JIS H4600 Class 23 TP483RN Titanium Plate | Ru-Ni Titanium

JIS H4600 Class 23 TP483RN titanium plate is Ru-Ni titanium supplied annealed. It is specified for 483–630 MPa tensile strength, 380 MPa yield and 18% minimum elongation. Typical uses include chemical plant heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
JIS H4600 Class 23 TP483RN titanium plate, Class 23 (TP483RN) titanium plate, Ru-Ni titanium plate, JIS H4600 titanium sheet, JIS H4600 Class 23 TP483RN titanium sheet
Equivalent Grades:
UNS R53415, ASTM B265 Gr.15, ASME SB-265 Gr.15
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS H4600 Class 23 TP483RN titanium plate?

JIS H4600 Class 23 TP483RN titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 23 contains 0.04–0.06% ruthenium and 0.40–0.60% nickel. These additions improve resistance to hydrochloric and sulfuric acid and to crevice corrosion; tensile range is 483–630 MPa.

This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.

SHH STEEL handles Class 23 (TP483RN) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 15, ASME SB-265 Grade 15.

Material specification for JIS H4600 Class 23 (TP483RN)

JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.

Ordering item JIS H4600 basis
Standard JIS H 4600 (current 2012 edition)
Class / symbol Class 23 (TP483RN); state H (hot rolled) or C (cold rolled) as needed, for example TP483RNH or TP483RNC
Thickness covered 0.2–50 mm for this class
Condition Annealed; hot rolled (H) or cold rolled (C)
Tests Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered
Certificate Inspection document with chemical and mechanical results

The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.

Chemical composition of JIS H4600 Class 23 (TP483RN)

Values are maximums except where a range is given. Titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.08 max
Hydrogen (H) 0.015 max
Iron (Fe) 0.30 max
Oxygen (O) 0.25 max
Nickel (Ni) 0.40–0.60
Ruthenium (Ru) 0.04–0.06
Titanium (Ti) Balance

Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.

Mechanical properties of JIS H4600 Class 23 (TP483RN)

The values below are the requirements for Class 23 (TP483RN) plate in the annealed condition.

Property Requirement
Thickness range covered 0.2–50 mm
Tensile strength 483–630 MPa
Proof stress (0.2%) 380 MPa min
Elongation, min 18%
Bend test (0.5 mm to under 5 mm) 180°, inside radius 3 × thickness; no cracks on the outside

Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.

For pressure equipment, design stresses come from the applicable code, not from the plate standard.

Delivery condition, finish and marking

JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.

  • Condition: Annealed; hot rolled (H) or cold rolled (C)
  • Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
  • Marking: class or symbol, size, heat or lot number and manufacturer, per the order
  • Packing: suitable for transport and to prevent iron contamination of the surface

The grade is supplied annealed and is not strengthened by heat treatment. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.

Welding and fabrication of Class 23 (TP483RN) titanium plate

Class 23 (TP483RN) is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.

  • Use trailing shields and back purging until the metal cools below about 400 °C
  • Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
  • Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
  • Check weld colour and reject heavily discoloured welds

Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.

For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.

Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Class 23 (TP483RN) titanium plate

Typical uses of Class 23 (TP483RN) plate include:

  • Chemical plant heat exchangers
  • Reducing-acid process equipment
  • Crevice-prone flanges and tube sheets
  • Salt and brine plant

The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.

When selecting Class 23 (TP483RN), compare it with Class 14 (TP345NPRC), Class 15 (TP450NPRC), Class 19 (TP345PCo). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Class 23 (TP483RN) with other JIS H4600 grades

The grades below are the closest neighbours of Class 23 (TP483RN) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Class 14 (TP345NPRC) 345 MPa min 275–450 MPa 20% Ni-Pd-Ru-Cr, lower-cost crevice resistance
Class 15 (TP450NPRC) 450 MPa min 380–550 MPa 18% Ni-Pd-Ru-Cr, lower-cost crevice resistance
Class 19 (TP345PCo) 345–515 MPa 275 MPa min 20% Pd-Co, higher strength
Class 20 (TP450PCo) 450–590 MPa 380 MPa min 18% Pd-Co, higher strength
Class 21 (TP275RN) 275–450 MPa 170 MPa min 24% Ru-Ni, reducing-acid and crevice resistance
Class 22 (TP410RN) 410–530 MPa 275 MPa min 20% Ru-Ni, reducing-acid and crevice resistance
Class 23 (TP483RN) 483–630 MPa 380 MPa min 18% Ru-Ni, reducing-acid and crevice resistance

The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.

JIS H4600 Class 23 (TP483RN) equivalent grades

The designations below are commonly compared with JIS H4600 Class 23 (TP483RN). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to JIS H4600 Class 23 (TP483RN)
ASTM B265 Grade 15 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 15 ASME Code version of the ASTM grade; ordered for pressure equipment
UNS R53415 Same unified number as ASTM Grade 15

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Class 23 (TP483RN) titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to JIS H4600 Class 23 (TP483RN) with the H or C finish you need
  • Certificates are checked against the JIS tensile range, proof stress and bend requirement
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for JIS H4600 Class 23 (TP483RN) plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material JIS H4600 Class 23 (TP483RN), with H or C suffix
Product form Plate, sheet or strip; hot or cold rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What does the symbol TP483RN mean in JIS H4600?
TP identifies plate or sheet, the number is the minimum tensile strength level in MPa, and any letters show the alloying addition. A final H means hot rolled and C means cold rolled, for example TP483RNH or TP483RNC.
What is the tensile strength of JIS H4600 Class 23 (TP483RN) titanium plate?
The requirement is 483–630 MPa. The 0.2% proof or yield strength is 380 MPa minimum. Minimum elongation is 18%. Values apply to the condition and thickness range stated in the standard.
What is Class 23 (TP483RN) mainly used for?
Typical uses include chemical plant heat exchangers, reducing-acid process equipment and crevice-prone flanges and tube sheets. The design engineer should confirm the grade for the actual service.
What thickness does JIS H4600 Class 23 (TP483RN) cover?
The property table for this class covers 0.2–50 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
What should I send for a quotation?
Send JIS H4600 Class 23 (TP483RN), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for JIS H4600 Class 23 TP483RN titanium plate

JIS H4600 Class 23 (TP483RN) is Ru-Ni titanium specified for 483–630 MPa tensile strength, 380 MPa minimum yield or proof strength and 18% minimum elongation in the annealed condition. Typical uses include chemical plant heat exchangers and reducing-acid process equipment.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X