ASME SB-265 Grade 17 Titanium Plate | Grade 1 Lean Pd (UNS R52252)
What is ASME SB-265 Grade 17 titanium plate?
ASME SB-265 Grade 17 titanium plate is made to ASME SB-265, the ASME Boiler and Pressure Vessel Code Section II, Part B specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R52252. Grade 17 is Grade 1 with 0.04–0.08% palladium. It is the formable, lower-strength companion of Grade 16.
This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.
Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Because SB-265 adopts ASTM B265, it uses the same grade numbers and UNS numbers. A grade being listed in SB-265 does not by itself mean it has allowable stresses for every Code; that depends on Section II, Part D and the Code of construction.
SHH STEEL handles Grade 17 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASME SB-265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 17, JIS H4600 Class 17 TP240Pd, GB/T 3621 TA8-1.
Material specification for ASME SB-265 Grade 17
ASME SB-265 is the specification for titanium and titanium alloy strip, sheet and plate in ASME Boiler and Pressure Vessel Code Section II, Part B. It adopts ASTM B265 with any ASME changes noted on its cover, so the product definitions and test requirements follow the adopted B265 edition.
| Ordering item | ASME SB-265 basis |
|---|---|
| Specification | ASME SB-265 in the BPVC Section II, Part B edition named by the Code of construction |
| Grade / UNS | Grade 17, Grade 1 Lean Pd, UNS R52252 |
| Product forms | Plate over 0.187 in (4.75 mm) and over 10 in (254 mm) wide; sheet and strip 0.187 in (4.75 mm) and under |
| Condition | Annealed |
| Code use | Allowable stresses, if any, come from Section II, Part D for the Code and edition being used |
| Certificate | Manufacturer’s report certifying SB-265; add ASTM B265 if dual certification is needed |
| Marking | Specification number, grade, heat number, manufacturer’s identification and nominal thickness |
The ASME edition referenced by a design may lag the newest ASTM B265 edition. If the plate will be stamped or used for Code construction, state SB-265, the Section II edition and any Code Case on the order, and confirm that the grade is accepted for the intended Code before design is fixed.
Chemical composition of ASME SB-265 Grade 17 (UNS R52252)
Single values are maximums; ranges are shown where an element is added. Titanium is the remainder. The product analysis column applies to check analysis on finished product.
| Element | Heat analysis, % | Permissible variation in product analysis, % |
|---|---|---|
| Nitrogen (N) | 0.03 | +0.02 |
| Carbon (C) | 0.08 | +0.02 |
| Hydrogen (H) | 0.015 | +0.002 |
| Iron (Fe) | 0.20 | +0.15 |
| Oxygen (O) | 0.18 | +0.03 |
| Palladium (Pd) | 0.04–0.08 | ±0.005 |
| Other elements, each | 0.1 | +0.02 |
| Other elements, total | 0.4 | — |
| Titanium (Ti) | Balance | — |
The heat is analysed for the listed elements and hydrogen is reported on the final product. Residual elements need not be reported unless they exceed the each or total limits. Because SB-265 adopts B265, the limits match the ASTM grade in the adopted edition.
Mechanical properties of ASME SB-265 Grade 17
The values below are the requirements for Grade 17 plate in the annealed condition.
| Property | Requirement |
|---|---|
| Tensile strength, min | 35 ksi (240 MPa) |
| Yield strength, 0.2% offset | 20–45 ksi (138–310 MPa) |
| Elongation in 2 in or 50 mm, min | 24% |
| Bend test, under 0.070 in (1.8 mm) | Mandrel radius 1.5T, bent 105° without outside fracture |
| Bend test, 0.070–0.187 in (1.8–4.75 mm) | Mandrel radius 2T |
| Bend test, over 0.187 in (4.75 mm) | Not applicable to material over 4.75 mm |
Tensile tests are made at room temperature. The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail the grade even if it is strong. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.
Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.
Delivery condition, finish and marking
ASME SB-265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.
- Condition: Annealed
- Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
- Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
- Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise
The grade is supplied annealed and is not strengthened by heat treatment. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.
Welding and fabrication of Grade 17 titanium plate
Grade 17 is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.
- Use trailing shields and back purging until the metal cools below about 400 °C
- Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
- Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
- Check weld colour and reject heavily discoloured welds
Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.
For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.
State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Grade 17 titanium plate
Typical uses of Grade 17 plate include:
- Linings and clad layers in crevice-prone chloride service
- Formed and deep-drawn chemical process parts
- Plate heat exchanger plates
- Electrochemical equipment
Strength is at Grade 1 level. The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.
When selecting Grade 17, compare it with Grade 7, Grade 7H, Grade 11. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Grade 17 with other ASME SB-265 grades
The grades below are the closest neighbours of Grade 17 in ASME SB-265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Grade 7 (R52400) | 50 ksi (345 MPa) | 40–65 ksi (275–450 MPa) | 20% | Pd-bearing Grade 2 for crevice and reducing-acid service |
| Grade 7H (R52400) | 58 ksi (400 MPa) | 40–65 ksi (275–450 MPa) | 20% | Grade 7 with higher guaranteed tensile |
| Grade 11 (R52250) | 35 ksi (240 MPa) | 20–45 ksi (138–310 MPa) | 24% | Pd-bearing Grade 1 |
| Grade 16 (R52402) | 50 ksi (345 MPa) | 40–65 ksi (275–450 MPa) | 20% | Lean-Pd Grade 2 |
| Grade 16H (R52402) | 58 ksi (400 MPa) | 40–65 ksi (275–450 MPa) | 20% | Grade 16 with higher guaranteed tensile |
| Grade 17 (R52252) | 35 ksi (240 MPa) | 20–45 ksi (138–310 MPa) | 24% | Lean-Pd Grade 1 |
| Grade 26 (R52404) | 50 ksi (345 MPa) | 40–65 ksi (275–450 MPa) | 20% | Ru-bearing Grade 2 |
| Grade 26H (R52404) | 58 ksi (400 MPa) | 40–65 ksi (275–450 MPa) | 20% | Grade 26 with higher guaranteed tensile |
| Grade 27 (R52254) | 35 ksi (240 MPa) | 20–45 ksi (138–310 MPa) | 24% | Ru-bearing Grade 1 |
The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.
ASME SB-265 Grade 17 equivalent grades
The designations below are commonly compared with ASME SB-265 Grade 17. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to ASME SB-265 Grade 17 |
|---|---|---|
| ASTM B265 | Grade 17 | ASTM specification adopted by SB-265; same grade requirements |
| JIS H4600 | Class 17 (TP240Pd) | Close equivalent; JIS strength range and tests differ |
| GB/T 3621 | TA8-1 | Close equivalent; confirm grade name and limits in the ordered edition |
| UNS | R52252 | Same unified number as ASTM Grade 17 |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Grade 17 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to ASME SB-265 and the Section II edition you name, and can arrange dual SB-265 / B265 certification
- Certificates are checked against the Grade 17 chemistry and tensile limits before shipment
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for ASME SB-265 Grade 17 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | ASME SB-265 Grade 17 (UNS R52252), Section II edition; add ASTM B265 if dual certification |
| Product form | Plate, sheet or strip; for sheet, cold or hot rolled |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
What is the difference between ASME SB-265 Grade 17 and ASTM B265 Grade 17?
- SB-265 adopts B265, so chemistry and tensile requirements normally match the adopted edition. SB-265 is the document cited by ASME Code construction; B265 is the ASTM industrial specification. Dual certification covers both.
-
What is the tensile strength of ASME SB-265 Grade 17 titanium plate?
- The requirement is 35 ksi (240 MPa) minimum. The 0.2% proof or yield strength is 20–45 ksi (138–310 MPa). Minimum elongation is 24%. Values apply to the condition and thickness range stated in the standard.
-
What is Grade 17 mainly used for?
- Typical uses include linings and clad layers in crevice-prone chloride service, formed and deep-drawn chemical process parts and plate heat exchanger plates. Strength is at Grade 1 level.
-
Does SB-265 use the same plate, sheet and strip definitions as B265?
- Yes. Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide; thinner product is sheet if 24 in (610 mm) or more wide, otherwise strip.
-
What should I send for a quotation?
- Send ASME SB-265 Grade 17, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for ASME SB-265 Grade 17 titanium plate
ASME SB-265 Grade 17 is Grade 1 lean-Pd titanium, UNS R52252, specified for 35 ksi (240 MPa) minimum tensile strength, 20–45 ksi (138–310 MPa) yield or proof strength and 24% minimum elongation in the annealed condition. Typical uses include linings and clad layers in crevice-prone chloride service and formed and deep-drawn chemical process parts.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASME SB-265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com