EN 10025-5 S355J2WP Steel Plate | S355J2WP Weathering Steel

EN 10025-5 S355J2WP is a weathering structural steel plate with a minimum yield strength of 355 MPa and impact tested at –20°C. It features higher phosphorus content for enhanced atmospheric corrosion resistance and improved low-temperature toughness. SHH STEEL is a China Mill-Direct Exporter supplying S355J2WP weathering steel plate worldwide.
Equivalent Grades:
ASTM A242 Type 1 (-20℃) / JIS SPA-H / GB Q355GNH (-20℃) / ISO E355WP
Material Specification:
EN 10025-5 — Delivery: As-rolled (AR), -20℃ impact, high-P
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-5 S355J2WP Steel Plate?

As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-5 S355J2WP Steel Plate (Material Number: 1.8946).

S355J2WP is a structural steel with improved atmospheric corrosion resistance under the European standard EN 10025-5. The “WP” designation indicates a higher phosphorus content that enhances the formation of a stable protective oxide layer (patina), providing better atmospheric corrosion resistance. It offers a minimum yield strength of 355 MPa (for thickness ≤ 16 mm) and is impact tested at –20°C with a minimum energy of 27 J. Compared with S355J0WP, S355J2WP provides improved toughness at lower temperature while maintaining the enhanced weathering performance associated with the high-phosphorus “WP” grades. This grade is commonly regarded as an equivalent to Corten A type weathering steels with better low-temperature properties.

SHH STEEL sources S355J2WP plates directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery. We supply thicknesses from 6 mm to 100 mm (thicker plates available on request), widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard EN 10025-5 Full compliance
Steel Grade S355J2WP (1.8946) Confirmed
Delivery Condition As-rolled, Normalized or TMCP Available
Product Form Steel Plate Available
Thickness Range 6 mm – 100 mm Custom sizes available
Width / Length Up to 3000–4000 mm / 12000–18000 mm Custom cutting supported
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

Chemical composition according to EN 10025-5 (Ladle Analysis and Product Analysis):

Element Ladle Analysis Max. / Range (%) Product Analysis Max. / Range (%)
Carbon (C) ≤ 0.12 ≤ 0.15
Silicon (Si) ≤ 0.75 ≤ 0.80
Manganese (Mn) ≤ 1.00 ≤ 1.10
Phosphorus (P) 0.06 – 0.15 0.05 – 0.16
Sulfur (S) ≤ 0.030 ≤ 0.035
Chromium (Cr) 0.30 – 1.25 0.25 – 1.35
Nickel (Ni) ≤ 0.65 ≤ 0.70
Copper (Cu) 0.25 – 0.55 0.20 – 0.60
Molybdenum (Mo) ≤ 0.30 ≤ 0.35
Nitrogen (N) ≤ 0.009 ≤ 0.010

Note: The elevated phosphorus content, combined with chromium and copper, significantly improves atmospheric corrosion resistance and accelerates the formation of a dense protective patina. The slightly tighter sulphur limit supports better toughness at –20°C.

Mechanical Properties

Mechanical properties of EN 10025-5 S355J2WP (longitudinal direction):

Thickness (mm) Yield Strength ReH (min) Tensile Strength Rm Elongation A (min) Impact Energy KV (min)
≤ 16 355 MPa 510 – 680 MPa 22% 27 J at –20°C
> 16 ≤ 40 345 MPa 470 – 630 MPa 22% 27 J at –20°C
> 40 ≤ 63 335 MPa 470 – 630 MPa 21% 27 J at –20°C
> 63 ≤ 80 325 MPa 470 – 630 MPa 20% 27 J at –20°C
> 80 ≤ 100 315 MPa 470 – 630 MPa 20% 27 J at –20°C

Density: 7.85 g/cm³

Delivery Conditions

SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-5 S355J2WP steel plate in as-rolled, normalized or thermomechanically rolled condition according to customer requirements.

Additional options:

  • Shot blasting and shop primer
  • Ultrasonic testing (EN 10160)
  • Z-direction testing (Z15 / Z25 / Z35)
  • Third-party inspection (SGS, BV, TUV, etc.)

Tolerances

Dimensional tolerances for S355J2WP steel plate follow EN 10029.

  • Thickness, width and length tolerances according to the ordered class.
  • Flatness according to EN 10029.
  • Edge conditions: Mill edge or cut edge (flame / plasma).

Tighter tolerances can be provided upon request.

Weldability

S355J2WP has good weldability. Due to the higher phosphorus content, welding procedures should be carefully controlled, and low-hydrogen consumables are recommended.

Recommended welding consumables:

Welding Process Recommended Consumables
SMAW (Stick) E7018, E7016
GMAW (MIG/MAG) ER70S-6
FCAW E71T-1
SAW EM12K + suitable flux

Matching weathering steel consumables can be used when the weld is required to form a protective patina similar to the base material.

Equivalent Material Grades

Grade Standard Notes
S355J2WP EN 10025-5 —
1.8946 EN Material number
Q355GNH GB/T 4171 Closest Chinese weathering steel
Corten A (approx.) ASTM A242 / A588 Similar high-phosphorus weathering concept
WTSt 37-3 DIN (old) Former related designation

Applications

EN 10025-5 S355J2WP is widely used in outdoor structures where enhanced atmospheric corrosion resistance and better low-temperature toughness are required. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Bridges Bridge girders, components – S355J2WP Bridge
Building Structures Facades, external frames – S355J2WP Structural Steel
Containers & Shipping Containers, cargo handling – S355J2WP Container
Railway Vehicles Wagon structures – S355J2WP Railway
Sculptures & Architecture Outdoor sculptures, architectural elements – S355J2WP Architecture
Cold Region Outdoor Structures Structures in colder climates – S355J2WP Low Temperature
General Outdoor Fabrication Weathering steel structures – S355J2WP Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-5 S355J2WP Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for weathering steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.

FAQ

What does the “J2WP” in S355J2WP mean?
“J2” indicates impact tested at –20°C with a minimum of 27 J, “W” indicates improved atmospheric corrosion resistance, and “P” indicates higher phosphorus content for enhanced patina formation.
What is the difference between S355J0WP and S355J2WP?
Both are high-phosphorus weathering steels. S355J0WP is impact tested at 0°C, while S355J2WP is tested at –20°C and offers better low-temperature toughness.
Is S355J2WP similar to Corten A?
Yes. S355J2WP is commonly regarded as an equivalent to Corten A type weathering steels with improved toughness.

Conclusion

EN 10025-5 S355J2WP (1.8946) Steel Plate from SHH STEEL is a high-phosphorus weathering structural steel offering 355 MPa yield strength, enhanced atmospheric corrosion resistance and reliable toughness at –20°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S355J2WP weathering steel plate requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-5 S355J2WP Steel Plate, S355J2WP steel plate, S355J2WP weathering steel, EN 10025 S355J2WP, S355J2WP equivalent, S355J2WP supplier, 1.8946

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *