GB/T 3621 TA2G Titanium Plate | TA2 Commercially Pure Titanium
What is GB/T 3621 TA2G titanium plate?
GB/T 3621 TA2G titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TA2G is the Chinese designation for Grade 2-type commercially pure titanium and the most widely ordered CP grade in China. Buyers still often write TA2; GB/T 3621-2022 lists TA2 and TA2G separately, so confirm which one is meant.
Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.
Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.
SHH STEEL handles TA2G plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 2, ASME SB-265 Grade 2, AMS 4902 Grade 2.
Material specification for GB/T 3621 TA2G
GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.
| Ordering item | GB/T 3621 basis |
|---|---|
| Standard | GB/T 3621-2022 (state the edition if an older one is required) |
| Grade | TA2G (TA2 Commercially Pure Titanium) |
| Condition | Annealed (M) |
| Size range (2022) | 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long |
| Marking example | Plate TA2G M 1.0×1000×2000 GB/T 3621 |
| Certificate | Quality certificate with chemistry, tensile results and other agreed tests |
Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.
The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.
Chemical composition of GB/T 3621 TA2G
Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.03 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.015 max |
| Iron (Fe) | 0.3 max |
| Oxygen (O) | 0.25 max |
| Other elements, each | 0.1 max |
| Other elements, total | 0.4 max |
| Titanium (Ti) | Balance |
Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.
Mechanical properties of GB/T 3621 TA2G
The values below are the requirements for TA2G plate in the annealed (M) condition.
| Thickness, mm | Tensile strength Rm, MPa | Proof strength Rp0.2, MPa | Elongation A, min, % |
|---|---|---|---|
| 0.3–50.0 | 400 min | 275–450 | 25 |
These are the room-temperature requirements of GB/T 3621-2022 for the annealed condition. The yield range has an upper limit as well as a lower one, which protects formability.
Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.
Delivery condition, finish and marking
GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.
- Condition: Annealed (M)
- Surface: pickled, ground or machined, as agreed
- Marking: grade, condition, size, heat number and standard number
- Packing: to GB/T 8180, or as stated on the contract
CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.
Welding and fabrication of TA2G titanium plate
TA2G is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.
- Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
- Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
- Use matching CP filler metal unless the design engineer specifies otherwise
- Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
- Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up
Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.
For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.
If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of TA2G titanium plate
Typical uses of TA2G plate include:
- Heat exchanger tube sheets, shells and channel covers in seawater and brine service
- Chemical process vessels, columns and tank linings
- Chlor-alkali, chlorine dioxide and pulp bleaching equipment
- Desalination plant, offshore and marine components
Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.
When selecting TA2G, compare it with TA1G, TA3G, TA4G. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare TA2G with other GB/T 3621 grades
The grades below are the closest neighbours of TA2G in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| TA1G | 240 MPa min | 140–310 MPa | 30% | Softest GB CP grade |
| TA2G | 400 MPa min | 275–450 MPa | 25% | Most common GB CP grade |
| TA3G | 500 MPa min | 380–550 MPa | 20% | Higher-strength GB CP grade |
| TA4G | 580 MPa min | 485–655 MPa | 20% | Highest-strength GB CP grade |
A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.
GB/T 3621 TA2G equivalent grades
The designations below are commonly compared with GB/T 3621 TA2G. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GB/T 3621 TA2G |
|---|---|---|
| ASTM B265 | Grade 2 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 2 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| AMS 4902 | CP titanium, annealed | Aerospace specification; tighter oxygen and added melting and grain-size requirements |
| JIS H4600 | Class 2 (TP340) | Close equivalent; JIS strength range and tests differ |
| GOST 22178 | VT1-0 | Approximate; GOST limits and sheet scope differ |
| ISO 5832-2 | Grade 2 | Implant-grade counterpart; medical scope and tighter controls |
| UNS | R50400 | Same unified number as ASTM Grade 2 |
| DIN / EN material number | 3.7035 (Ti 2) | Close CP equivalent; check the ordered European standard |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for TA2G titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
- Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GB/T 3621 TA2G plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GB/T 3621 TA2G, edition |
| Product form | Plate or sheet; condition as listed for the grade |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Which edition of GB/T 3621 applies to TA2G?
- GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
-
What is the tensile strength of GB/T 3621 TA2G titanium plate?
- The requirement is 400 MPa minimum. The 0.2% proof or yield strength is 275–450 MPa. Minimum elongation is 25%. Values apply to the condition and thickness range stated in the standard.
-
What is TA2G mainly used for?
- Typical uses include heat exchanger tube sheets, shells and channel covers in seawater and brine service, chemical process vessels, columns and tank linings and chlor-alkali, chlorine dioxide and pulp bleaching equipment. The design engineer should confirm the grade for the actual service.
-
What sizes does GB/T 3621-2022 cover?
- Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
-
What should I send for a quotation?
- Send GB/T 3621 TA2G, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GB/T 3621 TA2G titanium plate
GB/T 3621 TA2G is TA2 commercially pure titanium specified for 400 MPa minimum tensile strength, 275–450 MPa yield or proof strength and 25% minimum elongation in the annealed (M) condition. Typical uses include heat exchanger tube sheets, shells and channel covers in seawater and brine service and chemical process vessels, columns and tank linings.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com