ASTM A269 TP304 Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 TP304 Stainless Steel Tube

ASTM A269 TP304 / UNS S30400 nominal-wall seamless and welded austenitic stainless steel tubing with Cr 18.0–20.0%, Ni 8.0–11.0% and C ≤0.08%, solution annealed at ≥1900 °F [1040 °C] with hardness max 192 HBW / 200 HV or 90 HRB. SHH STEEL can produce and supply A269 TP304 tube with EN 10204 3.1 MTCs.
Grade
TP304 / UNS S30400
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall (instrument / process band); other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP304 Stainless Steel Tube

ASTM A269 / A269M is the product specification for nominal-wall-thickness, seamless and welded austenitic stainless steel tubing used in general corrosion-resisting and low- or high-temperature service — instrumentation, hydraulic lines, process transfer, food and pharma utilities, and similar duties. Grade TP304 is the workhorse 18-8 chromium-nickel austenitic in that Table 1 list, under UNS S30400, with melting limits of carbon ≤0.08%, chromium 18.0–20.0%, and nickel 8.0–11.0%. Writing “304 tube” or “S30400 instrumentation tube” on a bill of materials is not enough: the purchase order must name ASTM A269 (or A269M) so the mill applies nominal-wall tolerances, solution treatment, hardness, flaring or flange tests, and marking for tubing — not an A213 boiler-tube or A312 pipe text.

SHH STEEL can produce and supply ASTM A269 TP304 stainless steel tube as seamless and welded product across the usual instrument-to-process OD × nominal-wall band, solution annealed and quenched, with EN 10204 3.1 mill test certificates that report Table 1 ladle chemistry and Table 2 hardness. Typical enquiry sizes run from about 6 mm to 168 mm outside diameter with 0.5–8.0 mm nominal wall (or the matching inch / BWG list); other diameters and walls are available by agreement. Browse sister grades on the A269/A269M hub.

Commercially the grade is still called 304, 18-8, or S30400 general-service tube; those shop names never replace the ASTM grade line on the MTC. Closest A269 sisters include A269 TP304L, A269 TP304LN, A269 TP316 / A269 TP316L, and stabilized A269 TP321 / A269 TP347. When the same UNS chemistry is needed as boiler / heat-exchanger tube or as pipe, open A213 TP304 or A312 TP304 instead. A269’s wall basis is nominal wall — mention that early on the enquiry so nobody builds a minimum-wall A213 product by habit.

Chemical Composition of A269 TP304

Every TP304 heat under A269 must meet Table 1 melting (ladle) analysis. Product analysis on finished tube applies when the purchase order or supplementary requirement invokes it through ASTM A1016/A1016M, with tolerances typically taken from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not sell unpublished “tighter than Table 1” catalogue windows as if they were ASTM limits.

The table below reproduces Table 1 heat analysis for TP304 / UNS S30400 from public A269 excerpts (ASTM abstract Table 1 cross-checked with the tubingchina A269 PDF reproduction). Values are maximum unless a range is shown; ellipsis (…) means no requirement in the ordered edition. Confirm the purchased A269/A269M edition before treating any secondary catalogue as the acceptance text.

Melting analysis (heat / ladle analysis) — Table 1

Element TP304 (UNS S30400) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Source: ASTM A269/A269M Table 1 for Grade TP304 / UNS S30400 (ASTM abstract and public PDF excerpts cross-checked; Wikipedia SAE 304 summary used only for alloy-family context, not for acceptance numbers). Chromium 18–20% and nickel 8–11% are the classic 18-8 passive-film pair; carbon ≤0.08% is the standard (non-L) ceiling, so as-welded sensitization risk sits above TP304L. Molybdenum is not required — when chloride pitting resistance matters, move to TP316 / TP316L under the same A269 standard rather than hoping TP304 will behave like a Mo grade.

Mechanical Properties of A269 TP304

ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP304 the way A213 Table 4 or A312 mechanical tables do for the same UNS number. Finished-tube acceptance under A269 is built on hardness (Table 2), flaring (seamless), flange and reverse flattening (welded), and a hydrostatic or nondestructive electric test on each length. Quoting a 75/30 ksi tensile floor as an A269 TP304 requirement without a purchase-order supplement would be inventing a number from a sister product standard.

Table 2 sets the hardness maximum for TP304 / UNS S30400 at 192 HBW / 200 HV or 90 HRB after the required solution heat treatment. That ceiling matches the familiar 18-8 annealed hardness band buyers know from other ASTM stainless products, but under A269 it stands alone without a paired tensile table. Hardness testing is not required on tubes below the small-ID / thin-wall exemptions in the hardness clause, though heat treatment still is.

Property TP304 requirement (A269 Table 2)
Hardness, max 192 HBW / 200 HV or 90 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade (do not invent from A213/A312)

Source: ASTM A269/A269M Table 2 for TP304 / UNS S30400 (public PDF excerpt). Superficial Rockwell limits for thin-wall “all other grades” (including TP304) are stated in the hardness clause — typically not exceeding 74 on the 30 T scale or 88 on the 15 T scale when that method is used; confirm in the purchased edition. If a project needs guaranteed tensile values on tubing, either add them as purchase-order extras or open A213 / A312 for the matching UNS.

Seamless and Welded Tube

A269 allows TP304 tubing to be seamless or welded, and hot-finished or cold-finished at the manufacturer’s option unless the order locks the route. Welded A269 TP304 is produced without filler metal; the longitudinal seam is autogenous, then cold-worked and solution-treated with the tube. That is a different product-form story from A312 pipe, where WLD and HCW codes carry their own stencil identity — A269 simply states seamless or welded and does not use those pipe manufacturing-type letters as the primary claim.

Seamless TP304 takes a lot-basis flaring test; welded TP304 takes flange and reverse-flattening tests so the seam is opened and reverse-bent under controlled conditions. Both routes share Table 2 hardness and the mandatory hydro or NDE test per length. Cold-finished tube dominates instrumentation and bright process lines; hot-finished seamless is more common on heavier walls. SHH STEEL can produce and supply both seamless and welded A269 TP304 against the same chemistry and heat-treatment floors — say which route the line specification requires on the enquiry.

Dimensions and Tolerances

Order A269 TP304 by outside diameter and nominal wall thickness (or an agreed average-wall note). Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M. Thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%
8 to 12 in. [203–305 mm], excl. ±0.040 in. [1.01 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Heavy-wall or low ID/OD tubes may take the footnote ±12.5% wall variation; sub-½ in. ID non-mandrel tube may take ±15%. Cut-length over-tolerances apply up to 24 ft [7.3 m] with an incremental allowance beyond. Cross-check against mill datasheets from producers such as Sandvik or Tubacex-style stainless tube catalogues shows the same OD × wall enquiry bands buyers use for instrument and process A269 tube — those catalogues are size-range references, not a substitute for Table 4 acceptance numbers.

Equivalent Grades

TP304 / UNS S30400 is the ASTM tubing designation for standard 18-8 austenitic. The same UNS chemistry idea appears as A213 TP304 (seamless boiler/HX tube), A312 TP304 (pipe), and A240 Type 304 plate/sheet, but product form, wall basis, and mechanical acceptance are not interchangeable. European 1.4301 / X5CrNi18-10 is a common commercial cousin; confirm chemistry and product standard before treating it as a drop-in for an A269 order.

Reference Designation Note
ASTM A269 TP304 / UNS S30400 This product standard (nominal-wall tube)
UNS S30400 Chemistry identity
ASTM A213 TP304 Seamless boiler / HX tube; tensile table
ASTM A312 TP304 Pipe, not tubing
ASTM A240 Type 304 / S30400 Plate / sheet cousin
EN (approx.) 1.4301 / X5CrNi18-10 Commercial cousin — confirm before substituting

Inside A269, move to A269 TP304L for low-carbon as-welded duty, to A269 TP316L when molybdenum is required, or to A269 TP321 / A269 TP347 when titanium or niobium stabilization is specified.

Heat Treatment and Delivery Condition

All A269 TP304 tube is furnished solution heat-treated. Table 2 requires a minimum austenitizing temperature of 1900 °F [1040 °C], followed by water quench or other rapid cooling. Seamless tube may be individually quenched immediately after hot forming while still at or above that temperature. If the purchaser orders a final heat treatment below 1900 °F for controlled structural reasons, each tube must be stenciled with the actual temperature after the suffix “HT.”

Item TP304 (A269 Table 2)
Austenitizing temperature, min 1900 °F [1040 °C]
Cooling Water quench or rapid cool by other means
Hardness after heat treatment, max 192 HBW / 200 HV or 90 HRB
Delivery condition Solution heat-treated (pickled or bright-annealed by agreement)

Source: ASTM A269/A269M §6 and Table 2 for TP304. Pickled versus bright-annealed is a surface choice on top of the mandatory solution treatment. SHH STEEL ships A269 TP304 only in a heat-treated condition that meets the ordered Table 2 requirement, and the MTC states what was done.

Corrosion Resistance

TP304’s 18-8 chromium-nickel balance is the default austenitic for a wide band of aqueous, atmospheric, and food-contact services where chlorides stay moderate and reducing acids are absent. The passive film from ~18–20% Cr handles many plant utilities, dairy and beverage lines, and clean process transfer duties that do not need molybdenum. Wikipedia’s SAE 304 summary and mill practise both treat 304 as the most common stainless — that popularity is about versatility and formability, not about matching every chloride duty.

Carbon up to 0.08% means HAZ sensitization is possible if welded fabrications sit in the sensitizing temperature band and then see corrosive service without a post-weld anneal. For as-welded corrosive duty, prefer A269 TP304L or A269 TP304LN. For chlorides, seawater, or many chemical media, step to A269 TP316L or a 6Mo A269 grade. A269 itself does not publish PREN or CPT tables for TP304 — do not invent them from marketing sheets.

Applications of A269 TP304 Tube

A269 TP304 is the default stainless tubing grade on countless instrument air and impulse lines, hydraulic and pneumatic systems, food and beverage utility tubing, pharmaceutical water and clean-steam utilities (where the project’s material list allows 304), heat-transfer coils specified to A269 rather than A213, and general process transfer lines in mild media. Cold-finished bright-annealed TP304 dominates skid and panel work; pickled welded TP304 is common on larger utility runs.

It is the wrong first choice for Code boiler / superheater tube (use A213 / SA213), for pipe headers (use A312 / SA312), and for chloride-rich or reducing-acid service that needs Mo or higher alloys. SHH STEEL can produce and supply A269 TP304 across the general-service band above and will say when the stated medium needs TP304L, TP316L, or something higher.

Weldability

TP304 is readily welded by GTAW and GMAW with 308/308L-type fillers when filler is used on fabrication joints. Autogenous A269 welded tube already carries a mill seam that was cold-worked and solution-treated with the tube; cut-length shop welds are a separate fabrication step outside that mill anneal. Standard carbon means as-welded HAZ sensitization remains a design input whenever the assembly will see corrosive service without re-annealing.

Projects that must stay as-welded in corrosive or hygienic service usually specify A269 TP304L from the start. Filler selection, purge quality, and interpass control stay with the fabricator; SHH STEEL’s A269 scope is the mill tube, chemistry, hardness, and process route on the purchase order.

Surface Finishes

Pickled and bright-annealed are the two standard A269 TP304 deliveries. Bright anneal is preferred for instrumentation, semiconductor utility, and many hygienic lines; pickle is the workhorse for general process tube. Named OD polish grit (for example 180# or 320#) is a supplementary finish when the purchase order requires it — A269 does not mandate a polish grade.

Interior Ra limits, scrubbed ID, or electropolish notes belong in the enquiry text. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP304 when the mill can measure and report the finish; we do not claim an unverified surface grade.

Inspection and Testing

Lot testing for A269 TP304 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot size tied to heat, diameter, wall, and heat-treatment charge as written in the standard. Each length also takes a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method. NDE-tested lengths are marked “NDE” and certified accordingly.

SHH STEEL EN 10204 3.1 certificates report ladle chemistry, heat-treatment condition, hardness, and the hydro/NDE statement. PMI, product analysis, and third-party inspection are available when named on the order. We do not drop mandatory tests to shorten lead time.

Packaging and Shipping

TP304 tube ships with end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight. Bright-annealed and polished OD get sleeve protection against transit galling. Coiled tubing, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Marking typically includes ASTM A269, TP304 / S30400, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL aligns stencil and tags with the purchase-order marking clause before dispatch.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP304 as nominal-wall seamless or welded tubing — solution annealed to Table 2, hardness-tested, hydro- or NDE-tested, and documented on EN 10204 3.1 certificates — not as a generic “304 tube” label on whatever is in the rack. We keep A269 distinct from A213 and A312 on the MTC, we state seamless versus welded honestly, and we will not paste A213 tensile floors onto an A269 shipment to make the certificate look busier.

Grade advice stays practical. If as-welded corrosive service needs low carbon, we point to A269 TP304L; if chlorides need molybdenum, we point to A269 TP316L. Winning the order with the wrong 18-8 stamp is not a win for the project or for us.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP304 stainless steel tube against the edition, process route, and finish named on your enquiry. The capability table and Stock / Available sizes enquiry map below are what buyers use to frame a first-pass size list for instrument and process duty.

Item SHH STEEL capability for TP304
Standard ASTM A269 / A269M
Grade TP304 / UNS S30400
Product form Seamless and welded tube (no filler metal for welded), hot-finished or cold-finished
Delivery condition Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (other sizes by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range for A269 TP304 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats and finishing slots; send the OD × nominal-wall list and seamless/welded preference for confirmation.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrumentation / hydraulic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD process and utility
38.1 / 42.4 / 48.3 / 60.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Utility and light process; welded common
76.1 / 88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Cut lengths, coils, polished OD, and dual enquiries against A269 TP304L or A269 TP316L on the same size list are routine. Peer mill catalogues (Sandvik, Outokumpu, Tubacex-style stainless tube ranges) were used only to sanity-check typical OD × wall bands buyers ask for — acceptance remains A269 Table 4.

FAQ

What is ASTM A269 TP304 stainless steel tube used for?
A269 TP304 is the workhorse nominal-wall 18-8 tubing grade for instrumentation, hydraulic lines, food and pharma utilities, and mild process transfer. It covers seamless and welded general-service tube — not Code boiler tube (that is A213) and not pipe (that is A312). Put A269 on the purchase order so wall basis, hardness, and tests match the tubing product standard.
Is A269 TP304 the same as A213 TP304?
No. Both can share UNS S30400 chemistry, but A269 is nominal-wall general-service tubing (seamless or welded, hardness-based), while A213 is seamless boiler/superheater/HX tube with a tensile table and typically a minimum-wall basis. Order the standard that matches the drawing; do not treat “304 tube” as one interchangeable product.
Does A269 TP304 include welded tube?
Yes. A269 covers seamless and welded TP304. Welded tube is autogenous (no filler metal), cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. Site titles omit the word “Welded” by house style, but the order and MTC still state seamless or welded.
What hardness does A269 require for TP304?
Table 2 sets a maximum of 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. A269 does not publish a tensile/yield/elongation acceptance table for TP304, so do not invent 75/30 ksi floors from A213 unless the purchase order adds them as extras.
TP304 vs TP304L for A269 tubing — which should I buy?
Buy TP304 when standard carbon (≤0.08%) is acceptable and fabrication will be re-annealed or service is mild. Buy TP304L when as-welded intergranular corrosion resistance matters. They are separate A269 grades with different carbon ceilings and should not share one heat stamp on the MTC.
Is A269 nominal wall or minimum wall?
A269 is written on a nominal-wall-thickness basis. State OD × nominal wall on the enquiry unless you agree a different wall basis with the mill. Table 4 then governs OD, wall, and cut-length tolerances for the ordered size group.
What size range can SHH STEEL supply for A269 TP304?
SHH STEEL can produce and supply A269 TP304 in a typical band of about 6–168 mm OD × 0.5–8.0 mm nominal wall, seamless or welded, pickled or bright-annealed, with EN 10204 3.1 MTCs. Larger or heavier sizes are quoted by agreement — send the OD × wall list for a firm availability answer.
Hydrostatic or eddy-current test for A269 TP304?
Each tube must receive either a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks one method. NDE-tested lengths are marked “NDE.” Hardness and flaring/flange tests remain separate lot requirements beside that choice.
When should I choose TP316L instead of TP304 under A269?
Choose TP316L when the medium needs molybdenum for better chloride pitting and crevice resistance — seawater-adjacent utilities, many chemical process lines, and chloride-bearing washdown service. TP304 remains appropriate for milder aqueous and food-contact duties where Mo is not justified.
What documents come with SHH STEEL A269 TP304?
EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. Third-party inspection and PMI can be added on the order. Stencil carries ASTM A269, TP304 / S30400, size, heat, and seamless or welded identity.
How do I enquire for A269 TP304 with SHH STEEL?
Send ASTM A269, grade TP304 / UNS S30400, seamless or welded preference, OD × nominal-wall list and lengths (or coil), finish, and any hydro/NDE lock. Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend TP304L / TP316L when the duty needs them.

Conclusion

ASTM A269 TP304 / UNS S30400 remains the reference 18-8 nominal-wall stainless steel tubing grade for general corrosion service when molybdenum is not required and standard carbon is acceptable. SHH STEEL can produce and supply seamless and welded A269 TP304 tube, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. For sister grades and size discussions, start from the A269/A269M hub, then send your OD × nominal-wall list and process route. Contact admin@steelspecs.com with the size list and medium notes for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X