ASME SB-265 Grade 20 Titanium Plate | Beta C with Pd (UNS R58645)

ASME SB-265 Grade 20 titanium plate is Beta C with Pd titanium alloy (UNS R58645) supplied solution treated. It is specified for 793 MPa minimum tensile strength, 759 MPa yield and 15% minimum elongation. Typical uses include sour-gas and downhole oil and gas components. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASME SB-265 Grade 20 titanium plate, Grade 20 titanium plate, UNS R58645 plate, Beta C with Pd titanium alloy plate, ASME SB-265 titanium sheet
Equivalent Grades:
UNS R58645, ASTM B265 Gr.20, ASTM B265 Gr.19
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASME SB-265 Grade 20 titanium plate?

ASME SB-265 Grade 20 titanium plate is made to ASME SB-265, the ASME Boiler and Pressure Vessel Code Section II, Part B specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R58645. Grade 20 is Grade 19 (Beta C) with 0.04–0.08% palladium for improved corrosion resistance in reducing and sour environments.

This is a beta or metastable beta titanium alloy. Large additions of beta-stabilising elements such as vanadium, molybdenum, chromium or niobium keep a body-centred cubic structure after solution treatment. That structure is cold formable, and many beta alloys can then be aged to very high strength.

Its typical density of about 4.82 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Because SB-265 adopts ASTM B265, it uses the same grade numbers and UNS numbers. A grade being listed in SB-265 does not by itself mean it has allowable stresses for every Code; that depends on Section II, Part D and the Code of construction.

SHH STEEL handles Grade 20 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASME SB-265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 20, ASTM B265 Grade 19.

Material specification for ASME SB-265 Grade 20

ASME SB-265 is the specification for titanium and titanium alloy strip, sheet and plate in ASME Boiler and Pressure Vessel Code Section II, Part B. It adopts ASTM B265 with any ASME changes noted on its cover, so the product definitions and test requirements follow the adopted B265 edition.

Ordering item ASME SB-265 basis
Specification ASME SB-265 in the BPVC Section II, Part B edition named by the Code of construction
Grade / UNS Grade 20, Beta C with Pd, UNS R58645
Product forms Plate over 0.187 in (4.75 mm) and over 10 in (254 mm) wide; sheet and strip 0.187 in (4.75 mm) and under
Condition Solution treated, as required for this beta grade; aged properties by agreement
Code use Allowable stresses, if any, come from Section II, Part D for the Code and edition being used
Certificate Manufacturer’s report certifying SB-265; add ASTM B265 if dual certification is needed
Marking Specification number, grade, heat number, manufacturer’s identification and nominal thickness

The ASME edition referenced by a design may lag the newest ASTM B265 edition. If the plate will be stamped or used for Code construction, state SB-265, the Section II edition and any Code Case on the order, and confirm that the grade is accepted for the intended Code before design is fixed.

Chemical composition of ASME SB-265 Grade 20 (UNS R58645)

Single values are maximums; ranges are shown where an element is added. Titanium is the remainder. The product analysis column applies to check analysis on finished product.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.05 +0.02
Hydrogen (H) 0.02 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.12 +0.03
Aluminium (Al) 3.0–4.0 ±0.40
Vanadium (V) 7.5–8.5 ±0.40
Zirconium (Zr) 3.5–4.5 ±0.15
Molybdenum (Mo) 3.5–4.5 ±0.20
Chromium (Cr) 5.5–6.5 ±0.30
Palladium (Pd) 0.04–0.08 ±0.005
Other elements, each 0.15 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

The heat is analysed for the listed elements and hydrogen is reported on the final product. Residual elements need not be reported unless they exceed the each or total limits. Because SB-265 adopts B265, the limits match the ASTM grade in the adopted edition.

Mechanical properties of ASME SB-265 Grade 20

The values below are the requirements for Grade 20 plate in the solution treated condition.

Property Requirement
Tensile strength, min 115 ksi (793 MPa)
Yield strength, 0.2% offset 110 ksi (759 MPa) min
Elongation in 2 in or 50 mm, min 15%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 3T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 3T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. Only a minimum yield strength is set for this grade. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASME SB-265 covers material in the annealed condition, or for this beta alloy normally solution treated. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Solution treated, as required for this beta grade; aged properties by agreement
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

Material is normally purchased solution treated. Aged properties are not fixed by the plate specification and must be agreed between purchaser and manufacturer. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 20 titanium plate

Grade 20 can be welded by gas tungsten arc, electron beam or laser with full inert-gas shielding, but weld properties depend strongly on the heat treatment that follows.

  • Shield the weld, heat-affected zone and root until below about 400 °C
  • Agree the post-weld heat treatment with the designer, since ageing response differs between weld and base metal
  • Use qualified procedures and approved filler metal
  • Keep joints clean and free of iron contamination

In the solution-treated condition beta alloys can be cold formed more easily than alpha-beta alloys. Forming is normally done before ageing.

Beta alloys are machined with sharp carbide tools, low speeds and generous coolant, and tool wear is higher in the aged condition, so heavy machining is often done before ageing. Keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 20 titanium plate

Typical uses of Grade 20 plate include:

  • Sour-gas and downhole oil and gas components
  • High-strength corrosion-resistant fastener blanks
  • Geothermal equipment
  • Chemical process parts needing beta-alloy strength

Aged properties must be agreed between purchaser and manufacturer. Beta alloys have good resistance to many media, but they are not suited to hydrofluoric acid, fluoride-bearing media or dry chlorine. They are denser than Ti-6Al-4V, and aged properties, toughness and service temperature limits must be agreed for the part.

When selecting Grade 20, compare it with Grade 19, Grade 21, Grade 36. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 20 with other ASME SB-265 grades

The grades below are the closest neighbours of Grade 20 in ASME SB-265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 19 (R58640) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Beta C, heat-treatable beta alloy
Grade 20 (R58645) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Beta C with Pd
Grade 21 (R58210) 115 ksi (793 MPa) 110 ksi (759 MPa) min 15% Ti-15Mo-3Al-2.7Nb-0.25Si beta alloy
Grade 36 (R58450) 65 ksi (450 MPa) 60–95 ksi (410–655 MPa) 10% Ti-45Nb beta alloy

Beta alloys are usually chosen for formability before ageing and for high aged strength, not for corrosion alone. Compare the agreed heat-treated properties before changing grade.

ASME SB-265 Grade 20 equivalent grades

The designations below are commonly compared with ASME SB-265 Grade 20. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASME SB-265 Grade 20
ASTM B265 Grade 20 ASTM specification adopted by SB-265; same grade requirements
ASTM B265 Grade 19 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
UNS R58645 Same unified number as ASTM Grade 20

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 20 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to ASME SB-265 and the Section II edition you name, and can arrange dual SB-265 / B265 certification
  • Certificates are checked against the Grade 20 chemistry and tensile limits before shipment
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASME SB-265 Grade 20 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASME SB-265 Grade 20 (UNS R58645), Section II edition; add ASTM B265 if dual certification
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What is the difference between ASME SB-265 Grade 20 and ASTM B265 Grade 20?
SB-265 adopts B265, so chemistry and tensile requirements normally match the adopted edition. SB-265 is the document cited by ASME Code construction; B265 is the ASTM industrial specification. Dual certification covers both.
What is the tensile strength of ASME SB-265 Grade 20 titanium plate?
The requirement is 115 ksi (793 MPa) minimum. The 0.2% proof or yield strength is 110 ksi (759 MPa) minimum. Minimum elongation is 15%. Values apply to the condition and thickness range stated in the standard.
What is Grade 20 mainly used for?
Typical uses include sour-gas and downhole oil and gas components, high-strength corrosion-resistant fastener blanks and geothermal equipment. Aged properties must be agreed between purchaser and manufacturer.
Does SB-265 use the same plate, sheet and strip definitions as B265?
Yes. Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide; thinner product is sheet if 24 in (610 mm) or more wide, otherwise strip.
What should I send for a quotation?
Send ASME SB-265 Grade 20, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for ASME SB-265 Grade 20 titanium plate

ASME SB-265 Grade 20 is Beta C with Pd titanium alloy, UNS R58645, specified for 115 ksi (793 MPa) minimum tensile strength, 110 ksi (759 MPa) minimum yield or proof strength and 15% minimum elongation in the solution treated condition. Typical uses include sour-gas and downhole oil and gas components and high-strength corrosion-resistant fastener blanks.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASME SB-265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X