Product Showcase
JIS G3114 Carbon Steel Plates
SHH STEEL offers JIS G3114-compliant SMA 50AW weathering steel plates. JIS G3114 specifies hot-rolled atmospheric corrosion-resisting steels for welded structures like bridges and architecture. Durable, low-maintenance, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
SMA570P Steel Plate | JIS G3114 Weathering Steel
SMA570P is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. P-suffixed grades are normally used painted (JIS G3114 use note). Strength class is the 570 MPa tensile family. JIS applicable thickness for this designation is ≤ 100 mm. SHH STEEL supplies SMA570P plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA570W Steel Plate | JIS G3114 Weathering Steel
SMA570W is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 570 MPa tensile family. JIS applicable thickness for this designation is ≤ 100 mm. SHH STEEL supplies SMA570W plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA490CW Steel Plate | JIS G3114 Weathering Steel
SMA490CW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 490 MPa tensile family with quality letter C. JIS applicable thickness for this designation is ≤ 100 mm. SHH STEEL supplies SMA490CW plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA490BW Steel Plate | JIS G3114 Weathering Steel
SMA490BW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 490 MPa tensile family with quality letter B. JIS applicable thickness for this designation is ≤ 200 mm. SHH STEEL supplies SMA490BW plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA490AW Steel Plate | JIS G3114 Weathering Steel
SMA490AW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 490 MPa tensile family with quality letter A. JIS applicable thickness for this designation is ≤ 200 mm. SHH STEEL supplies SMA490AW plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA400CW Steel Plate | JIS G3114 Weathering Steel
SMA400CW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 400 MPa tensile family with quality letter C. JIS applicable thickness for this designation is ≤ 100 mm. SHH STEEL supplies SMA400CW plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA400BW Steel Plate | JIS G3114 Weathering Steel
SMA400BW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used bare or with rust-stabilizing treatment. Strength class is the 400 MPa tensile family with quality letter B. JIS applicable thickness for this designation is ≤ 200 mm. SHH STEEL supplies SMA400BW plate with EN 10204 3.1 (or 3.2) mill test certificates.View More -
SMA400AW Steel Plate | JIS G3114 Weathering Steel
SMA400AW is a hot-rolled atmospheric corrosion resisting steel for welded structures under JIS G3114. W-suffixed grades are normally used baView More
JIS G3114 Carbon Steel Plates
Weathering Steel Plates
SHH STEEL, a premier Weathering Steel Plates exporter, produces and exports weathering steel plates for outdoor structures like bridges and architecture. Our plates, such as Corten steel, provide corrosion resistance and aesthetic appeal, meeting ASTM standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Corten steel plates and custom weather-resistant solutions.
Weathering Steel Plates