EN 10025-5 S235J0W Steel Plate | S235J0W Weathering Steel
General Description
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-5 S235J0W Steel Plate (Material Number: 1.8958).
S235J0W is a structural steel with improved atmospheric corrosion resistance under the European standard EN 10025-5. The “W” designation indicates enhanced resistance to atmospheric corrosion through the formation of a stable protective oxide layer (patina). It provides a minimum yield strength of 235 MPa (for thickness ≤ 16 mm) and is impact tested at 0°C with a minimum energy of 27 J. This grade is suitable for outdoor applications where moderate strength combined with good weathering performance is required, and painting costs can be reduced or eliminated.
SHH STEEL sources S235J0W plates directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery. We supply thicknesses from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | EN 10025-5 | Full compliance |
| Steel Grade | S235J0W (1.8958) | Confirmed |
| Delivery Condition | As-rolled, Normalized or TMCP | Available |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 150 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / 3.2 | Available |
Chemical Composition
Chemical composition according to EN 10025-5 (Ladle Analysis and Product Analysis):
| Element | Ladle Analysis Max. / Range (%) | Product Analysis Max. / Range (%) |
|---|---|---|
| Carbon (C) | ≤ 0.13 | ≤ 0.16 |
| Silicon (Si) | ≤ 0.40 | ≤ 0.45 |
| Manganese (Mn) | 0.20 – 0.60 | 0.15 – 0.70 |
| Phosphorus (P) | ≤ 0.035 | ≤ 0.040 |
| Sulfur (S) | ≤ 0.035 | ≤ 0.040 |
| Chromium (Cr) | 0.40 – 0.80 | 0.35 – 0.85 |
| Nickel (Ni) | ≤ 0.65 | ≤ 0.70 |
| Copper (Cu) | 0.25 – 0.55 | 0.20 – 0.60 |
| Molybdenum (Mo) | ≤ 0.30 | ≤ 0.35 |
| Nitrogen (N) | ≤ 0.009 | ≤ 0.010 |
Note: The combination of chromium, copper and nickel provides the improved atmospheric corrosion resistance that distinguishes weathering steels from conventional structural steels.
Mechanical Properties
Mechanical properties of EN 10025-5 S235J0W (longitudinal direction):
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) | Impact Energy KV (min) |
|---|---|---|---|---|
| ≤ 16 | 235 MPa | 360 – 510 MPa | 26% | 27 J at 0°C |
| > 16 ≤ 40 | 225 MPa | 360 – 510 MPa | 26% | 27 J at 0°C |
| > 40 ≤ 63 | 215 MPa | 360 – 510 MPa | 25% | 27 J at 0°C |
| > 63 ≤ 80 | 215 MPa | 360 – 510 MPa | 24% | 27 J at 0°C |
| > 80 ≤ 100 | 215 MPa | 360 – 510 MPa | 24% | 27 J at 0°C |
| > 100 ≤ 150 | 195 MPa | 350 – 500 MPa | 22% | 27 J at 0°C |
Density: 7.85 g/cm³
Delivery Conditions
SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-5 S235J0W steel plate in as-rolled, normalized or thermomechanically rolled condition according to customer requirements.
Additional options:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160)
- Z-direction testing (Z15 / Z25 / Z35)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for S235J0W steel plate follow EN 10029.
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to EN 10029.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
S235J0W has excellent weldability, similar to conventional S235 structural steels. The alloying elements added for corrosion resistance do not significantly affect welding performance when proper procedures are followed.
Recommended welding consumables:
| Welding Process | Recommended Consumables |
|---|---|
| SMAW (Stick) | E7018, E7016 |
| GMAW (MIG/MAG) | ER70S-6 |
| FCAW | E71T-1 |
| SAW | EM12K + suitable flux |
Preheating is generally not required. Matching weathering steel consumables can be used when the weld itself must also form a protective patina.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| S235J0W | EN 10025-5 | — |
| 1.8958 | EN | Material number |
| Q235NH / Q235GNH | GB/T 4171 | Closest Chinese weathering steels |
| Corten (approx.) | ASTM A242 / A588 | Similar weathering concept |
| WTSt 37-2 | DIN (old) | Former designation |
Applications
EN 10025-5 S235J0W is widely used in outdoor structures where atmospheric corrosion resistance is required and strength demands are moderate. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Facades, external frames – S235J0W Structural Steel |
| Bridges | Secondary bridge components – S235J0W Bridge |
| Containers & Shipping | Containers, cargo handling – S235J0W Container |
| Railway Vehicles | Wagon structures – S235J0W Railway |
| Sculptures & Architecture | Outdoor sculptures, architectural elements – S235J0W Architecture |
| General Outdoor Fabrication | Weathering steel structures – S235J0W Fabrication |
Why Choose SHH STEEL
SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-5 S235J0W Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for weathering steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What does the “W” in S235J0W mean?
- “W” indicates improved atmospheric corrosion resistance (weathering steel). The steel forms a stable protective oxide layer (patina) when exposed to the atmosphere.
-
What is the difference between S235J0W and S355J0W?
- Both are weathering steels. S235J0W has a lower yield strength of 235 MPa, while S355J0W has 355 MPa. S235J0W is suitable for less demanding structural applications.
-
What is the material number of S235J0W?
- 1.8958
-
Is S235J0W similar to Corten steel?
- Yes. S235J0W is a weathering steel with similar atmospheric corrosion resistance characteristics to Corten-type steels, but at a lower strength level.
Conclusion
EN 10025-5 S235J0W (1.8958) Steel Plate from SHH STEEL is a weathering structural steel offering 235 MPa yield strength and improved atmospheric corrosion resistance. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S235J0W weathering steel plate requirements.
Contact SHH STEEL today for stock availability, pricing and technical support. EN 10025-5 S235J0W Steel Plate, S235J0W steel plate, S235J0W weathering steel, EN 10025 S235J0W, S235J0W equivalent, S235J0W supplier, 1.8958