SPA-C Steel Plate | JIS G3125 Weathering Steel
What is SPA-C steel (JIS G3125 cold-rolled)?
SPA-C is the cold-rolled grade in JIS G3125 (Superior atmospheric corrosion resisting rolled steels). JIS lists SPA-C as cold-rolled plate and strip with applicable thickness 0.6 mm to 2.3 mm. In purchasing language this usually means weathering sheet and coil, not thick hot-rolled plate.
SPA-C uses the same ladle-analysis chemistry table as JIS G3125 SPA-H (elevated phosphorus with copper, chromium and nickel). Mechanical minima are lower than SPA-H because the product is cold-reduced thin gauge. Buyers typically choose SPA-C for formed thin parts, panels and cladding where cold-rolled flatness and gauge control matter.
Do not auto-substitute SPA-C for hot-rolled SPA-H (or for thicker plate grades such as GB/T 4171 Q355GNH, ASTM A242 Type 1 or Corten A) without checking form, thickness and mechanical tables. Those grades are chemistry talk tracks, not identical supply forms.
SHH STEEL is a China mill-direct source for JIS G3125 weathering products. For SPA-C we supply sheet/coil packages and cut sheet within the JIS 0.6-2.3 mm window, with EN 10204 3.1 (or 3.2) certificates. Hubs: JIS G3125 Weathering Steel Plates · Weathering Steel Plates.
Material Specification for SPA-C (JIS G3125)
| Parameter | Specification |
|---|---|
| Standard | JIS G3125 (edition as ordered; primary reference JIS G3125:2021) |
| Grade | SPA-C |
| Family | Superior atmospheric corrosion resisting (high weathering / elevated P) |
| Product form (JIS) | Cold-rolled plate and strip (sheet / coil) |
| JIS applicable thickness | 0.6-2.3 mm |
| SHH supply note | Cold-rolled sheet/coil packages and cut sheet within 0.6-2.3 mm; not a thick-plate grade |
| Width | Per order / mill practice for cold-rolled strip |
| Length / coil | Cut sheet or coil as ordered |
| Delivery / finish | Cold-reduced; annealed and/or skin-passed / oiled as agreed |
| Surface | Cold-rolled finish; oiling per JIS G3125 / order |
| Edge | Mill edge or slit / cut edge |
| Dimensional reference | JIS G 3141 (cold-rolled steel sheet and strip) for dimension expression / practice cited by JIS G3125 |
| Certification | EN 10204 3.1 / 3.2 |
| Corresponding ISO talk | ISO 5952:2019 (MOD basis of JIS G3125:2021) |
| Density | 7.85 g/cm³ |
Chemical Composition of SPA-C (ladle / heat analysis, JIS G3125:2021)
Ladle (heat) analysis limits below follow JIS G3125:2021 Table 2. SPA-C and SPA-H share the same chemistry table. Other alloying elements not listed may be added as necessary. Always verify the mill test certificate before forming, welding or substitution.
| Element | SPA-C (mass %) | Note |
|---|---|---|
| Carbon (C) | ≤ 0.12 | Heat analysis |
| Silicon (Si) | 0.20-0.75 | |
| Manganese (Mn) | ≤ 0.60 | May be ≤ 1.0 by agreement between purchaser and supplier |
| Phosphorus (P) | 0.070-0.150 | Elevated intentionally for patina behaviour |
| Sulfur (S) | ≤ 0.035 | |
| Copper (Cu) | 0.25-0.55 | Essential for atmospheric corrosion resistance |
| Chromium (Cr) | 0.30-1.25 | |
| Nickel (Ni) | ≤ 0.65 |
Same high-P package as SPA-H. For low-P weldable weathering chemistry instead, see Q355NH, Q235NH, A242 Type 2 or EN W grades such as S355J2W.
Mechanical Properties of SPA-C (JIS G3125:2021)
Tensile requirements for SPA-C under JIS G3125:2021 Table 3. Values apply across the JIS cold-rolled thickness window (0.6-2.3 mm). Confirm actual results on the MTC.
| Grade | Yield / proof (N/mm²) | Tensile (N/mm²) | Elongation (%) | Tensile test piece |
|---|---|---|---|---|
| SPA-C | ≥ 315 | ≥ 450 | ≥ 26 | No. 5 |
Compared with SPA-H (YS ≥ 355 N/mm², TS ≥ 490 N/mm²), SPA-C is intentionally the lower-strength cold-rolled track suited to thin gauge forming.
Bendability (JIS Table 4): 180° bend without crack on the outside of the test piece. For SPA-C the inner spacing follows the cold-rolled bend practice referenced in JIS G3125 (inner radius column not applied the same way as for SPA-H plate).
Density is approximately 7.85 g/cm³. If the project needs impact values on thin SPA-C, specify them separately; they are not a mandatory SPA-C tensile table item in JIS G3125:2021.
Delivery Conditions for SPA-C sheet and coil
SPA-C is a cold-reduced product. Delivery finish is ordered with the mill: typically annealed and/or skin-passed cold-rolled sheet/coil, with or without oiling as allowed by JIS G3125 and the purchase order. It is not quenched and tempered.
Because gauge is thin (0.6-2.3 mm), surface protection in transit (oil, packaging) and coil handling practice matter as much as the metallurgical condition. SHH STEEL supplies the finish and packaging named on the order within the JIS SPA-C thickness window.
Weldability and joining of SPA-C
SPA-C carries the same elevated-phosphorus chemistry as SPA-H, so hydrogen control and qualified procedures still matter when welding. Thin cold-rolled sheet also brings distortion, burn-through and heat-input control concerns that differ from thicker hot-rolled plate.
Use a WPS written for thin weathering sheet. Prefer low-hydrogen consumables / processes suited to the gauge. Resistance welding, spot welding or mechanical fastening may be specified instead of arc welding for some panel applications. Do not copy a thick-plate SPA-H or GNH WPS onto SPA-C without requalification.
If the design needs heavier hot-rolled weathering plate instead, move to SPA-H or an international plate grade such as Q355GNH / A242 Type 1 after engineering review.
Dimensional Tolerances for SPA-C
JIS G3125 points cold-rolled SPA-C dimension expression to JIS G 3141 practice. Thickness, width, length, flatness and coil mass tolerances follow the ordered cold-rolled dimensional agreement (JIS G 3141 tables or purchaser agreement).
Respect the JIS applicable thickness for SPA-C (0.6-2.3 mm). SPA-C is not a route to certify thick plate as “SPA-C”. For hot-rolled material up to 16 mm, order SPA-H instead. SHH STEEL can supply slit coil and cut sheet within the agreed gauge.
Applications and service limits for SPA-C
Typical applications for SPA-C (thin cold-rolled sheet/coil):
- Vehicle and equipment panels, covers and formed thin parts
- Architectural weathering sheet, facade skins and decorative cladding (when thin gauge is specified)
- Containers and enclosures using cold-rolled weathering sheet
- Fabricated assemblies that need cold-rolled flatness and gauge control more than hot-rolled plate thickness
Patina behaviour still needs wet/dry atmospheric cycles. Thin sheet can show appearance change faster and is more sensitive to handling scratches, edge corrosion and continuous wet pockets. Coating or design detailing may still be required in chloride-rich or sheltered service.
Related pages: SPA-H · Q355GNH · A242 Type 1 · Corten A · Corten B · S355J2WP · S355J0WP · S355J2W · Weathering Steel Plates.
Atmospheric exposure guidance for SPA-C
Bare SPA-C is intended for atmospheres where a stable patina can form and dry periodically. Thin sheet needs the same environmental judgment as thicker weathering plate, plus extra attention to edge sealing and fastening details.
| Environment | Typical fit for bare SPA-C | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check appearance and pollution loading |
| Coastal / marine splash with moderate chloride | Use with caution | Thin gauge + chloride often needs coating or another material |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for SPA-C
SPA-C is primarily compared with its hot-rolled sibling SPA-H and with high-P weathering chemistries used on thicker products. Form and thickness differences usually block direct substitution.
| Standard / family | Grade | Relation to SPA-C | Product page |
|---|---|---|---|
| JIS G3125 | SPA-C | This page (cold-rolled 0.6-2.3 mm) | – |
| JIS G3125 | SPA-H | Same chemistry; hot-rolled ≤ 16 mm; higher strength minima | SPA-H |
| GB/T 4171 | Q355GNH | High-P chemistry talk; usually hot-rolled plate/strip, different thickness rules | Q355GNH |
| ASTM | A242 Type 1 | High-P plate talk; not a cold-rolled SPA-C substitute | A242 Type 1 |
| Commercial | Corten A | Chemistry talk track for high-P weathering | Corten A |
| EN 10025-5 | S355J0WP / S355J2WP | EN WP talk; confirm form and thickness separately | S355J0WP · S355J2WP |
| GB/T 4171 NH | Q355NH / Q235NH | Low-P weldable alternatives (different track) | Q355NH · Q235NH |
| Commercial / EN W | Corten B / S355J2W | Often lower-P / W talk rather than SPA-C | Corten B · S355J2W |
| Category | JIS G3125 hub | SPA-H and SPA-C only under this JIS hub | JIS G3125 hub · Weathering Steel Plates |
SPA-C vs SPA-H vs Q355GNH / A242 Type 1 / Corten A (selection aid)
Use this table to keep cold-rolled SPA-C from being confused with hot-rolled plate grades that share high-P chemistry talk.
| Item | SPA-C | SPA-H | Q355GNH / A242 Type 1 / Corten A |
|---|---|---|---|
| Process | Cold-rolled sheet/coil | Hot-rolled plate/strip/sections | Usually hot-rolled plate/strip |
| JIS / typical thickness | 0.6-2.3 mm | ≤ 16 mm | Per each standard (often thicker ceilings than SPA-C) |
| Min YS / TS (guide) | ≥ 315 / ≥ 450 N/mm² | ≥ 355 / ≥ 490 N/mm² | Confirm each standard |
| Best for | Thin formed panels, cladding skins, coil feed | Hot-rolled structural / vehicle plate within 16 mm | Project cites GB / ASTM / commercial plate grade |
| Pages | This page | SPA-H | Q355GNH · A242 Type 1 · Corten A |
Why choose SHH STEEL for SPA-C
- China mill-direct supply of JIS G3125 SPA-C cold-rolled weathering sheet/coil within the honest 0.6-2.3 mm JIS window
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Clear separation from hot-rolled SPA-H so RFQs are not filled with the wrong form
- Slitting and cut-sheet processing available when ordered
- JIS sibling coverage: SPA-H · hub JIS G3125 Weathering Steel Plates · parent Weathering Steel Plates
- Related high-P plate grades when the project actually needs plate: Q355GNH, A242 Type 1, S355J2WP, Corten A
Supply, processing and inspection for SPA-C
| Item | SHH STEEL supply note |
|---|---|
| Thickness | JIS G3125 SPA-C window 0.6-2.3 mm (sheet/coil; cut sheet on request) |
| Size | Coil width / cut length per order; slitting available |
| Delivery / finish | Cold-reduced; annealed and/or skin-passed; oiling as agreed. Not quenched and tempered. |
| Processing | Slitting, cut-to-length sheet; other processing by agreement |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade SPA-C, thickness × width × length or coil mass, quantity, finish (annealed / skin pass / oil), inspection level |
FAQ
-
Is SPA-C a plate grade or a sheet/coil grade?
- JIS G3125 lists SPA-C as cold-rolled plate and strip with applicable thickness 0.6-2.3 mm. In practice that is weathering sheet and coil. For hot-rolled plate/strip/sections up to 16 mm, use SPA-H.
-
Do SPA-C and SPA-H have the same chemistry?
- Yes. JIS G3125:2021 Table 2 is shared. Mechanical minima differ: SPA-C is ≥ 315 / ≥ 450 N/mm² (YS/TS); SPA-H is ≥ 355 / ≥ 490 N/mm².
-
Can SPA-C replace Corten A or A242 Type 1 plate?
- Not as a thickness or form substitute. Those plate grades are only approximate chemistry talk tracks. See Corten A and A242 Type 1, or move to SPA-H / Q355GNH when hot-rolled plate is required.
-
What finish should I order for SPA-C?
- State annealed and/or skin-passed, and whether oiling is required. Cold-rolled finish and packaging affect forming and surface appearance as much as chemistry.
-
Is SPA-C quenched and tempered?
- No. It is cold-reduced sheet/coil under JIS G3125, not a quenched and tempered product.
Request a quotation
Send grade SPA-C, thickness × width × length or coil mass, quantity, finish (annealed / skin pass / oil), and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation. If you need hot-rolled material ≤ 16 mm, ask for SPA-H instead.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: JIS G3125 Weathering Steel Plates · SPA-H · Weathering Steel Plates · A242 Type 1 · Q355GNH