Product Showcase
ASME SB-265 Titanium Alloys
SHH STEEL offers ASME SB-265-compliant Grade 2/5 titanium alloy sheets and plates. ASME SB-265 specifies pressure vessel-grade materials for chemical processing and desalination with high strength-to-weight ratio. Weldable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SB-265 Grade 13 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53413)
ASME SB-265 Grade 13 titanium plate is Ti-0.5Ni-0.05Ru titanium (UNS R53413) supplied annealed. It is specified for 275 MPa minimum tensile strength, 170 MPa yield and 24% minimum elongation. Typical uses include heat exchangers and process equipment in hot chloride media. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 14 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53414)
ASME SB-265 Grade 14 titanium plate is Ti-0.5Ni-0.05Ru titanium (UNS R53414) supplied annealed. It is specified for 410 MPa minimum tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include heat exchangers and process equipment in hot chloride media. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 15 Titanium Plate | Ti-0.5Ni-0.05Ru (UNS R53415)
ASME SB-265 Grade 15 titanium plate is Ti-0.5Ni-0.05Ru titanium (UNS R53415) supplied annealed. It is specified for 483 MPa minimum tensile strength, 380 MPa yield and 18% minimum elongation. Typical uses include heat exchangers and process equipment in hot chloride media. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 16 Titanium Plate | Lean Pd CP Titanium (UNS R52402)
ASME SB-265 Grade 16 titanium plate is lean-Pd CP titanium (UNS R52402) supplied annealed. It is specified for 345 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 16H Titanium Plate | Grade 16 High Strength (UNS R52402)
ASME SB-265 Grade 16H titanium plate is Grade 16 high strength titanium (UNS R52402) supplied annealed. It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 7H Titanium Plate | Grade 7 High Strength (UNS R52400)
ASME SB-265 Grade 7H titanium plate is Grade 7 high strength titanium (UNS R52400) supplied annealed. It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 9 Titanium Plate | Ti-3Al-2.5V (UNS R56320)
ASME SB-265 Grade 9 titanium plate is Ti-3Al-2.5V titanium alloy (UNS R56320) supplied annealed. It is specified for 620 MPa minimum tensile strength, 483 MPa yield and 15% minimum elongation. Typical uses include lightweight sheet structures and ducting. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 11 Titanium Plate | Grade 1 with Pd (UNS R52250)
ASME SB-265 Grade 11 titanium plate is Grade 1 with Pd titanium (UNS R52250) supplied annealed. It is specified for 240 MPa minimum tensile strength, 138–310 MPa yield and 24% minimum elongation. Typical uses include clad and lined equipment in hot chloride or mildly reducing acids. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 12 Titanium Plate | Ti-0.3Mo-0.8Ni (UNS R53400)
ASME SB-265 Grade 12 titanium plate is Ti-0.3Mo-0.8Ni titanium (UNS R53400) supplied annealed. It is specified for 483 MPa minimum tensile strength, 345 MPa yield and 18% minimum elongation. Typical uses include heat exchangers and evaporators in hot brine and salt production. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 3 Titanium Plate | CP Titanium (UNS R50550)
ASME SB-265 Grade 3 titanium plate is CP titanium (UNS R50550) supplied annealed. It is specified for 450 MPa minimum tensile strength, 380–550 MPa yield and 18% minimum elongation. Typical uses include pressure vessels and heat exchangers needing higher design strength than Grade 2. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 4 Titanium Plate | CP Titanium (UNS R50700)
ASME SB-265 Grade 4 titanium plate is CP titanium (UNS R50700) supplied annealed. It is specified for 550 MPa minimum tensile strength, 483–655 MPa yield and 15% minimum elongation. Typical uses include airframe and engine secondary parts where CP titanium is specified. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
ASME SB-265 Grade 5 Titanium Plate | Ti-6Al-4V (UNS R56400)
ASME SB-265 Grade 5 titanium plate is Ti-6Al-4V titanium alloy (UNS R56400) supplied annealed. It is specified for 895 MPa minimum tensile strength, 828 MPa yield and 10% minimum elongation. Typical uses include aerospace airframe and engine structural parts. SHH STEEL reviews size, finish and certificate requirements before quoting.View More
ASME SB-265 Titanium Alloys
Titanium Alloy Plates and Sheets
SHH STEEL, a premier Titanium Alloy Plates and Sheets exporter, produces and exports titanium alloy plates and sheets for aerospace, marine, and chemical industries. Our products, like Grade 2 and Grade 5 (ASTM B265), offer high strength and corrosion resistance. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Grade 5 titanium plates and custom solutions for high-performance projects.