Q460NH Steel Plate | GB/T 4171 NH Weathering Steel
What is Q460NH steel plate?
Q460NH belongs to the weldable weathering (NH) series of GB/T 4171. The series is intended for vehicles, bridges, containers, buildings and other welded, bolted or riveted outdoor structures where atmospheric corrosion resistance is required and weldability matters more than the high-phosphorus GNH package.
Order the quality letter with the grade (A, B, C, D or E), for example Q460NHC or Q460NHD. Quality levels change Charpy V-notch test temperature and minimum energy; they stay on this product page and are not separate SKUs.
SHH STEEL is a China mill-direct source for GB/T 4171 weathering plates. Category hubs: Weathering Steel Plates · GB/T 4171.
If the project needs the high-phosphorus patina package instead, see the GNH pages: Q235GNH · Q295GNH · Q345GNH · Q390GNH · Q355GNH. Sibling NH grades: Q235NH · Q295NH · Q355NH · Q415NH · Q460NH · Q500NH · Q550NH.
Material Specification for Q460NH
| Parameter | Specification |
|---|---|
| Standard | GB/T 4171 (edition as ordered; primary reference GB/T 4171-2008) |
| Grade | Q460NH (quality levels A-E as ordered, e.g. Q460NHD) |
| Family | Weldable weathering (NH) |
| Product form | Plate / strip (hot-rolled) |
| GB thickness limit (plate/strip) | ≤ 60 mm (larger by agreement) |
| SHH supply thickness | 6-60 mm |
| Width | 1500-4000 mm (confirm for thin strip) |
| Length | 6000-16000 mm; cut-to-size on request |
| Delivery condition | As-rolled / controlled-rolled / normalized; quenched and tempered permitted for Q460NH per GB/T 4171-2008 |
| Surface | As-rolled or shot blasted |
| Edge | Mill edge or cut edge |
| Certification | EN 10204 3.1 / 3.2 |
| Dimensional standard | GB/T 709 (hot-rolled plate/strip) |
| Density | 7.85 g/cm³ |
Chemical Composition of Q460NH (ladle analysis)
Ladle (heat) analysis limits below follow GB/T 4171-2008. Product analysis tolerances follow GB/T 222. Always verify the mill test certificate before fabrication or substitution.
| Grade | C | Si | Mn | P | S | Cu | Cr | Ni |
|---|---|---|---|---|---|---|---|---|
| Q460NH | ≤0.12 | ≤0.65 | ≤1.50 | ≤0.025 | ≤0.030* | 0.20-0.55 | 0.30-1.25 | 0.12-0.65** |
- *By agreement S may be ≤0.008%.
- **By agreement Ni lower limit may be waived.
- Nb+V+Ti total ≤0.22%.
Optional micro-alloying per GB/T 4171: Nb 0.015-0.060%, V 0.02-0.12%, Ti 0.02-0.10%, Alt ≥0.020% (at least one reaches its lower limit when used in combination). Mo ≤0.30%, Zr ≤0.15% may be added. For Q415NH-Q550NH, Nb+V+Ti total ≤0.22%.
NH vs GNH: NH (weldable weathering) keeps phosphorus low (typically ≤0.025-0.030%) for better weldability. GNH (high weathering) intentionally elevates phosphorus to accelerate and densify the protective patina. Do not treat NH and GNH as interchangeable without a chemistry and fabrication review.
Mechanical Properties of Q460NH (including quality levels A-E)
Tensile requirements for Q460NH under GB/T 4171-2008. When yield is not pronounced, Rp0.2 may be used. Quality levels A-E stay on the same product page: they change Charpy temperature/energy, not the base grade chemistry table.
| Thickness (mm) | Yield ReL (MPa) | Tensile Rm (MPa) | Elongation A (%) |
|---|---|---|---|
| ≤16 | ≥460 | 570-730 | ≥20 |
| >16-40 | ≥450 | 570-730 | ≥20 |
| >40-60 | ≥440 | 570-730 | ≥19 |
Bend test: 180°: mandrel a (≤6 mm); 2a (>6-16); 3a (>16).
GB/T 4171-2008 Table 5 (longitudinal Charpy V-notch, 10x10x55 mm). Quality letter is part of the ordered designation (e.g. Q355NHD). High-weathering GNH grades may omit impact by agreement.
| Quality level | Test temperature | Min average KV2 |
|---|---|---|
| A | 20 °C | ≥ 47 J |
| B | 0 °C | ≥ 34 J |
| C | -20 °C | ≥ 34 J |
| D | -40 °C | ≥ 27 J |
| E | -40 °C | ≥ 27 J |
Density is approximately 7.85 g/cm³.
Delivery Conditions for Q460NH plate
As-rolled / controlled-rolled / normalized; quenched and tempered permitted for Q460NH per GB/T 4171-2008.
Hot-rolled weathering plates are normally supplied as-rolled. Controlled rolling (TMCP) or normalizing is used when toughness, thickness or fabrication needs require it. Normalization, when applied, is typically in the 900-950 °C range followed by air cooling, subject to mill practice.
For Q460NH, GB/T 4171-2008 also allows quenched and tempered delivery. State Q+T explicitly on the purchase order when required; otherwise as-rolled / controlled-rolled / normalized is the usual path.
Surface may be as-rolled or shot blasted. Stress relieving after fabrication is available when the purchaser specifies it. SHH STEEL supplies the delivery condition named on the order.
Weldability of Q460NH weathering steel
Q460NH is in the low-phosphorus weldable weathering family. Common processes include SMAW, GMAW and SAW. Use a qualified WPS. Low-hydrogen consumables (for example E7018-class or weathering-matched wires/electrodes agreed with the welding engineer) are preferred for many structural joints. Preheat and interpass temperature follow thickness, carbon equivalent, joint restraint and the approved procedure.
Matching or undermatching consumables must be chosen so the weld metal’s atmospheric corrosion behaviour and strength meet the design intent. Post-weld heat treatment is not normally required for atmospheric-exposure structures, but may be specified for critical joints. Compared with GNH high-P grades, Q460NH is generally the more fabrication-friendly choice when extensive welding is planned.
Dimensional Tolerances for Q460NH
Hot-rolled plate and strip dimensional tolerances follow GB/T 709 unless the order cites another dimensional standard. Width and length tolerances are normally agreed as plus-only or per GB/T 709 tables. Flatness follows the ordered class; tighter flatness and cut-to-size plates with edge preparation are available on request.
Respect the GB/T 4171 thickness window for this grade (plate/strip ≤ 60 mm unless otherwise agreed). SHH STEEL can supply cut-to-size plates within the agreed thickness range.
Applications and service limits for Q460NH
Typical applications for Q460NH:
- Highway and railway bridges (when GB/T 4171 NH is specified; bridge-dedicated GB/T 714 qNH grades are a separate track)
- Welded building frames and outdoor industrial structures
- Transmission and communication towers
- Containers, vehicle frames and rolling-stock components
- Architectural exteriors where weldable weathering chemistry is preferred
The self-protecting patina can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material. Bridge projects that cite GB/T 714 weathering bridge steel should not be auto-filled with GB/T 4171 grades.
Related pages: Weathering Steel Plates · A242 Type 1 · Corten A · Corten B · S355J2W · S355J2WP · A588 Gr.A · A709 50W.
Atmospheric exposure guidance for Q460NH
Bare Q460NH is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit for bare weathering plate | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, higher-Ni practice, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for Q460NH
These grades are commonly compared with Q460NH. They are approximate, not automatic substitutes. Match chemistry, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.
Approximate: ISO 4952 S460W; JIS G3114 SMA570W/P; ASTM A871 Grade 65 talk. Confirm.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| GB/T 4171 | Q460NH | This page | – |
| EN 10025-5 | S355J2W family (strength class dependent) | W talk track | S355J2W |
| ASTM | A588 / A709 50W | Related weathering role | A588 · A709 50W |
| Commercial | Corten B | Often closer for NH/W discussions | Corten B |
| Category | GB/T 4171 hub | All NH / GNH product pages | GB/T 4171 · Weathering Steel Plates |
Q460NH vs Q415NH vs Q500NH (selection aid)
Why choose SHH STEEL for Q460NH
- China mill-direct supply of Q460NH weathering plate under the GB/T 4171 family
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Supply thickness aligned to GB limits: 6-60 mm
- Cutting, beveling and shot blasting available to shorten fabrication lead time
- Full NH and GNH coverage under one supply chain: GB/T 4171 hub · Weathering Steel Plates
- International near-equivalents available when the project cites ASTM / EN / JIS instead: A242 Type 1, S355J2W, S355J2WP, Corten A, Corten B, A588
Supply, cutting and inspection for Q460NH
| Item | SHH STEEL supply note |
|---|---|
| Thickness | 6-60 mm (GB plate/strip limit ≤ 60 mm unless agreed) |
| Size | Width 1500-4000 mm; length 6000-16000 mm; cut-to-size on request |
| Delivery condition | As-rolled / controlled-rolled / normalized; quenched and tempered permitted for Q460NH per GB/T 4171-2008. |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade + quality letter (e.g. Q460NHD), thickness × width × length, quantity, delivery condition, inspection level |
FAQ
-
What does the quality letter mean on Q460NHA / B / C / D / E?
- Quality levels set Charpy V-notch test temperature and minimum energy (GB/T 4171 Table 5). They are ordered as part of the grade name and documented on this page; they are not separate product URLs.
-
What is the difference between Q460NH and Q460GNH?
- Q460NH is weldable NH (low P). Q460GNH is high-weathering GNH (elevated P). See Q355GNH for the high-P track.
-
What thickness can SHH supply for Q460NH?
- 6-60 mm. The GB/T 4171 plate/strip limit for this designation is ≤ 60 mm unless otherwise agreed with the mill.
-
Can Q460NH replace A242, Corten or S355J2W?
- Only when the project specification allows the substitution and chemistry, toughness, thickness and delivery condition are checked. See the equivalent-grade section and Weathering Steel Plates.
-
Is quenched and tempered delivery allowed?
- Q+T is permitted for this grade under GB/T 4171-2008 when ordered; otherwise AR / controlled-rolled / normalized is standard.
Request a quotation
Send grade and quality letter (for example Q460NHD), thickness × width × length (or cut size), quantity, delivery condition (AR / normalized / controlled rolled / Q+T), and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: GB/T 4171 · Weathering Steel Plates · A242 Type 1 · S355J2W