AMS 4902 Grade 2 Titanium Plate | CP Titanium (UNS R50400)

AMS 4902 Grade 2 titanium plate is CP titanium (UNS R50400 (composition similar)) supplied annealed. It is specified for 345 MPa minimum tensile strength, 276–448 MPa yield and 20% minimum elongation. Typical uses include aerospace ducting and formed sheet parts. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
AMS 4902 Grade 2 titanium plate, AMS 4902 titanium plate, UNS R50400 (composition similar) plate, CP titanium plate, AMS 4902 titanium sheet
Equivalent Grades:
UNS R50400, ASTM B265 Gr.2, ASME SB-265 Gr.2, JIS Class 2 (TP340), GB/T TA2G, GOST VT1-0 (approx.), ISO 5832-2 Gr.2, 3.7035
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is AMS 4902 Grade 2 titanium plate?

AMS 4902 Grade 2 titanium plate is made to AMS 4902, the SAE aerospace material specification for annealed commercially pure titanium sheet, strip and plate. It carries the UNS number R50400 (composition similar). AMS 4902 covers one grade of commercially pure titanium sheet, strip and plate up to 1.000 in (25.40 mm) thick, annealed to a 40.0 ksi (276 MPa) minimum yield strength, with composition similar to UNS R50400. Its oxygen limit of 0.20% is tighter than the 0.25% of ASTM B265 Grade 2.

Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

AMS specifications are written for aerospace procurement. Each covers one material, form and condition, and the purchaser’s drawing names the revision. AMS 4902 is the common call-out for CP titanium sheet and plate in airframe and engine secondary structure.

SHH STEEL handles CP titanium plate enquiries within its range of titanium alloy plates and sheets, checking the ordered AMS 4902 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 2, ASME SB-265 Grade 2, JIS H4600 Class 2 TP340.

Material specification for AMS 4902 CP titanium

AMS 4902 is an SAE aerospace material specification for one grade of commercially pure titanium sheet, strip and plate, annealed to a 40.0 ksi (276 MPa) minimum yield strength. It covers product up to and including 1.000 in (25.40 mm) thick, with composition similar to UNS R50400.

Ordering item AMS 4902 basis
Specification AMS 4902, current revision unless the drawing names another
Material Commercially pure titanium, composition similar to UNS R50400 (Grade 2 type)
Product forms Sheet, strip and plate up to 1.000 in (25.40 mm) inclusive
Melting Cold-hearth melting, or multiple melting with the final melt under vacuum
Condition Sheet and strip hot rolled with or without cold reduction, annealed, descaled and levelled; plate hot rolled, annealed, descaled and flattened
Annealing 1200–1500 °F (649–816 °C), or validated continuous annealing for sheet and strip
Traceability Production and distribution to AS6279

Plate must be produced as plate; bar, billet or forgings may not be supplied in its place. The product must be free of alpha case and surface contamination, uniform in quality and free from oil cans beyond the flatness tolerance. Any exception to the specification must be authorised by the purchaser and reported on the certificate.

Chemical composition of AMS 4902 CP titanium (UNS R50400 (composition similar))

Composition is determined by the analytical methods required by the specification, with hydrogen determined on the product.

Element Limit, % by weight
Iron (Fe) 0.30 max
Oxygen (O) 0.20 max
Carbon (C) 0.08 max
Nitrogen (N) 0.05 max (500 ppm)
Hydrogen (H) 0.0150 max (150 ppm)
Other elements, each 0.10 max
Other elements, total 0.30 max
Titanium (Ti) Remainder

The 0.20% oxygen maximum is tighter than the 0.25% limit for ASTM B265 Grade 2. It is the main reason a B265 Grade 2 certificate cannot be assumed to meet AMS 4902.

Mechanical properties of AMS 4902 CP titanium

The values below are the requirements for CP titanium plate in the annealed condition.

Property Requirement
Tensile strength, min 50.0 ksi (345 MPa)
Yield strength, 0.2% offset 40.0–65.0 ksi (276–448 MPa)
Elongation in 2 in (50.8 mm) or 4D, min 20% (product 0.025 in / 0.64 mm and over)
Bend factor, up to 0.070 in (1.78 mm) 2 × nominal thickness, 105°, no cracking at 20X
Bend factor, over 0.070–0.1874 in (1.78–4.76 mm) 2.5 × nominal thickness
Grain size ASTM No. 6 or finer

The yield range has an upper limit as well as a lower one, which protects formability. Bend tests are made with the axis of bend parallel to the rolling direction and must show no cracking when examined at 20X. Grain size must be ASTM No. 6 or finer.

Elevated-temperature design values are not set by the specification and come from the purchaser’s design data.

Delivery condition, finish and marking

Plate is hot rolled, annealed, descaled and flattened, with a surface comparable to a No. 1 finish on corrosion-resistant steel. Sheet and strip are hot rolled with or without cold reduction, annealed, descaled and levelled, with a surface comparable to a No. 2D finish.

  • Condition: annealed, per the specification
  • Surface: descaled, free of alpha case and other surface contamination
  • Quality: uniform, sound and free from oil cans beyond flatness tolerance, ripples and foreign material
  • Marking and packing: per the specification and the purchase order, with heat and lot identification

Report and marking requirements follow the specification revision on the order. If a size outside the specification range is ordered, the exception must be authorised by the purchaser and reported.

Welding and fabrication of CP titanium titanium plate

CP titanium is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.

  • Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
  • Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
  • Use matching CP filler metal unless the design engineer specifies otherwise
  • Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
  • Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up

Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.

For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Tolerances conform to AMS 2242, the SAE tolerance specification for titanium and titanium alloy sheet, strip and plate. For AMS 4911 plate, special flatness may be specified, in which case the special flatness tolerances of AMS 2242 apply.

State nominal thickness, width, length and quantity, and any cut-to-size drawing or special flatness requirement on the order. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of CP titanium titanium plate

Typical uses of CP titanium plate include:

  • Aerospace ducting and formed sheet parts
  • Airframe secondary structure
  • Firewalls and heat shields
  • Parts needing aqueous corrosion resistance up to 400 °F (204 °C)

Typical service is moderate strength up to 400 °F (204 °C) and oxidation resistance up to 600 °F (316 °C). Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.

When selecting CP titanium, compare it with ASTM B265 Grade 2, ASME SB-265 Grade 2, JIS H4600 Class 2 (TP340). The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare CP titanium with related grades

The grades below are commonly compared with this material across standards. Values are minimum tensile, yield and minimum elongation as set by each standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
CP titanium, annealed 50.0 ksi (345 MPa) 40.0–65.0 ksi (276–448 MPa) 20% Aerospace CP titanium (Grade 2-type)
ASTM B265 Grade 2 (R50400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% General process equipment
ASME SB-265 Grade 2 (R50400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% General process equipment
JIS H4600 Class 2 (TP340) 340–510 MPa 215 MPa min 23% Most common JIS CP class
GB/T 3621 TA2G 400 MPa min 275–450 MPa 25% Most common GB CP grade

A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.

AMS 4902 CP titanium equivalent grades

The designations below are commonly compared with AMS 4902 CP titanium. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to AMS 4902 CP titanium
ASTM B265 Grade 2 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 2 ASME Code version of the ASTM grade; ordered for pressure equipment
JIS H4600 Class 2 (TP340) Close equivalent; JIS strength range and tests differ
GB/T 3621 TA2G Close equivalent; confirm grade name and limits in the ordered edition
GOST 22178 VT1-0 Approximate; GOST limits and sheet scope differ
ISO 5832-2 Grade 2 Implant-grade counterpart; medical scope and tighter controls
UNS R50400 Same unified number as ASTM Grade 2
DIN / EN material number 3.7035 (Ti 2) Close CP equivalent; check the ordered European standard

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for CP titanium titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the AMS 4902 revision on your drawing and keep it distinct from ASTM B265 Grade 2
  • Certificates are checked against the 0.20% oxygen limit, yield range, bend factor and grain size
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for AMS 4902 CP titanium plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material AMS 4902 CP titanium, revision
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Is AMS 4902 the same as ASTM B265 Grade 2?
Both are Grade 2-type CP titanium, but AMS 4902 limits oxygen to 0.20% instead of 0.25%, caps yield at 65.0 ksi (448 MPa), and adds melting, grain size and surface contamination requirements. B265 Grade 2 plate does not automatically meet AMS 4902.
What is the tensile strength of AMS 4902 CP titanium titanium plate?
The requirement is 50.0 ksi (345 MPa) minimum. The 0.2% proof or yield strength is 40.0–65.0 ksi (276–448 MPa). Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is CP titanium mainly used for?
Typical uses include aerospace ducting and formed sheet parts, airframe secondary structure and firewalls and heat shields. Typical service is moderate strength up to 400 °F (204 °C) and oxidation resistance up to 600 °F (316 °C).
What thickness does AMS 4902 cover?
Sheet, strip and plate up to and including 1.000 in (25.40 mm). Elongation applies to product 0.025 in (0.64 mm) and over.
What should I send for a quotation?
Send AMS 4902 CP titanium, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for AMS 4902 Grade 2 titanium plate

AMS 4902 CP titanium is CP titanium, UNS R50400 (composition similar), specified for 50.0 ksi (345 MPa) minimum tensile strength, 40.0–65.0 ksi (276–448 MPa) yield or proof strength and 20% minimum elongation in the annealed condition. Typical uses include aerospace ducting and formed sheet parts and airframe secondary structure.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the AMS 4902 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X