ASTM A242 Type 1 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL
ASTM A242 Type 1 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL
ASTM A242 Type 1 Steel Plate | ASTM A242/A242M Weathering Steel - SHH STEEL

ASTM A242 Type 1 Steel Plate | A242 Gr.1 Weathering Steel

ASTM A242 Type 1 (also called A242 Gr.1) is a high-strength low-alloy weathering steel plate made for outdoor structures that need higher strength than ordinary carbon steel and better atmospheric corrosion resistance than grades such as ASTM A36. In outdoor exposure it forms a dense, adherent oxide layer (patina) that slows further corrosion and can reduce the need for continuous painting where the environment suits bare weathering steel.
Equivalent Grades:
ASTM A242 Type 1 / EN 10025-5 S355J0WP or S355J2WP / JIS G3125 SPA-H / GB/T 4171 Q355GNH (often compared with Corten A). Confirm against project specs.
Heat Treatment
As-rolled (AR) or controlled-rolled / TMCP as standard; normalized by agreement (typically 900–950 °C, then air cool). This is weathering HSLA plate, not quenched and tempered.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
A242 Type 1 vs Corten vs A588
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A242 Type 1 steel?

ASTM A242 Type 1 (also called A242 Gr.1) is a high-strength low-alloy weathering steel plate made for outdoor structures that need higher strength than ordinary carbon steel and better atmospheric corrosion resistance than grades such as ASTM A36. In outdoor exposure it forms a dense, adherent oxide layer (patina) that slows further corrosion and can reduce the need for continuous painting where the environment suits bare weathering steel.

Approximate equivalents (confirm against project specs): ASTM A242 Type 1 / EN 10025-5 S355J0WP or S355J2WP / JIS G3125 SPA-H / GB/T 4171 Q355GNH (often compared with Corten A).

Browse related ranges: Weathering Steel Plates · Structural Steel Plates · Corten A / B · ASTM A588 / A588M.

Material note: ASTM A242 / A242M. Usual delivery is as-rolled (AR) or controlled-rolled / TMCP; normalized by agreement. This is weathering HSLA plate, not quenched and tempered.

ASTM A242 Type 1 steel plate is a weathering structural grade under ASTM A242 / A242M. Compared with ASTM A36 / A36M, it offers higher strength and better long-term performance in many outdoor atmospheres. The higher phosphorus content in Type 1 is intentional: it helps form a stable protective patina. Copper is mandatory; chromium and nickel may be added when the purchaser specifies them.

Common uses include bridges, building facades, transmission towers, architectural structures, and other outdoor work where maintenance access is limited or costly.

SHH STEEL supplies ASTM A242 Type 1 plate as a China mill-direct source, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. Plates can be supplied as-rolled, normalized, or controlled-rolled to project requirements. For the wider weathering range, see Weathering Steel Plates.

Material Specification

Parameter Specification
Standard ASTM A242 / A242M
Grade Type 1 (A242 Gr.1)
Product form Plate
Thickness 6–100 mm (stock 8–50 mm)
Width 1500–4000 mm
Length 6000–16000 mm
Delivery condition As-rolled / Normalized / Controlled rolled
Surface As-rolled or shot blasted
Edge Mill edge or cut edge
Certification EN 10204 3.1 / 3.2
Density 7.85 g/cm³
Hardness 140–180 HB (typical, as-rolled)

Chemical Composition

ASTM A242 Type 1 is controlled by ladle analysis and product analysis. Typical limits:

Element Ladle Analysis (%) Product Analysis (%)
Carbon (C) ≤ 0.15 ≤ 0.15
Manganese (Mn) ≤ 1.00 ≤ 1.00
Phosphorus (P) 0.15 max 0.15 max
Sulfur (S) ≤ 0.05 ≤ 0.05
Copper (Cu) ≥ 0.20 ≥ 0.20
Silicon (Si) 0.25–0.75 0.25–0.75
Chromium (Cr) 0.50–1.25* 0.50–1.25*
Nickel (Ni) ≤ 0.65* ≤ 0.65*

* Chromium and nickel are added when specified by the purchaser. Elevated phosphorus is a defining feature of Type 1 and supports patina formation. Copper is required for atmospheric corrosion resistance. Product analysis allows the small deviations permitted by ASTM A242.

Mechanical Properties

Thickness Tensile Strength Yield Strength Elongation
≤ 19 mm 480–620 MPa ≥ 345 MPa ≥ 18%
> 19 to 38 mm 460–620 MPa ≥ 315 MPa ≥ 18%
> 38 to 102 mm 435–620 MPa ≥ 290 MPa ≥ 16%

Hardness is typically 140–180 HB in the as-rolled condition. Density is approximately 7.85 g/cm³.

Delivery Conditions

Plates are normally supplied as-rolled. For thicker plates or when improved toughness is required, normalized or controlled-rolled delivery can be arranged. Normalization is typically performed at 900–950 °C followed by air cooling. Stress relieving after fabrication can be carried out if the purchaser specifies it. SHH STEEL supplies the delivery condition required by the project.

Weldability

ASTM A242 Type 1 welds with common processes including SMAW, GMAW, and SAW. Because of the higher phosphorus content, preheating is recommended for sections thicker than about 20–25 mm to reduce the risk of hydrogen cracking. Low-hydrogen electrodes such as E7018 or equivalent are preferred. Post-weld heat treatment is not normally required for atmospheric-exposure applications, but may be specified for critical structures. Qualified welding procedures and consumable selection are required for joint performance.

Tolerances

Dimensional tolerances comply with ASTM A6/A6M. Typical thickness tolerance is ±0.3 mm for plates up to 10 mm and increases with thickness. Width and length tolerances are normally +20 mm / –0 mm unless otherwise agreed. Flatness follows ASTM A6 Class A, or tighter if requested. SHH STEEL can supply cut-to-size plates with tighter tolerances and edge preparation on request.

Applications and service limits

Typical applications:

  • Highway and railway bridges
  • Building exteriors and architectural cladding
  • Transmission and communication towers
  • Outdoor sculptures and landscaping structures
  • Container and railcar components
  • Marine and coastal structures with moderate exposure

The self-protecting patina can lower long-term maintenance cost versus painted carbon steel in many rural and industrial atmospheres. It is not a universal substitute for coating systems: sheltered pockets that stay wet, aggressive chloride environments, and continuously immersed or heavily polluted marine sites often need extra protection or a different material selection. For European phosphorus-bearing weathering grades, see EN 10025-5 S355J0WP and S355J2WP. For bridge-oriented weathering grades, see also ASTM A709 Grade 50W and ASTM A709 weathering plates.

Atmospheric exposure guidance

Bare ASTM A242 Type 1 is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit for bare A242 Type 1 Note
Rural / mild industrial Usually suitable Patina forms with wet/dry cycles
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating or a different grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

Equivalent and related grades

These grades are commonly compared with ASTM A242 Type 1. They are not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits, and the project specification before replacing one grade with another.

Standard / family Grade Relation to A242 Type 1 Product page
Commercial Corten A Closest commercial name often used in purchasing Corten A Steel Plate
Commercial Corten B Related weathering grade; closer to A588-type chemistry in many projects Corten B Steel Plate
ASTM A588 Grade A / B / C / K Similar weathering role; different chemistry and property tables A588 Gr.A · Gr.B · Gr.C · Gr.K
EN 10025-5 (P-bearing) S355J0WP / S355J2WP Closest EN phosphorus-bearing weathering pair for Type 1 discussions S355J0WP · S355J2WP
EN 10025-5 (W family) S355J0W / S355J2W / S355K2W Related weathering steels; different impact and composition packages S355J0W · S355J2W · S355K2W
JIS G3125 SPA-H; SMA490AW / SMA570W (G3114 family) Japanese weathering grades often listed in cross-reference tables See Weathering Steel Plates
GB Q355GNH / Q355NH / Q345GNH (GB/T 4171 family) Chinese weathering grades commonly listed as near equivalents See Weathering Steel Plates
ASTM bridge A709 Grade 50W Bridge weathering grade; specify by A709 when the project requires it A709 Grade 50W

Many projects accept ASTM A242 Type 1 as a candidate substitute for Corten A when chemical and mechanical requirements are met. See Corten A Steel Plate and the Corten A / B series for purchasing alternatives.

A242 Type 1 vs Corten A vs ASTM A588 (selection aid)

These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes. Confirm chemistry, mechanical properties, toughness, and thickness limits against the project specification.

Item ASTM A242 Type 1 Corten A (commercial) ASTM A588 (Gr. A/B typical)
Role High-strength weathering plate; Type 1 uses higher P for patina Commercial name commonly compared with A242 Type 1 Structural weathering plate widely used for bridges and frames
Phosphorus Elevated in Type 1 (intentional) Usually similar “Type A” chemistry story in purchasing Generally lower P than A242 Type 1
Strength class See A242 thickness table (e.g. ≥345 MPa yield ≤19 mm) Match to mill datasheet / agreed equivalent Follow A588 grade and thickness table
Closest EN talk track S355J0WP / S355J2WP (P-bearing) Often mapped to WP / Corten A discussions Often mapped to EN W grades (e.g. S355J2W)
When buyers ask for it Spec calls out ASTM A242 Type 1 / A242 Gr.1 RFQ says “Corten A” Spec calls out A588 or bridge weathering without A242

Related product pages: Corten A · A588 Gr.A · S355J0WP · S355J2WP · S355J2W.

Why choose SHH STEEL for A242 Type 1

  • China mill-direct supply of ASTM A242 Type 1 weathering plate
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Stock focus on common thicknesses 8–50 mm; production range 6–100 mm
  • Cutting, beveling, and shot blasting available to shorten fabrication lead time
  • Related grades under one supply chain: A588, Corten A/B, EN 10025-5 WP/W, A709 50W

Supply, cutting, and inspection

Item SHH STEEL supply note
Thickness Production 6–100 mm; common stock focus 8–50 mm
Size Width 1500–4000 mm; length 6000–16000 mm; cut-to-size on request
Delivery condition As-rolled / normalized / controlled-rolled per order
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV, or ABS can be arranged
Quotation needs Thickness × width × length (or cut size), quantity, delivery condition, inspection level

FAQ

What are the ASTM types under A242?
ASTM A242 has Type 1 and Type 2. Type 1 has higher phosphorus and is generally used where atmospheric corrosion resistance outdoors is the priority. Type 2 has lower phosphorus and is often preferred when weldability is the stronger concern. Both belong to the weathering steel family.
Is A242 Gr.1 the same as Corten A?
ASTM A242 Type 1 (A242 Gr.1) is the closest standard grade commonly compared with Corten A. Both develop a protective patina and serve similar outdoor roles. Substitution still depends on chemistry, mechanical properties, and the project specification.
What are fy and fu for A242 Type 1?
For plates up to 19 mm thick, minimum yield strength (fy) is 345 MPa and tensile strength (fu) is 480–620 MPa. For thicker plates, minimum yield decreases by thickness range as shown in the mechanical properties table above.
What is ASTM A242 Type 1 equivalent to?
It is commonly compared with Corten A, EN 10025-5 S355J0WP / S355J2WP, JIS G3125 SPA-H, and Chinese GB/T 4171 grades such as Q355GNH. Related (not identical) options include A588 and EN W grades such as S355J2W. Exact substitution must follow the project specification.

Request a quotation

Send thickness × width × length (or cut size), quantity, delivery condition (AR / normalized / controlled rolled), and any inspection requirement. SHH STEEL will return mill availability, certification scope, and a quotation for your weathering steel package.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: Weathering Steel Plates · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X