JIS H4600 Class 80 TAP4220 Titanium Plate | Ti-4Al-22V

JIS H4600 Class 80 TAP4220 titanium plate is Ti-4Al-22V titanium alloy supplied solution treated. It is specified for 640–900 MPa tensile strength, 850 MPa maximum yield and 10% minimum elongation. Typical uses include golf club heads. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
JIS H4600 Class 80 TAP4220 titanium plate, Class 80 (TAP4220) titanium plate, Ti-4Al-22V titanium alloy plate, JIS H4600 titanium sheet, JIS H4600 Class 80 TAP4220 titanium sheet
Equivalent Grades:
No direct equivalent; see the Equivalent Material Grade table
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is JIS H4600 Class 80 TAP4220 titanium plate?

JIS H4600 Class 80 TAP4220 titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 80 is Ti-4Al-22V, a beta alloy with excellent cold workability and a 640–900 MPa tensile range in the supplied condition.

This is a beta or metastable beta titanium alloy. Large additions of beta-stabilising elements such as vanadium, molybdenum, chromium or niobium keep a body-centred cubic structure after solution treatment. That structure is cold formable, and many beta alloys can then be aged to very high strength.

The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.

SHH STEEL handles Class 80 (TAP4220) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply.

Material specification for JIS H4600 Class 80 (TAP4220)

JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.

Ordering item JIS H4600 basis
Standard JIS H 4600 (current 2012 edition)
Class / symbol Class 80 (TAP4220); state H (hot rolled) or C (cold rolled) as needed, for example TAP4220H or TAP4220C
Thickness covered 0.6 to under 5 mm for this class
Condition Solution treated
Tests Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered
Certificate Inspection document with chemical and mechanical results

The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.

Chemical composition of JIS H4600 Class 80 (TAP4220)

Values are maximums except where a range is given. Titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.10 max
Hydrogen (H) 0.015 max
Iron (Fe) 1.00 max
Oxygen (O) 0.25 max
Aluminium (Al) 3.50–4.50
Vanadium (V) 20.0–23.0
Titanium (Ti) Balance

Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.

Mechanical properties of JIS H4600 Class 80 (TAP4220)

The values below are the requirements for Class 80 (TAP4220) plate in the solution treated condition.

Property Requirement
Thickness range covered 0.6 to under 5 mm
Tensile strength 640–900 MPa
Proof stress (0.2%) 850 MPa max
Elongation, min 10%
Bend test (0.5 mm to under 5 mm) 180°, inside radius 5.5 × thickness under 1.5 mm; 6 × thickness for 1.5 mm to under 5 mm; no cracks on the outside

Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the solution treated condition at room temperature.

For pressure equipment, design stresses come from the applicable code, not from the plate standard.

Delivery condition, finish and marking

JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.

  • Condition: Solution treated
  • Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
  • Marking: class or symbol, size, heat or lot number and manufacturer, per the order
  • Packing: suitable for transport and to prevent iron contamination of the surface

Material is normally purchased solution treated. Aged properties are not fixed by the plate specification and must be agreed between purchaser and manufacturer. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.

Welding and fabrication of Class 80 (TAP4220) titanium plate

Class 80 (TAP4220) can be welded by gas tungsten arc, electron beam or laser with full inert-gas shielding, but weld properties depend strongly on the heat treatment that follows.

  • Shield the weld, heat-affected zone and root until below about 400 °C
  • Agree the post-weld heat treatment with the designer, since ageing response differs between weld and base metal
  • Use qualified procedures and approved filler metal
  • Keep joints clean and free of iron contamination

In the solution-treated condition beta alloys can be cold formed more easily than alpha-beta alloys. Forming is normally done before ageing.

Beta alloys are machined with sharp carbide tools, low speeds and generous coolant, and tool wear is higher in the aged condition, so heavy machining is often done before ageing. Keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.

Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Class 80 (TAP4220) titanium plate

Typical uses of Class 80 (TAP4220) plate include:

  • Golf club heads
  • Eyeglass frames
  • Fishing tackle and consumer products
  • Cold-formed springs and clips

Its high vanadium content makes it denser than Ti-6Al-4V. Beta alloys have good resistance to many media, but they are not suited to hydrofluoric acid, fluoride-bearing media or dry chlorine. They are denser than Ti-6Al-4V, and aged properties, toughness and service temperature limits must be agreed for the part.

When selecting Class 80 (TAP4220), compare it with Class 50 (TAP1500), Class 61 (TAP3250), Class 61F (TAP3250F). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Class 80 (TAP4220) with other JIS H4600 grades

The grades below are the closest neighbours of Class 80 (TAP4220) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Class 50 (TAP1500) 345 MPa min 215 MPa min 20% Ti-1.5Al, heat- and seawater-resistant
Class 61 (TAP3250) 620 MPa min 485 MPa min 15% Ti-3Al-2.5V, weldable and cold-workable
Class 61F (TAP3250F) 650 MPa min 600 MPa min 10% Ti-3Al-2.5V with S and rare earths, free-machining
Class 60 (TAP6400) 895 MPa min 825 MPa min 10% Ti-6Al-4V, high strength
Class 60E (TAP6400E) 825 MPa min 755 MPa min 10% Ti-6Al-4V ELI, low-temperature toughness
Class 80 (TAP4220) 640–900 MPa 850 MPa max 10% Ti-4Al-22V beta alloy, cold formable

Beta alloys are usually chosen for formability before ageing and for high aged strength, not for corrosion alone. Compare the agreed heat-treated properties before changing grade.

JIS H4600 Class 80 (TAP4220) equivalent grades

The designations below are commonly compared with JIS H4600 Class 80 (TAP4220). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to JIS H4600 Class 80 (TAP4220)
GB/T 3620.1 designation TB13 (Ti-4Al-22V) Similar nominal composition

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Class 80 (TAP4220) titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to JIS H4600 Class 80 (TAP4220) with the H or C finish you need
  • Certificates are checked against the JIS tensile range, proof stress and bend requirement
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for JIS H4600 Class 80 (TAP4220) plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material JIS H4600 Class 80 (TAP4220), with H or C suffix
Product form Plate, sheet or strip; hot or cold rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

What does the symbol TAP4220 mean in JIS H4600?
TAP identifies structural titanium alloy plate or sheet, and the digits show the nominal alloy content, for example 6400 for Ti-6Al-4V. A final H means hot rolled and C means cold rolled, for example TAP4220H or TAP4220C.
What is the tensile strength of JIS H4600 Class 80 (TAP4220) titanium plate?
The requirement is 640–900 MPa. The 0.2% proof or yield strength is 850 MPa maximum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
What is Class 80 (TAP4220) mainly used for?
Typical uses include golf club heads, eyeglass frames and fishing tackle and consumer products. Its high vanadium content makes it denser than Ti-6Al-4V.
What thickness does JIS H4600 Class 80 (TAP4220) cover?
The property table for this class covers 0.6 to under 5 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
What should I send for a quotation?
Send JIS H4600 Class 80 (TAP4220), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for JIS H4600 Class 80 TAP4220 titanium plate

JIS H4600 Class 80 (TAP4220) is Ti-4Al-22V titanium alloy specified for 640–900 MPa tensile strength, 850 MPa maximum yield or proof strength and 10% minimum elongation in the solution treated condition. Typical uses include golf club heads and eyeglass frames.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X