SMA400AW Steel Plate | JIS G3114 Weathering Steel
What is SMA400AW steel plate (JIS G3114)?
JIS G3114 SMA400AW belongs to the hot-rolled atmospheric corrosion resisting steels for welded structure family. The standard covers bridges, buildings and other welded outdoor structures where atmospheric corrosion resistance and weldability are required.
W-suffixed grades are normally used bare or with rust-stabilizing treatment. W-suffixed grades are normally used bare or with rust-stabilizing treatment. P-suffixed grades are normally used painted. Do not auto-substitute W and P chemistries. The final letter before W/P is the quality level for Charpy practice: A has no mandatory Table 8 Charpy row; B is 0 °C / ≥ 27 J; C is 0 °C / ≥ 47 J (thickness > 12 mm).
JIS product forms for this designation: Plate, strip, sections and flat bars. Applicable thickness: ≤ 200 mm. Do not assume thicker material can be certified as SMA400AW without a special agreement outside the JIS thickness table.
SHH STEEL is a China mill-direct source for JIS G3114 weathering plates, with EN 10204 3.1 (or 3.2) mill test certificates. Category hubs: JIS G3114 Weathering Steel Plates · Weathering Steel Plates.
Sibling grades under the same hub: JIS G3114 SMA400BW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P. Related international pages: GB/T 4171 Q355NH · Q235NH · Q355GNH · JIS G3125 SPA-H · SPA-C · ASTM A242 Type 1 · A242 Type 2 · EN 10025-5 S355J2W · S355J2WP · Corten A · Corten B · ASTM A606 Type 2 · A606 Type 4.
Material Specification for SMA400AW
| Parameter | Specification |
|---|---|
| Standard | JIS G3114 (Primary reference JIS G3114:2008 (ISO 4952:2006 MOD); confirm ordered edition on the MTC) |
| Grade | SMA400AW |
| Family | Hot-rolled atmospheric corrosion resisting steel for welded structure (W / bare track) |
| Product form (JIS) | Plate, strip, sections and flat bars |
| JIS applicable thickness | ≤ 200 mm |
| SHH supply note | Within JIS ≤ 200 mm window (stock focus often 8-50 mm when available; confirm mill); cut-to-size on request |
| Width | Per order / mill practice (confirm for strip) |
| Length | Cut length or coil; cut-to-size plates on request |
| Delivery condition | As-rolled / normalized / TMC as agreed |
| Surface | As-rolled or descaled / shot blasted as agreed |
| Edge | Mill edge or cut edge |
| Dimensional references | JIS G 3193 (plate/strip); JIS G 3192 (sections); JIS G 3194 (flat bars) |
| Certification | EN 10204 3.1 / 3.2 |
| Corresponding ISO talk | ISO 4952 (MOD basis noted in JIS G3114:2008) |
| Density | 7.85 g/cm³ |
Chemical Composition of SMA400AW (ladle / heat analysis, JIS G3114:2008)
Ladle (heat) analysis limits below follow JIS G3114:2008 Table 2 for SMA400AW. Always verify the mill test certificate before fabrication or substitution.
| Grade | C | Si | Mn | P | S | Cu | Cr | Ni |
|---|---|---|---|---|---|---|---|---|
| SMA400AW | ≤0.18 | 0.15-0.65 | ≤1.25 | ≤0.035 | ≤0.035 | 0.30-0.50 | 0.45-0.75 | 0.05-0.30 |
Other alloying elements may be added as necessary. When Mo, Nb, Ti and/or V are added for weathering effectiveness, their total shall not exceed 0.15% (JIS G3114:2008 Table 2 note).
W vs P chemistry: W grades use higher Cu/Cr/Ni ranges intended for bare or rust-stabilized service. P grades use a painted-service chemistry package (lower Cu/Cr ranges; Ni not specified in the P table). Do not substitute a P heat for a W designation (or the reverse) without project approval.
Mechanical Properties of SMA400AW (JIS G3114:2008)
Tensile requirements for SMA400AW under JIS G3114:2008 Table 7. Yield point or proof stress depends on thickness. Tensile strength upper limit applies to plate, strip and flat bars (sections by purchaser option). Confirm ordered thickness and test piece type on the MTC.
| Thickness (mm) | Yield / proof (N/mm²) | Tensile Rm (N/mm²) |
|---|---|---|
| ≤16 | ≥245 | 400-540 |
| >16-40 | ≥235 | 400-540 |
| >40-75 | ≥215 | 400-540 |
| >75-100 | ≥215 | 400-540 |
| >100-160 | ≥205 | 400-540 |
| >160-200 | ≥195 | 400-540 |
Elongation (Table 7) depends on thickness and tensile test piece:
| Thickness | Test piece | Elongation min (%) |
|---|---|---|
| ≤5 mm | No.5 | ≥22 |
| >5-16 mm | No.1A | ≥17 |
| >16-50 mm | No.1A | ≥21 |
| >40 mm | No.4 | ≥23 |
SMA400AW is an A-quality designation. JIS G3114 Table 8 does not list a mandatory Charpy row for A grades. If the project needs impact values, specify temperature and energy on the order and confirm mill capability.
Charpy applies to steels listed in JIS G3114 Table 8 when thickness exceeds 12 mm. Average of three longitudinal V-notch specimens. A-quality letters (SMA400AW / SMA490AW) have no mandatory Charpy row in Table 8. Purchaser may specify higher energy or lower test temperature by agreement.
Density is approximately 7.85 g/cm³.
Delivery Conditions for SMA400AW
As-rolled as common supply; normalized (N), tempered (T) or TMC by agreement. Heat-treatment symbols are appended to the grade designation when applied (e.g. SMA490BWN).
When heat treatment is applied, append the symbol to the grade designation (examples in JIS: N, T, Q, TMC). Surface may be as-rolled or descaled / shot blasted as agreed. SHH STEEL supplies the delivery condition named on the order within the JIS ≤ 200 mm window for SMA400AW.
Weldability of SMA400AW weathering steel
SMA400AW is designed as a weldable atmospheric corrosion resisting steel under JIS G3114. Qualify SMAW / GMAW / SAW (or other agreed processes) on production-representative chemistry. Prefer low-hydrogen consumables and consumables selected for weathering service when bare weld exposure is intended.
Keep hydrogen control, preheat and interpass aligned with thickness, carbon equivalent and joint restraint.
Related alternatives when the project shifts standards: Q355NH · Q235NH · S355J2W · A242 Type 2 · A606 Type 2.
Dimensional Tolerances for SMA400AW
Shape, dimensions, mass and permissible variations follow JIS G 3193 for hot-rolled plate and strip, JIS G 3192 for sections, and JIS G 3194 for flat bars, unless another agreement is cited. For cut-edge plate/strip, width and length tolerances default to JIS G 3193 tolerance A unless otherwise specified.
Respect the JIS G3114 applicable thickness for SMA400AW (≤ 200 mm). SHH STEEL can supply cut-to-size plates and edge preparation within the agreed thickness range.
Applications and service limits for SMA400AW
Typical applications for SMA400AW (within JIS ≤ 200 mm):
- Highway and railway bridges (when JIS G3114 is specified)
- Building frames and outdoor industrial structures
- Transmission and communication towers
- Welded outdoor fabrications where bare weathering chemistry is specified
- RFQs historically calling EN W / GB NH / ASTM weathering packages at similar strength talk (confirm match)
The self-protecting patina on W grades can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. P grades are intended for painted service. Sheltered wet pockets, aggressive chloride splash and continuous immersion often need coating or another material.
Related pages: SMA400BW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P · SPA-H · Q355NH · Q355GNH · S355J2W · S355J2WP · A242 Type 1 · A242 Type 2 · Corten A · Corten B · Weathering Steel Plates.
Atmospheric exposure guidance for SMA400AW
Bare SMA400AW is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable bare | Needs wet/dry cycles for patina on bare W grades |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, higher-Ni practice, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for SMA400AW
These grades are commonly compared with SMA400AW. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.
Approximate: EN 10025-5 S235J0W / S235J2W; GB/T 4171 Q235NH; ISO 4952 S235W talk. Confirm against project specs.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| JIS G3114 | SMA400AW | This page | – |
| JIS G3114 | Sibling SMA grades | Same standard; different strength / quality / W-P track | SMA400BW · SMA400CW · SMA490AW · SMA490BW · SMA490CW · SMA570W · SMA570P |
| EN 10025-5 | S235J0W / S235J2W | Approximate W talk for 400 class | S235J0W · S235J2W |
| GB/T 4171 | Q235NH | Approximate NH talk | Q235NH |
| Commercial | Corten B | Purchasing talk (confirm strength class) | Corten B |
| JIS G3125 | SPA-H / SPA-C | High-P superior weathering; different JIS family | SPA-H · SPA-C |
| EN 10025-5 (WP) | S355J0WP / S355J2WP | P-bearing EN talk (closer to GNH / SPA-H than to SMA W) | S355J0WP · S355J2WP |
| Category | JIS G3114 / weathering hubs | All SMA product pages | JIS G3114 hub · Weathering Steel Plates |
SMA400AW vs SMA490AW vs Q235NH (selection aid)
These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.
| Item | SMA400AW | SMA490AW | Q235NH / EN S235W talk |
|---|---|---|---|
| Strength class | 400 MPa tensile family | 490 MPa tensile family | Per GB / EN edition |
| Track | Bare/W | Bare/W | Weldable NH / W |
| JIS thickness | ≤ 200 mm | ≤ 200 mm | Per GB/T 4171 |
| When buyers ask | Spec cites SMA400AW | Higher strength JIS SMA | Spec cites GB NH or EN S235W |
| Pages | This page | SMA490AW | Q235NH · S235J2W |
Why choose SHH STEEL for SMA400AW
- China mill-direct supply of JIS G3114 SMA400AW weathering plate / strip within the JIS ≤ 200 mm window
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Thickness kept honest to JIS G3114 (no invented certification above the applicable thickness)
- Cutting, beveling and shot blasting available to shorten fabrication time
- Full SMA coverage under one hub: JIS G3114 Weathering Steel Plates · parent Weathering Steel Plates
- International near-equivalents when the project cites ASTM / EN / GB / JIS G3125 instead: Q355NH, Q355GNH, S355J2W, S355J2WP, A242 Type 1, A242 Type 2, SPA-H, Corten A, Corten B
Supply, cutting and inspection for SMA400AW
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Within JIS ≤ 200 mm window (stock focus often 8-50 mm when available; confirm mill) |
| Size | Width and length per order; cut-to-size plates on request; coil available when ordered as strip |
| Delivery condition | As-rolled / normalized / TMC as agreed. |
| Processing | Cutting, beveling, shot blasting / descaling available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade SMA400AW, thickness × width × length (or coil), quantity, delivery condition / heat-treatment symbol, surface/edge, inspection level |
FAQ
-
What does the W or P mean on SMA400AW?
- W-suffixed JIS G3114 grades are normally used bare or with rust-stabilizing treatment. P-suffixed grades are normally used painted and follow a different chemistry table. See the chemical composition section and JIS G3114 hub.
-
What do the A / B / C letters mean?
- For SMA400 and SMA490, A/B/C are quality letters tied to Charpy practice (Table 8): A has no mandatory Charpy row; B is 0 °C / ≥ 27 J; C is 0 °C / ≥ 47 J for thickness > 12 mm. SMA570 uses -5 °C / ≥ 47 J.
-
What thickness does JIS allow for SMA400AW?
- JIS G3114:2008 lists applicable thickness ≤ 200 mm for SMA400AW. SHH keeps supply notes inside that window unless a special mill agreement is documented.
-
What is SMA400AW equivalent to?
- Approximate: EN 10025-5 S235J0W / S235J2W; GB/T 4171 Q235NH; ISO 4952 S235W talk. Confirm against project specs. Substitution still requires project approval and MTC review.
-
Is SMA400AW quenched and tempered?
- Not as a default. Common supply is as-rolled; normalized or TMC may be agreed. Q&T is not the usual route for SMA400/SMA490.
Request a quotation
Send grade SMA400AW, thickness × width × length (or coil mass / cut size), quantity, delivery condition / heat-treatment symbol, surface/edge preference and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation for your weathering steel package.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: JIS G3114 Weathering Steel Plates · Weathering Steel Plates · SPA-H · Q355NH · S355J2W · Structural Steel Plates