GB/T 1591 Q460ME thermomechanically rolled high-strength low-alloy structural steel plate, 460 MPa yield, −40 °C impact, SHH STEEL

Q460ME TMCP Steel Plate GB/T 1591 Supplier

GB/T 1591 Q460ME is thermomechanical controlled process plate with 460 MPa minimum yield and −40°C impact. SHH STEEL supplies Q460ME plate mill-direct for bridges, cold-region frames and outdoor fabrication that names the M condition. This is not normalized Q460NE and not hot-rolled Q460E.
Keywords
Q460ME, Q460ME steel plate, GB/T 1591 Q460ME, Q460ME TMCP, Q460ME supplier, EN 10025-4 S460ML, ASTM A572 Gr.65, Q460NE, Q460MD
Equivalent Grades:
GB/T 1591 Q460ME / EN 10025-4 S460ML (near) / ASTM A572 Gr 65 (struct near) / JIS G3106 SM570 (near) — Material Specification: GB/T 1591 — Delivery: TMCP; -40℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery and Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is Q460ME TMCP Steel Plate GB/T 1591?

Q460ME, also searched as GB/T 1591 Q460ME, Q460ME steel plate, Q460ME TMCP plate and Q460 ME, is the 460 MPa quality-grade-E grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 460 is the thin-plate minimum yield in MPa, M is the delivery letter, and E is the quality letter for Charpy impact at −40°C.

The M is the point of this page. Normalized GB/T 1591 Q460NE has an N. A normalized certificate cannot be stamped ME. Hot-rolled GB/T 1591 Q460E has neither M nor N. Grade C on the TMCP route is GB/T 1591 Q460MC. Grade D is GB/T 1591 Q460MD. The 420 MPa TMCP sister at the same temperature is GB/T 1591 Q420ME. The full family sits on GB/T 1591. Do not drop a 460 MPa drawing onto a 420 MPa plate, and do not upgrade it to quenched-and-tempered GB/T 16270 Q460E without a price check.

The closest European TMCP comparison is EN 10025-4 S460ML, tested colder than −20°C. EN 10025-4 S460M is only −20°C. EN 10025-4 S420ML is one yield step lower. EN 10025-3 S460NL is normalized and closer to Q460NE in process. On the US side, ASTM A572 Grade 65 is 65 ksi / 450 MPa, one step lower, and it is not an ME twin. ASTM A572 Gr.55 is 55 ksi. JIS G3106 SM570 is the usual Japanese comparison. Dual mark only when both books are fully met. See EN 10025-4 and high strength low alloy plates.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q460ME from first-line structural mills that can actually run the TMCP schedule at 460 MPa and hold −40°C impact, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book GB/T 1591-2018 Q460ME Confirmed
Other search names Q460ME steel plate, Q460 ME, Q460ME TMCP Covered
Delivery condition Thermomechanical controlled process Confirmed
Yield, ≤ 16 mm 460 MPa min Confirmed
Quality grade E, impact at −40°C Confirmed
Not this page Normalized GB/T 1591 Q460NE Different condition
Warmer TMCP sister GB/T 1591 Q460MD −20°C
EN comparison EN 10025-4 S460ML is colder TMCP Not a swap
US comparison ASTM A572 Gr.65 is 450 MPa Not a twin
Product analysis GB/T 222 column when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 As ordered

Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q460NC, GB/T 1591 Q420ME and ASTM A572 Gr.55.

Chemical Composition

Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q460. Product analysis, when ordered, follows GB/T 222. Q460ME is a microalloyed HSLA plate. Grade E is the tightest cleanliness letter on this TMCP family, because the impact test is at −40°C. Mills may add Nb, V or Ti, and some heats use a small nickel addition to hold the 460 MPa window. The certificate shows the elements actually used. TMCP chemistry is often leaner than a normalized heat of the same yield, because the rolling schedule does part of the grain refinement.

Heat Analysis and Product Analysis — GB/T 1591 Q460ME, TMCP

Element Heat analysis (%) Product analysis (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.60 0.65
Manganese (Mn), max 1.80 1.90
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.020 0.025
Niobium (Nb), max 0.11 0.12
Vanadium (V), max 0.20 0.22
Titanium (Ti), max 0.20 0.21
Chromium (Cr), max 0.30 0.35
Nickel (Ni), max 0.80 0.85
Copper (Cu), max 0.55 0.60
Molybdenum (Mo), max 0.20 0.21
Nitrogen (N), max 0.015 0.017
Aluminium (Als), min when used 0.015 0.010

Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than normalized GB/T 1591 Q460NE. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. Do not treat this chemistry as quenched-and-tempered GB/T 16270 Q460E. A 420 MPa file is GB/T 1591 Q420ME, not this grade.

Mechanical Properties

Buyers search Q460ME mechanical properties, Q460ME yield strength, GB/T 1591 Q460ME tensile and Q460ME impact −40°C.

Tensile and impact — GB/T 1591 Q460ME, TMCP

Thickness Yield min Tensile Elongation min Impact
≤ 16 mm 460 MPa 550–720 MPa 17% −40°C, grade E
> 16–40 mm 440 MPa 550–720 MPa 17% −40°C, grade E
> 40–63 mm 420 MPa 550–720 MPa 16% −40°C, grade E
> 63–80 mm 400 MPa 550–720 MPa 16% −40°C, grade E
> 80–100 mm 390 MPa 550–720 MPa 16% −40°C, grade E

Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 27 J to 34 J minimum at −40°C, depending on the ordered edition and thickness. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it. Not every TMCP heat will hold E on very thick plate. SHH STEEL confirms the thickness before promising the letter.

Yield steps down with thickness. A 460 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 460 MPa is about 67 ksi. ASTM A572 Grade 65 is 65 ksi and is not this book. Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the E letter.

Material Comparison

Grade Book Delivery Yield, thin plate Impact Swap?
GB/T 1591 Q460NE GB/T 1591-2018 Normalized 460 MPa −40°C Different process
GB/T 1591 Q460MD GB/T 1591-2018 TMCP 460 MPa −20°C Warmer M sister
Q460ME GB/T 1591-2018 TMCP 460 MPa −40°C This page
GB/T 1591 Q420ME GB/T 1591-2018 TMCP 420 MPa −40°C Lower yield
GB/T 16270 Q460E GB/T 16270 QT 460 MPa −40°C Different process
EN 10025-4 S460ML EN 10025-4 TMCP 460 MPa −50°C Closest comparison
EN 10025-3 S460NL EN 10025-3 Normalized 460 MPa −50°C Different process
ASTM A572 Gr.55 ASTM A572 As rolled 380 MPa Different Lower yield

A warmer hot-rolled file is GB/T 1591 Q460C. A 390 MPa file is GB/T 1591 Q390ME.

Equivalent Material Grades

There is no official one-to-one substitute for Q460ME. What buyers compare is a 460 MPa TMCP plate tested at −40°C.

EN 10025-4 S460ML is the closest process comparison and is tested colder. EN 10025-4 S460M is only −20°C. EN 10025-4 S420ML is lower yield. EN 10025-3 S460NL is normalized. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A572 Grade 65 is 65 ksi / 450 MPa. ASTM A572 Gr.55 is 55 ksi. ASTM A36 is 36 ksi and is well below this yield. In Japan, JIS G3106 SM570 is the usual comparison. SHH STEEL will not stamp EN 10025-4 S460ML or ASTM A572 Gr.65 on a Q460ME certificate unless the purchase order names both books and both tables are met.

Designation Country / region Standard Notes
Q460ME China GB/T 1591-2018 Name on this page
GB/T 1591 Q460NE China GB/T 1591-2018 Normalized, not this page
GB/T 1591 Q460MD China GB/T 1591-2018 TMCP, −20°C
GB/T 1591 Q420ME China GB/T 1591-2018 420 MPa, TMCP
EN 10025-4 S460ML Europe EN 10025-4 TMCP, −50°C
EN 10025-3 S460NL Europe EN 10025-3 Normalized comparison
ASTM A572 Gr.65 USA ASTM A572 65 ksi, lower yield
JIS G3106 SM570 Japan JIS G3106 Usual Japanese comparison

Structural Service

Buyers pick Q460ME when a bridge, building member or welded fabrication wants about 460 MPa yield, a TMCP condition, and impact at −40°C. Search phrases such as Q460ME steel plate and GB/T 1591 Q460ME all point here. The family index is GB/T 1591.

It is the wrong plate when the drawing says normalized. That work is GB/T 1591 Q460NE. It is the wrong plate when the drawing says hot rolled. That work is GB/T 1591 Q460E. It is the wrong plate for a −20°C file. That work is GB/T 1591 Q460MD, and the normalized sister is GB/T 1591 Q460ND. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q460MC. It is the wrong plate for a 420 MPa file. That work is GB/T 1591 Q420ME or GB/T 1591 Q420NE. It is the wrong plate for a QT file. That work is GB/T 16270 Q460E. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.

SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade E, and the M condition at 460 MPa.

Weldability

Q460ME is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q460ME. Carbon equivalent on the M route is often lower than normalized GB/T 1591 Q460NE, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at −20°C may miss the −40°C coupon.

Typical consumables are matching 70 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 does not cover 460 MPa. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.

The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q460ME procedure on GB/T 1591 Q355MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q420MB either if the joint must develop 460 MPa.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for Q460ME is thermomechanical controlled process. The plate is not normalized as GB/T 1591 Q460NE and not hot rolled as GB/T 1591 Q460E.

TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q460ME as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.

The certificate lists GB/T 1591 Q460ME, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-4 S460ML is available only when both books are fully met.

Dimensions

Usual supply range from SHH STEEL for Q460ME steel plate:

  • Thickness: commonly 8 mm – 50 mm, heavier plate to 60 mm by mill confirmation
  • Width: 1500 mm – 3000 mm, wider by enquiry
  • Length: 3000 mm – 12000 mm

Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.

Tolerances

Dimensional limits for Q460ME follow GB/T 709 unless the purchase order names EN 10029 or another table.

Typical thickness tolerance idea for Q460ME plate

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
8 – 15 −0.3 +0.8
15 – 25 −0.4 +0.9
25 – 40 −0.5 +1.1
40 – 60 −0.6 +1.3

Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q460ME unless the order says so.

Supplementary Requirements

Q460ME already defines 460 MPa yield, TMCP delivery and −40°C impact. Extra items still have to be written on the purchase order.

Book name. Write GB/T 1591 Q460ME. Do not write only Q460, and do not write Q460NE if the mill must stamp M. The family page is GB/T 1591.

Impact. Grade E is −40°C. Write a higher energy if the owner requires it. Do not expect this result from GB/T 1591 Q460MD.

Delivery condition. Write thermomechanical controlled process. Write GB/T 1591 Q460NE if normalized is required.

EN or US comparison. Write EN 10025-4 S460ML or ASTM A572 Gr.65 only if dual mark is required and both tables are met. Do not treat EN 10025-4 S460M as a −40°C grade.

Product analysis. Write it if the file needs the second chemistry column.

Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.

NDE. UT to GB/T 2970 or the named class.

Identification. Heat number, Q460ME, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.

Applications

Industry Typical components
Cold-region bridges Q460ME webs and flanges from SHH STEEL
Outdoor structures Q460ME columns and base plates tested at −40°C
Construction machinery Q460ME frames where the drawing names M and −40°C
General fabrication Q460ME gussets and connection plates
Comparison vs EN 10025-4 Q460ME next to EN 10025-4 S420ML
Comparison vs ASTM A572 Q460ME next to ASTM A572 Gr.55
Lower yield option GB/T 1591 Q420MF when 420 MPa and −60°C are the file

Q460ME is the plate for a 460 MPa TMCP file tested at −40°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A warmer normalized file is GB/T 1591 Q460ND.

Supply Capability

SHH STEEL sources Q460ME from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm, 50 mm. Heavier plate is confirmed before order.

Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery and Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days when an E heat is in yard; standard TMCP with −40°C test about 35–50 days; 3.2 inspection about 45–55 days.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q460ME that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule at 460 MPa and test at −40°C, so the M and the E are both on the certificate.

Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard ME heat about 35–50 days, 3.2 inspection about 45–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.

Experience on this grade is simple: print GB/T 1591 Q460ME, keep the TMCP route, and do not ship GB/T 1591 Q460NE or GB/T 1591 Q460MD as ME. We will not drop the M to save a cooling cycle, and we will not change E to D to save a cold test. If the drawing only needs −20°C, we will move the inquiry to Q460MD. If the drawing needs 420 MPa, we will move it to GB/T 1591 Q420MF or GB/T 1591 Q420ND.

FAQ

What is Q460ME steel plate?
Q460ME in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 460 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is Q460ME the same as Q460NE?
No. Both yield at 460 MPa and both are tested at −40°C. Q460NE is normalized. Q460ME is TMCP.
Is Q460ME the same as Q460MD?
No. Both are TMCP. Q460MD is tested at −20°C. Q460ME is tested at −40°C.
Is Q460ME the same as Q420ME?
No. Both are TMCP and both are tested at −40°C. Q420ME is 420 MPa. Q460ME is 460 MPa.
What is the European equivalent of Q460ME?
The nearest comparison is EN 10025-4 S460ML, which is TMCP and tested colder than −20°C. EN 10025-4 S460M is only −20°C. Dual mark only when both books are fully met.
What is the US equivalent of Q460ME?
There is no official ASTM twin. ASTM A572 Grade 65 is 65 ksi / 450 MPa, slightly lower, and it does not carry an ME letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
What thickness can SHH STEEL supply?
Common supply is 8 mm to 50 mm. Plate to 60 mm is confirmed with the mill before order. Yield on plate over 16 mm is lower than the 460 MPa thin-plate number.

Conclusion

Q460ME steel plate to GB/T 1591 is 460 MPa TMCP structural plate with impact at −40°C. It is not normalized GB/T 1591 Q460NE and not hot-rolled GB/T 1591 Q460E. EN 10025-4 S460ML is the closest TMCP comparison. ASTM A572 Grade 65 is 450 MPa and is not a substitute. Whether the inquiry says Q460ME, GB/T 1591 Q460ME or Q460ME TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q460ME chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies Q460ME Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.

Contact SHH STEEL for mill rolling, −40°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.

Q460ME, Q460ME steel plate, GB/T 1591 Q460ME, Q460ME TMCP, Q460ME supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response