JIS H4600 Class 60E TAP6400E Titanium Plate | Ti-6Al-4V ELI

JIS H4600 Class 60E TAP6400E titanium plate is Ti-6Al-4V ELI titanium alloy supplied annealed. It is specified for 825 MPa minimum tensile strength, 755 MPa yield and 10% minimum elongation. Typical uses include medical and dental device material. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
JIS H4600 Class 60E TAP6400E titanium plate, Class 60E (TAP6400E) titanium plate, Ti-6Al-4V ELI titanium alloy plate, JIS H4600 titanium sheet, JIS H4600 Class 60E TAP6400E titanium sheet
Equivalent Grades:
UNS R56407, ASTM B265 Gr.23, ASME SB-265 Gr.23, GB/T TC4ELI, GOST VT6S (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS H4600 Class 60E TAP6400E titanium plate?

JIS H4600 Class 60E TAP6400E titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 60E is the extra-low-interstitial version of Class 60, with oxygen limited to 0.13% and iron to 0.25%. It trades some strength for better ductility and low-temperature toughness.

This is an alpha-beta titanium alloy. Aluminium strengthens the alpha phase and vanadium or molybdenum stabilises the beta phase, so the structure and properties depend on hot working and heat treatment. Plate is normally supplied mill annealed, giving high strength, good fatigue performance and a strength-to-weight ratio well above that of steels.

Its typical density of about 4.43 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.

SHH STEEL handles Class 60E (TAP6400E) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 23, ASME SB-265 Grade 23, GB/T 3621 TC4ELI.

Material specification for JIS H4600 Class 60E (TAP6400E)

JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.

Ordering item JIS H4600 basis
Standard JIS H 4600 (current 2012 edition)
Class / symbol Class 60E (TAP6400E); state H (hot rolled) or C (cold rolled) as needed, for example TAP6400EH or TAP6400EC
Thickness covered 0.5–75 mm for this class
Condition Annealed; hot rolled (H) or cold rolled (C)
Tests Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered
Certificate Inspection document with chemical and mechanical results

The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.

Chemical composition of JIS H4600 Class 60E (TAP6400E)

Values are maximums except where a range is given. Titanium is the balance.

Element Limit, %
Nitrogen (N) 0.03 max
Carbon (C) 0.08 max
Hydrogen (H) 0.0125 max
Iron (Fe) 0.25 max
Oxygen (O) 0.13 max
Aluminium (Al) 5.50–6.50
Vanadium (V) 3.50–4.50
Other elements, each 0.10 max
Other elements, total 0.40 max
Titanium (Ti) Balance

Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.

Mechanical properties of JIS H4600 Class 60E (TAP6400E)

The values below are the requirements for Class 60E (TAP6400E) plate in the annealed condition.

Property Requirement
Thickness range covered 0.5–75 mm
Tensile strength 825 MPa min
Proof stress (0.2%) 755 MPa min
Elongation, min 10%
Bend test (0.5 mm to under 5 mm) 105°, inside radius 5.5 × thickness under 1.5 mm; 6 × thickness for 1.5 mm to under 5 mm; no cracks on the outside

Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.

For pressure equipment, design stresses come from the applicable code, not from the plate standard.

Delivery condition, finish and marking

JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.

  • Condition: Annealed; hot rolled (H) or cold rolled (C)
  • Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
  • Marking: class or symbol, size, heat or lot number and manufacturer, per the order
  • Packing: suitable for transport and to prevent iron contamination of the surface

Plate is supplied annealed. Solution treating and ageing, where wanted, is normally done on the part and its properties are agreed separately. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.

Welding and fabrication of Class 60E (TAP6400E) titanium plate

Class 60E (TAP6400E) can be welded by gas tungsten arc, plasma arc, electron beam and laser processes, but it needs more control than CP titanium.

  • Shield the weld, heat-affected zone and root with inert gas until below about 400 °C
  • Use qualified procedures and matching or engineer-approved filler metal
  • Expect lower weld-zone ductility than in the base plate; stress relief after welding is common
  • Clean joints thoroughly and avoid iron contamination

Cold formability is limited. Most forming of alpha-beta plate is done hot or by creep forming, and machining needs sharp tools, rigid set-ups and generous coolant.

Plan machining around the low thermal conductivity of the alloy: heat stays at the tool edge, so cutting speeds are low and coolant flow is high. Avoid interrupted light cuts that work-harden the surface, and keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.

Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Class 60E (TAP6400E) titanium plate

Typical uses of Class 60E (TAP6400E) plate include:

  • Medical and dental device material
  • Cryogenic parts
  • Fracture-critical structures
  • High-toughness machined parts

Alpha-beta alloys resist seawater and many oxidizing media well, but they are less resistant than CP titanium in hot reducing acids. They are not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. Maximum service temperature and fatigue design values come from the applicable design code, not from the plate specification.

When selecting Class 60E (TAP6400E), compare it with Class 50 (TAP1500), Class 61 (TAP3250), Class 61F (TAP3250F). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Class 60E (TAP6400E) with other JIS H4600 grades

The grades below are the closest neighbours of Class 60E (TAP6400E) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Class 50 (TAP1500) 345 MPa min 215 MPa min 20% Ti-1.5Al, heat- and seawater-resistant
Class 61 (TAP3250) 620 MPa min 485 MPa min 15% Ti-3Al-2.5V, weldable and cold-workable
Class 61F (TAP3250F) 650 MPa min 600 MPa min 10% Ti-3Al-2.5V with S and rare earths, free-machining
Class 60 (TAP6400) 895 MPa min 825 MPa min 10% Ti-6Al-4V, high strength
Class 60E (TAP6400E) 825 MPa min 755 MPa min 10% Ti-6Al-4V ELI, low-temperature toughness
Class 80 (TAP4220) 640–900 MPa 850 MPa max 10% Ti-4Al-22V beta alloy, cold formable

A higher strength level is not automatically better. Interstitial limits, toughness, bend radius and fatigue behaviour differ between grades, so changes need engineer approval.

JIS H4600 Class 60E (TAP6400E) equivalent grades

The designations below are commonly compared with JIS H4600 Class 60E (TAP6400E). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to JIS H4600 Class 60E (TAP6400E)
ASTM B265 Grade 23 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 23 ASME Code version of the ASTM grade; ordered for pressure equipment
GB/T 3621 TC4ELI Close equivalent; confirm grade name and limits in the ordered edition
GOST 22178 VT6S Approximate; GOST limits and sheet scope differ
UNS R56407 Same unified number as ASTM Grade 23

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Class 60E (TAP6400E) titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to JIS H4600 Class 60E (TAP6400E) with the H or C finish you need
  • Certificates are checked against the JIS tensile range, proof stress and bend requirement
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for JIS H4600 Class 60E (TAP6400E) plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material JIS H4600 Class 60E (TAP6400E), with H or C suffix
Product form Plate, sheet or strip; hot or cold rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What does the symbol TAP6400E mean in JIS H4600?
TAP identifies structural titanium alloy plate or sheet, and the digits show the nominal alloy content, for example 6400 for Ti-6Al-4V. A final H means hot rolled and C means cold rolled, for example TAP6400EH or TAP6400EC.
What is the tensile strength of JIS H4600 Class 60E (TAP6400E) titanium plate?
The requirement is 825 MPa minimum. The 0.2% proof or yield strength is 755 MPa minimum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
What is Class 60E (TAP6400E) mainly used for?
Typical uses include medical and dental device material, cryogenic parts and fracture-critical structures. The design engineer should confirm the grade for the actual service.
What thickness does JIS H4600 Class 60E (TAP6400E) cover?
The property table for this class covers 0.5–75 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
What should I send for a quotation?
Send JIS H4600 Class 60E (TAP6400E), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for JIS H4600 Class 60E TAP6400E titanium plate

JIS H4600 Class 60E (TAP6400E) is Ti-6Al-4V ELI titanium alloy specified for 825 MPa minimum tensile strength, 755 MPa minimum yield or proof strength and 10% minimum elongation in the annealed condition. Typical uses include medical and dental device material and cryogenic parts.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X