JIS H4600

Product Showcase

JIS H4600 Titanium Alloys

SHH STEEL offers JIS H4600-compliant TR270C/TP340C titanium and titanium alloy sheets and plates. JIS H4600 specifies dimensions, mechanical properties, and testing for industrial, medical, and aerospace uses. High purity, corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!

JIS H4600 Class 80 TAP4220 Titanium Plate | Ti-4Al-22V

JIS H4600 Class 80 TAP4220 titanium plate is Ti-4Al-22V titanium alloy supplied solution treated. It is specified for 640–900 MPa tensile strength, 850 MPa maximum yield and 10% minimum elongation. Typical uses include golf club heads. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 22 TP410RN Titanium Plate | Ru-Ni Titanium

JIS H4600 Class 22 TP410RN titanium plate is Ru-Ni titanium supplied annealed. It is specified for 410–530 MPa tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include chemical plant heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 23 TP483RN Titanium Plate | Ru-Ni Titanium

JIS H4600 Class 23 TP483RN titanium plate is Ru-Ni titanium supplied annealed. It is specified for 483–630 MPa tensile strength, 380 MPa yield and 18% minimum elongation. Typical uses include chemical plant heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 50 TAP1500 Titanium Plate | Ti-1.5Al

JIS H4600 Class 50 TAP1500 titanium plate is Ti-1.5Al titanium alloy supplied annealed. It is specified for 345 MPa minimum tensile strength, 215 MPa yield and 20% minimum elongation. Typical uses include motorcycle mufflers and exhaust systems. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 60 TAP6400 Titanium Plate | Ti-6Al-4V

JIS H4600 Class 60 TAP6400 titanium plate is Ti-6Al-4V titanium alloy supplied annealed. It is specified for 895 MPa minimum tensile strength, 825 MPa yield and 10% minimum elongation. Typical uses include aircraft structural parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 60E TAP6400E Titanium Plate | Ti-6Al-4V ELI

JIS H4600 Class 60E TAP6400E titanium plate is Ti-6Al-4V ELI titanium alloy supplied annealed. It is specified for 825 MPa minimum tensile strength, 755 MPa yield and 10% minimum elongation. Typical uses include medical and dental device material. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 61 TAP3250 Titanium Plate | Ti-3Al-2.5V

JIS H4600 Class 61 TAP3250 titanium plate is Ti-3Al-2.5V titanium alloy supplied annealed. It is specified for 620 MPa minimum tensile strength, 485 MPa yield and 15% minimum elongation. Typical uses include bicycle and sporting components. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 61F TAP3250F Titanium Plate | Ti-3Al-2.5V

JIS H4600 Class 61F TAP3250F titanium plate is Ti-3Al-2.5V titanium alloy supplied annealed. It is specified for 650 MPa minimum tensile strength, 600 MPa yield and 10% minimum elongation. Typical uses include machined parts made in volume. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 17 TP240Pd Titanium Plate | Lean Pd CP Titanium

JIS H4600 Class 17 TP240Pd titanium plate is lean-Pd CP titanium supplied annealed. It is specified for 240–380 MPa tensile strength, 170 MPa yield and 24% minimum elongation. Typical uses include plate heat exchanger plates. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 18 TP345Pd Titanium Plate | Lean Pd CP Titanium

JIS H4600 Class 18 TP345Pd titanium plate is lean-Pd CP titanium supplied annealed. It is specified for 345–515 MPa tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include plate heat exchanger plates. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 19 TP345PCo Titanium Plate | Pd-Co Titanium

JIS H4600 Class 19 TP345PCo titanium plate is Pd-Co titanium supplied annealed. It is specified for 345–515 MPa tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include shell-and-tube heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

JIS H4600 Class 20 TP450PCo Titanium Plate | Pd-Co Titanium

JIS H4600 Class 20 TP450PCo titanium plate is Pd-Co titanium supplied annealed. It is specified for 450–590 MPa tensile strength, 380 MPa yield and 18% minimum elongation. Typical uses include shell-and-tube heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
View More

Titanium Alloy Plates and Sheets

SHH STEEL, a premier Titanium Alloy Plates and Sheets exporter, produces and exports titanium alloy plates and sheets for aerospace, marine, and chemical industries. Our products, like Grade 2 and Grade 5 (ASTM B265), offer high strength and corrosion resistance. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Grade 5 titanium plates and custom solutions for high-performance projects.

Titanium Alloy Plates and Sheets

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X