GB/T 3621 TA8 Titanium Plate | Lean Pd Titanium

GB/T 3621 TA8 titanium plate is lean-Pd titanium supplied annealed (M). It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
GB/T 3621 TA8 titanium plate, TA8 titanium plate, lean-Pd titanium plate, GB/T 3621 titanium sheet, GB/T 3621 TA8 titanium sheet
Equivalent Grades:
UNS R52402, ASTM B265 Gr.16, ASME SB-265 Gr.16, JIS Class 18 (TP345Pd)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 3621 TA8 titanium plate?

GB/T 3621 TA8 titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TA8 is Ti-0.05Pd at Grade 2-type interstitial levels. The lean palladium addition improves crevice and reducing-acid corrosion resistance; it corresponds in role to ASTM Grade 16.

This grade belongs to the corrosion-resistant alloyed group: its base is commercially pure titanium, and small additions such as palladium, ruthenium, nickel, molybdenum, cobalt, chromium or tantalum change how the oxide film behaves in reducing acids and tight crevices. Strength still depends mainly on oxygen and iron, so mechanical properties track the matching CP strength level, and the material is used in the annealed condition.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.

SHH STEEL handles TA8 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 16, ASME SB-265 Grade 16, ASTM B265 Grade 16H.

Material specification for GB/T 3621 TA8

GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.

Ordering item GB/T 3621 basis
Standard GB/T 3621-2022 (state the edition if an older one is required)
Grade TA8 (Lean Pd Titanium)
Condition Annealed (M)
Size range (2022) 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long
Marking example Plate TA8 M 1.0×1000×2000 GB/T 3621
Certificate Quality certificate with chemistry, tensile results and other agreed tests

Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.

The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.

Chemical composition of GB/T 3621 TA8

Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.

Element Limit, %
Nitrogen (N) 0.03 max
Carbon (C) 0.08 max
Hydrogen (H) 0.015 max
Iron (Fe) 0.3 max
Oxygen (O) 0.25 max
Palladium (Pd) 0.04–0.08
Other elements, each 0.1 max
Other elements, total 0.4 max
Titanium (Ti) Balance

Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.

Mechanical properties of GB/T 3621 TA8

The values below are the requirements for TA8 plate in the annealed (M) condition.

Thickness, mm Tensile strength Rm, MPa Proof strength Rp0.2, MPa Elongation A, min, %
0.8–10.0 400 min 275–450 20

Values follow the GB/T 3621-2007 property table for the annealed condition. The 2022 edition revised this table, so confirm the values against the edition named on the order before acceptance.

Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.

Delivery condition, finish and marking

GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.

  • Condition: Annealed (M)
  • Surface: pickled, ground or machined, as agreed
  • Marking: grade, condition, size, heat number and standard number
  • Packing: to GB/T 8180, or as stated on the contract

The grade is supplied annealed and is not strengthened by heat treatment. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.

Welding and fabrication of TA8 titanium plate

TA8 is welded in the same way as CP titanium, by gas tungsten arc, plasma arc or other inert-gas processes with full shielding of the weld pool, the hot heat-affected zone and the root.

  • Use trailing shields and back purging until the metal cools below about 400 °C
  • Select filler metal that keeps the alloying addition in the weld, normally matching filler, so the weld does not become the least corrosion-resistant zone
  • Keep joints, wire and gloves clean; avoid iron contamination from carbon steel tools
  • Check weld colour and reject heavily discoloured welds

Forming behaviour is close to the CP grade of the same oxygen level. Allow for springback, and keep forming tools clean so iron is not smeared into the surface.

For machining, use sharp tools, low cutting speeds, steady feeds and plenty of coolant, as for CP titanium. Keep chips separate by grade so the alloying addition can be traced in scrap, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.

If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of TA8 titanium plate

Typical uses of TA8 plate include:

  • Equipment handling hot chloride brines where crevice corrosion is a risk
  • Reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid
  • Flue gas desulfurisation and chemical process heat exchangers
  • Gasket faces, flange areas and crevice-prone parts of titanium equipment

The alloying addition improves resistance in mildly reducing acids and hot chloride crevices, but it does not make titanium suitable for hydrofluoric acid, fluoride-bearing media, dry chlorine, strongly reducing hot concentrated acids or red fuming nitric acid. Corrosion performance depends on acid concentration, temperature, aeration and impurities, so the design engineer should confirm the grade with corrosion data or tests for the actual medium.

When selecting TA8, compare it with TA8-1, TA9, TA9-1. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare TA8 with other GB/T 3621 grades

The grades below are the closest neighbours of TA8 in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
TA8 400 MPa min 275–450 MPa 20% Ti-0.05Pd, Grade 16-type
TA8-1 240 MPa min 140–310 MPa 24% Ti-0.05Pd, Grade 17-type
TA9 400 MPa min 275–450 MPa 20% Ti-0.2Pd, Grade 7-type
TA9-1 240 MPa min 140–310 MPa 24% Ti-0.2Pd, Grade 11-type
TA10 485 MPa min 345 MPa min 18% Ti-0.3Mo-0.8Ni, Grade 12-type

The grades in this group differ in the alloying addition and in oxygen level. The addition sets the corrosion behaviour and cost; the oxygen level sets strength and formability. A change of grade should be approved by the engineer responsible for corrosion design.

GB/T 3621 TA8 equivalent grades

The designations below are commonly compared with GB/T 3621 TA8. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to GB/T 3621 TA8
ASTM B265 Grade 16 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 16 ASME Code version of the ASTM grade; ordered for pressure equipment
ASTM B265 Grade 16H Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 16H ASME Code version of the ASTM grade; ordered for pressure equipment
JIS H4600 Class 18 (TP345Pd) Close equivalent; JIS strength range and tests differ
UNS R52402 Same unified number as ASTM Grade 16

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for TA8 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
  • Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for GB/T 3621 TA8 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material GB/T 3621 TA8, edition
Product form Plate or sheet; condition as listed for the grade
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Which edition of GB/T 3621 applies to TA8?
GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
What is the tensile strength of GB/T 3621 TA8 titanium plate?
The requirement is 400 MPa minimum. The 0.2% proof or yield strength is 275–450 MPa. Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is TA8 mainly used for?
Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk, reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid and flue gas desulfurisation and chemical process heat exchangers. The design engineer should confirm the grade for the actual service.
What sizes does GB/T 3621-2022 cover?
Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
What should I send for a quotation?
Send GB/T 3621 TA8, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for GB/T 3621 TA8 titanium plate

GB/T 3621 TA8 is lean-Pd titanium specified for 400 MPa minimum tensile strength, 275–450 MPa yield or proof strength and 20% minimum elongation in the annealed (M) condition. Typical uses include equipment handling hot chloride brines where crevice corrosion is a risk and reactors and vessels in mildly reducing acids such as dilute hydrochloric or sulfuric acid.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X