II edition and any Code Case on the order, and confirm that the grade is accepted for the intended Code before design is fixed.
Chemical composition of ASME SB-265 Grade 29 (UNS R56404)
Single values are maximums; ranges are shown where an element is added. Titanium is the remainder. The product analysis column applies to check analysis on finished product.
| Element | Heat analysis, % | Permissible variation in product analysis, % |
|---|---|---|
| Nitrogen (N) | 0.03 | +0.02 |
| Carbon (C) | 0.08 | +0.02 |
| Hydrogen (H) | 0.0125 | +0.002 |
| Iron (Fe) | 0.25 | +0.15 |
| Oxygen (O) | 0.13 | +0.03 |
| Aluminium (Al) | 5.5–6.5 | ±0.40 |
| Vanadium (V) | 3.5–4.5 | ±0.15 |
| Ruthenium (Ru) | 0.08–0.14 | ±0.01 |
| Other elements, each | 0.1 | +0.02 |
| Other elements, total | 0.4 | — |
| Titanium (Ti) | Balance | — |
The heat is analysed for the listed elements and hydrogen is reported on the final product. Residual elements need not be reported unless they exceed the each or total limits. Because SB-265 adopts B265, the limits match the ASTM grade in the adopted edition.
Mechanical properties of ASME SB-265 Grade 29
The values below are the requirements for Grade 29 plate in the annealed condition.
| Property | Requirement |
|---|---|
| Tensile strength, min | 120 ksi (828 MPa) |
| Yield strength, 0.2% offset | 110 ksi (759 MPa) min |
| Elongation in 2 in or 50 mm, min | 10% |
| Bend test, under 0.070 in (1.8 mm) | Mandrel radius 4.5T, bent 105° without outside fracture |
| Bend test, 0.070–0.187 in (1.8–4.75 mm) | Mandrel radius 5T |
| Bend test, over 0.187 in (4.75 mm) | Not applicable to material over 4.75 mm |
Tensile tests are made at room temperature. Only a minimum yield strength is set for this grade. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.
Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.
Delivery condition, finish and marking
ASME SB-265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.
- Condition: Annealed
- Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
- Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
- Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise
Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.
Welding and fabrication of Grade 29 titanium plate
Grade 29 can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.
- Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
- Use qualified procedures and matching or engineer-approved filler metal
- Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
- Clean joints thoroughly and avoid iron contamination
Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.
Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.
State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Grade 29 titanium plate
Typical uses of Grade 29 plate include:
- Offshore drilling and production riser components
- Sour-service oil and gas equipment
- Geothermal parts
- Subsea hardware
Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.
When selecting Grade 29, compare it with Grade 5, Grade 23, Grade 24. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Grade 29 with other ASME SB-265 grades
The grades below are the closest neighbours of Grade 29 in ASME SB-265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Grade 5 (R56400) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Workhorse alpha-beta alloy |
| Grade 23 (R56407) | 120 ksi (828 MPa) | 110 ksi (759 MPa) min | 10% | Ti-6Al-4V ELI, damage-tolerant |
| Grade 24 (R56405) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Ti-6Al-4V with Pd |
| Grade 25 (R56403) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 10% | Ti-6Al-4V with Ni and Pd |
| Grade 29 (R56404) | 120 ksi (828 MPa) | 110 ksi (759 MPa) min | 10% | Ti-6Al-4V ELI with Ru |
| Grade 35 (R56340) | 130 ksi (895 MPa) | 120 ksi (828 MPa) min | 5% | Ti-4.5Al-2Mo-1.6V-0.5Fe-0.3Si alpha-beta alloy |
| Grade 38 (R54250) | 130 ksi (895 MPa) | 115 ksi (794 MPa) min | 10% | Ti-4Al-2.5V-1.5Fe alpha-beta alloy |
A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.
ASME SB-265 Grade 29 equivalent grades
The designations below are commonly compared with ASME SB-265 Grade 29. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to ASME SB-265 Grade 29 |
|---|---|---|
| ASTM B265 | Grade 29 | ASTM specification adopted by SB-265; same grade requirements |
| ASTM B265 | Grade 23 | Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified |
| UNS | R56404 | Same unified number as ASTM Grade 29 |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Grade 29 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to ASME SB-265 and the Section II edition you name, and can arrange dual SB-265 / B265 certification
- Certificates are checked against the Grade 29 chemistry and tensile limits before shipment
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for ASME SB-265 Grade 29 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | ASME SB-265 Grade 29 (UNS R56404), Section II edition; add ASTM B265 if dual certification |
| Product form | Plate, sheet or strip; for sheet, cold or hot rolled |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
What is the difference between ASME SB-265 Grade 29 and ASTM B265 Grade 29?
- SB-265 adopts B265, so chemistry and tensile requirements normally match the adopted edition. SB-265 is the document cited by ASME Code construction; B265 is the ASTM industrial specification. Dual certification covers both.
-
What is the tensile strength of ASME SB-265 Grade 29 titanium plate?
- The requirement is 120 ksi (828 MPa) minimum. The 0.2% proof or yield strength is 110 ksi (759 MPa) minimum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
-
What is Grade 29 mainly used for?
- Typical uses include offshore drilling and production riser components, sour-service oil and gas equipment and geothermal parts. The design engineer should confirm the grade for the actual service.
-
Does SB-265 use the same plate, sheet and strip definitions as B265?
- Yes. Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide; thinner product is sheet if 24 in (610 mm) or more wide, otherwise strip.
-
What should I send for a quotation?
- Send ASME SB-265 Grade 29, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for ASME SB-265 Grade 29 titanium plate
ASME SB-265 Grade 29 is Ti-6Al-4V ELI with Ru titanium alloy, UNS R56404, specified for 120 ksi (828 MPa) minimum tensile strength, 110 ksi (759 MPa) minimum yield or proof strength and 10% minimum elongation in the annealed condition. Typical uses include offshore drilling and production riser components and sour-service oil and gas equipment.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASME SB-265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com