GB/T 1591 Q690MD thermomechanically rolled high-strength low-alloy structural steel plate, 690 MPa yield, −20 °C impact, SHH STEEL

Q690MD TMCP Steel Plate GB/T 1591 Supplier

GB/T 1591 Q690MD is thermomechanical controlled process plate with 690 MPa minimum yield and −20°C impact. SHH STEEL supplies Q690MD plate mill-direct for bridges, buildings and cold-weather frames that name the M condition. This is not quenched-and-tempered GB/T 16270 Q690D.
Keywords
Q690MD, Q690MD steel plate, GB/T 1591 Q690MD, Q690MD TMCP, Q690MD supplier, EN 10025-6 S690Q, ASTM A514, Q690MC, Q690D
Equivalent Grades:
GB/T 1591 Q690MD / EN 10025-4 S690ML (near) / ASTM A514 Gr Q / EN 10028-6 P690Q (vessel QT near) — Material Specification: GB/T 1591 — Delivery: TMCP; -20℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q690MD TMCP Steel Plate GB/T 1591?

Q690MD, also searched as GB/T 1591 Q690MD, Q690MD steel plate, Q690MD TMCP plate and Q690 MD, is the 690 MPa quality-grade-D grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 690 is the thin-plate minimum yield in MPa, M is the delivery letter, and D is the quality letter for Charpy impact at −20°C.

The M is the point of this page. A quenched-and-tempered certificate cannot be stamped MD. That route is GB/T 16270 Q690D. Grade C on the TMCP route is GB/T 1591 Q690MC. The 620 MPa TMCP sister at the same temperature is GB/T 1591 Q620MD. The 550 MPa TMCP sister is GB/T 1591 Q550MD. The full family sits on GB/T 1591. Do not drop a 690 MPa drawing onto a 620 MPa plate, and do not upgrade it to GB/T 16270 Q800D without a price check.

EN 10025-4 stops at S460M and S460ML. There is no S690M. The usual European comparison is EN 10025-6 S690Q, which is quenched and tempered, not TMCP, and is also tested at −20°C. EN 10025-4 S460M is well below this yield. EN 10025-6 is the QT book. On the US side, ASTM A514 is about 100 ksi / 690 MPa and is quenched and tempered, so it matches the yield number but not the M condition. ASTM A572 Gr.55 is 55 ksi. Dual mark only when both books are fully met. See high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q690MD from first-line structural mills that can actually run the TMCP schedule at 690 MPa and test at −20°C, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q690MD Confirmed
Other search names Q690MD steel plate, Q690 MD, Q690MD TMCP Covered
Delivery condition Thermomechanical controlled process Confirmed
Yield, ≤ 16 mm 690 MPa min Confirmed
Quality grade D, impact at −20°C Confirmed
Not this page GB/T 16270 Q690D QT, different book
Warmer TMCP sister GB/T 1591 Q690MC 0°C
EN comparison EN 10025-6 S690Q is QT Not a swap
US comparison ASTM A514 is QT, about 690 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q620MD, GB/T 16270 Q690E and ASTM A572 Gr.55.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q690. Product analysis, when ordered, follows GB/T 222. Q690MD is a microalloyed HSLA plate. Grade D is tighter on phosphorus and sulfur than grade B or C, because the impact test is at −20°C. Mills may add Nb, V or Ti, and some heats use nickel, chromium, molybdenum or a controlled boron addition to hold the 690 MPa window. The certificate shows the elements actually used. TMCP chemistry is often leaner than a QT heat of the same yield, because the rolling schedule does part of the strengthening.

Heat Analysis and Product Analysis — GB/T 1591 Q690MD, TMCP

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.60 0.65
Manganese (Mn), max 2.00 2.10
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.015 0.020
Niobium (Nb), max 0.11 0.12
Vanadium (V), max 0.12 0.13
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 1.20 1.25
Nickel (Ni), max 2.00 2.05
Copper (Cu), max 0.50 0.55
Molybdenum (Mo), max 0.60 0.65
Boron (B), max 0.004 0.005
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than quenched-and-tempered GB/T 16270 Q690D. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. A 620 MPa file is GB/T 1591 Q620MD, not this grade.

Mechanical Properties

Buyers search Q690MD mechanical properties, Q690MD yield strength, GB/T 1591 Q690MD tensile and Q690MD impact −20°C.

Tensile and impact — GB/T 1591 Q690MD, TMCP

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 690 MPa 770–940 MPa 14% −20°C, grade D
> 16–40 mm 670 MPa 750–920 MPa 14% −20°C, grade D
> 40–63 mm 650 MPa 730–900 MPa 14% −20°C, grade D
> 63–80 mm 630 MPa 710–900 MPa 14% −20°C, grade D
> 80–100 mm 620 MPa 690–890 MPa 13% −20°C, grade D

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 34 J minimum at −20°C. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it.

Yield steps down with thickness. A 690 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 690 MPa is about 100 ksi. ASTM A514 is about 100 ksi and is quenched and tempered. SHH STEEL quotes the thickness band and the M condition on the offer.

Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the D letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 16270 Q690D GB/T 16270 QT 690 MPa −20°C Different process
GB/T 1591 Q690MC GB/T 1591-2018 TMCP 690 MPa 0°C Warmer M sister
Q690MD GB/T 1591-2018 TMCP 690 MPa −20°C This page
Q690ME GB/T 1591-2018 TMCP 690 MPa −40°C Colder M sister
GB/T 1591 Q620MD GB/T 1591-2018 TMCP 620 MPa −20°C Lower yield
GB/T 16270 Q800D GB/T 16270 QT 800 MPa −20°C Higher yield
EN 10025-6 S690Q EN 10025-6 QT 690 MPa −20°C Different process
ASTM A572 Gr.55 ASTM A572 As rolled 380 MPa Different Lower yield

A colder QT file is GB/T 16270 Q690E. A 550 MPa file is GB/T 1591 Q550MD.

Equivalent Material Grades

There is no official one-to-one substitute for Q690MD. What buyers compare is a 690 MPa TMCP plate tested at −20°C.

EN 10025-4 has no S690M. EN 10025-6 S690Q is the strength comparison at the same impact temperature, but it is quenched and tempered. EN 10025-4 S460M is the nearest TMCP book grade and is well below this yield. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A514 is about 100 ksi and is quenched and tempered. ASTM A572 Gr.55 is 55 ksi. ASTM A36 is 36 ksi and is well below this yield. SHH STEEL will not stamp EN 10025-6 S690Q or ASTM A514 on a Q690MD certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q690MD China GB/T 1591-2018 Name on this page
GB/T 16270 Q690D China GB/T 16270 QT, not this page
GB/T 1591 Q690MC China GB/T 1591-2018 TMCP, 0°C
GB/T 1591 Q620MD China GB/T 1591-2018 620 MPa, TMCP
EN 10025-6 S690Q Europe EN 10025-6 QT, −20°C
EN 10025-4 S460M Europe EN 10025-4 TMCP, lower yield
ASTM A514 USA ASTM A514 QT, about 690 MPa
JIS G3106 SM570 Japan JIS G3106 Lower yield comparison

Structural Service

Buyers pick Q690MD when a bridge, building member or welded fabrication wants about 690 MPa yield, a TMCP condition, and impact at −20°C. Search phrases such as Q690MD steel plate and GB/T 1591 Q690MD all point here. The family index is GB/T 1591.

It is the wrong plate when the drawing says quenched and tempered. That work is GB/T 16270 Q690D. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q690MC, and the QT sister is GB/T 16270 Q690C. It is the wrong plate for a −40°C file. That work is Q690ME, and the QT sister is GB/T 16270 Q690E. It is the wrong plate for a 620 MPa file. That work is GB/T 1591 Q620MD or GB/T 1591 Q620ME. It is the wrong plate for an 800 MPa file. That work is GB/T 16270 Q800D. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade D, and the M condition at 690 MPa.

Weldability

Q690MD is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q690MD. Carbon equivalent on the M route is often lower than quenched-and-tempered GB/T 16270 Q690D, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at 0°C may miss the −20°C coupon.

Typical consumables are matching 100 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 does not cover 690 MPa. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q690MD procedure on GB/T 1591 Q420MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q620MC either if the joint must develop 690 MPa.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q690MD is thermomechanical controlled process. The plate is not quenched and tempered as GB/T 16270 Q690D.

TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q690MD as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.

The certificate lists GB/T 1591 Q690MD, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −20°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-6 S690Q is available only when both books are fully met. S690Q is not a TMCP grade.

Dimensions

Usual supply range from SHH STEEL for Q690MD steel plate:

  • Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by mill confirmation
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q690MD follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q690MD plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 50 −0.6 +1.3

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q690MD unless the order says so.

Supplementary Requirements

Q690MD already defines 690 MPa yield, TMCP delivery and −20°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q690MD. Do not write only Q690, and do not write GB/T 16270 if the mill must stamp M. The family page is GB/T 1591.

Impact. Grade D is −20°C. Write a higher energy if the owner requires it. Do not expect a −40°C result unless the grade is changed to Q690ME.

Delivery condition. Write thermomechanical controlled process. Write GB/T 16270 Q690D if quenched and tempered is required.

EN or US comparison. Write EN 10025-6 S690Q or ASTM A514 only if dual mark is required and both tables are met. S690Q is QT, not TMCP.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q690MD, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Bridges and towers Q690MD webs and flanges from SHH STEEL
Buildings in cold regions Q690MD columns, beams and base plates
Construction machinery Q690MD frames where the drawing names M and −20°C
General fabrication Q690MD gussets and connection plates
Comparison vs EN 10025-4 Q690MD next to EN 10025-4 S460M
Comparison vs ASTM A572 Q690MD next to ASTM A572 Gr.55
Lower yield option GB/T 1591 Q620ME when 620 MPa is enough

Q690MD is the plate for a 690 MPa TMCP file tested at −20°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for an 800 MPa QT boom under GB/T 16270. A colder QT file is GB/T 16270 Q690E.

Supply Capability

SHH STEEL sources Q690MD from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an M heat is in yard; standard TMCP about 35–50 days; 3.2 inspection about 45–55 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q690MD that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule at 690 MPa and test at −20°C, so the M and the D are both on the certificate.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard M heat about 35–50 days, 3.2 inspection about 45–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q690MD, keep the TMCP route, and do not ship GB/T 16270 Q690D as MD. We will not drop the M to save a cooling cycle, and we will not change D to C to save a cold test. If the drawing needs quenched and tempered plate, we will move the inquiry to Q690D under GB/T 16270. If the drawing needs 620 MPa, we will move it to GB/T 1591 Q620ME or GB/T 1591 Q620MF.

FAQ

What is Q690MD steel plate?
Q690MD in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 690 MPa minimum yield on thin plate and Charpy impact at −20°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q690MD the same as GB/T 16270 Q690D?
No. Both can yield at 690 MPa and both can be tested at −20°C. GB/T 16270 Q690D is quenched and tempered. Q690MD is TMCP.
Is Q690MD the same as Q690MC?
No. Both are TMCP. Q690MC is tested at 0°C. Q690MD is tested at −20°C.
Is Q690MD the same as Q620MD?
o. Both are TMCP and both are tested at −20°C. Q620MD is 620 MPa. Q690MD is 690 MPa.
What is the European equivalent of Q690MD?
There is no S690M in EN 10025-4. The strength comparison is EN 10025-6 S690Q, which is quenched and tempered and tested at −20°C. Dual mark only when both books are fully met.
What is the US equivalent of Q690MD?
There is no official ASTM twin. ASTM A514 is about 100 ksi and is quenched and tempered. SHH STEEL does not dual-mark ASTM A514 unless both books are met.

Conclusion

Q690MD steel plate to GB/T 1591 is 690 MPa TMCP structural plate with impact at −20°C. It is not quenched-and-tempered GB/T 16270 Q690D. EN 10025-4 has no S690M. EN 10025-6 S690Q is the strength comparison and is QT. ASTM A514 is about 690 MPa and is not a substitute. Whether the inquiry says Q690MD, GB/T 1591 Q690MD or Q690MD TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q690MD chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q690MD Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.

Contact SHH STEEL for mill rolling, TMCP Q690MD, cutting, UT, 3.2 inspection or a worldwide quotation.

Q690MD, Q690MD steel plate, GB/T 1591 Q690MD, Q690MD TMCP, Q690MD supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X