JIS H4600 Class 12 TP340Pd Titanium Plate | Pd-Bearing CP Titanium

JIS H4600 Class 12 TP340Pd titanium plate is Pd-bearing CP titanium supplied annealed. It is specified for 340–510 MPa tensile strength, 215 MPa yield and 23% minimum elongation. Typical uses include plate heat exchangers in reducing-acid or hot-chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
JIS H4600 Class 12 TP340Pd titanium plate, Class 12 (TP340Pd) titanium plate, Pd-bearing CP titanium plate, JIS H4600 titanium sheet, JIS H4600 Class 12 TP340Pd titanium sheet
Equivalent Grades:
UNS R52400, ASTM B265 Gr.7, ASME SB-265 Gr.7, GB/T TA9, 3.7235
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS H4600 Class 12 TP340Pd titanium plate?

JIS H4600 Class 12 TP340Pd titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 12 is JIS Class 2 chemistry with 0.12–0.25% palladium. The palladium improves resistance to hydrochloric and sulfuric acid and to crevice corrosion, at the same 340–510 MPa tensile range as Class 2.

This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.

SHH STEEL handles Class 12 (TP340Pd) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 7, ASME SB-265 Grade 7, ASTM B265 Grade 7H.

Material specification for JIS H4600 Class 12 (TP340Pd)

JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.

Ordering item JIS H4600 basis
Standard JIS H 4600 (current 2012 edition)
Class / symbol Class 12 (TP340Pd); state H (hot rolled) or C (cold rolled) as needed, for example TP340PdH or TP340PdC
Thickness covered 0.2–50 mm for this class
Condition Annealed; hot rolled (H) or cold rolled (C)
Tests Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered
Certificate Inspection document with chemical and mechanical results

The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.

Chemical composition of JIS H4600 Class 12 (TP340Pd)

Values are maximums except where a range is given. Titanium is the balance.

Element Limit, %
Nitrogen (N) 0.03 max
Carbon (C) 0.08 max
Hydrogen (H) 0.013 max
Iron (Fe) 0.25 max
Oxygen (O) 0.20 max
Palladium (Pd) 0.12–0.25
Titanium (Ti) Balance

Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.

Mechanical properties of JIS H4600 Class 12 (TP340Pd)

The values below are the requirements for Class 12 (TP340Pd) plate in the annealed condition.

Property Requirement
Thickness range covered 0.2–50 mm
Tensile strength 340–510 MPa
Proof stress (0.2%) 215 MPa min
Elongation, min 23%
Bend test (0.5 mm to under 5 mm) 180°, inside radius 2 × thickness; no cracks on the outside

Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.

For pressure equipment, design stresses come from the applicable code, not from the plate standard.

Delivery condition, finish and marking

JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.

  • Condition: Annealed; hot rolled (H) or cold rolled (C)
  • Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
  • Marking: class or symbol, size, heat or lot number and manufacturer, per the order
  • Packing: suitable for transport and to prevent iron contamination of the surface

The grade is supplied annealed and is not strengthened by heat treatment. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.

Welding and fabrication of Class 12 (TP340Pd) titanium plate

Class 12 (TP340Pd) is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.

  • Use trailing shields and back purging until the metal cools below about 400 °C
  • Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
  • Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
  • Check weld colour and reject heavily discoloured welds

Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.

For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.

Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Class 12 (TP340Pd) titanium plate

Typical uses of Class 12 (TP340Pd) plate include:

  • Plate heat exchangers in reducing-acid or hot-chloride service
  • Reaction vessels and columns
  • Crevice-prone flange and gasket areas
  • Chemical process equipment where unalloyed titanium is marginal

Palladium adds cost; leaner Pd or Ru classes are alternatives to evaluate. The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.

When selecting Class 12 (TP340Pd), compare it with Class 11 (TP270Pd), Class 13 (TP480Pd), Class 17 (TP240Pd). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Class 12 (TP340Pd) with other JIS H4600 grades

The grades below are the closest neighbours of Class 12 (TP340Pd) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Class 11 (TP270Pd) 270–410 MPa 165 MPa min 27% Pd-bearing Class 1
Class 12 (TP340Pd) 340–510 MPa 215 MPa min 23% Pd-bearing Class 2
Class 13 (TP480Pd) 480–620 MPa 345 MPa min 18% Pd-bearing Class 3
Class 17 (TP240Pd) 240–380 MPa 170 MPa min 24% Lean-Pd (0.05% Pd), lower cost
Class 18 (TP345Pd) 345–515 MPa 275 MPa min 20% Lean-Pd (0.05% Pd), lower cost

The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.

JIS H4600 Class 12 (TP340Pd) equivalent grades

The designations below are commonly compared with JIS H4600 Class 12 (TP340Pd). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to JIS H4600 Class 12 (TP340Pd)
ASTM B265 Grade 7 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 7 ASME Code version of the ASTM grade; ordered for pressure equipment
ASTM B265 Grade 7H Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 7H ASME Code version of the ASTM grade; ordered for pressure equipment
GB/T 3621 TA9 Close equivalent; confirm grade name and limits in the ordered edition
UNS R52400 Same unified number as ASTM Grade 7
DIN / EN material number 3.7235 (Ti 2 Pd) Close equivalent

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Class 12 (TP340Pd) titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to JIS H4600 Class 12 (TP340Pd) with the H or C finish you need
  • Certificates are checked against the JIS tensile range, proof stress and bend requirement
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for JIS H4600 Class 12 (TP340Pd) plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material JIS H4600 Class 12 (TP340Pd), with H or C suffix
Product form Plate, sheet or strip; hot or cold rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What does the symbol TP340Pd mean in JIS H4600?
TP identifies plate or sheet, the number is the minimum tensile strength level in MPa, and any letters show the alloying addition. A final H means hot rolled and C means cold rolled, for example TP340PdH or TP340PdC.
What is the tensile strength of JIS H4600 Class 12 (TP340Pd) titanium plate?
The requirement is 340–510 MPa. The 0.2% proof or yield strength is 215 MPa minimum. Minimum elongation is 23%. Values apply to the condition and thickness range stated in the standard.
What is Class 12 (TP340Pd) mainly used for?
Typical uses include plate heat exchangers in reducing-acid or hot-chloride service, reaction vessels and columns and crevice-prone flange and gasket areas. Palladium adds cost; leaner Pd or Ru classes are alternatives to evaluate.
What thickness does JIS H4600 Class 12 (TP340Pd) cover?
The property table for this class covers 0.2–50 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
What should I send for a quotation?
Send JIS H4600 Class 12 (TP340Pd), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for JIS H4600 Class 12 TP340Pd titanium plate

JIS H4600 Class 12 (TP340Pd) is Pd-bearing CP titanium specified for 340–510 MPa tensile strength, 215 MPa minimum yield or proof strength and 23% minimum elongation in the annealed condition. Typical uses include plate heat exchangers in reducing-acid or hot-chloride service and reaction vessels and columns.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X