JIS H4600 Class 3 TP480 Titanium Plate | Commercially Pure Titanium

JIS H4600 Class 3 TP480 titanium plate is commercially pure titanium supplied annealed. It is specified for 480–620 MPa tensile strength, 345 MPa yield and 18% minimum elongation. Typical uses include pressure-containing chemical plant parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
JIS H4600 Class 3 TP480 titanium plate, Class 3 (TP480) titanium plate, commercially pure titanium plate, JIS H4600 titanium sheet, JIS H4600 Class 3 TP480 titanium sheet
Equivalent Grades:
UNS R50550, ASTM B265 Gr.3, ASME SB-265 Gr.3, GB/T TA3G, ISO 5832-2 Gr.3, 3.7055
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS H4600 Class 3 TP480 titanium plate?

JIS H4600 Class 3 TP480 titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 3 allows 0.30% oxygen and gives a 480–620 MPa tensile range, for parts that need more strength than Class 2 with moderate forming.

Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.

SHH STEEL handles Class 3 (TP480) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 3, ASME SB-265 Grade 3, GB/T 3621 TA3G.

Material specification for JIS H4600 Class 3 (TP480)

JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.

Ordering item JIS H4600 basis
Standard JIS H 4600 (current 2012 edition)
Class / symbol Class 3 (TP480); state H (hot rolled) or C (cold rolled) as needed, for example TP480H or TP480C
Thickness covered 0.2–50 mm for this class
Condition Annealed; hot rolled (H) or cold rolled (C)
Tests Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered
Certificate Inspection document with chemical and mechanical results

The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.

Chemical composition of JIS H4600 Class 3 (TP480)

Values are maximums except where a range is given. Titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.08 max
Hydrogen (H) 0.013 max
Iron (Fe) 0.30 max
Oxygen (O) 0.30 max
Titanium (Ti) Balance

Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.

Mechanical properties of JIS H4600 Class 3 (TP480)

The values below are the requirements for Class 3 (TP480) plate in the annealed condition.

Property Requirement
Thickness range covered 0.2–50 mm
Tensile strength 480–620 MPa
Proof stress (0.2%) 345 MPa min
Elongation, min 18%
Bend test (0.5 mm to under 5 mm) 180°, inside radius 3 × thickness; no cracks on the outside

Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.

For pressure equipment, design stresses come from the applicable code, not from the plate standard.

Delivery condition, finish and marking

JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.

  • Condition: Annealed; hot rolled (H) or cold rolled (C)
  • Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
  • Marking: class or symbol, size, heat or lot number and manufacturer, per the order
  • Packing: suitable for transport and to prevent iron contamination of the surface

CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.

Welding and fabrication of Class 3 (TP480) titanium plate

Class 3 (TP480) is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.

  • Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
  • Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
  • Use matching CP filler metal unless the design engineer specifies otherwise
  • Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
  • Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up

Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.

For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.

Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Class 3 (TP480) titanium plate

Typical uses of Class 3 (TP480) plate include:

  • Pressure-containing chemical plant parts
  • Marine and seawater equipment
  • Higher-strength heat exchanger parts
  • Industrial structures in corrosive service

Formability is lower than Class 1 and Class 2. Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.

When selecting Class 3 (TP480), compare it with Class 1 (TP270), Class 2 (TP340), Class 4 (TP550). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Class 3 (TP480) with other JIS H4600 grades

The grades below are the closest neighbours of Class 3 (TP480) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Class 1 (TP270) 270–410 MPa 165 MPa min 27% Softest JIS CP class, best formability
Class 2 (TP340) 340–510 MPa 215 MPa min 23% Most common JIS CP class
Class 3 (TP480) 480–620 MPa 345 MPa min 18% Higher-strength JIS CP class
Class 4 (TP550) 550–750 MPa 485 MPa min 15% Highest-strength JIS CP class

A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.

JIS H4600 Class 3 (TP480) equivalent grades

The designations below are commonly compared with JIS H4600 Class 3 (TP480). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to JIS H4600 Class 3 (TP480)
ASTM B265 Grade 3 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 3 ASME Code version of the ASTM grade; ordered for pressure equipment
GB/T 3621 TA3G Close equivalent; confirm grade name and limits in the ordered edition
ISO 5832-2 Grade 3 Implant-grade counterpart; medical scope and tighter controls
UNS R50550 Same unified number as ASTM Grade 3
DIN / EN material number 3.7055 (Ti 3) Close CP equivalent

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Class 3 (TP480) titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to JIS H4600 Class 3 (TP480) with the H or C finish you need
  • Certificates are checked against the JIS tensile range, proof stress and bend requirement
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for JIS H4600 Class 3 (TP480) plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material JIS H4600 Class 3 (TP480), with H or C suffix
Product form Plate, sheet or strip; hot or cold rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What does the symbol TP480 mean in JIS H4600?
TP identifies plate or sheet, the number is the minimum tensile strength level in MPa, and any letters show the alloying addition. A final H means hot rolled and C means cold rolled, for example TP480H or TP480C.
What is the tensile strength of JIS H4600 Class 3 (TP480) titanium plate?
The requirement is 480–620 MPa. The 0.2% proof or yield strength is 345 MPa minimum. Minimum elongation is 18%. Values apply to the condition and thickness range stated in the standard.
What is Class 3 (TP480) mainly used for?
Typical uses include pressure-containing chemical plant parts, marine and seawater equipment and higher-strength heat exchanger parts. Formability is lower than Class 1 and Class 2.
What thickness does JIS H4600 Class 3 (TP480) cover?
The property table for this class covers 0.2–50 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
What should I send for a quotation?
Send JIS H4600 Class 3 (TP480), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for JIS H4600 Class 3 TP480 titanium plate

JIS H4600 Class 3 (TP480) is commercially pure titanium specified for 480–620 MPa tensile strength, 345 MPa minimum yield or proof strength and 18% minimum elongation in the annealed condition. Typical uses include pressure-containing chemical plant parts and marine and seawater equipment.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X