SMA400BW Steel Plate | JIS G3114 Weathering Steel - SHH STEEL

SMA400BW Steel Plate | JIS G3114 Weathering Steel

SMA400BW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 400 MPa tensile family with quality letter B. JIS applicable thickness for this designation is ≤ 200 mm. SHH STEEL supplies SMA400BW plate with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
Approximate: EN 10025-5 S235J0W / S235J2W; GB/T 4171 Q235NH; ISO 4952 S235W talk. Confirm against project specs.
Heat Treatment
As-rolled as common supply; normalized (N), tempered (T) or TMC by agreement. Heat-treatment symbols are appended to the grade designation when applied (e.g. SMA490BWN).
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
SMA400BW vs SMA490AW vs Q235NH
Why choose Us
Our Service
FAQ
Conclusion

What is SMA400BW steel plate (JIS G3114)?

JIS G3114 SMA400BW belongs to the hot-rolled atmospheric corrosion resisting steels for welded structure family. The standard covers bridges, buildings and other welded outdoor structures where atmospheric corrosion resistance and weldability are required.

W-suffixed grades are normally used bare or with rust-stabilizing treatment. W-suffixed grades are normally used bare or with rust-stabilizing treatment. P-suffixed grades are normally used painted. Do not auto-substitute W and P chemistries. The final letter before W/P is the quality level for Charpy practice: A has no mandatory Table 8 Charpy row; B is 0 °C / ≥ 27 J; C is 0 °C / ≥ 47 J (thickness > 12 mm).

JIS product forms for this designation: Plate, strip, sections and flat bars. Applicable thickness: ≤ 200 mm. Do not assume thicker material can be certified as SMA400BW without a special agreement outside the JIS thickness table.

SHH STEEL is a China mill-direct source for JIS G3114 weathering plates, with EN 10204 3.1 (or 3.2) mill test certificates. Category hubs: JIS G3114 Weathering Steel Plates · Weathering Steel Plates.

Sibling grades under the same hub: JIS G3114 SMA400AW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P. Related international pages: GB/T 4171 Q355NH · Q235NH · Q355GNH · JIS G3125 SPA-H · SPA-C · ASTM A242 Type 1 · A242 Type 2 · EN 10025-5 S355J2W · S355J2WP · Corten A · Corten B · ASTM A606 Type 2 · A606 Type 4.

Material Specification for SMA400BW

Parameter Specification
Standard JIS G3114 (Primary reference JIS G3114:2008 (ISO 4952:2006 MOD); confirm ordered edition on the MTC)
Grade SMA400BW
Family Hot-rolled atmospheric corrosion resisting steel for welded structure (W / bare track)
Product form (JIS) Plate, strip, sections and flat bars
JIS applicable thickness ≤ 200 mm
SHH supply note Within JIS ≤ 200 mm window (stock focus often 8-50 mm when available; confirm mill); cut-to-size on request
Width Per order / mill practice (confirm for strip)
Length Cut length or coil; cut-to-size plates on request
Delivery condition As-rolled / normalized / TMC as agreed
Surface As-rolled or descaled / shot blasted as agreed
Edge Mill edge or cut edge
Dimensional references JIS G 3193 (plate/strip); JIS G 3192 (sections); JIS G 3194 (flat bars)
Certification EN 10204 3.1 / 3.2
Corresponding ISO talk ISO 4952 (MOD basis noted in JIS G3114:2008)
Density 7.85 g/cm³

Chemical Composition of SMA400BW (ladle / heat analysis, JIS G3114:2008)

Ladle (heat) analysis limits below follow JIS G3114:2008 Table 2 for SMA400BW. Always verify the mill test certificate before fabrication or substitution.

Grade C Si Mn P S Cu Cr Ni
SMA400BW ≤0.18 0.15-0.65 ≤1.25 ≤0.035 ≤0.035 0.30-0.50 0.45-0.75 0.05-0.30

Other alloying elements may be added as necessary. When Mo, Nb, Ti and/or V are added for weathering effectiveness, their total shall not exceed 0.15% (JIS G3114:2008 Table 2 note).

W vs P chemistry: W grades use higher Cu/Cr/Ni ranges intended for bare or rust-stabilized service. P grades use a painted-service chemistry package (lower Cu/Cr ranges; Ni not specified in the P table). Do not substitute a P heat for a W designation (or the reverse) without project approval.

Mechanical Properties of SMA400BW (JIS G3114:2008)

Tensile requirements for SMA400BW under JIS G3114:2008 Table 7. Yield point or proof stress depends on thickness. Tensile strength upper limit applies to plate, strip and flat bars (sections by purchaser option). Confirm ordered thickness and test piece type on the MTC.

Thickness (mm) Yield / proof (N/mm²) Tensile Rm (N/mm²)
≤16 ≥245 400-540
>16-40 ≥235 400-540
>40-75 ≥215 400-540
>75-100 ≥215 400-540
>100-160 ≥205 400-540
>160-200 ≥195 400-540

Elongation (Table 7) depends on thickness and tensile test piece:

Thickness Test piece Elongation min (%)
≤5 mm No.5 ≥22
>5-16 mm No.1A ≥17
>16-50 mm No.1A ≥21
>40 mm No.4 ≥23

For thickness > 12 mm, SMA400BW Charpy V-notch (JIS G3114 Table 8): test temperature 0 °C, minimum average energy ≥ 27 J (longitudinal).

Charpy applies to steels listed in JIS G3114 Table 8 when thickness exceeds 12 mm. Average of three longitudinal V-notch specimens. A-quality letters (SMA400AW / SMA490AW) have no mandatory Charpy row in Table 8. Purchaser may specify higher energy or lower test temperature by agreement.

Density is approximately 7.85 g/cm³.

Delivery Conditions for SMA400BW

As-rolled as common supply; normalized (N), tempered (T) or TMC by agreement. Heat-treatment symbols are appended to the grade designation when applied (e.g. SMA490BWN).

When heat treatment is applied, append the symbol to the grade designation (examples in JIS: N, T, Q, TMC). Surface may be as-rolled or descaled / shot blasted as agreed. SHH STEEL supplies the delivery condition named on the order within the JIS ≤ 200 mm window for SMA400BW.

Weldability of SMA400BW weathering steel

SMA400BW is designed as a weldable atmospheric corrosion resisting steel under JIS G3114. Qualify SMAW / GMAW / SAW (or other agreed processes) on production-representative chemistry. Prefer low-hydrogen consumables and consumables selected for weathering service when bare weld exposure is intended.

Keep hydrogen control, preheat and interpass aligned with thickness, carbon equivalent and joint restraint.

Related alternatives when the project shifts standards: Q355NH · Q235NH · S355J2W · A242 Type 2 · A606 Type 2.

Dimensional Tolerances for SMA400BW

Shape, dimensions, mass and permissible variations follow JIS G 3193 for hot-rolled plate and strip, JIS G 3192 for sections, and JIS G 3194 for flat bars, unless another agreement is cited. For cut-edge plate/strip, width and length tolerances default to JIS G 3193 tolerance A unless otherwise specified.

Respect the JIS G3114 applicable thickness for SMA400BW (≤ 200 mm). SHH STEEL can supply cut-to-size plates and edge preparation within the agreed thickness range.

Applications and service limits for SMA400BW

Typical applications for SMA400BW (within JIS ≤ 200 mm):

  • Highway and railway bridges (when JIS G3114 is specified)
  • Building frames and outdoor industrial structures
  • Transmission and communication towers
  • Welded outdoor fabrications where bare weathering chemistry is specified
  • RFQs historically calling EN W / GB NH / ASTM weathering packages at similar strength talk (confirm match)

The self-protecting patina on W grades can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. P grades are intended for painted service. Sheltered wet pockets, aggressive chloride splash and continuous immersion often need coating or another material.

Related pages: SMA400AW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P · SPA-H · Q355NH · Q355GNH · S355J2W · S355J2WP · A242 Type 1 · A242 Type 2 · Corten A · Corten B · Weathering Steel Plates.

Atmospheric exposure guidance for SMA400BW

Bare SMA400BW is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit Note
Rural / mild industrial Usually suitable bare Needs wet/dry cycles for patina on bare W grades
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating, higher-Ni practice, or another grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

Equivalent and related grades for SMA400BW

These grades are commonly compared with SMA400BW. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.

Approximate: EN 10025-5 S235J0W / S235J2W; GB/T 4171 Q235NH; ISO 4952 S235W talk. Confirm against project specs.

Standard / family Grade Relation Product page
JIS G3114 SMA400BW This page –
JIS G3114 Sibling SMA grades Same standard; different strength / quality / W-P track SMA400AW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P
EN 10025-5 S235J0W / S235J2W Approximate W talk for 400 class S235J0W · S235J2W
GB/T 4171 Q235NH Approximate NH talk Q235NH
Commercial Corten B Purchasing talk (confirm strength class) Corten B
JIS G3125 SPA-H / SPA-C High-P superior weathering; different JIS family SPA-H · SPA-C
EN 10025-5 (WP) S355J0WP / S355J2WP P-bearing EN talk (closer to GNH / SPA-H than to SMA W) S355J0WP · S355J2WP
Category JIS G3114 / weathering hubs All SMA product pages JIS G3114 hub · Weathering Steel Plates

SMA400BW vs SMA490AW vs Q235NH (selection aid)

These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.

Item SMA400BW SMA490AW Q235NH / EN S235W talk
Strength class 400 MPa tensile family 490 MPa tensile family Per GB / EN edition
Track Bare/W Bare/W Weldable NH / W
JIS thickness ≤ 200 mm ≤ 200 mm Per GB/T 4171
When buyers ask Spec cites SMA400BW Higher strength JIS SMA Spec cites GB NH or EN S235W
Pages This page SMA490AW Q235NH · S235J2W

Why choose SHH STEEL for SMA400BW

  • China mill-direct supply of JIS G3114 SMA400BW weathering plate / strip within the JIS ≤ 200 mm window
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Thickness kept honest to JIS G3114 (no invented certification above the applicable thickness)
  • Cutting, beveling and shot blasting available to shorten fabrication time
  • Full SMA coverage under one hub: JIS G3114 Weathering Steel Plates · parent Weathering Steel Plates
  • International near-equivalents when the project cites ASTM / EN / GB / JIS G3125 instead: Q355NH, Q355GNH, S355J2W, S355J2WP, A242 Type 1, A242 Type 2, SPA-H, Corten A, Corten B

Supply, cutting and inspection for SMA400BW

Item SHH STEEL supply note
Thickness Within JIS ≤ 200 mm window (stock focus often 8-50 mm when available; confirm mill)
Size Width and length per order; cut-to-size plates on request; coil available when ordered as strip
Delivery condition As-rolled / normalized / TMC as agreed.
Processing Cutting, beveling, shot blasting / descaling available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs Grade SMA400BW, thickness × width × length (or coil), quantity, delivery condition / heat-treatment symbol, surface/edge, inspection level

FAQ

What does the W or P mean on SMA400BW?
W-suffixed JIS G3114 grades are normally used bare or with rust-stabilizing treatment. P-suffixed grades are normally used painted and follow a different chemistry table. See the chemical composition section and JIS G3114 hub.
What do the A / B / C letters mean?
For SMA400 and SMA490, A/B/C are quality letters tied to Charpy practice (Table 8): A has no mandatory Charpy row; B is 0 °C / ≥ 27 J; C is 0 °C / ≥ 47 J for thickness > 12 mm. SMA570 uses -5 °C / ≥ 47 J.
What thickness does JIS allow for SMA400BW?
JIS G3114:2008 lists applicable thickness ≤ 200 mm for SMA400BW. SHH keeps supply notes inside that window unless a special mill agreement is documented.
What is SMA400BW equivalent to?
Approximate: EN 10025-5 S235J0W / S235J2W; GB/T 4171 Q235NH; ISO 4952 S235W talk. Confirm against project specs. Substitution still requires project approval and MTC review.
Is SMA400BW quenched and tempered?
Not as a default. Common supply is as-rolled; normalized or TMC may be agreed. Q&T is not the usual route for SMA400/SMA490.

Request a quotation

Send grade SMA400BW, thickness × width × length (or coil mass / cut size), quantity, delivery condition / heat-treatment symbol, surface/edge preference and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation for your weathering steel package.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: JIS G3114 Weathering Steel Plates · Weathering Steel Plates · SPA-H · Q355NH · S355J2W · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X