SPA-H Steel Plate | JIS G3125 Weathering Steel - SHH STEEL

SPA-H Steel Plate | JIS G3125 Weathering Steel

SPA-H is the hot-rolled superior atmospheric corrosion resisting steel under JIS G3125. Elevated phosphorus with copper, chromium and nickel supports a protective patina in proper wet/dry outdoor exposure. It is commonly compared with high-weathering packages such as GB/T 4171 Q355GNH, Corten A, EN 10025-5 WP grades and ASTM A242 Type 1. JIS applies SPA-H to hot-rolled plate, strip and sections up to 16 mm. SHH STEEL supplies SPA-H with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
Approximate: GB/T 4171 Q355GNH; ASTM A242 Type 1; Corten A; EN 10025-5 S355J0WP / S355J2WP; ISO 5952 / ISO 4952 WP talk. Sibling grade: JIS G3125 SPA-C (cold-rolled). Confirm against project specs.
Heat Treatment
As-rolled or controlled-rolled as standard for hot-rolled SPA-H; normalized by agreement when toughness or fabrication needs require it. This is weathering HSLA plate/strip, not quenched and tempered.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
SPA-H vs related grades
Why choose Us
Our Service
FAQ
Conclusion

What is SPA-H steel plate (JIS G3125)?

SPA-H is the hot-rolled grade in JIS G3125 (Superior atmospheric corrosion resisting rolled steels). The standard covers rolled steels with high atmospheric corrosion resistance for vehicles, buildings, steel towers and other structures. SPA-H is supplied as hot-rolled plate, strip (coil) and sections within the JIS applicable thickness of ≤ 16 mm.

Chemistry intentionally elevates phosphorus (together with copper, chromium and nickel) so a denser protective rust layer can form under alternating wet and dry exposure. That places SPA-H on the same purchasing talk track as high-weathering / WP packages: GB/T 4171 Q355GNH, Corten A, EN 10025-5 S355J2WP / S355J0WP, and ASTM A242 Type 1. These are approximate comparisons, not automatic substitutes.

The cold-rolled counterpart under the same JIS is JIS G3125 SPA-C (sheet/coil, 0.6-2.3 mm). Do not treat SPA-H and SPA-C as interchangeable forms.

SHH STEEL is a China mill-direct source for JIS G3125 weathering products, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. Category hubs: JIS G3125 Weathering Steel Plates · Weathering Steel Plates.

Material Specification for SPA-H (JIS G3125)

Parameter Specification
Standard JIS G3125 (edition as ordered; primary reference JIS G3125:2021)
Grade SPA-H
Family Superior atmospheric corrosion resisting (high weathering / elevated P)
Product form (JIS) Hot-rolled plate, strip (coil) and sections
JIS applicable thickness ≤ 16 mm
SHH supply note Hot-rolled plate / sheet / coil packages within the JIS ≤ 16 mm window; cut-to-size on request
Width Per order / mill practice (confirm for strip)
Length Cut length or coil; cut-to-size plates on request
Delivery condition As-rolled / controlled-rolled; normalized by agreement
Surface As-rolled or descaled / shot blasted as agreed
Edge Mill edge or cut edge
Dimensional references JIS G 3193 (hot-rolled plate/strip); JIS G 3192 (sections)
Certification EN 10204 3.1 / 3.2
Corresponding ISO talk ISO 5952:2019 (MOD basis of JIS G3125:2021)
Density 7.85 g/cm³

Chemical Composition of SPA-H (ladle / heat analysis, JIS G3125:2021)

Ladle (heat) analysis limits below follow JIS G3125:2021 Table 2. SPA-H and SPA-C share the same chemistry table. Other alloying elements not listed may be added as necessary. Always verify the mill test certificate before fabrication or substitution.

Element SPA-H (mass %) Note
Carbon (C) ≤ 0.12 Heat analysis
Silicon (Si) 0.20-0.75
Manganese (Mn) ≤ 0.60 May be ≤ 1.0 by agreement between purchaser and supplier
Phosphorus (P) 0.070-0.150 Elevated intentionally for patina behaviour
Sulfur (S) ≤ 0.035
Copper (Cu) 0.25-0.55 Essential for atmospheric corrosion resistance
Chromium (Cr) 0.30-1.25
Nickel (Ni) ≤ 0.65

High-P vs low-P talk: SPA-H sits with high-weathering / WP packages (elevated P). Low-P weldable weathering grades such as GB/T 4171 Q355NH, ASTM A242 Type 2 and EN 10025-5 W grades are a different fabrication track. Do not substitute across tracks without chemistry, toughness and WPS review.

Mechanical Properties of SPA-H (JIS G3125:2021)

Tensile requirements for SPA-H under JIS G3125:2021 Table 3. Yield point or proof stress, tensile strength and elongation depend on product form and thickness. Confirm the ordered thickness and test piece type on the MTC.

Product / thickness Yield / proof (N/mm²) Tensile (N/mm²) Elongation (%) Tensile test piece
Plate and strip ≤ 6.0 mm ≥ 355 ≥ 490a ≥ 22 No. 5
Plate and strip > 6.0 mm (and ≤ 16 mm JIS window) ≥ 355 ≥ 490 ≥ 15 No. 1A
Sections ≥ 355 ≥ 490 ≥ 15 No. 1A

a For SPA-H plate and strip thinner than 3 mm, tensile strength ≥ 510 N/mm² may be agreed between purchaser and supplier.

Bendability (JIS Table 4): 180° bend without crack on the outside of the test piece. For plate/strip ≤ 6.0 mm, inner radius is 0.5× thickness (1.0× thickness may be agreed). For plate/strip > 6.0 mm and for sections, inner radius is 1.5× thickness.

Density is approximately 7.85 g/cm³. Charpy impact is not a mandatory SPA-H table requirement in JIS G3125:2021; if the project needs toughness values, specify them on the order and confirm mill capability.

Delivery Conditions for SPA-H

Hot-rolled SPA-H is normally supplied as-rolled. Controlled rolling (TMCP) or normalizing can be arranged when toughness, thickness near the JIS ceiling, or fabrication needs require it. Normalization, when applied, is typically in the 900-950 °C range followed by air cooling, subject to mill practice. SPA-H is not a quenched and tempered product under JIS G3125.

Surface may be as-rolled or descaled / shot blasted as agreed (JIS G3125 also addresses scale removal and oiling practice by product type). Stress relieving after fabrication is available when the purchaser specifies it. SHH STEEL supplies the delivery condition named on the order within the JIS ≤ 16 mm SPA-H window.

Weldability of SPA-H weathering steel

SPA-H is a high-phosphorus superior weathering grade. Elevated P improves patina behaviour but increases the need for disciplined hydrogen control, preheat practice and procedure qualification, especially on thicker sections within the JIS window and on highly restrained joints.

Qualify SMAW / GMAW / SAW (or other agreed processes) on production-representative chemistry. Prefer low-hydrogen consumables and consumables selected for weathering service when bare exposure of welds is intended. Matching or undermatching filler must be chosen so weld-metal atmospheric corrosion behaviour and strength meet the design intent. Post-weld heat treatment is not normally required for atmospheric-exposure structures, but may be specified for critical joints.

If extensive welding is the stronger project constraint, evaluate lower-P alternatives such as Q355NH, GB/T 4171 Q235NH, A242 Type 2 or EN W grades (for example EN 10025-5 S355J2W). Do not assume a low-P WPS automatically covers SPA-H heats.

Dimensional Tolerances for SPA-H

Shape, dimensions, mass and permissible variations for SPA-H follow JIS G 3193 for hot-rolled plate and strip, and JIS G 3192 for hot-rolled sections, unless the order cites another dimensional agreement. Width, length and flatness classes are ordered per those dimensional standards or by purchaser agreement.

Respect the JIS G3125 applicable thickness for SPA-H (≤ 16 mm). Do not assume thicker plate can be certified as SPA-H under JIS without a special agreement outside the standard thickness table. SHH STEEL can supply cut-to-size plates and edge preparation within the agreed thickness range.

Applications and service limits for SPA-H

Typical applications for SPA-H (within the JIS ≤ 16 mm window):

  • Vehicle, container and transport equipment skin and structural parts
  • Building exteriors, facade panels and landscape structures
  • Transmission and communication towers
  • Outdoor frames and architectural weathering details where high-P chemistry is specified
  • RFQs historically calling Corten A / A242 Type 1 / Q355GNH / EN WP style packages (confirm match)

The self-protecting patina can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material.

Related pages: SPA-C · Q355GNH · A242 Type 1 · Corten A · Corten B · S355J2WP · S355J0WP · S355J2W · ASTM A588 Grade A · ASTM A709 Grade 50W · Weathering Steel Plates.

Atmospheric exposure guidance for SPA-H

Bare SPA-H is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit for bare SPA-H Note
Rural / mild industrial Usually suitable Needs wet/dry cycles for patina
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating, higher-Ni practice, or another grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

Equivalent and related grades for SPA-H

These grades are commonly compared with SPA-H. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.

Standard / family Grade Relation to SPA-H Product page
JIS G3125 SPA-H This page (hot-rolled ≤ 16 mm) –
JIS G3125 SPA-C Same chemistry table; cold-rolled sheet/coil 0.6-2.3 mm SPA-C
GB/T 4171 Q355GNH High-P GNH talk track often mapped to SPA-H Q355GNH
ASTM A242 Type 1 High-P A242 track; common SPA-H comparison A242 Type 1
Commercial Corten A Common purchasing talk for SPA-H / WP chemistry Corten A
EN 10025-5 S355J0WP / S355J2WP EN WP / P-bearing weathering talk S355J0WP · S355J2WP
GB/T 4171 NH Q355NH Same strength class talk; low-P weldable (different track) Q355NH
ASTM A242 Type 2 Lower-P A242 track; fabrication-focused alternative talk A242 Type 2
Commercial Corten B Often closer to W / lower-P discussions than to SPA-H Corten B
EN 10025-5 (W) S355J2W / S355J0W / S355K2W W-family; usually lower P than SPA-H / WP S355J2W · S355J0W · S355K2W
Category JIS G3125 / weathering hubs SPA-H and SPA-C under one JIS hub JIS G3125 hub · Weathering Steel Plates

SPA-H vs SPA-C vs Q355GNH / Corten A / A242 Type 1 / EN WP (selection aid)

These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.

Item JIS G3125 SPA-H JIS G3125 SPA-C Q355GNH / Corten A / A242 Type 1 / EN WP
Form Hot-rolled plate, strip, sections Cold-rolled plate and strip (sheet/coil) Usually hot-rolled plate/strip per each standard
JIS / typical thickness ≤ 16 mm (JIS G3125) 0.6-2.3 mm (JIS G3125) Per GB / ASTM / EN edition (often different ceilings)
Phosphorus 0.070-0.150% Same chemistry table as SPA-H Elevated on GNH / Type 1 / WP / Corten A talk
Strength talk YS ≥ 355 MPa; TS ≥ 490 MPa YS ≥ 315 MPa; TS ≥ 450 MPa Confirm each standard’s table
When buyers ask Spec cites JIS G3125 SPA-H or hot-rolled SPA Spec cites SPA-C thin sheet/coil Spec cites GB GNH, ASTM Type 1, Corten A or EN WP
Pages This page SPA-C Q355GNH · Corten A · A242 Type 1 · S355J2WP

Why choose SHH STEEL for SPA-H

  • China mill-direct supply of JIS G3125 SPA-H hot-rolled weathering plate / sheet / coil within the JIS ≤ 16 mm window
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Thickness kept honest to JIS G3125 (no invented SPA-H certification above the standard applicable thickness)
  • Cutting, beveling and shot blasting available to shorten fabrication time
  • JIS sibling coverage: SPA-C · hub JIS G3125 Weathering Steel Plates · parent Weathering Steel Plates
  • International near-equivalents when the project cites ASTM / EN / GB instead: A242 Type 1, Q355GNH, S355J2WP, S355J0WP, Corten A, Corten B, S355J2W, A588

Supply, cutting and inspection for SPA-H

Item SHH STEEL supply note
Thickness Within JIS G3125 SPA-H applicable range ≤ 16 mm (plate / sheet / coil packages)
Size Width and length per order; cut-to-size plates on request; coil available when ordered as strip
Delivery condition As-rolled / controlled-rolled; normalized by agreement. Not quenched and tempered.
Processing Cutting, beveling, shot blasting / descaling available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs Grade SPA-H, thickness × width × length (or coil mass), quantity, delivery condition, surface/edge, inspection level

FAQ

What is the difference between SPA-H and SPA-C?
SPA-H is hot-rolled plate, strip and sections under JIS G3125 (applicable thickness ≤ 16 mm). SPA-C is the cold-rolled plate and strip counterpart (0.6-2.3 mm) with the same chemistry table but lower tensile/yield minima. See SPA-C.
Is SPA-H the same as Corten A or A242 Type 1?
Not automatically. SPA-H is often compared with Corten A, ASTM A242 Type 1, Q355GNH and EN WP grades, but substitution still depends on chemistry, mechanical properties, thickness limits and the project specification.
What thickness does JIS allow for SPA-H?
JIS G3125:2021 lists SPA-H applicable thickness as ≤ 16 mm for hot-rolled plate, strip and sections. SHH keeps supply notes inside that window unless a special mill agreement is documented.
What are fy and fu for SPA-H?
Minimum yield / proof stress is 355 N/mm² and minimum tensile strength is 490 N/mm² (with a possible ≥ 510 N/mm² agreement for plate/strip thinner than 3 mm). Elongation depends on thickness and test piece type. Confirm on the MTC.
Is SPA-H quenched and tempered?
No. Standard delivery is as-rolled or controlled-rolled; normalizing may be agreed. It is not quenched and tempered under JIS G3125.

Request a quotation

Send grade SPA-H, thickness × width × length (or coil mass / cut size), quantity, delivery condition (AR / controlled rolled / normalized if needed), surface/edge preference and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation for your weathering steel package.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: JIS G3125 Weathering Steel Plates · SPA-C · Weathering Steel Plates · A242 Type 1 · Q355GNH · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X