Q235NH Steel Plate | GB/T 4171 NH Weathering Steel
What is Q235NH steel plate?
Q235NH belongs to the weldable weathering (NH) series of GB/T 4171. The series is intended for vehicles, bridges, containers, buildings and other welded, bolted or riveted outdoor structures where atmospheric corrosion resistance is required and weldability matters more than the high-phosphorus GNH package.
Order the quality letter with the grade (A, B, C, D or E), for example Q235NHC or Q235NHD. Quality levels change Charpy V-notch test temperature and minimum energy; they stay on this product page and are not separate SKUs.
SHH STEEL is a China mill-direct source for GB/T 4171 weathering plates. Category hubs: Weathering Steel Plates · GB/T 4171.
If the project needs the high-phosphorus patina package instead, see the GNH pages: Q235GNH · Q295GNH · Q345GNH · Q390GNH · Q355GNH. Sibling NH grades: Q235NH · Q295NH · Q355NH · Q415NH · Q460NH · Q500NH · Q550NH.
Material Specification for Q235NH
| Parameter | Specification |
|---|---|
| Standard | GB/T 4171 (edition as ordered; primary reference GB/T 4171-2008) |
| Grade | Q235NH (quality levels A-E as ordered, e.g. Q235NHD) |
| Family | Weldable weathering (NH) |
| Product form | Plate / strip (hot-rolled) |
| GB thickness limit (plate/strip) | ≤ 100 mm (larger by agreement) |
| SHH supply thickness | 6-100 mm (stock focus 8-50 mm) |
| Width | 1500-4000 mm (confirm for thin strip) |
| Length | 6000-16000 mm; cut-to-size on request |
| Delivery condition | As-rolled / controlled-rolled / normalized |
| Surface | As-rolled or shot blasted |
| Edge | Mill edge or cut edge |
| Certification | EN 10204 3.1 / 3.2 |
| Dimensional standard | GB/T 709 (hot-rolled plate/strip) |
| Density | 7.85 g/cm³ |
Chemical Composition of Q235NH (ladle analysis)
Ladle (heat) analysis limits below follow GB/T 4171-2008. Product analysis tolerances follow GB/T 222. Always verify the mill test certificate before fabrication or substitution.
| Grade | C | Si | Mn | P | S | Cu | Cr | Ni |
|---|---|---|---|---|---|---|---|---|
| Q235NH | ≤0.13* | 0.10-0.40 | 0.20-0.60 | ≤0.030 | ≤0.030 | 0.25-0.55 | 0.40-0.80 | ≤0.65 |
- *By agreement C may be ≤0.15%.
Optional micro-alloying per GB/T 4171: Nb 0.015-0.060%, V 0.02-0.12%, Ti 0.02-0.10%, Alt ≥0.020% (at least one reaches its lower limit when used in combination). Mo ≤0.30%, Zr ≤0.15% may be added. For Q415NH-Q550NH, Nb+V+Ti total ≤0.22%.
NH vs GNH: NH (weldable weathering) keeps phosphorus low (typically ≤0.025-0.030%) for better weldability. GNH (high weathering) intentionally elevates phosphorus to accelerate and densify the protective patina. Do not treat NH and GNH as interchangeable without a chemistry and fabrication review.
Mechanical Properties of Q235NH (including quality levels A-E)
Tensile requirements for Q235NH under GB/T 4171-2008. When yield is not pronounced, Rp0.2 may be used. Quality levels A-E stay on the same product page: they change Charpy temperature/energy, not the base grade chemistry table.
| Thickness (mm) | Yield ReL (MPa) | Tensile Rm (MPa) | Elongation A (%) |
|---|---|---|---|
| ≤16 | ≥235 | 360-510 | ≥25 |
| >16-40 | ≥225 | 360-510 | ≥25 |
| >40-60 | ≥215 | 360-510 | ≥24 |
| >60 | ≥215 | 360-510 | ≥23 |
Bend test: 180°: mandrel a (≤16 mm); 2a (>16 mm).
GB/T 4171-2008 Table 5 (longitudinal Charpy V-notch, 10x10x55 mm). Quality letter is part of the ordered designation (e.g. Q355NHD). High-weathering GNH grades may omit impact by agreement.
| Quality level | Test temperature | Min average KV2 |
|---|---|---|
| A | 20 °C | ≥ 47 J |
| B | 0 °C | ≥ 34 J |
| C | -20 °C | ≥ 34 J |
| D | -40 °C | ≥ 27 J |
| E | -40 °C | ≥ 27 J |
Density is approximately 7.85 g/cm³.
Delivery Conditions for Q235NH plate
As-rolled / controlled-rolled / normalized. Not quenched and tempered.
Hot-rolled weathering plates are normally supplied as-rolled. Controlled rolling (TMCP) or normalizing is used when toughness, thickness or fabrication needs require it. Normalization, when applied, is typically in the 900-950 °C range followed by air cooling, subject to mill practice.
Surface may be as-rolled or shot blasted. Stress relieving after fabrication is available when the purchaser specifies it. SHH STEEL supplies the delivery condition named on the order.
Weldability of Q235NH weathering steel
Q235NH is in the low-phosphorus weldable weathering family. Common processes include SMAW, GMAW and SAW. Use a qualified WPS. Low-hydrogen consumables (for example E7018-class or weathering-matched wires/electrodes agreed with the welding engineer) are preferred for many structural joints. Preheat and interpass temperature follow thickness, carbon equivalent, joint restraint and the approved procedure.
Matching or undermatching consumables must be chosen so the weld metal’s atmospheric corrosion behaviour and strength meet the design intent. Post-weld heat treatment is not normally required for atmospheric-exposure structures, but may be specified for critical joints. Compared with GNH high-P grades, Q235NH is generally the more fabrication-friendly choice when extensive welding is planned.
Dimensional Tolerances for Q235NH
Hot-rolled plate and strip dimensional tolerances follow GB/T 709 unless the order cites another dimensional standard. Width and length tolerances are normally agreed as plus-only or per GB/T 709 tables. Flatness follows the ordered class; tighter flatness and cut-to-size plates with edge preparation are available on request.
Respect the GB/T 4171 thickness window for this grade (plate/strip ≤ 100 mm unless otherwise agreed). SHH STEEL can supply cut-to-size plates within the agreed thickness range.
Applications and service limits for Q235NH
Typical applications for Q235NH:
- Highway and railway bridges (when GB/T 4171 NH is specified; bridge-dedicated GB/T 714 qNH grades are a separate track)
- Welded building frames and outdoor industrial structures
- Transmission and communication towers
- Containers, vehicle frames and rolling-stock components
- Architectural exteriors where weldable weathering chemistry is preferred
The self-protecting patina can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material. Bridge projects that cite GB/T 714 weathering bridge steel should not be auto-filled with GB/T 4171 grades.
Related pages: Weathering Steel Plates · A242 Type 1 · Corten A · Corten B · S355J2W · S355J2WP · A588 Gr.A · A709 50W.
Atmospheric exposure guidance for Q235NH
Bare Q235NH is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit for bare weathering plate | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, higher-Ni practice, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for Q235NH
These grades are commonly compared with Q235NH. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.
Approximate: EN 10025-5 S235J0W / S235J2W; JIS G3114 SMA400AW/BW/CW; ISO 4952 S235W.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| GB/T 4171 | Q235NH | This page | – |
| EN 10025-5 | S235J0W / S235J2W | Approximate | S235J0W · S235J2W |
| JIS G3114 | SMA400AW/BW/CW | Approximate | Weathering hub |
| GB/T 4171 | Q235GNH | High-P counterpart talk | Q235GNH |
| Category | GB/T 4171 hub | All NH / GNH product pages | GB/T 4171 · Weathering Steel Plates |
Q235NH vs Q355NH vs Q235GNH (selection aid)
Why choose SHH STEEL for Q235NH
- China mill-direct supply of Q235NH weathering plate under the GB/T 4171 family
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Supply thickness aligned to GB limits: 6-100 mm (stock focus 8-50 mm)
- Cutting, beveling and shot blasting available to shorten fabrication lead time
- Full NH and GNH coverage under one supply chain: GB/T 4171 hub · Weathering Steel Plates
- International near-equivalents available when the project cites ASTM / EN / JIS instead: A242 Type 1, S355J2W, S355J2WP, Corten A, Corten B, A588
Supply, cutting and inspection for Q235NH
| Item | SHH STEEL supply note |
|---|---|
| Thickness | 6-100 mm (stock focus 8-50 mm) (GB plate/strip limit ≤ 100 mm unless agreed) |
| Size | Width 1500-4000 mm; length 6000-16000 mm; cut-to-size on request |
| Delivery condition | As-rolled / controlled-rolled / normalized. Not quenched and tempered. |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade + quality letter (e.g. Q235NHD), thickness × width × length, quantity, delivery condition, inspection level |
FAQ
-
What does the quality letter mean on Q235NHA / B / C / D / E?
- Quality levels set Charpy V-notch test temperature and minimum energy (GB/T 4171 Table 5). They are ordered as part of the grade name and documented on this page; they are not separate product URLs.
-
What is the difference between Q235NH and Q235GNH?
- Q235NH is weldable NH (low P). Q235GNH is high-weathering GNH (elevated P). See Q235GNH for the high-P track.
-
What thickness can SHH supply for Q235NH?
- 6-100 mm (stock focus 8-50 mm). The GB/T 4171 plate/strip limit for this designation is ≤ 100 mm unless otherwise agreed with the mill.
-
What is Q235NH equivalent to?
- Approximate: EN 10025-5 S235J0W / S235J2W; JIS G3114 SMA400AW/BW/CW; ISO 4952 S235W. Substitution still requires project approval and MTC review.
-
Is Q235NH quenched and tempered?
- No. Standard delivery is as-rolled, controlled-rolled or normalized, not quenched and tempered.
Request a quotation
Send grade and quality letter (for example Q235NHD), thickness × width × length (or cut size), quantity, delivery condition (AR / normalized / controlled rolled), and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: GB/T 4171 · Weathering Steel Plates · A242 Type 1 · S355J2W