Q690F QT Carbon Steel Plate GB/T 16270 | GB/T 16270 High-Strength Structural Steel - SHH STEEL

Q690F QT Carbon Steel Plate GB/T 16270 Supplier

GB/T 16270 Q690F is quenched-and-tempered carbon structural plate with 690 MPa minimum yield and −60°C impact toughness. SHH STEEL supplies Q690F QT plate mill-direct for arctic frames, mining equipment and cold-region fabrication.
Keywords
Q690F, Q690F steel plate, GB/T 16270 Q690F, Q690F QT plate, Q690F carbon steel plate, Q690F supplier, ASTM A514, S690QL1, GB/T 16270 QT plate
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q690F QT Carbon Steel Plate GB/T 16270?

Q690F, also searched as GB/T 16270 Q690F, Q690F QT plate, Q690F carbon steel plate, Q690F steel plate and Q690F quenched and tempered plate, is the 690 MPa quality-grade-F grade in GB/T 16270. That standard covers high-strength structural steel plate delivered quenched and tempered. Q is the yield symbol, 690 is the thin-plate minimum yield in MPa, and F is the quality letter for Charpy impact at −60°C.

Q690F is the coldest letter in the Q690 family. C is 0°C. D is −20°C. E is −40°C. F is −60°C. It is the 100 ksi QT plate for arctic frames and any drawing that names −60°C at 690 MPa. A mill that only tested at −40°C cannot stamp F. Not every QT mill will accept F on heavy plate.

The closest European name is EN 10025-6 S690QL1. Both are about 690 MPa QT plate tested at −60°C. S690QL is −40°C and lines up with Q690E. S690Q is 0°C and lines up with Q690C. On the US side, A514 Grade Q is also 100 ksi / 690 MPa QT structural plate. The books are not the same, and A514 does not carry an F letter. Dual mark only when both tables are fully met. See EN 10025-6 steel plate.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q690F from first-line QT mills that can run a −60°C route, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include high strength low alloy plates and structural steel plates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 16270 Q690F Confirmed
Other search names Q690F QT plate, Q690F carbon steel plate Covered
Delivery condition Quenched and tempered Confirmed
Yield, thin plate 690 MPa min Confirmed
Quality grade F, impact at −60°C Confirmed
US comparison ASTM A514, 100 ksi Comparison, not a swap
Product analysis GB/T 222 column when ordered Confirmed
Not the same letter Q690E or Q690D Do not substitute
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include S690QL1, S690QL and A514 Gr.Q.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 16270. Product analysis, when ordered, follows GB/T 222. Grade F is the tightest cleanliness letter in the Q690 family, because the impact test is at −60°C. Mills add Nb, V, Ti or Al for grain refinement, and may add Ni, Cr, Mo or B by thickness. Nickel is often used on F heats to hold the cold impact. Boron is common on 690 MPa heats. The certificate shows the elements actually used.

Heat Analysis and Product Analysis — GB/T 16270 Q690F

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.80 0.85
Manganese (Mn), max 1.70 1.78
Phosphorus (P), max 0.015 0.020
Sulfur (S), max 0.005 0.008
Copper (Cu), max 0.50 0.55
Chromium (Cr), max 1.50 1.55
Nickel (Ni), max 2.00 2.05
Molybdenum (Mo), max 0.70 0.75
Boron (B), max 0.005 0.006
Vanadium (V), max 0.12 0.13
Niobium (Nb), max 0.06 0.07
Titanium (Ti), max 0.05 0.06
Aluminium (Als), min when used 0.015 0.010

If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as weathering plate. Do not treat it as S355JR.

Mechanical Properties

Buyers search Q690F mechanical properties, Q690F yield strength, GB/T 16270 Q690F tensile and Q690F impact −60°C.

Tensile and impact — GB/T 16270 Q690F

Thickness Yield min Tensile Elongation min Impact
≤ 50 mm 690 MPa 770–940 MPa 14% −60°C, grade F
> 50–100 mm 670 MPa 770–940 MPa 14% −60°C, grade F
> 100–150 mm 630 MPa as standard table 14% −60°C, grade F

Impact energy is the average of three longitudinal Charpy V-notch specimens. One value may fall below the table, but not below 70% of that value. A −60°C test at 690 MPa is harder to hold than a −40°C test. Write the energy on the purchase order if the owner wants a number above the book minimum. Not every QT mill will accept F on plate over 50 mm. SHH STEEL confirms the thickness before promising the letter.

Yield steps down with thickness. A 690 MPa name on 16 mm plate is not the minimum on an 80 mm flange. 690 MPa is 100 ksi. ASTM A514 uses the same yield number, but it does not carry this −60°C quality letter. Density is 7.85 g/cm³. Hardness after temper is a mill control, not a design value. Z15, Z25 or Z35 through-thickness tensile is an extra.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
Q690C GB/T 16270 QT 690 MPa 0°C No
Q690D GB/T 16270 QT 690 MPa −20°C No
Q690E GB/T 16270 QT 690 MPa −40°C Warmer sister
Q690F GB/T 16270 QT 690 MPa −60°C This page
Q620F GB/T 16270 QT 620 MPa −60°C Lower yield
S690QL EN 10025-6 QT 690 MPa −40°C No
S690QL1 EN 10025-6 QT 690 MPa −60°C Closest comparison
A514 Gr.Q ASTM A514 QT 690 MPa Different Yield match only

Equivalent Material Grades

There is no official one-to-one substitute for Q690F. What buyers compare is a 690 MPa QT plate tested at −60°C.

In the United States the nearest name is ASTM A514/A514M, including A514 Grade Q. A514 is 100 ksi / 690 MPa minimum yield up to 65 mm. That matches the Q690F thin-plate number. It does not match the −60°C quality letter. A572 Gr.65 is only 65 ksi. ASTM A656 Grade 80 is 80 ksi. SHH STEEL will not stamp A514 on a Q690F certificate unless the purchase order names both books and both tables are met.

The usual European pair is S690QL1. S690QL is warmer. S690Q is only 0°C. In Japan, SM570 is a welded structural grade and is well below this yield.

Designation Country / region Standard Notes
Q690F China GB/T 16270 Name on this page
Q690C / Q690D / Q690E China GB/T 16270 Warmer impact letters
Q620F China GB/T 16270 Lower yield sister
A514 Gr.Q USA ASTM A514 100 ksi QT yield comparison
ASTM A656 Grade 80 USA ASTM A656 80 ksi, lower yield
A572 Gr.65 USA ASTM A572 65 ksi, lower yield
S690QL1 Europe EN 10025-6 −60°C QT comparison
S690QL Europe EN 10025-6 −40°C, closer to Q690E

QT Structural Service

Buyers pick Q690F when a welded frame, boom or chassis wants 690 MPa yield, QT delivery and impact at −60°C. Search phrases such as Q690F steel plate, GB/T 16270 Q690F and Q690F QT plate all point here.

It is the wrong plate for a 0°C file that can use Q690C. It is the wrong plate for a −40°C file that can use Q690E. It is the wrong plate for an 800 MPa arctic boom. That work is Q800F, if the mill can make the letter. It is the wrong plate for a US file that actually names ASTM A514 and a named grade letter. That work stays on A514 unless the order also accepts GB/T 16270. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 16270 and quality grade F at 690 MPa.

Weldability

Q690F is weldable QT carbon plate, but the joint must keep −60°C toughness. Many heats use boron. A procedure written for S355JR is not a Q690F procedure. A procedure qualified only at −20°C is not enough either.

Typical consumables are matching 690 MPa low-hydrogen electrodes or wires, qualified on a QT 690 MPa family with a −60°C impact coupon. Nickel-bearing wires are common on F-grade joints. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for S690QL1 is the usual starting point. An A514 procedure is a useful strength reference, not a finished WPS for the F letter.

Preheat follows thickness, hydrogen and the approved WPS. Interpass temperature should stay below the mill temper range, or local yield and the −60°C result can drop. After heavy cold forming, a stress relief may be required. The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q690F is quenched and tempered. Austenitize typically in the 880–930°C range, quench, then temper in the window that holds 690 MPa yield and the −60°C impact. Exact temperatures stay on the mill process sheet. F-grade heats at 690 MPa are not every mill’s standard route.

Do not order Q690F as as-rolled or TMCP unless the contract leaves GB/T 16270. ASTM A514 is not a delivery instruction for this page unless dual mark is written. Stress relief after fabrication, if used, must stay below the original temper temperature.

The certificate lists GB/T 16270 Q690F, heat number, heat analysis, product analysis when ordered, tensile by thickness band, and −60°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to S690QL1 is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q690F QT carbon steel plate:

  • Thickness: commonly 8 mm – 50 mm, heavier plate to 80 mm by mill confirmation
  • Width: 1500 mm – 3200 mm
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges and base plates are available. Browse more sizes on structural steel plates and the products index.

Tolerances

Dimensional limits for Q690F follow GB/T 709 unless the purchase order names another table.

Typical thickness tolerance idea for Q690F QT plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 10 −0.3 +0.8
10 – 20 −0.4 +0.9
20 – 30 −0.4 +1.0
30 – 40 −0.5 +1.1
40 – 50 −0.5 +1.2
50 – 80 −0.6 +1.4

Width on 1500–3200 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness after QT follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q690F unless the order says so.

Supplementary Requirements

Q690F already defines 690 MPa yield, QT delivery and −60°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 16270 Q690F. Do not write only Q690F.

Impact. Grade F is −60°C. Write a higher energy if the owner requires it.

US comparison. Write A514 only if dual mark is required and both tables are met.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Heat-treatment record. QT temperatures when the inspector asks.

Identification. Heat number, Q690F, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Arctic equipment Q690F QT frames tested at −60°C
Mining equipment Q690F chassis plate from SHH STEEL
Cranes in cold regions Q690F webs and flanges
High-altitude winter work Q690F base plates
Comparison vs S690QL1 Q690F next to S690QL1
Comparison vs S690QL Q690F next to S690QL
Comparison vs A514 Q690F next to A514 Gr.Q

Q690F is the plate for a 690 MPa QT file tested at −60°C. It is the wrong plate for a painted warehouse that can use S355JR. It is the wrong plate for an 800 MPa member unless the drawing names that grade.

Supply Capability

SHH STEEL sources Q690F from first-line Chinese QT mills that can run a −60°C route and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an F heat is in yard; standard QT rolling with −60°C test about 40–50 days; 3.2 inspection about 50–60 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q690F that means mill-direct QT price, not a multi-layer stockist mark-up on a cold-impact heat. We buy from mills that can actually test at −60°C, so the letter F is on the certificate and not only in the enquiry.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard F heat about 40–50 days, 3.2 inspection about 50–60 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 16270 Q690F, keep the QT route, and do not ship Q690E or a silent A514 stamp as F. We will not change F to E to save a cold test, and we will not treat Q690F as S355. If the drawing only needs −40°C, we will move the inquiry to Q690E and keep the price on the right grade.

FAQ

What is Q690F steel plate?
Q690F in GB/T 16270 is quenched-and-tempered carbon structural plate with 690 MPa minimum yield on thin plate and Charpy impact at −60°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q690F the same as Q690E?
No. Both yield at 690 MPa. Q690E is tested at −40°C. Q690F is tested at −60°C.
What is the US equivalent of Q690F?
The nearest comparison is ASTM A514, 100 ksi / 690 MPa QT plate. A514 does not carry a −60°C F letter. A572 Grade 65 and A656 Grade 80 are lower. SHH STEEL does not dual-mark A514 unless both books are met.
Is Q690F the same as S690QL1?
They are the usual comparison pair: both are about 690 MPa QT plate tested at −60°C. Dual mark only when both books are fully met. S690QL is warmer.

Conclusion

Q690F QT carbon steel plate to GB/T 16270 is 690 MPa quenched-and-tempered structural plate with impact at −60°C. The nearest US comparison is ASTM A514, which matches the 100 ksi yield but is not a silent substitute. Whether the inquiry says Q690F, GB/T 16270 Q690F, Q690F QT plate or Q690F carbon steel plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q690F chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q690F QT Carbon Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names this grade.

Contact SHH STEEL for mill rolling, −60°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.

Q690F, Q690F steel plate, GB/T 16270 Q690F, Q690F QT plate, Q690F carbon steel plate, Q690F supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X