Product Showcase
JIS H4600 Titanium Alloys
SHH STEEL offers JIS H4600-compliant TR270C/TP340C titanium and titanium alloy sheets and plates. JIS H4600 specifies dimensions, mechanical properties, and testing for industrial, medical, and aerospace uses. High purity, corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
JIS H4600 Class 18 TP345Pd Titanium Plate | Lean Pd CP Titanium
JIS H4600 Class 18 TP345Pd titanium plate is lean-Pd CP titanium supplied annealed. It is specified for 345–515 MPa tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include plate heat exchanger plates. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 19 TP345PCo Titanium Plate | Pd-Co Titanium
JIS H4600 Class 19 TP345PCo titanium plate is Pd-Co titanium supplied annealed. It is specified for 345–515 MPa tensile strength, 275 MPa yield and 20% minimum elongation. Typical uses include shell-and-tube heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 20 TP450PCo Titanium Plate | Pd-Co Titanium
JIS H4600 Class 20 TP450PCo titanium plate is Pd-Co titanium supplied annealed. It is specified for 450–590 MPa tensile strength, 380 MPa yield and 18% minimum elongation. Typical uses include shell-and-tube heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 21 TP275RN Titanium Plate | Ru-Ni Titanium
JIS H4600 Class 21 TP275RN titanium plate is Ru-Ni titanium supplied annealed. It is specified for 275–450 MPa tensile strength, 170 MPa yield and 24% minimum elongation. Typical uses include chemical plant heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 1 TP270 Titanium Plate | Commercially Pure Titanium
JIS H4600 Class 1 TP270 titanium plate is commercially pure titanium supplied annealed. It is specified for 270–410 MPa tensile strength, 165 MPa yield and 27% minimum elongation. Typical uses include plate heat exchanger plates and pressed parts. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 2 TP340 Titanium Plate | Commercially Pure Titanium
JIS H4600 Class 2 TP340 titanium plate is commercially pure titanium supplied annealed. It is specified for 340–510 MPa tensile strength, 215 MPa yield and 23% minimum elongation. Typical uses include chemical plant vessels and heat exchangers. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 3 TP480 Titanium Plate | Commercially Pure Titanium
JIS H4600 Class 3 TP480 titanium plate is commercially pure titanium supplied annealed. It is specified for 480–620 MPa tensile strength, 345 MPa yield and 18% minimum elongation. Typical uses include pressure-containing chemical plant parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 4 TP550 Titanium Plate | Commercially Pure Titanium
JIS H4600 Class 4 TP550 titanium plate is commercially pure titanium supplied annealed. It is specified for 550–750 MPa tensile strength, 485 MPa yield and 15% minimum elongation. Typical uses include load-bearing chemical and marine parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 11 TP270Pd Titanium Plate | Pd-Bearing CP Titanium
JIS H4600 Class 11 TP270Pd titanium plate is Pd-bearing CP titanium supplied annealed. It is specified for 270–410 MPa tensile strength, 165 MPa yield and 27% minimum elongation. Typical uses include plate heat exchangers in reducing-acid or hot-chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 12 TP340Pd Titanium Plate | Pd-Bearing CP Titanium
JIS H4600 Class 12 TP340Pd titanium plate is Pd-bearing CP titanium supplied annealed. It is specified for 340–510 MPa tensile strength, 215 MPa yield and 23% minimum elongation. Typical uses include plate heat exchangers in reducing-acid or hot-chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.View More -
JIS H4600 Class 13 TP480Pd Titanium Plate | Pd-Bearing CP Titanium
JIS H4600 Class 13 TP480Pd titanium plate is Pd-bearing CP titanium supplied annealed. It is specified for 480–620 MPa tensile strength, 345 MPa yield and 18% minimum elongation. Typical uses include plate heat exchangers in reducing-acid or hot-chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.View More
JIS H4600 Titanium Alloys
Titanium Alloy Plates and Sheets
SHH STEEL, a premier Titanium Alloy Plates and Sheets exporter, produces and exports titanium alloy plates and sheets for aerospace, marine, and chemical industries. Our products, like Grade 2 and Grade 5 (ASTM B265), offer high strength and corrosion resistance. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Grade 5 titanium plates and custom solutions for high-performance projects.
Titanium Alloy Plates and Sheets