ISO 630-5 S235W Steel Plate | ISO↔EN 10025-5 Map
What is ISO 630-5 S235W steel plate?
ISO 630-5 S235W belongs to ISO 630-5 Annex A structural weathering steels. Class: W (standard phosphorus weathering). ISO 630-5 Annex A grade designations (S235W, S295W, S355W, S355WP, S420W, …) overlap heavily with EN 10025-5 W/WP purchasing. These pages map ISO ↔ EN and link to existing EN product pages. They are not an SEO grade farm that duplicates every EN URL.
ISO designation uses a grade name plus a quality letter (Qualities A (no impact), B (+20 °C), C (0 °C), D and D1 (-20 °C; D1 higher energy), E (-40 °C).). It does not embed EN-style J0 / J2 tokens inside the ISO grade string. ISO qualities C / D / E align in temperature talk with EN J0 / J2 packages. Order the ISO quality letter explicitly; do not invent an ISO grade named S235J2W.
For day-to-day purchasing, start from the matching EN pages: EN 10025-5 S235J0W · EN 10025-5 S235J2W. Category hubs: ISO 630-5 · EN 10025-5 · Weathering Steel Plates.
Sibling ISO pages: ISO 630-5 S355W · ISO 630-5 S355WP. Related: Corten B · Q355NH · ASTM A242 Type 1 · JIS G3125 SPA-H.
Material Specification for ISO 630-5 S235W
| Parameter | Specification |
|---|---|
| Standard | ISO 630-5 (Primary reference ISO 630-5:2023; confirm ordered edition on the MTC) |
| Grade | S235W + quality letter (A-E / D1 as ordered) |
| Class | W (standard phosphorus weathering) |
| EN map (primary) | S235J0W / S235J2W |
| Product form | Plate (reversing mill), wide flats, hot-rolled sections and bars (not sheet/strip; not tubular) |
| Thickness window | Plates / wide flats / sections / bars: maximum nominal thickness 150 mm for S235W under ISO 630-5:2023 |
| Delivery condition | S235 / S295 / S355 families: as-rolled, normalized/normalized rolled, TMCP or Q&T as ordered. Higher S420-S550: TMCP or Q&T. |
| Certification | EN 10204 3.1 / 3.2; ISO 10474 inspection documents as ordered; dual EN 10025-5 marking when agreed |
| Density | 7.85 g/cm³ |
Chemical Composition guidance for ISO 630-5 S235W (EN dual-cert talk)
Important: ISO 630-5 heat and product analysis shall meet Tables A.1 / A.2 of the ordered edition. Public preview copies of ISO 630-5 often omit the full annex tables, so this page does not invent ISO cell values. When mills dual-certify to EN 10025-5, the EN chemistry below is the practical purchasing reference. Always verify every element on the MTC against the ordered ISO (and EN, if dual-certified) edition.
EN heat-analysis talk commonly used when mills dual-certify ISO 630-5 S235W with EN 10025-5 S235J0W / S235J2W. Confirm ISO Table A.1 on the MTC.
| Element | EN 10025-5 S235J0W / S235J2W (dual-cert talk) |
|---|---|
| C | ≤0.13 |
| Si | ≤0.40 |
| Mn | 0.20-0.60 |
| P | ≤0.035 |
| S | ≤0.035 (J0) / ≤0.030 (J2) |
| Cr | 0.40-0.80 |
| Cu | 0.25-0.55 |
| Ni | ≤0.65 |
Optional micro-alloying / nitrogen-binding practice follows the ordered standard (Al, Nb, V, Ti as applicable). Mo and Zr may appear within EN / ISO limits.
Mechanical Properties guidance for ISO 630-5 S235W
Mechanical properties for ISO 630-5 S235W shall meet Table A.3 (tensile) and Table A.4 (Charpy) of the ordered edition. Common dual-cert talk with EN 10025-5 uses the values below as a purchasing guide. Confirm every figure on the MTC.
| Item | Purchasing guide |
|---|---|
| Yield class | ≥235 MPa (≤16 mm class; thickness steps per ISO Table A.3) |
| Tensile class | About 360-510 MPa class (confirm ISO Table A.3 / dual-cert EN package) |
| Impact | ISO qualities C / D / E align in temperature talk with EN J0 / J2 packages. Order the ISO quality letter explicitly; do not invent an ISO grade named S235J2W. |
Prefer ordering against the live EN product page when the contract accepts EN 10025-5: EN 10025-5 S235J0W · EN 10025-5 S235J2W.
Density is approximately 7.85 g/cm³.
Delivery Conditions for ISO 630-5 S235W
S235 / S295 / S355 families: as-rolled, normalized/normalized rolled, TMCP or Q&T as ordered. Higher S420-S550: TMCP or Q&T.
The delivery condition shall be indicated in the inspection document. SHH STEEL supplies the condition named on the order and can dual-mark ISO 630-5 + EN 10025-5 when the mill package supports it.
Weldability of ISO 630-5 S235W
S235W is intended for welded or bolted structures. See ISO 630-5 Annex C for weldability notes and follow a qualified WPS based on composition, thickness and service temperature. W grades are generally the more fabrication-friendly track versus WP.
Related EN fabrication pages: EN 10025-5 S235J0W · EN 10025-5 S235J2W. Also: Q355NH · A588 Grade A.
Dimensional Tolerances for ISO 630-5 S235W
Dimensions, tolerances and mass follow ISO 630-1 as referenced by ISO 630-5, unless the order cites another dimensional agreement (for dual-cert EN packages, EN 10029 / EN 10051 etc. may apply as ordered).
Plates / wide flats / sections / bars: maximum nominal thickness 150 mm for S235W under ISO 630-5:2023
Applications and service limits for ISO 630-5 S235W
Typical applications for S235W (ISO / EN dual-cert talk):
- Bridges and outdoor structural frames
- Building facades and architectural weathering structures
- Vehicles, containers and industrial outdoor fabrications
- RFQs that cite ISO 630-5 S235W or the matching EN 10025-5 grade
Prefer the EN product pages for detailed fabrication content: EN 10025-5 S235J0W · EN 10025-5 S235J2W.
Related: ISO 630-5 S355W · ISO 630-5 S355WP · Corten A · Corten B · A242 Type 1 · SPA-H · Weathering Steel Plates.
Atmospheric exposure guidance for ISO 630-5 S235W
Bare S235W is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit for bare ISO / EN weathering plate | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, WSE talk, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
ISO 630-5 also defines S355WSE (saline-environment weathering) as a separate class; it is not covered on this page.
ISO 630-5 S235W ↔ EN 10025-5 map and related grades
These grades are commonly compared with ISO 630-5 S235W. They are approximate, not automatic substitutes. Prefer the EN product page when the purchase order cites EN 10025-5.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| ISO 630-5 | S235W | This page | – |
| ISO 630-5 | S355W | Sibling ISO designation | S355W |
| ISO 630-5 | S355WP | Sibling ISO designation | S355WP |
| EN 10025-5 | S235J0W | Primary overlap / dual-cert map | S235J0W |
| EN 10025-5 | S235J2W | Primary overlap / dual-cert map | S235J2W |
| Commercial / ASTM | Corten B / A588 | W-family talk | Corten B · A588 Gr.A |
| GB/T 4171 | Q355NH / Q235NH | NH talk by strength class | Q355NH · Q235NH |
| Category | ISO / EN hubs | Navigation | ISO 630-5 · EN 10025-5 · Weathering Steel Plates |
ISO 630-5 S235W vs sibling ISO vs EN 10025-5 (selection aid)
Selection aid for ISO ↔ EN purchasing. Not automatic substitutes.
| Item | S235W | S355W | EN S235J2W |
|---|---|---|---|
| Standard home | ISO 630-5 | ISO 630-5 | EN 10025-5 (live product pages) |
| Phosphorus track | W (standard P) | W (standard P) | W |
| When buyers ask | PO cites ISO 630-5 S235W | PO cites ISO 630-5 S355W | PO cites EN 10025-5 |
| Pages | This page | S355W | EN 10025-5 S235J0W · EN 10025-5 S235J2W |
Why choose SHH STEEL for ISO 630-5 S235W
- China mill-direct supply of ISO 630-5 S235W / EN 10025-5 dual-cert weathering plate when the mill package supports it
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection on request
- Content strategy: map ISO ↔ EN and link existing EN pages instead of duplicating grade farms
- Cutting, beveling and shot blasting available
- Hubs: ISO 630-5 · EN 10025-5 · Weathering Steel Plates
- Primary EN targets: EN 10025-5 S235J0W · EN 10025-5 S235J2W
Supply, cutting and inspection for ISO 630-5 S235W
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Within ISO 630-5 window for S235W; confirm against ordered form |
| Size | Width / length per order; cut-to-size on request |
| Delivery condition | As ordered (AR / N / TMCP / Q&T per ISO rules for the grade family) |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request; dual ISO+EN marking when agreed |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | ISO 630-5 S235W + quality letter (and/or EN grade), thickness × width × length, quantity, delivery condition, inspection level |
FAQ
-
Is ISO 630-5 S235W the same as EN 10025-5?
- Not identical as a document, but purchasing overlap is strong. Prefer the EN product pages when the contract cites EN 10025-5: EN 10025-5 S235J0W · EN 10025-5 S235J2W. Dual-certification is common when mill practice supports both.
-
How do ISO qualities map to EN J0 / J2?
- ISO qualities C / D / E align in temperature talk with EN J0 / J2 packages. Order the ISO quality letter explicitly; do not invent an ISO grade named S235J2W.
-
Why does this page avoid inventing ISO chemistry cells?
- ISO Annex tables are normative and edition-specific. This page gives EN dual-cert chemistry as a practical reference and requires MTC verification against ISO 630-5 Tables A.1 / A.2.
-
Should I order ISO or EN on the PO?
- Order the document the project specification cites. If both are acceptable, naming the EN grade often matches existing steelspecs product pages and mill dual-cert practice.
-
Are S295W / S420W / S460W covered here?
- Not in this tight set. See INDEX.md for the overlap note and future-page list. S355W / S355WP / S235W are the priority ISO↔EN maps.
Request a quotation
Send ISO 630-5 S235W + quality letter (and/or the matching EN 10025-5 grade), thickness × width × length, quantity, delivery condition and any inspection requirement. SHH STEEL will return mill availability, dual-cert options and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: ISO 630-5 · EN 10025-5 · EN 10025-5 S235J0W · EN 10025-5 S235J2W · Weathering Steel Plates · Structural Steel Plates