JIS H4600 Class 4 TP550 Titanium Plate | Commercially Pure Titanium
What is JIS H4600 Class 4 TP550 titanium plate?
JIS H4600 Class 4 TP550 titanium plate is made to JIS H4600, the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. Class 4 is the strongest unalloyed class in JIS H4600, with 0.40% oxygen, 0.50% iron and a 550–750 MPa tensile range.
Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.
Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
The standard groups its classes into unalloyed titanium (Classes 1 to 4), corrosion-resistant titanium alloys with palladium, ruthenium, nickel, cobalt, chromium or tantalum, and structural alloys in the 50, 60 and 80 series. Each class has a matching symbol used on drawings and certificates.
SHH STEEL handles Class 4 (TP550) plate enquiries within its range of titanium alloy plates and sheets, checking the ordered JIS H4600 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 4, ASME SB-265 Grade 4, GB/T 3621 TA4G.
Material specification for JIS H4600 Class 4 (TP550)
JIS H 4600 is the Japanese Industrial Standard for titanium and titanium alloy sheets, plates and strips. It assigns each material a class number and a symbol; for plate and sheet the symbol starts with TP for unalloyed and corrosion-resistant titanium alloys and TAP for structural titanium alloys, and a final H or C indicates hot-rolled or cold-rolled finish.
| Ordering item | JIS H4600 basis |
|---|---|
| Standard | JIS H 4600 (current 2012 edition) |
| Class / symbol | Class 4 (TP550); state H (hot rolled) or C (cold rolled) as needed, for example TP550H or TP550C |
| Thickness covered | 0.2–50 mm for this class |
| Condition | Annealed; hot rolled (H) or cold rolled (C) |
| Tests | Chemical composition, tensile test, bend test for 0.5 mm to under 5 mm, and internal soundness if ordered |
| Certificate | Inspection document with chemical and mechanical results |
The bend test applies to material 0.5 mm to under 5 mm thick, and internal soundness testing of the CP and Pd classes is applied only when the purchaser asks for it. State the class, symbol suffix, size, quantity and any agreed surface requirements on the order.
Chemical composition of JIS H4600 Class 4 (TP550)
Values are maximums except where a range is given. Titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.05 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.013 max |
| Iron (Fe) | 0.50 max |
| Oxygen (O) | 0.40 max |
| Titanium (Ti) | Balance |
Analysis is reported on the inspection document. If the order also cites another standard, the tighter of the two limits must be met and stated on the certificate.
Mechanical properties of JIS H4600 Class 4 (TP550)
The values below are the requirements for Class 4 (TP550) plate in the annealed condition.
| Property | Requirement |
|---|---|
| Thickness range covered | 0.2–50 mm |
| Tensile strength | 550–750 MPa |
| Proof stress (0.2%) | 485 MPa min |
| Elongation, min | 15% |
| Bend test (0.5 mm to under 5 mm) | 180°, inside radius 3 × thickness; no cracks on the outside |
Tensile tests are made on specimens taken as specified in the standard. The bend test applies to sheet 0.5 mm to under 5 mm thick, and the bent specimen must show no cracks on the outside of the bend. Values are for the annealed condition at room temperature.
For pressure equipment, design stresses come from the applicable code, not from the plate standard.
Delivery condition, finish and marking
JIS H4600 plates and sheets are supplied hot rolled (symbol suffix H) or cold rolled (suffix C), in the condition required by the class. The appearance must be free of defects harmful in use; acceptance criteria for surface defects and their treatment are agreed between the parties.
- Condition: Annealed; hot rolled (H) or cold rolled (C)
- Finish: hot-rolled and descaled, or cold-rolled finish, as ordered
- Marking: class or symbol, size, heat or lot number and manufacturer, per the order
- Packing: suitable for transport and to prevent iron contamination of the surface
CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. State the symbol with its H or C suffix on the order so the finish and tolerance table are clear.
Welding and fabrication of Class 4 (TP550) titanium plate
Class 4 (TP550) is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.
- Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
- Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
- Use matching CP filler metal unless the design engineer specifies otherwise
- Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
- Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up
Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.
For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
JIS H4600 gives thickness tolerances by finish and thickness. For hot-rolled CP and Pd classes, for example, the tolerance is ±0.36 mm at 3 to under 5 mm and ±1.0 mm at 10 to 15 mm; cold-rolled tolerances are tighter, from ±0.05 mm at 0.2 mm thickness. Width and length tolerances are plus-only, and plate flatness is limited by length.
Sizes wider than 1000 mm, longer than 3000 mm or thicker than 15 mm need agreed tolerances. A one-sided thickness tolerance can be ordered at twice the tabulated value. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Class 4 (TP550) titanium plate
Typical uses of Class 4 (TP550) plate include:
- Load-bearing chemical and marine parts
- Industrial components needing CP corrosion resistance with high strength
- Machined parts from plate
- Secondary aerospace parts where CP titanium is accepted
It is the least formable JIS CP class. Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.
When selecting Class 4 (TP550), compare it with Class 1 (TP270), Class 2 (TP340), Class 3 (TP480). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Class 4 (TP550) with other JIS H4600 grades
The grades below are the closest neighbours of Class 4 (TP550) in JIS H4600. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Class 1 (TP270) | 270–410 MPa | 165 MPa min | 27% | Softest JIS CP class, best formability |
| Class 2 (TP340) | 340–510 MPa | 215 MPa min | 23% | Most common JIS CP class |
| Class 3 (TP480) | 480–620 MPa | 345 MPa min | 18% | Higher-strength JIS CP class |
| Class 4 (TP550) | 550–750 MPa | 485 MPa min | 15% | Highest-strength JIS CP class |
A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.
JIS H4600 Class 4 (TP550) equivalent grades
The designations below are commonly compared with JIS H4600 Class 4 (TP550). They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to JIS H4600 Class 4 (TP550) |
|---|---|---|
| ASTM B265 | Grade 4 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 4 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| GB/T 3621 | TA4G | Close equivalent; confirm grade name and limits in the ordered edition |
| ISO 5832-2 | Grade 4A | Implant-grade counterpart; medical scope and tighter controls |
| ISO 5832-2 | Grade 4B | Implant-grade counterpart; medical scope and tighter controls |
| UNS | R50700 | Same unified number as ASTM Grade 4 |
| DIN / EN material number | 3.7065 (Ti 4) | Close CP equivalent |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Class 4 (TP550) titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to JIS H4600 Class 4 (TP550) with the H or C finish you need
- Certificates are checked against the JIS tensile range, proof stress and bend requirement
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for JIS H4600 Class 4 (TP550) plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | JIS H4600 Class 4 (TP550), with H or C suffix |
| Product form | Plate, sheet or strip; hot or cold rolled |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
What does the symbol TP550 mean in JIS H4600?
- TP identifies plate or sheet, the number is the minimum tensile strength level in MPa, and any letters show the alloying addition. A final H means hot rolled and C means cold rolled, for example TP550H or TP550C.
-
What is the tensile strength of JIS H4600 Class 4 (TP550) titanium plate?
- The requirement is 550–750 MPa. The 0.2% proof or yield strength is 485 MPa minimum. Minimum elongation is 15%. Values apply to the condition and thickness range stated in the standard.
-
What is Class 4 (TP550) mainly used for?
- Typical uses include load-bearing chemical and marine parts, industrial components needing CP corrosion resistance with high strength and machined parts from plate. It is the least formable JIS CP class.
-
What thickness does JIS H4600 Class 4 (TP550) cover?
- The property table for this class covers 0.2–50 mm. The bend test applies from 0.5 mm to under 5 mm, and larger sizes need agreed tolerances.
-
What should I send for a quotation?
- Send JIS H4600 Class 4 (TP550), the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for JIS H4600 Class 4 TP550 titanium plate
JIS H4600 Class 4 (TP550) is commercially pure titanium specified for 550–750 MPa tensile strength, 485 MPa minimum yield or proof strength and 15% minimum elongation in the annealed condition. Typical uses include load-bearing chemical and marine parts and industrial components needing CP corrosion resistance with high strength.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the JIS H4600 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com