ASTM A606 Type 4 Steel Plate | A606/A606M Weathering Sheet
What is ASTM A606 Type 4 steel plate?
ASTM A606/A606M Type 4 is the enhanced atmospheric-corrosion track in A606. Type 4 and Type 5 provide a level of corrosion resistance substantially better than carbon steels with or without copper addition. When properly exposed to the atmosphere, Type 4 can be used bare for many applications (A606 1.1).
Scope note (A606 1.1): cold-rolled sheet/strip; hot-rolled sheet/strip in cut lengths or coils with ordered thickness less than 0.230 in [6.0 mm]; and hot-rolled sheet coils (not cut lengths) with ordered thickness 0.230 in [6.0 mm] and thicker. This is a sheet and strip specification. Cut-to-size plate packages are typically processed from coil within that scope.
Type 4 corrosion evidence path (A606 6.2.2): Guide G101 corrosion-resistance index ≥ 6.0 calculated from chemistry. Additional alloying (such as chromium, nickel, copper and phosphorus) is at the manufacturer’s discretion within Table 1 limits (note B). For the copper-minimum sibling track, see ASTM A606 Type 2.
SHH STEEL is a China mill-direct source for ASTM A606/A606M weathering sheet and strip products, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. Category hubs: ASTM A606/A606M · Weathering Steel Plates.
Related weathering pages: ASTM A242 Type 1 · EN 10025-5 S355J2WP · Corten A · GB/T 4171 Q355GNH · JIS G3125 SPA-H · Type 2.
Material Specification for ASTM A606 Type 4
| Parameter | Specification |
|---|---|
| Standard | ASTM A606/A606M (Primary reference ASTM A606/A606M-23; confirm ordered edition on the MTC) |
| Type | Type 4 |
| Family | HSLA sheet and strip with improved atmospheric corrosion resistance |
| Product form (ASTM) | Cold-rolled sheet/strip; hot-rolled sheet/strip (cut lengths or coils) < 6.0 mm; hot-rolled sheet coils ≥ 6.0 mm (not cut lengths) |
| SHH supply note | Sheet / strip / cut-from-coil plate packages within A606 scope; cut-to-size on request |
| Default strength class | Hot-rolled Grade 50 (if not specified); cold-rolled Grade 45 (if not specified); or CS by order |
| Delivery condition | Hot-rolled as standard for Type 2 / Type 4; annealed or normalized when specified on the PO |
| Surface / oiling | Dry or oiled as ordered; pickled / blast-cleaned when agreed |
| Edge | Mill edge or cut edge (must be specified for hot-rolled) |
| Dimensional references | ASTM A568/A568M, A635/A635M (HR sheet), A749/A749M (HR strip), A109/A109M (CR strip tolerances) |
| Certification | EN 10204 3.1 / 3.2 |
| Density | 7.85 g/cm³ |
Chemical Composition of ASTM A606 Type 4 (Table 1)
Limits below follow ASTM A606/A606M Table 1 for Type 2 and Type 4. Always verify the mill test certificate before fabrication or substitution.
| Element | Heat / cast analysis | Product check |
|---|---|---|
| C | ≤0.22 | ≤0.26 |
| Mn | ≤1.25 | ≤1.30 |
| S | ≤0.04 | ≤0.06 |
| Cu | ≥0.20 | ≥0.18 |
Heat and product C/Mn/S/Cu limits share Table 1 with Type 2. Additional alloying elements for Type 4 atmospheric performance are at the manufacturer’s discretion (Table 1 note B). Type 4 must meet Guide G101 minimum corrosion-resistance index 6.0 (6.2.2). Use the Larabee-Coburn or Townsend G101 method as required by composition (Note 5).
Enhanced atmospheric-corrosion HSLA sheet/strip. Producer adds alloying (such as Cr, Ni, Cu, P) so the steel reaches a Guide G101 corrosion-resistance index of at least 6.0. Intended for many bare (unpainted) atmospheric applications when properly exposed.
Mechanical Properties of ASTM A606 Type 4
Tensile requirements for material ordered as hot-rolled Grade 50 or cold-rolled Grade 45 under ASTM A606/A606M Tables 2 and 3. Material ordered as CS has no mandatory tensile properties unless agreed. Confirm ordered grade, condition and test orientation on the MTC.
| Condition / grade | Tensile strength min | Yield strength min | Elongation min |
|---|---|---|---|
| Hot-rolled Grade 50, as-rolled | ≥70 ksi [480 MPa] | ≥50 ksi [340 MPa] | ≥22% in 2 in [50 mm] |
| Hot-rolled Grade 50, annealed or normalized | ≥65 ksi [450 MPa] | ≥45 ksi [310 MPa] | ≥22% in 2 in [50 mm] |
| Cold-rolled Grade 45 | ≥65 ksi [450 MPa] | ≥45 ksi [310 MPa] | ≥22% in 2 in [50 mm] (≥20% for ≤0.0448 in [1.1 mm]) |
Yield strength may be determined by 0.2% offset or 0.5% extension under load unless otherwise specified (A606 7.2.4). For coil products, producer testing is limited to the coil end; properties throughout the coil shall still meet the minima.
Purchaser may require Charpy V-notch ≥ 15 ft-lbf [20 J] (or higher) at a specified temperature on a full-size 10 mm specimen (A606 7.4). Subsize limits follow ASTM A370.
Density is approximately 7.85 g/cm³.
Delivery Conditions for ASTM A606 Type 4
Unless otherwise specified, Type 2 and Type 4 are furnished as hot-rolled. Hot-rolled annealed or hot-rolled normalized must be stated on the purchase order. CS (commercial steel) has chemistry of Type 2, 4 or 5 but no mandatory tensile properties unless agreed.
Surface may be dry or oiled; pickled or blast-cleaned material is typically supplied with cut edges. SHH STEEL supplies the condition named on the order within the A606 sheet/strip scope.
Weldability of ASTM A606 Type 4
A606 states that steels listed in the specification are generally weldable with commonly obtained welding electrodes. When the steel is to be welded, use a suitable procedure based on composition, intended use and service temperatures (A606 1.3). Type 4 heats can carry higher alloying (including phosphorus in some practices) to reach the G101 index. Qualify the WPS on production-representative chemistry; do not assume a Type 2 WPS automatically covers every Type 4 heat.
Common processes include SMAW, GMAW and SAW. Prefer low-hydrogen consumables and consumables selected for weathering service when bare weld exposure is intended. Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved WPS. Matching or undermatching filler must be chosen so weld-metal atmospheric behaviour and strength meet the design intent.
Related fabrication-friendly alternatives when the project shifts standards: A242 Type 2, Q355NH, S355J2W.
Dimensional Tolerances for ASTM A606 Type 4
Dimensional tolerances follow the applicable general requirements cited by A606: ASTM A568/A568M and A635/A635M for hot-rolled sheet, A749/A749M for hot-rolled strip, and A109/A109M dimensional tables for cold-rolled strip, unless otherwise provided in A606. Not all producers can meet every thickness-tolerance table in A568/A568M; confirm capability before ordering (A606 Note 3).
Respect the A606 product-form and thickness windows. Do not assume heavy cut-length plate above the coil/sheet practice can be certified as A606 without checking the ordered form against 1.1. SHH STEEL can supply cut-to-size packages within the agreed scope.
Applications and service limits for ASTM A606 Type 4
Typical applications for A606 Type 4 (within sheet/strip scope):
- Truck and transport equipment frames and panels
- Architectural cladding, facade panels and landscape details
- Containers, cabinets and outdoor fabricated housings
- Structural and miscellaneous sheet components where atmospheric durability and weight saving matter
- RFQs that cite A606 Type 4 / bare weathering sheet (confirm match)
The self-protecting patina (especially on Type 4) can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material.
Related pages: Type 2 · ASTM A242 Type 1 · EN 10025-5 S355J2WP · Corten A · GB/T 4171 Q355GNH · JIS G3125 SPA-H · Weathering Steel Plates.
Atmospheric exposure guidance for ASTM A606 Type 4
Bare A606 Type 4 is intended for atmospheres where a stable patina can form and dry periodically (Type 4 is explicitly positioned for many bare uses when properly exposed). Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit for bare A606 Type 4 | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, higher-Ni practice, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for ASTM A606 Type 4
These grades are commonly compared with ASTM A606 Type 4. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, product form, thickness limits and the project specification before replacing one grade with another.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| ASTM A606/A606M | Type 4 | This page | – |
| ASTM A606/A606M | Type 2 | Same C/Mn/S/Cu table lines; Cu-minimum corrosion evidence | Type 2 |
| ASTM | A242 Type 1 | High-P A242 track; common bare-weathering comparison | A242 Type 1 |
| ASTM | A242 Type 2 | Lower-P A242; closer to Type 2 fabrication talk | A242 Type 2 |
| EN 10025-5 (WP) | S355J0WP / S355J2WP | EN P-bearing weathering talk | S355J0WP · S355J2WP |
| Commercial | Corten A | Common purchasing talk for Type 4 / WP chemistry | Corten A |
| GB/T 4171 | Q355GNH | High-P GNH talk; different thickness practice | Q355GNH |
| JIS G3125 | SPA-H / SPA-C | Superior high-P weathering sheet/plate talk | SPA-H · SPA-C |
| EN 10025-5 (W) | S355J2W | W-family; usually lower P than WP / Type 4 talk | S355J2W |
| Category | A606 / weathering hubs | Sheet/strip weathering family | ASTM A606/A606M · Weathering Steel Plates |
ASTM A606 Type 4 vs Type 2 vs A242 Type 1 / EN WP (selection aid)
These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.
| Item | A606 Type 4 | A606 Type 2 | A242 Type 1 / EN WP / SPA-H talk |
|---|---|---|---|
| Product form | Sheet and strip (A606 scope) | Sheet and strip (A606 scope) | Per each standard (often plate/sheet) |
| Corrosion evidence | Guide G101 index ≥ 6.0 | Cu minimum confirmation | Per A242 / EN / JIS edition |
| Bare exposure | Intended for many bare atmospheric uses when properly exposed | Enhanced vs carbon steel; not automatic Type 4 package | Often bare-weathering talk |
| When buyers ask | Spec cites A606 Type 4 / bare HSLA sheet | Spec cites A606 Type 2 | Spec cites A242 Type 1, Corten A, EN WP or SPA-H |
| Pages | This page | Type 2 | A242 Type 1 · S355J2WP · SPA-H |
Why choose SHH STEEL for ASTM A606 Type 4
- China mill-direct supply of ASTM A606/A606M Type 4 weathering sheet / strip / cut-from-coil packages
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Thickness and form kept honest to A606 scope (sheet/strip practice, not invented heavy-plate certification)
- Cutting, beveling and shot blasting / descaling available to shorten fabrication time
- Sibling coverage: ASTM A606 Type 2 · hub ASTM A606/A606M · parent Weathering Steel Plates
- International near-equivalents when the project cites other standards: ASTM A242 Type 1 · EN 10025-5 S355J2WP · Corten A · GB/T 4171 Q355GNH · JIS G3125 SPA-H
Supply, cutting and inspection for ASTM A606 Type 4
| Item | SHH STEEL supply note |
|---|---|
| Form / thickness | Within ASTM A606/A606M sheet and strip scope (including HR coils ≥ 6.0 mm where ordered as coils) |
| Size | Width and length / coil mass per order; cut-to-size packages on request |
| Delivery condition | Hot-rolled as standard; annealed or normalized when specified. Not Q&T for Type 2 / Type 4. |
| Processing | Cutting, beveling, shot blasting / descaling available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Type (Type 4), Grade 50 / Grade 45 / CS, thickness × width × length (or coil), quantity, HR/CR, dry/oiled, edge, delivery condition, inspection level |
FAQ
-
What makes Type 4 different from Type 2?
- Type 4 requires a Guide G101 corrosion-resistance index of at least 6.0 and additional alloying at the producer's discretion. Type 2 corrosion evidence is confirmation of the copper minimum. See Type 2.
-
Can Type 4 be used bare (unpainted)?
- Yes, when properly exposed to the atmosphere, Type 4 is intended for many bare applications (A606 1.1). Sheltered wet pockets, aggressive chlorides and immersion still need design review or coating.
-
Is A606 Type 4 the same as Corten A or A242 Type 1?
- Not automatically. Type 4 is often compared with Corten A, A242 Type 1, Q355GNH and EN WP grades, but substitution depends on chemistry, mechanical properties, product form and the project specification.
-
What strength class is ordered for hot-rolled Type 4?
- Hot-rolled Grade 50 is supplied if not otherwise specified. Cold-rolled defaults to Grade 45. CS may be ordered when chemistry matters more than mandatory tensile properties.
-
Is Type 4 quenched and tempered?
- No for standard Type 4 supply. Unless otherwise specified, Type 4 is furnished as hot-rolled; annealed or normalized hot-rolled must be ordered. (Type 5 under A606 has a distinct normalize / precipitation-harden practice; Type 5 is not covered on this page.)
Request a quotation
Send ASTM A606 Type 4, Grade 50 / Grade 45 / CS, thickness × width × length (or coil mass), hot-rolled or cold-rolled, dry/oiled, edge, delivery condition (as-rolled / annealed / normalized), quantity and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: ASTM A606/A606M · Type 2 · Weathering Steel Plates · A242 Type 1 · A242 Type 2 · Structural Steel Plates