GOST 14637 St2sp Steel Plate | St2sp Killed Carbon Steel Plate | GOST 14637 Steel - SHH STEEL

GOST 14637 St2sp Steel Plate | St2sp Killed Carbon Steel Plate

GOST 14637 St2sp (Ст2сп) steel plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this killed grade to the ordered 2024 requirements.
Equivalent Grades:
Commonly compared with GB/T 700 Q215B; not equivalent. Killed (sp) St2sp is not interchangeable with rimmed St2kp or with semi-killed St2ps, even where Table 2 shares a mechanical row. Engineer approval is required for substitution.
Delivery Condition
Category 1 or category 2. Manufactured hot-rolled without heat treatment, or thermomechanically treated, or heat-treated, under clause 7.1.6. Table 2 tensile 330–430 N/mm².
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GOST 14637-2024 St2sp steel plate?

GOST 14637 St2sp Steel Plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026. It was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89.

St2sp is listed in clause 6.1. The sp suffix marks a killed steel. In Table 2, St2sp shares one mechanical row with GOST 14637 St2ps Steel Plate (tensile strength 330–430 N/mm²). A shared mechanical row is not interchangeability: St2sp is killed and St2ps is semi-killed. GOST 14637 St2kp Steel Plate is the rimmed grade in the same carbon class and has a different Table 2 row (320–410 N/mm², with its own yield and elongation). In Table 1, St2sp is listed in category 1 and category 2. Impact toughness is not a specified characteristic in either category for this grade.

SHH STEEL supplies this plate in the GOST 14637 range. We review the ordered category, delivery condition and deoxidation before quoting production and export requirements.

Material specification for GOST 14637 St2sp

The applicable product standard for this page is GOST 14637-2024. The official English title is Rolled plates from nonalloyed steel of general quality. Specifications. Orders should state that edition, the grade St2sp, the category, dimensions, quantity and any agreed options. A grade name without an edition is incomplete. The thickness and width figures below are the standard scope, not a stock promise.

Parameter Detail
Standard GOST 14637-2024; in force from 1 March 2025; replaces GOST 14637-89
Official English title Rolled plates from nonalloyed steel of general quality Specifications
Grade St2sp
Deoxidation Killed (sp), as marked by the designation suffix
Scope, sheets Thickness 4 to 160 mm inclusive; width 500 mm and more
Scope, coils Thickness 4 to 25 mm
Dimensions and tolerances Remaining assortment requirements follow GOST 19903; state thickness accuracy and flatness on the order
Permitted inspection categories 1 or 2 (Table 1). Impact categories 3–7 are not listed for this grade
Chemical composition Shall conform to GOST 380 (clause 7.1.1.1). Category 2 adds chemical-composition control in Table 1. Numeric GOST 380 limits are not tabulated on this page
Tensile properties Table 2 for categories 1–5 and 7
Yield strength σT Table 2 minima, by thickness band, in the row shared with St2ps; see Mechanical Properties
180° bend Table 5; see Mechanical Properties
Impact toughness Not a specified characteristic for the Table 1 categories listed for this grade
Delivery condition Clause 7.1.6: categories 1–5 and 7 without heat treatment (hot-rolled), or thermomechanically treated, or heat-treated. Category 6 is not listed for this grade
Ultrasonic testing By agreement, to a class of GOST 22727; class and volume are not implied by the grade
Acceptance, marking and packaging GOST 7566, with the additions in the 2024 standard

GOST 14637 is a general-quality nonalloyed plate standard. It is not a boiler or pressure-vessel plate standard, and it is not a quality carbon structural plate standard. Do not copy figures from those systems onto a GOST 14637 order.

Chemical composition of GOST 14637-2024 St2sp

Clause 7.1.1.1 of GOST 14637-2024 requires the chemical composition of the steel by ladle analysis of the ladle sample, and the permissible deviations in the finished product, to conform to GOST 380. This page does not tabulate GOST 380 heat-analysis limits. Confirm every chemistry cell against the applicable official GOST 380 table. This page is not a substitute for that table.

In Table 1, category 1 does not specify or control chemical composition; category 2 does. Order category 2 when chemistry is to be a controlled characteristic. In either case, ladle analysis and product deviations shall conform to GOST 380.

Clause 7.1.1.2 permits manufacture without a lower limit on carbon and manganese, except for plate intended for shipbuilding, wagon-building or welded cylinders, provided the mechanical properties of this standard are met. State that option on the order if it is required.

On purchaser request, clause 7.1.1.4 tightens sulphur and phosphorus for categories 1–5 of this grade to S not more than 0.040 % and P not more than 0.030 %. For categories 6 and 7, each of these elements shall not exceed 0.025 %; those categories are not listed for this grade in Table 1. If the tighter 7.1.1.4 limits are required, state them on the order.

For subsequent hot-dip galvanizing, clause 7.1.1.5 allows agreed silicon classes. Classes B (silicon 0.14 % to 0.25 %) and D (silicon 0.25 % to 0.35 %) are the classes written for killed (sp) steel. Class A is written for rimmed (kp) steel and is not the class for this killed grade. Galvanizing class is an agreed option, not a default.

A maximum sign is an upper limit, not a target addition. Product-analysis deviations belonging to GOST 380 must not be used to widen ladle-analysis order limits. Numeric GOST 380 element ranges are not tabulated on this page.

Mechanical properties of GOST 14637-2024 St2sp

Clause 7.1.7.1 requires the tensile properties of plate in categories 1–5 and 7 to meet Table 2. The values below are from GOST 14637-2024 Table 2. Units are N/mm² for strength (the unit used in the 2024 tables) and % for elongation δ5. Table 2 heading is “not less than or within limits.”

Property Thickness Requirement (Table 2)
Tensile strength σB, N/mm² All thicknesses in the 2024 scope 330–430
Yield strength σT, N/mm² ≤20 mm ≥225
Yield strength σT, N/mm² >20 mm to 40 mm inclusive ≥215
Yield strength σT, N/mm² >40 mm to 100 mm inclusive ≥205
Yield strength σT, N/mm² >100 mm ≥195
Elongation δ5, % ≤20 mm ≥32
Elongation δ5, % >20 mm to 40 mm inclusive ≥31
Elongation δ5, % >40 mm ≥29

This Table 2 row is shared by St2sp and GOST 14637 St2ps Steel Plate. A shared row is not interchangeability: the two grades differ by deoxidation (killed against semi-killed). GOST 14637 St2kp Steel Plate has a different Table 2 row (320–410 N/mm², with lower yield minima and higher elongation). Do not take figures from that rimmed row, and do not take yield or tensile values from another product standard.

Table 2 footnotes that apply when the corresponding cell is a specified value include the following. For coil plate of thickness over 12 mm to 25 mm inclusive, the mechanical-property norms are optional for two years from the date of introduction of the 2024 standard (1 March 2025); results are stated in the quality document. The upper tensile-strength limit may be increased by not more than 50 N/mm² while the other mechanical-property norms are observed, and by agreement with the purchaser without limiting the upper bound. By agreement, for thickness over 20 mm, the yield value may be reduced by 10 N/mm². Table 2 also permits a stated reduction of elongation for thinner plate: for thickness up to 8 mm inclusive, by 1 % absolute for each millimetre of thickness reduction; for thickness over 8 mm, by 1 % absolute. Confirm the application of this footnote against the official table when thin plate is ordered.

Clause 7.1.8 requires the plate to withstand a 180° cold bend on a mandrel of the diameter in Table 5. At the bend there shall be no fracture, delamination or cracks.

Property Thickness (a = plate thickness) Requirement (Table 5)
180° cold bend, mandrel diameter d ≤20 mm d = 1.5a
180° cold bend, mandrel diameter d >20 mm to 40 mm inclusive d = 2.5a
180° cold bend, mandrel diameter d >40 mm d = 2.5a

The 1.5a / 2.5a / 2.5a diameters apply to this grade except category 6; category 6 is not listed for this grade in Table 1.

Impact values from Table 4 are not tabulated here: Table 4 applies to categories 3–7, which are not listed for St2sp in Table 1.

Delivery conditions for GOST 14637 St2sp

Under clause 7.1.6, plate of categories 1–5 and 7 is manufactured without heat treatment (in the hot-rolled condition), or in the thermomechanically treated or heat-treated condition. The type of thermomechanical or heat treatment, in accordance with the classification in the 2024 standard, is chosen by the manufacturer and stated in the quality document.

State the required delivery condition on the order. If the condition is omitted, do not assume a heat-treated or thermomechanically treated delivery from the grade name alone; for categories 1–5 and 7 the manufacturer may supply the plate hot-rolled. Record the actual condition on the quality document.

St2sp may be ordered in category 1 or category 2. State the category on the order. Category 2 adds chemical-composition control; neither category specifies impact toughness for this grade. Category 6, which is required to be thermomechanically treated or heat-treated, is not listed for this grade in Table 1.

Weldability and fabrication of GOST 14637 St2sp

On purchaser request, clause 7.1.2 allows plate to be supplied with a weldability guarantee, designated in the standard as GS. That guarantee is ensured by limiting the ladle-analysis carbon content to not more than 0.22 %. If a weldability guarantee is required, state it on the order. The designation alone does not include it.

This page does not give preheat, interpass, heat-input or post-weld heat-treatment figures. The fabricator is responsible for welding-procedure qualification, consumable selection, preheat and any post-weld heat treatment required by the project specification. Do not take those figures from another standard or from a handbook and apply them as GOST 14637 rules.

St2sp is a killed steel. Killed, semi-killed and rimmed plates in the same carbon class are not automatic welding substitutes for each other. Do not assume that a procedure qualified on GOST 14637 St2ps Steel Plate or GOST 14637 St2kp Steel Plate is valid for this killed grade without qualification. If the weldability guarantee is required, order it and confirm the 0.22 % carbon restriction against the official texts.

Dimensions, surface quality and inspection

Remaining assortment requirements — dimensions, shape and permissible deviations beyond the thickness and width scope in clause 6.2.1 — follow GOST 19903. State the required thickness-accuracy class, edge condition and, for plate supplied as sheets, the flatness class on the order. This page does not tabulate numerical deviation limits from GOST 19903.

Surface quality is specified in clause 7.1.3 of the 2024 standard. Defects of the types listed there are not permitted. Dressing is allowed within the depth and area limits stated in that clause; confirm those limits against the official text. Delamination on ends and on untrimmed edges is not permitted.

Ultrasonic testing is not a default requirement. By agreement, clause 7.1.9 allows plate in sheets to be supplied with ultrasonic testing to a class of GOST 22727. The continuity class and the test volume (solid or selective) are agreed at the order; they are not implied by the grade.

Acceptance is by batch under GOST 7566, with the additions in the 2024 standard. A batch consists of sheets or coils of one steel grade, from one ladle-heat for ingot-cast product or one heat for continuously cast product. Marking and packaging follow GOST 7566. The 2024 standard allows the conventional grade number to be marked without the letters St. For destinations in the Far North and equivalent regions, packaging follows GOST 15846 when that service (HL) is stated on the order.

Applications and specification limits of St2sp

St2sp is specified where a killed general-quality plate, the Table 2 row that this grade shares with St2ps (330–430 N/mm² tensile, with the stated yield and elongation), the Table 5 bend, and category 1 or 2 inspection are required. Typical general-fabrication or construction use is not a design approval and is not a licence to substitute this killed plate for GOST 14637 St2kp Steel Plate or GOST 14637 St2ps Steel Plate, or for a different carbon class. A shared Table 2 row with St2ps does not authorise substitution.

The 2024 scope is hot-rolled plate of nonalloyed steel of general quality, width 500 mm and more, thickness 4 to 160 mm inclusive (sheets) and 4 to 25 mm (coils). That is the standard scope, not a stock range. Confirm available sizes on the enquiry.

GOST 14637 is not a boiler or pressure-vessel material standard. It is not a quality carbon structural plate standard. Service temperature, toughness and forming limits are set by the project specification, not by a generic maximum-temperature claim on this page.

Compare GOST 14637 St2sp with related general-quality plates

The other general-quality designations below are in the same GOST 14637-2024 set. They are shown for a product comparison, not as equivalents. Tensile, yield and elongation figures are from Table 2 as specified in GOST 14637-2024 Table 2; the yield and elongation columns are the Table 2 values for thickness up to 20 mm inclusive. Confirm every cell, including the other thickness bands, against the official table. A similar tensile class does not authorise substitution.

Material Table 2 σB, N/mm² Table 2 σT, N/mm² (≤20 mm) Table 2 δ5, % (≤20 mm) Relationship
GOST 14637 St2sp Steel Plate (this plate) 330–430 ≥225 ≥32 GOST 14637-2024; this product
GOST 14637 St0 Steel Plate Not less than 300 Not specified ≥23 2024 edition; related, not interchangeable
GOST 14637 St2kp Steel Plate 320–410 ≥215 ≥33 2024 edition; different Table 2 row and deoxidation (rimmed); related, not interchangeable
GOST 14637 St2ps Steel Plate 330–430 ≥225 ≥32 2024 edition; shares this Table 2 row; different deoxidation (semi-killed); related, not interchangeable
GOST 14637 St3kp Steel Plate 360–460 ≥235 ≥27 2024 edition; different carbon class; related, not interchangeable
GOST 14637 St3ps Steel Plate 370–480 ≥245 ≥26 2024 edition; different carbon class; related, not interchangeable
GOST 14637 St3sp Steel Plate 370–480 ≥245 ≥26 2024 edition; different carbon class; related, not interchangeable

St2sp shares its Table 2 row with GOST 14637 St2ps Steel Plate and is not that semi-killed grade. GOST 14637 St2kp Steel Plate is the rimmed grade in the same carbon class and has a different Table 2 row. GOST 14637 St3kp Steel Plate and GOST 14637 St3ps Steel Plate are a higher carbon class in the 2024 set. None of these is a substitute for this killed plate.

GB/T 700 ordinary carbon structural steel is a different standard with a different chemistry and property system. St2sp is commonly compared with GB/T 700 Q215B; that comparison is not equivalence. Related ordinary structural plate systems, including EN 10025-2, JIS G3101 and ASTM A283, are sometimes listed on comparison charts. A chart cannot replace a review of chemistry, deoxidation, category, mechanical tests and the project specification.

Equivalent material grades for GOST 14637 St2sp

No formal equivalence has been verified for the designations below. They are related designations only and are not equivalent to this GOST 14637-2024 plate. Engineer approval is required before any substitution. This page does not link any external catalogue.

Standard Country-Region Equivalent Grade Note
GOST 14637-2024 Interstate (GOST) St2sp This product under GOST 14637-2024, category 1 or category 2. Killed (sp) deoxidation; Table 2 row shared with St2ps, not interchangeable with it.
GB/T 700 China GB/T 700 Q215B Commonly compared; not equivalent. Verify chemistry, mechanicals, deoxidation, inspection category and the project specification. A similar tensile class does not authorise substitution. Engineer approval is required. Not a verified formal equivalent.

Related ordinary structural plate systems, including EN 10025-2, JIS G3101 and ASTM A283, are sometimes listed on comparison charts. No specific grade in those systems is listed as a verified equivalent on this page. A chart cannot replace a review of chemistry, product form, delivery condition, mechanical tests and the project specification.

Within this site, compare the present plate with GOST 14637 St0 Steel Plate, GOST 14637 St2kp Steel Plate, GOST 14637 St2ps Steel Plate, GOST 14637 St2sp Steel Plate, GOST 14637 St3kp Steel Plate, GOST 14637 St3ps Steel Plate, GOST 14637 St3sp Steel Plate in the GOST 14637 range, and with the different structural system under GB/T 700.

Why choose SHH STEEL for GOST 14637 St2sp

  • SHH STEEL produces and exports St2sp killed general-quality plate to the ordered GOST 14637-2024 specification
  • We quote against the 2024 edition that is in force, and we keep this killed grade distinct from the rimmed St2kp row and from semi-killed St2ps, even where Table 2 shares a mechanical row
  • Category (1 or 2), deoxidation and any agreed chemistry, galvanizing-class or weldability options are written on the quotation
  • The quotation states thickness, width, delivery condition, any agreed ultrasonic test, and the inspection document — not a generic stock grade alone
  • We review cutting, packaging, traceability and export documentation before confirming the order

How to enquire for GOST 14637 St2sp plate

Send the drawing or material schedule with the following details. Production feasibility, dimensions, documentation and delivery are confirmed against the enquiry.

Item What to specify
Edition and grade GOST 14637-2024 St2sp (killed, sp); do not assume the withdrawn 1989 edition, a different deoxidation, or dual certification
Category Category 1 or category 2, as required; category 2 adds chemistry control
Dimensions and quantity Thickness, width, length and tonnage, within the 2024 scope of 4–160 mm for sheets (4–25 mm for coils) and width 500 mm and more
Product form Sheets or coils, as applicable
Delivery condition Hot-rolled without heat treatment, or a stated thermomechanical or heat-treatment condition; record the actual condition on the quality document
Chemistry options GOST 380 conformity; tighter S and P under clause 7.1.1.4 (S ≤0.040 %, P ≤0.030 %) if required for categories 1–5; galvanizing class B or D if required
Weldability guarantee If required: GS, ladle carbon not more than 0.22 %; not implied by the grade
Ultrasonic examination GOST 22727 class and volume as ordered; not implied by the grade
Surface and tolerances GOST 19903 thickness accuracy, edge condition and flatness class as ordered
Documentation Quality-document requirements under GOST 7566, heat traceability, and any third-party inspection

FAQ

Is GOST 14637-2024 current for St2sp?
Yes. GOST 14637-2024 is the current edition as of 12 November 2026. It was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. State the 2024 edition, the grade St2sp, the category (1 or 2) and the killed (sp) deoxidation on the order. Do not use 1989 tables for a 2024 order.
What thickness and width does GOST 14637-2024 specify for St2sp?
The 2024 scope is thickness 4 to 160 mm inclusive for sheets and 4 to 25 mm for coils, with width 500 mm and more. That is the standard scope, not a stock range. Confirm available sizes on the enquiry. Remaining dimensional requirements follow GOST 19903.
How does St2sp differ from St2kp and St2ps?
St2sp is killed (sp). In Table 2 it shares one mechanical row with St2ps (semi-killed): tensile strength 330–430 N/mm², yield ≥225 / ≥215 / ≥205 / ≥195 N/mm² and elongation δ5 ≥32 / ≥31 / ≥29 % in the stated thickness bands. A shared Table 2 row is not interchangeability. St2kp is the rimmed grade in the same carbon class and has a different Table 2 row (320–410 N/mm²). State the required deoxidation on the order.
What inspection categories apply to St2sp?
Table 1 lists St2sp in category 1 and category 2. Category 1 specifies tensile properties and a 180° bend; category 2 adds chemical-composition control. Impact toughness is not a specified characteristic in either category for this grade. State the category on the order.
Is GOST 14637 St2sp equivalent to GB/T 700 Q215B?
No. St2sp is commonly compared with GB/T 700 Q215B; that comparison is not equivalence. The two products belong to different standards, with different chemistry rules, mechanical tables, deoxidation practice and inspection categories. Engineer approval is required before any substitution. Send the design requirements with the enquiry; we do not assume interchangeability.

Request a quotation for GOST 14637 St2sp plate

Contact SHH STEEL for a quotation for GOST 14637-2024 St2sp killed general-quality steel plate. Send thickness, width, length, quantity, destination and the project material specification.

Specify the 2024 edition, the killed (sp) grade St2sp, the category (1 or 2), the product form, the delivery condition, any agreed chemistry option, ultrasonic test or weldability guarantee, and the quality-document requirement. Do not assume a rimmed or semi-killed deoxidation, a substitute from the shared St2ps Table 2 row, or the withdrawn 1989 edition.

If a related grade or another standard is being considered, send the design requirements for review. We do not assume interchangeability from a grade comparison alone.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X