ASME SB-265 Grade 2H Titanium Plate | Grade 2 High Strength (UNS R50400)

ASME SB-265 Grade 2H titanium plate is Grade 2 high strength titanium (UNS R50400) supplied annealed. It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include pressure vessel shells and heads in chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASME SB-265 Grade 2H titanium plate, Grade 2H titanium plate, UNS R50400 plate, Grade 2 high strength titanium plate, ASME SB-265 titanium sheet
Equivalent Grades:
UNS R50400, ASTM B265 Gr.2H
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASME SB-265 Grade 2H titanium plate?

ASME SB-265 Grade 2H titanium plate is made to ASME SB-265, the ASME Boiler and Pressure Vessel Code Section II, Part B specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R50400. Grade 2H has the same chemistry and yield range as Grade 2 but guarantees 58 ksi (400 MPa) minimum tensile strength. The H grades were introduced mainly for pressure vessel design, where the higher guaranteed tensile can support higher design values under the applicable code.

Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Because SB-265 adopts ASTM B265, it uses the same grade numbers and UNS numbers. A grade being listed in SB-265 does not by itself mean it has allowable stresses for every Code; that depends on Section II, Part D and the Code of construction.

SHH STEEL handles Grade 2H plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASME SB-265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 2H, ASTM B265 Grade 2, ASME SB-265 Grade 2.

Material specification for ASME SB-265 Grade 2H

ASME SB-265 is the specification for titanium and titanium alloy strip, sheet and plate in ASME Boiler and Pressure Vessel Code Section II, Part B. It adopts ASTM B265 with any ASME changes noted on its cover, so the product definitions and test requirements follow the adopted B265 edition.

Ordering item ASME SB-265 basis
Specification ASME SB-265 in the BPVC Section II, Part B edition named by the Code of construction
Grade / UNS Grade 2H, Grade 2 High Strength, UNS R50400
Product forms Plate over 0.187 in (4.75 mm) and over 10 in (254 mm) wide; sheet and strip 0.187 in (4.75 mm) and under
Condition Annealed
Code use Allowable stresses, if any, come from Section II, Part D for the Code and edition being used
Certificate Manufacturer’s report certifying SB-265; add ASTM B265 if dual certification is needed
Marking Specification number, grade, heat number, manufacturer’s identification and nominal thickness

The ASME edition referenced by a design may lag the newest ASTM B265 edition. If the plate will be stamped or used for Code construction, state SB-265, the Section II edition and any Code Case on the order, and confirm that the grade is accepted for the intended Code before design is fixed.

Chemical composition of ASME SB-265 Grade 2H (UNS R50400)

Single values are maximums; ranges are shown where an element is added. Titanium is the remainder. The product analysis column applies to check analysis on finished product.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.08 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.25 +0.03
Other elements, each 0.1 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

The heat is analysed for the listed elements and hydrogen is reported on the final product. Residual elements need not be reported unless they exceed the each or total limits. Because SB-265 adopts B265, the limits match the ASTM grade in the adopted edition.

Mechanical properties of ASME SB-265 Grade 2H

The values below are the requirements for Grade 2H plate in the annealed condition.

Property Requirement
Tensile strength, min 58 ksi (400 MPa)
Yield strength, 0.2% offset 40–65 ksi (275–450 MPa)
Elongation in 2 in or 50 mm, min 20%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 2T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 2.5T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail the grade even if it is strong. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASME SB-265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Annealed
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 2H titanium plate

Grade 2H is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.

  • Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
  • Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
  • Use matching CP filler metal unless the design engineer specifies otherwise
  • Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
  • Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up

Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.

For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 2H titanium plate

Typical uses of Grade 2H plate include:

  • Pressure vessel shells and heads in chloride service
  • Heat exchanger tube sheets and channel covers
  • Desalination and seawater cooling equipment
  • Chemical process columns where Grade 2 corrosion behaviour is needed with higher guaranteed tensile

Plate certified as Grade 2H may also be certified as Grade 2, but Grade 2 plate cannot be assumed to meet 2H. Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.

When selecting Grade 2H, compare it with Grade 1, Grade 2, Grade 3. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 2H with other ASME SB-265 grades

The grades below are the closest neighbours of Grade 2H in ASME SB-265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 1 (R50250) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Best formability, lowest strength
Grade 2 (R50400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% General process equipment
Grade 2H (R50400) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 2 with higher guaranteed tensile
Grade 3 (R50550) 65 ksi (450 MPa) 55–80 ksi (380–550 MPa) 18% Higher strength, less formable
Grade 4 (R50700) 80 ksi (550 MPa) 70–95 ksi (483–655 MPa) 15% Highest-strength CP grade

A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.

ASME SB-265 Grade 2H equivalent grades

The designations below are commonly compared with ASME SB-265 Grade 2H. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASME SB-265 Grade 2H
ASTM B265 Grade 2H ASTM specification adopted by SB-265; same grade requirements
ASTM B265 Grade 2 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
ASME SB-265 Grade 2 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
JIS H4600 Class 2 (TP340) Nearest by role only; composition and properties differ
GB/T 3621 TA2G Nearest by role only; composition and properties differ
UNS R50400 Same unified number; the H suffix is a tensile requirement, not a separate UNS

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 2H titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to ASME SB-265 and the Section II edition you name, and can arrange dual SB-265 / B265 certification
  • Certificates are checked against the Grade 2H chemistry and tensile limits before shipment
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASME SB-265 Grade 2H plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASME SB-265 Grade 2H (UNS R50400), Section II edition; add ASTM B265 if dual certification
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What is the difference between ASME SB-265 Grade 2H and ASTM B265 Grade 2H?
SB-265 adopts B265, so chemistry and tensile requirements normally match the adopted edition. SB-265 is the document cited by ASME Code construction; B265 is the ASTM industrial specification. Dual certification covers both.
What is the tensile strength of ASME SB-265 Grade 2H titanium plate?
The requirement is 58 ksi (400 MPa) minimum. The 0.2% proof or yield strength is 40–65 ksi (275–450 MPa). Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is Grade 2H mainly used for?
Typical uses include pressure vessel shells and heads in chloride service, heat exchanger tube sheets and channel covers and desalination and seawater cooling equipment. Plate certified as Grade 2H may also be certified as Grade 2, but Grade 2 plate cannot be assumed to meet 2H.
Does SB-265 use the same plate, sheet and strip definitions as B265?
Yes. Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide; thinner product is sheet if 24 in (610 mm) or more wide, otherwise strip.
What should I send for a quotation?
Send ASME SB-265 Grade 2H, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for ASME SB-265 Grade 2H titanium plate

ASME SB-265 Grade 2H is Grade 2 high strength titanium, UNS R50400, specified for 58 ksi (400 MPa) minimum tensile strength, 40–65 ksi (275–450 MPa) yield or proof strength and 20% minimum elongation in the annealed condition. Typical uses include pressure vessel shells and heads in chloride service and heat exchanger tube sheets and channel covers.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASME SB-265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response