Product Showcase
ASTM A264/A264M Clad Steel Plates
SHH STEEL offers ASTM A264/A264M (ASME SA-264) stainless steel clad plates, with 304L, 316L, 321, 904L or 2205 cladding bonded to SA516 Gr.70 and other pressure vessel steels. ASTM A264 specifies carbon or low-alloy steel base plate integrally bonded to stainless chromium-nickel cladding, with shear, bend and ultrasonic bond tests. Explosion or roll bonded, certified, customizable. Trust SHH STEEL!
-
ASTM A264 SA516 Gr.70 + 309S Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 309S stainless steel clad plate bonds a 23 % chromium, 13 % nickel heat-resistant layer to a carbon steel base. It resists oxidation and sulfur-bearing hot gases on the clad face at lower cost than 310S. SHH STEEL produces it by explosion bonding with shear and ultrasonic tests when ordered.View More -
ASTM A264 SA537 Cl.1 + 316L Stainless Steel Clad Plate
ASTM A264 SA537 Cl.1 + 316L stainless steel clad plate bonds 316L stainless steel to normalized SA537 Class 1 carbon steel. The stronger, tougher base saves thickness on large high-pressure vessels in chloride service. SHH STEEL produces it by explosion bonding with shear, UT and base impact tests as ordered.View More -
ASTM A264 SA285 Gr.C + 304 Stainless Steel Clad Plate
ASTM A264 SA285 Gr.C + 304 stainless steel clad plate joins a type 304 layer to an SA285 Grade C carbon steel base. It is the economical stainless clad plate for storage tanks, hoppers and low-pressure vessels that need a clean stainless face. SHH STEEL produces it by explosion bonding with shear and UT tests on request.View More -
ASTM A264 SA387 Gr.22 Cl.2 + 347 Stainless Steel Clad Plate
ASTM A264 SA387 Gr.22 Cl.2 + 347 clad plate bonds niobium-stabilized 347 stainless steel to a 2¼Cr-1Mo pressure vessel base. It is the classic clad combination for hydroprocessing reactors and high-pressure hydrogen vessels. SHH STEEL produces this SA387 Gr.22 Cl.2 + 347 clad plate by explosion bonding, tested after simulated PWHT when ordered.View More -
ASTM A264 SA387 Gr.11 Cl.2 + 321 Stainless Steel Clad Plate
ASTM A264 SA387 Gr.11 Cl.2 + 321 clad plate bonds titanium-stabilized 321 stainless steel to a 1¼Cr-½Mo pressure vessel base. The Cr-Mo steel gives creep strength and hydrogen resistance; the 321 face resists corrosion and survives the base's PWHT. SHH STEEL produces this SA387 Gr.11 Cl.2 + 321 clad plate by explosion bonding.View More -
ASTM A264 SA516 Gr.60 + 304L Stainless Steel Clad Plate
ASTM A264 SA516 Gr.60 + 304L clad plate bonds low-carbon 304L stainless steel to SA516 Grade 60 vessel steel. It is an economical clad plate for tanks, low-pressure vessels and formed heads in nitric acid, food and water service. SHH STEEL produces this SA516 Gr.60 + 304L clad plate by explosion or roll bonding, with shear and UT tests.View More -
ASTM A264 SA516 Gr.60 + 316L Stainless Steel Clad Plate
ASTM A264 SA516 Gr.60 + 316L clad plate bonds low-carbon 316L stainless steel to SA516 Grade 60, the softer, lower-carbon A516 vessel steel. It suits moderate-pressure vessels, heavily formed heads and low-temperature service where chloride resistance is needed. SHH STEEL produces this SA516 Gr.60 + 316L clad plate by explosion or roll bonding.View More -
ASTM A264 SA516 Gr.70 + 254SMO (S31254) Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 254SMO clad plate bonds UNS S31254, a 6 % molybdenum super austenitic stainless steel, to a carbon steel pressure vessel base. It resists pitting and crevice corrosion in seawater, brines and bleach plant liquors at a fraction of solid alloy cost. SHH STEEL produces it by explosion bonding with shear and UT tests.View More -
ASTM A264 SA516 Gr.70 + 2507 Super Duplex Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 2507 super duplex clad plate bonds UNS S32750 super duplex stainless steel to a carbon steel pressure vessel base. With a PREN of at least 41, it resists seawater, brines and chloride stress corrosion far beyond 316L and 2205. SHH STEEL produces it by explosion bonding with shear and ultrasonic tests when ordered.View More -
ASTM A264 SA516 Gr.70 + 310S Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 310S stainless steel clad plate bonds a 25 % chromium, 20 % nickel austenitic layer to a carbon steel base. It resists oxidation and hot corrosion on the clad face, and some strongly oxidizing acids, while the steel carries the load. SHH STEEL produces it by explosion bonding with shear and ultrasonic tests when ordered.View More -
ASTM A264 SA516 Gr.70 + 347 Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 347 stainless steel clad plate bonds a niobium-stabilized austenitic layer to a carbon steel pressure vessel base. Stabilization keeps the cladding resistant to intergranular corrosion after welding, stress relief and service in the sensitizing range. SHH STEEL produces it by explosion or roll bonding with shear and ultrasonic tests.View More -
ASTM A264 SA516 Gr.70 + 317L Stainless Steel Clad Plate
ASTM A264 SA516 Gr.70 + 317L stainless steel clad plate bonds a 3 to 4 % molybdenum, low-carbon stainless layer to a carbon steel pressure vessel base. It handles chlorides and acids beyond the reach of 316L, in FGD, pulp bleaching and chemical service. SHH STEEL produces it by explosion or roll bonding with shear and ultrasonic tests.View More
ASTM A264/A264M Clad Steel Plates
Stainless Steel Clad Plates
SHH STEEL, a leading Stainless Steel Clad Plates exporter, produces and exports stainless steel clad plates for pressure vessels and chemical processing. Our plates, with 304 or 316L cladding (ASTM A264), offer corrosion resistance and strength. We deliver in 15-35 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for stainless clad steel plates and custom solutions for your projects.
Stainless Steel Clad Plates
X