ASME SA533 Type C Class 3 Q&T Mn-Mo-Ni vessel plate, Gr.C Cl.3, Ni 0.70–1.00%, TS 100–125 ksi, SHH STEEL

ASME SA533 Type C Class 3 Steel Plate | SA533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate

ASME SA533 Type C Class 3 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type C has the highest nickel band. Tensile 690–860 MPa, yield 570 MPa, max 65 mm. SHH STEEL supplies SA533 Type C Cl.3 / A533 Gr.C Cl.3 mill-direct with 3.1 or 3.2 certificates.
Keywords:
ASME SA533 Type C Class 3, SA533 Gr.C Cl.3, SA533GRCCL3, SA533 Grade C Class 3, ASTM A533 Type C Class 3, A533 Gr.C Cl.3, Mn-Mo-Ni QT vessel plate, SA-533 Type C Class 3
Equivalent Grades:
ASME SA533 Type C / ASTM A533 Type C / GB 20MnMoNi (near, higher Ni) / EN 10028-3 P355NL2 (near) — Material Specification: ASME SA-533 / ASTM A533 — Delivery: Quenched + Tempered (Q+T) (Type C = Mn-½Mo-¾Ni)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Quenched-and-Tempered Mn-Mo-Ni Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA533 Type C Class 3 Steel?

ASME SA533 Type C Class 3 is the highest-nickel manganese-molybdenum-nickel combination in ASME SA-533/SA-533M at the Class 3 strength window. The current specification lists five Types (A, B, C, D, E) and three Classes (1, 2, 3). Type C heat nickel is about 0.70–1.00%. Type B is about 0.40–0.70%. Type D is about 0.20–0.40%. Type A has no nickel requirement. Class 3 is 690–860 MPa tensile and 570 MPa yield. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-533/SA-533M.

The same plate is written SA533 Type C Class 3, SA533 Gr.C Cl.3, SA533 Grade C Class 3, SA533GRCCL3, SA-533 Type C Cl.3, ASTM A533 Type C Class 3 and A533 Gr.C Cl.3. The standard text says Type. Buyers still search Grade C Class 3. They mean the same plate. Do not ship Type B and call it Type C. Do not ship Class 2 and call it Class 3. Do not treat this page as normalized SA302 Gr.C. SA302 Grade C is Mn-Mo-Ni in the normalized condition. SA533 Type C Class 3 is quenched and tempered.

Class 3 has a hard thickness cap that Class 1 and Class 2 do not share. Maximum thickness of Class 3 plates is 65 mm (2.5 in.) for Types A through D. If the inquiry is 80 mm at Class 3 strength, this specification cannot be used at Class 3. Move the conversation to Class 1 or Class 2, or to another QT specification such as SA517 Gr.Q, after the drawing is revised. Company scope: China steel Mill Agent-SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Type / Grade ASME SA533 Type C / Gr.C Confirmed
Class Class 3 Confirmed
Product Specification ASME SA-533/SA-533M Applied
Companion Spec ASTM A533 Type C Class 3 Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Alloy Mn-Mo-Ni, highest Ni band Confirmed
Condition Quenched and tempered Confirmed
Maximum Thickness 65 mm for Type C Class 3 Per SA-533
Typical Supply 6.5 mm – 65 mm By mill enquiry
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate is a vessel product under ASME Section VIII when dual marked. It is not structural ASTM A36 steel plate. It is not fine-grain carbon like SA516 Gr.70 or A516 Gr.70. It is not SA515 Gr.70. It is not SA285 Gr.C. Minimum nominal thickness is 6.5 mm.

Chemical Composition

Chemistry for ASME SA533 Type C is the Type table. Class 3 shares Type C chemistry unless S3 raises manganese.

Heat Analysis — ASME SA533 Type C

Element Heat Analysis (%)
Carbon (C), max 0.25
Manganese (Mn) 1.15 – 1.50
Phosphorus (P), max 0.025
Sulfur (S), max 0.025
Silicon (Si) 0.15 – 0.40
Molybdenum (Mo) 0.45 – 0.60
Nickel (Ni) 0.70 – 1.00

Product Analysis — SA533 Gr.C / A533 Type C

Element Product Analysis (%)
Carbon (C), max 0.25
Manganese (Mn) 1.07 – 1.62
Phosphorus (P), max 0.025
Sulfur (S), max 0.025
Silicon (Si) 0.13 – 0.45
Molybdenum (Mo) 0.41 – 0.64
Nickel (Ni) 0.67 – 1.03

A ladle at 0.55% Ni sits in Type B, not Type C. A ladle at 0.30% Ni sits in Type D, not Type C. A ladle with no nickel sits in Type A, not Type C. For Class 3, manganese maximum may rise to 1.60% heat and 1.65% product when S3 is specified. SHH STEEL applies that increase only when the purchase order says S3.

Compare that ladle with SA302 Gr.C, SA302 Gr.D, SA387 Gr.11 Cl.2 and SA516 Gr.60. If the drawing says ASME SA533 Type C Class 3 or SA533 Gr.C Cl.3, the ladle must sit in the Type C nickel window and the tensile test must sit in the Class 3 window. SHH STEEL reports heat analysis on every certificate, including nickel and molybdenum.

Mechanical Properties

Class 3 is the highest strength line in SA-533.

Tensile Requirements — ASME SA533 Class 3

Property Class 3
Tensile strength 690 – 860 MPa (100 – 125 ksi)
Yield strength, min 570 MPa (83 ksi)
Elongation in 50 mm (2 in.), min 16%

Class 1 is 550–690 MPa and 345 MPa yield. Class 2 is 620–795 MPa and 485 MPa yield. A Class 2 heat cannot be stamped Class 3 because someone wants the higher name. Density is 7.85 g/cm³. Charpy is not a hidden default. Class 3 work almost always writes impact temperature, location and orientation.

Compare SA537 Cl.2 and SA517 Gr.Q. Overlap on a number is not a substitute.

Material Comparison

Grade Route Strength / thickness Swap?
SA533 Type C Cl.1 QT Mn-Mo-Ni 550–690 / 345 MPa, ~300 mm practice Same Type, lower Class
SA533 Type C Cl.2 QT Mn-Mo-Ni 620–795 / 485 MPa, ~300 mm practice Same Type, lower Class
SA533 Type C Cl.3 QT Mn-Mo-Ni 690–860 / 570 MPa, 65 mm max This page
SA533 Type B Cl.3 QT Mn-Mo-Ni Same Class, lower Ni No
SA533 Type D Cl.3 QT Mn-Mo-Ni Same Class, lower Ni No
SA302 Gr.C Normalized Mn-Mo-Ni Not QT No
SA516 Gr.70 Fine-grain carbon 485–620 MPa No
SA517 Gr.B QT alloy 690 MPa class, 32 mm max No

Order ASME SA533 Type C Class 3 when the drawing names Type C and Class 3 and thickness is 65 mm or less. SHH STEEL does not swap this plate for A516 Gr.70 or A517 Gr.Q.

Quenched-and-Tempered Mn-Mo-Ni Vessel Service

ASME SA533 Type C Class 3 is selected when the vessel needs the top SA-533 strength window, nickel in the Type C band, and the wall stays inside 65 mm. Allowable stress comes from ASME Section II Part D for SA-533 Type C Class 3 after dual marking.

Typical use is high-strength shells and heads specified to SA-533 Type C Class 3. If the drawing says Type B Class 3, nickel is lower. If the wall is 80 mm, Class 3 is the wrong Class.

It is not a replacement for SA387 Gr.22 Cl.2 or SA203 Gr.E. It is not a replacement for SA537 Cl.2.

Weldability

SA533 Gr.C Cl.3 is QT Mn-Mo-Ni at the highest Class with the highest nickel band. Welding is Code welding, not structural fillet practice from ASTM A36 steel plate.

Procedures are qualified to ASME Section IX. Low-hydrogen practice is mandatory. Carbon can sit at 0.25%. Molybdenum is in the 0.45–0.60% heat band. Nickel is in the 0.70–1.00% heat band. Calculate carbon equivalent from the actual ladle.

Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want to PWHT. Simulated PWHT of mill coupons should be on the purchase order.

Do not copy a SA387 Gr.22 Cl.1 or SA517 Gr.A procedure onto Type C Class 3 without review. The fabricator owns the WPS.

Heat Treatment

Plates shall be quenched and tempered. The steel shall be killed and shall meet fine austenitic grain practice under ASME SA-20.

Tempering shall be at a suitable temperature to produce the specified Class 3 properties, but not less than 595 °C (1100 °F), with a minimum holding time of ½ h/in. (1.2 min/mm) and not less than ½ h.

As-rolled delivery is not the specified condition. As-rolled shipping is crack-sensitive above about 25 mm and requires written agreement. SHH STEEL reports quench and temper data on the MTC.

Do not apply the normalize-only route used for SA302 Gr.C and call the plate SA533 Type C Class 3.

Delivery Condition

Usual delivery is quenched and tempered Type C Class 3 plate, 6.5–65 mm.

The certificate lists ASME SA533 Type C Class 3 and, when dual certified, ASTM A533 Type C Class 3; heat number; heat analysis including Ni and Mo; product analysis when ordered; tensile results to the Class 3 table; QT temperatures; Charpy results when ordered; and supplementary tests.

Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for SA533 Gr.C Cl.3 Mn-Mo-Ni vessel plate:

  • Thickness: 6.5 mm – 65 mm (Class 3 maximum on Type C)
  • Width: up to about 4000 mm
  • Length: up to about 12000 mm

If the inquiry is 70 mm, Class 3 cannot be used. Use Class 1 or Class 2, or revise the specification.

Tolerances

Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. UT to A435 / A577 / A578 is commonly added on Class 3 plate.

Supplementary Requirements

Most export ASME SA533 Type C Class 3 orders add extras. SHH STEEL does not assume them.

S3 manganese increase. Allowed for Class 2 and Class 3. Written on the order or not applied.

Charpy details. Temperature, energy, location and orientation.

Simulated PWHT. Same-heat coupons follow the vessel cycle.

NDE. UT to A435 / A577 / A578.

Restricted residuals / P / S. When specified.

Third-party. EN 10204 3.2.

Equivalent Material Grades

Designation Standard Notes
ASME SA533 Type C Class 3 / SA533 Gr.C Cl.3 ASME SA-533/SA-533M Code name on this page
ASTM A533 Type C Class 3 / A533 Gr.C Cl.3 ASTM A533/A533M Companion spec
SA533 Type C Class 1 / Class 2 SA-533 Same Type, lower strength, thicker capability
SA533 Type B Class 3 SA-533 Lower nickel band
SA302 Gr.C SA-302 Normalized Mn-Mo-Ni; not QT
EN 10028-6 P690QL related EN Project comparison only
JIS G3124 related JIS Confirm QT and 65 mm cap
GB/T 19189 related GB Confirm Type and Class
A537CL2 ASTM A537 QT carbon; not a substitute
A517 Gr.A ASTM A517 Different QT family
A203 Gr.A ASTM A203 Nickel family; not QT Mn-Mo-Ni

Applications

Industry Typical components
High-strength vessels ASME SA533 Type C Class 3 shells and SA533 Gr.C Cl.3 heads to 65 mm
Process equipment SA-533 Type C Cl.3 Mn-Mo-Ni courses
Energy ASME SA533 Type C Class 3 QT vessel plate
Dual-certified export SA533 / A533 Type C Cl.3 plate
Fabrication SA533 Gr.C Cl.3 cut to nest sizes inside 65 mm

Do not use this grade as a silent stand-in for SA203 Gr.B or SA517 Gr.S.

Why Choose SHH STEEL

SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-533/SA-533M. On ASME SA533 Type C Class 3 that means mill pricing, dual SA533/A533 marking, Type C chemistry with nickel in the 0.70–1.00% heat band, recorded quench and temper, Class 3 tensile results at 690–860 MPa and 570 MPa yield, the 65 mm ceiling respected, 3.1 as standard and 3.2 when specified.

We keep the order on the right Type and Class. Type C is not Type B, not Type D and not Type A. Class 3 is not Class 1 and is not Class 2. SA533 is not SA516 Gr.55. SA533 is not SA285 Gr.A. SA533 Type C Cl.3 is not SA517 Gr.Q. If the drawing names a wall over 65 mm at this strength, we will say Class 3 cannot be used. If it names Type B, we will not ship Type C and call extra nickel an upgrade.

Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA533 Type C Class 3?
Buyers write SA533 Type C Class 3, SA533 Gr.C Cl.3, SA533 Grade C Class 3, SA533GRCCL3, ASTM A533 Type C Class 3 and A533 Gr.C Cl.3. SHH STEEL prints the wording on the purchase order.
How is Type C different from Type B and Type D?
Type C heat nickel is 0.70–1.00%. Type B is 0.40–0.70%. Type D is 0.20–0.40%. Class 3 is the same tensile table and the same 65 mm cap on Types A–D.
Is ASME SA533 Type C Class 3 the same as ASTM A533 Type C Class 3?
Chemistry and tensile limits match. ASME SA-533 is the Code version. ASTM A533 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies both names when the vessel must be stamped.
What is the yield strength of SA533 Gr.C Cl.3?
570 MPa minimum. Tensile is 690–860 MPa. Elongation is 16% in 50 mm, per ASME SA-533 Class 3.
What is the maximum thickness for Class 3?
65 mm for Type C. Class 1 and Class 2 on Type C follow current practice to about 300 mm. Do not order 80 mm Class 3.
: Is SA533 Type C the same as SA302 Grade C?
No. SA302 Grade C is normalized Mn-Mo-Ni. SA533 Type C is quenched and tempered.
What heat treatment does ASME SA533 Type C Class 3 require?
Quench and temper. Temper not less than 595 °C with a minimum hold of ½ h/in., not less than ½ h.
Can welding be qualified to ASME Section IX?
Yes. Use a low-hydrogen WPS written for QT Mn-Mo-Ni at Class 3 strength. The fabricator owns the procedure.

Conclusion

ASME SA533 Type C Class 3 Steel Plate is quenched-and-tempered manganese-molybdenum-nickel vessel plate under ASME SA-533/SA-533M, limited to 65 mm, with 690–860 MPa tensile and 570 MPa yield, using the highest nickel band among Types A–D. Whether the inquiry says SA533 Type C Class 3, SA533 Gr.C Cl.3, SA533 Grade C Class 3 or A533 Type C Class 3, SHH STEEL supplies plate with Type C chemistry, recorded QT, Class 3 tensile results, and EN 10204 3.1 or 3.2 certification.

As a China mill Distributor, SHH STEEL provides ASME SA533 Type C Class 3 / SA533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate for ASME Section VIII work.

Contact SHH STEEL for mill rolling, dual SA533/A533 marking, 3.2 inspection or a quotation.

ASME SA533 Type C Class 3 Steel Plate, SA533 Gr.C Cl.3, SA533 Grade C Class 3, ASTM A533 Type C Class 3, Mn-Mo-Ni QT vessel plate, Direct Mill Supply by SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X