ASTM A242 Type 2 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL
ASTM A242 Type 2 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL
ASTM A242 Type 2 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL

ASTM A242 Type 2 Steel Plate | A242 Gr.2 Weathering Steel

ASTM A242 Type 2 (also called A242 Gr.2) is a high-strength low-alloy weathering steel plate under ASTM A242 / A242M. It offers higher strength than ordinary carbon steel such as ASTM A36 and improved atmospheric corrosion resistance for outdoor structures. Type 2 is the lower-phosphorus A242 track, preferred when weldability and fabrication matter more than the Type 1 high-phosphorus chemistry package.
Equivalent Grades:
ASTM A242 Type 2 / often compared with EN 10025-5 S355J2W family, ASTM A588, and Corten B purchasing tracks. Confirm against project specs. Sibling grade: ASTM A242 Type 1.
Heat Treatment
As-rolled (AR) or controlled-rolled / TMCP as standard; normalized by agreement (typically 900–950 °C, then air cool). This is weathering HSLA plate, not quenched and tempered.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
A242 Type 2 vs Type 1 vs A588
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A242 Type 2 steel?

ASTM A242 Type 2 steel plate (also called A242 Gr.2) is a high-strength low-alloy weathering structural steel under ASTM A242 / A242M. It is designed for outdoor structures that need higher strength than ordinary carbon steel such as ASTM A36, plus better atmospheric corrosion resistance than plain carbon steel when exposed with proper wet/dry cycles.

Type 2 is the lower-phosphorus composition track in the A242 family. Type 1 uses a higher phosphorus ceiling to help form a stable patina quickly; Type 2 keeps phosphorus lower and relies on copper plus other alloying chosen by the producer so the plate still meets the specification’s atmospheric-corrosion intent. Buyers usually choose Type 2 when weldability and fabrication friendliness matter more than the Type 1 chemistry package.

SHH STEEL supplies ASTM A242 Type 2 plates as a China mill-direct source, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. For the sibling grade, see ASTM A242 Type 1 Steel Plate. More weathering options: Weathering Steel Plates.

Material Specification

Parameter Specification
Standard ASTM A242 / A242M
Grade Type 2 (A242 Gr.2)
Product form Plate
Thickness 6–100 mm (stock 8–50 mm)
Width 1500–4000 mm
Length 6000–16000 mm
Delivery condition As-rolled / Normalized / Controlled rolled
Surface As-rolled or shot blasted
Edge Mill edge or cut edge
Certification EN 10204 3.1 / 3.2
Density 7.85 g/cm³
Hardness 140–180 HB (typical, as-rolled)

Chemical Composition

ASTM A242 Type 2 is controlled by heat (ladle) analysis and product analysis. Compared with Type 1, Type 2 is specified and ordered as the lower-phosphorus track. Copper remains essential for atmospheric corrosion resistance. Other alloying elements (commonly chromium, nickel, silicon, and similar additions within the producer’s practice) are selected so the steel meets the mechanical properties and the atmospheric corrosion-resistance intent of ASTM A242 / A242M.

Element Typical Type 2 control (guide) vs Type 1 (this site)
Carbon (C) ≤ 0.15 (heat analysis family limit commonly used with A242 plates) Same order of limit
Manganese (Mn) ≤ 1.00 (confirm ordered ASTM edition / MTC) Same order of limit
Phosphorus (P) Lower ceiling than Type 1 (Type 2 purchasing track; confirm exact max on MTC) Type 1 allows higher P (up to 0.15 max on this site’s Type 1 table)
Sulfur (S) ≤ 0.05 Same order of limit
Copper (Cu) ≥ 0.20 Mandatory for both types
Cr / Ni / Si and others Producer additions within A242 practice to meet corrosion index and properties Type 1 page lists optional Cr/Ni when specified

Do not treat commercial cross-reference tables as a substitute for the ordered ASTM edition. Always verify the heat analysis on the mill test certificate before fabrication or substitution.

Mechanical Properties

Plate mechanical requirements under ASTM A242 / A242M are thickness-dependent. The values below match the Type 1 plate table used on this site for A242 plates (shared A242 plate strength classes). Confirm the ordered thickness range on the MTC.

Thickness Tensile Strength Yield Strength Elongation
≤ 19 mm 480–620 MPa ≥ 345 MPa ≥ 18%
> 19 to 38 mm 460–620 MPa ≥ 315 MPa ≥ 18%
> 38 to 102 mm 435–620 MPa ≥ 290 MPa ≥ 16%

Hardness is typically 140–180 HB in the as-rolled condition. Density is approximately 7.85 g/cm³.

Delivery Conditions

Plates are normally supplied as-rolled. For thicker plates or when improved toughness is required, normalized or controlled-rolled delivery can be arranged. Normalization is typically performed at 900–950 °C followed by air cooling. Stress relieving after fabrication can be carried out if the purchaser specifies it. SHH STEEL supplies the delivery condition required by the project.

Weldability

ASTM A242 Type 2 is generally preferred over Type 1 when welding and shop fabrication are the stronger concern, because Type 2 follows the lower-phosphorus track. Common processes include SMAW, GMAW, and SAW. Use a qualified welding procedure specification (WPS). Low-hydrogen consumables such as E7018 or equivalent are preferred for many structural joints. Preheat and interpass temperature still follow thickness, joint restraint, and the approved procedure – do not skip procedure qualification just because Type 2 is lower in phosphorus than Type 1. Post-weld heat treatment is not normally required for atmospheric-exposure applications, but may be specified for critical structures.

Tolerances

Dimensional tolerances comply with ASTM A6/A6M. Typical thickness tolerance is ±0.3 mm for plates up to 10 mm and increases with thickness. Width and length tolerances are normally +20 mm / –0 mm unless otherwise agreed. Flatness follows ASTM A6 Class A, or tighter if requested. SHH STEEL can supply cut-to-size plates with tighter tolerances and edge preparation on request.

Applications and service limits

Typical applications:

  • Highway and railway bridges
  • Building exteriors and architectural cladding
  • Transmission and communication towers
  • Welded outdoor frames where Type 2 chemistry is preferred
  • Container and railcar components
  • Marine and coastal structures with moderate exposure

The self-protecting patina can lower long-term maintenance cost versus painted carbon steel in many rural and industrial atmospheres. It is not a universal substitute for coating systems: sheltered pockets that stay wet, aggressive chloride environments, and continuously immersed service often need extra protection or another material. Related grades: A242 Type 1, EN 10025-5 S355J2W, ASTM A588 Grade A, ASTM A709 Grade 50W.

Atmospheric exposure guidance

Bare ASTM A242 Type 2 is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit for bare A242 Type 2 Note
Rural / mild industrial Usually suitable Needs wet/dry cycles for patina
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating or a different grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

Equivalent and related grades

These grades are commonly compared with ASTM A242 Type 2. They are not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits, and the project specification before replacing one grade with another.

Standard / family Grade Relation to A242 Type 2 Product page
ASTM A242 Type 1 Same standard; higher-P track, closer to WP / Corten A talk A242 Type 1
Commercial Corten B Often closer than Corten A for Type 2 / lower-P discussions Corten B Steel Plate
Commercial Corten A More often mapped to Type 1 / WP purchasing Corten A Steel Plate
ASTM A588 Grade A / B / C / K Related weathering role; different chemistry tables A588 Gr.A · Gr.B
EN 10025-5 (W family) S355J0W / S355J2W / S355K2W Common EN talk track for Type 2 / lower-P weathering S355J2W · S355J0W · S355K2W
EN 10025-5 (P-bearing) S355J0WP / S355J2WP Closer to Type 1 discussions S355J2WP
ASTM bridge A709 Grade 50W Bridge weathering grade when the project calls A709 A709 Grade 50W
Category Weathering plates JIS / GB near-equivalents when no dedicated page exists Weathering Steel Plates

A242 Type 2 vs Type 1 vs ASTM A588 (selection aid)

These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.

Item ASTM A242 Type 2 ASTM A242 Type 1 ASTM A588 (Gr. A/B typical)
Role A242 weathering plate; lower-P track for fabrication-friendly orders A242 weathering plate; higher-P track for patina-focused Type 1 chemistry Structural weathering plate widely used for bridges and frames
Phosphorus Lower ceiling than Type 1 Elevated (intentional) on Type 1 tables Generally lower P than A242 Type 1
Weldability talk track Often preferred when welding is the stronger concern Needs more attention to hydrogen / preheat on thicker sections Follow A588 WPS and thickness practice
Closest EN talk track EN W grades (e.g. S355J2W) EN WP grades (e.g. S355J2WP) Often mapped to EN W grades
When buyers ask for it Spec calls out A242 Type 2 / Gr.2 Spec calls out A242 Type 1 / Gr.1 or Corten A style RFQs Spec calls out A588

Why choose SHH STEEL for A242 Type 2

  • China mill-direct supply of ASTM A242 Type 2 weathering plate
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Stock focus on common thicknesses 8–50 mm; production range 6–100 mm
  • Cutting, beveling, and shot blasting available to shorten fabrication lead time
  • Related grades under one supply chain: A242 Type 1, A588, Corten A/B, EN 10025-5 W, A709 50W

Supply, cutting, and inspection

Item SHH STEEL supply note
Thickness Production 6–100 mm; common stock focus 8–50 mm
Size Width 1500–4000 mm; length 6000–16000 mm; cut-to-size on request
Delivery condition As-rolled / normalized / controlled-rolled per order
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV, or ABS can be arranged
Quotation needs Thickness × width × length (or cut size), quantity, delivery condition, inspection level, Type 1 or Type 2

FAQ

What is the difference between A242 Type 1 and Type 2?
Type 1 is the higher-phosphorus track commonly discussed with Corten A / EN WP grades. Type 2 is the lower-phosphorus track, often preferred when weldability is the stronger concern. Both are weathering steels under ASTM A242 / A242M. See A242 Type 1.
Is A242 Type 2 the same as Corten B?
Not automatically. Type 2 is sometimes discussed alongside Corten B and EN W grades, but substitution still depends on chemistry, mechanical properties, and the project specification.
What are fy and fu for A242 Type 2 plate?
For plates up to 19 mm thick on this site’s A242 plate table, minimum yield strength (fy) is 345 MPa and tensile strength (fu) is 480–620 MPa. Thicker plates follow the thickness ranges in the mechanical properties table. Confirm on the MTC.
What is ASTM A242 Type 2 equivalent to?
It is commonly compared with EN 10025-5 W grades such as S355J2W, ASTM A588, and Corten B purchasing tracks. Exact substitution must follow the project specification.

Request a quotation

Send thickness × width × length (or cut size), quantity, delivery condition (AR / normalized / controlled rolled), Type 2 confirmation, and any inspection requirement. SHH STEEL will return mill availability, certification scope, and a quotation for your weathering steel package.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: Weathering Steel Plates · A242 Type 1 · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X