What is JIS H4600 Class 17 TP240Pd titanium plate?
JIS H4600 Class 17 TP240Pd titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 17 carries 0.04–0.08% palladium, a lean addition that gives much of the crevice-corrosion benefit of the 0.15% Pd classes at lower cost. Its tensile range is 240–380 MPa, in the Class 1 strength band.
This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.
Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.
SHH STEEL handles Class 17 (TP240Pd) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 17, ASME SB-265 Grade 17, GB/T 3621 TA8-1.
Material specification for JIS H4600 Class 17 (TP240Pd)
JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.
| Ordering item | JIS H4600 basis |
|---|---|
| Standard | JIS H 4600 (current 2012 edition) |
| Class / symbol | Class 17 (TP240Pd); state H (hot rolled) or C (cold rolled) as needed, for example TP240PdH or TP240PdC |
| Thickness covered | 0.2–50 mm for this class |
| Condition | Annealed; hot rolled (H) or cold rolled (C) |
| Tests | Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered |
| Certificate | Inspection document with chemical and mechanical results |
The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.
Chemical composition of JIS H4600 Class 17 (TP240Pd)
Values are maximums except where a range is given. Titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.03 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.015 max |
| Iron (Fe) | 0.20 max |
| Oxygen (O) | 0.18 max |
| Palladium (Pd) | 0.04–0.08 |
| Titanium (Ti) | Balance |
Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.
Mechanical properties of JIS H4600 Class 17 (TP240Pd)
The values below are the requirements for Class 17 (TP240Pd) plate in the annealed condition.
| Property | Requirement |
|---|---|
| Thickness range covered | 0.2–50 mm |
| Tensile strength | 240–380 MPa |
| Proof stress (0.2%) | 170 MPa min |
| Elongation, min | 24% |
| Bend test (0.5 mm to under 5 mm) | 180°, inside radius 2 × thickness; no cracks on the outside |
Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.
For pressure equipment, design stresses come from the applicable code, not from the plate standard.
Delivery condition, finish and marking
JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.
- Condition: Annealed; hot rolled (H) or cold rolled (C)
- Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
- Marking: class or symbol, size, heat or lot number and manufacturer, per the order
- Packing: suitable for transport and to prevent iron contamination of the surface
The grade is supplied annealed and is not strengthened by heat treatment. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.
Welding and fabrication of Class 17 (TP240Pd) titanium plate
Class 17 (TP240Pd) is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.
- Use trailing shields and back purging until the metal cools below about 400 °C
- Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
- Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
- Check weld colour and reject heavily discoloured welds
Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.
For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.
Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Class 17 (TP240Pd) titanium plate
Typical uses of Class 17 (TP240Pd) plate include:
- Plate heat exchanger plates
- Crevice-prone chemical plant parts
- Hot chloride and brine equipment
- Process equipment where Class 1 or Class 2 is marginal
The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.
When selecting Class 17 (TP240Pd), compare it with Class 11 (TP270Pd), Class 12 (TP340Pd), Class 13 (TP480Pd). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Class 17 (TP240Pd) with other JIS H4600 grades
The grades below are the closest neighbours of Class 17 (TP240Pd) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Class 11 (TP270Pd) | 270–410 MPa | 165 MPa min | 27% | Pd-bearing Class 1 |
| Class 12 (TP340Pd) | 340–510 MPa | 215 MPa min | 23% | Pd-bearing Class 2 |
| Class 13 (TP480Pd) | 480–620 MPa | 345 MPa min | 18% | Pd-bearing Class 3 |
| Class 17 (TP240Pd) | 240–380 MPa | 170 MPa min | 24% | Lean-Pd (0.05% Pd), lower cost |
| Class 18 (TP345Pd) | 345–515 MPa | 275 MPa min | 20% | Lean-Pd (0.05% Pd), lower cost |
The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.
JIS H4600 Class 17 (TP240Pd) equivalent grades
The designations below are commonly compared with JIS H4600 Class 17 (TP240Pd). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to JIS H4600 Class 17 (TP240Pd) |
|---|---|---|
| ASTM B265 | Grade 17 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 17 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| GB/T 3621 | TA8-1 | Close equivalent; confirm grade name and limits in the ordered edition |
| UNS | R52252 | Same unified number as ASTM Grade 17 |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Class 17 (TP240Pd) titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to JIS H4600 Class 17 (TP240Pd) with the H or C finish you need
- Certificates are checked against the JIS tensile range, proof stress and bend requirement
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for JIS H4600 Class 17 (TP240Pd) plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | JIS H4600 Class 17 (TP240Pd), with H or C suffix |
| Product form | Plate, sheet or strip; hot or cold rolled |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
What does the symbol TP240Pd mean in JIS H4600?
- TP identifies plate or sheet, the number is the minimum tensile strength level in MPa, and any letters show the alloying addition. A final H means hot rolled and C means cold rolled, for example TP240PdH or TP240PdC.
-
What is the tensile strength of JIS H4600 Class 17 (TP240Pd) titanium plate?
- The requirement is 240–380 MPa. The 0.2% proof or yield strength is 170 MPa minimum. Minimum elongation is 24%. Values apply to the condition and thickness range stated in the standard.
-
What is Class 17 (TP240Pd) mainly used for?
- Typical uses include plate heat exchanger plates, crevice-prone chemical plant parts and hot chloride and brine equipment. The design engineer should confirm the grade for the actual service.
-
What thickness does JIS H4600 Class 17 (TP240Pd) cover?
- The property table for this class covers 0.2–50 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
-
What should I send for a quotation?
- Send JIS H4600 Class 17 (TP240Pd), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for JIS H4600 Class 17 TP240Pd titanium plate
JIS H4600 Class 17 (TP240Pd) is lean-Pd CP titanium specified for 240–380 MPa tensile strength, 170 MPa minimum yield or proof strength and 24% minimum elongation in the annealed condition. Typical uses include plate heat exchanger plates and crevice-prone chemical plant parts.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com