ASTM B265 Grade 2 Titanium Plate | CP Titanium (UNS R50400)

ASTM B265 Grade 2 titanium plate is commercially pure, unalloyed titanium (UNS R50400) supplied in the annealed condition. It is specified for 345 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation, with strong corrosion resistance in seawater and chloride media. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASTM B265 Grade 2 titanium plate, Grade 2 titanium plate, UNS R50400 plate, CP titanium plate, commercially pure titanium sheet
Equivalent Grades:
ASME SB-265 Gr.2, UNS R50400, 3.7035, JIS Class 2 (TP340), GB/T TA2, GOST VT1-0 (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM B265 Grade 2 titanium plate?

ASTM B265 Grade 2 titanium plate is unalloyed, commercially pure (CP) titanium made to ASTM B265, the specification for annealed titanium and titanium alloy strip, sheet and plate. Grade 2 carries the UNS number R50400 and is the standard-oxygen member of the CP series between Grade 1 and Grade 3.

Its strength comes from controlled interstitial levels, mainly oxygen and iron, not from alloying additions. Grade 2 cannot be hardened by heat treatment. It offers a practical balance of moderate strength, good cold formability and weldability, which is why it is the most widely ordered CP grade for process equipment.

The main reason buyers select Grade 2 is corrosion resistance. A stable, self-healing oxide film protects the surface in seawater, brines, wet chlorine and many oxidizing acids. Its typical density of about 4.51 g/cm³ is roughly 57% of that of carbon steel.

SHH STEEL handles Grade 2 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered B265 edition, product form and certificate type before confirming supply.

Material specification for ASTM B265 Grade 2

ASTM B265 classifies flat titanium products by thickness and width. The same Grade 2 chemistry and tensile requirements apply to all three forms, but tolerances and bend testing differ.

Ordering item ASTM B265 basis
Standard ASTM B265, Titanium and Titanium Alloy Strip, Sheet, and Plate; state the edition on the order
Grade / UNS Grade 2, unalloyed titanium, UNS R50400
Plate Over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide
Sheet 0.187 in (4.75 mm) and under, 24 in (610 mm) wide or more; state cold or hot rolled
Strip 0.187 in (4.75 mm) and under, less than 24 in (610 mm) wide
Condition Annealed
Certificate Manufacturer’s report with chemical analysis, tensile results and other required tests

Order information listed by the specification includes grade, product limitations, special mechanical properties, marking, finish, packaging, any additional reports and the disposition of rejected material. For ASME Code construction, order to ASME SB-265 Grade 2 and state any dual certification on the purchase order.

Chemical composition of ASTM B265 Grade 2 (UNS R50400)

Single values are maximums. Titanium is determined by difference. Product analysis tolerances cover variation between laboratories and do not broaden the heat analysis limits.

Element Heat analysis, % max Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.08 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.25 +0.03
Other elements, each 0.10 +0.02
Other elements, total 0.40 —
Titanium (Ti) Balance —

Ingot top and bottom are analysed for the listed elements. Hydrogen is tested and reported on at least one final product sample, and a lower hydrogen limit may be negotiated. Other elements need not be reported unless they exceed 0.10% each or 0.40% total, and they may not be added intentionally.

Mechanical properties of ASTM B265 Grade 2

The values below are the room-temperature requirements for Grade 2 in the annealed condition.

Property Requirement
Tensile strength, min 50 ksi (345 MPa)
Yield strength, 0.2% offset 40–65 ksi (275–450 MPa)
Elongation in 2 in or 50 mm, min 20%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 2T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 2.5T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail Grade 2 even if it is strong. Grade 2H uses the same chemistry with a 58 ksi (400 MPa) minimum tensile strength and may also be certified as Grade 2.

Delivery condition, finish and marking

ASTM B265 covers annealed material. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: annealed, Grade 2
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness
  • Packaging: manufacturer’s standard practice unless the order states otherwise

If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 2 titanium plate

Grade 2 is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld.

  • Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool
  • Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
  • Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
  • Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances for B265 products are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Applications and service limits of Grade 2 titanium plate

Typical uses of Grade 2 plate and sheet include:

  • Heat exchanger tube sheets, shells and channel covers in seawater and brine service
  • Chemical process vessels, columns and tank linings
  • Chlor-alkali, chlorine dioxide and pulp bleaching equipment
  • Desalination plant, offshore and marine components
  • Plate heat exchanger and electrode substrates (sheet)

Grade 2 has limits. It is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd- or Ni-Mo-bearing grades such as Grade 7 or Grade 12 are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.

Compare Grade 2 with other ASTM B265 CP grades

The unalloyed grades in ASTM B265 differ mainly in oxygen and iron, which sets their strength and formability. Values are minimum tensile, yield range and minimum elongation.

Grade (UNS) Tensile, min Yield, 0.2% offset Elongation, min Typical role
Grade 1 (R50250) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Best formability, lowest strength
Grade 2 (R50400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% General process equipment
Grade 2H (R50400) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 2 with higher guaranteed tensile
Grade 3 (R50550) 65 ksi (450 MPa) 55–80 ksi (380–550 MPa) 18% Higher strength, less formable
Grade 4 (R50700) 80 ksi (550 MPa) 70–95 ksi (483–655 MPa) 15% Highest-strength CP grade

A higher grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.

ASTM B265 Grade 2 equivalent grades

The designations below are commonly compared with ASTM B265 Grade 2. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to B265 Grade 2
ASME SB-265 SB-265 Grade 2 ASME Code adoption of B265; ordered for pressure equipment
AMS 4902 CP titanium, annealed Aerospace sheet, strip and plate; composition similar to UNS R50400
UNS R50400 Same unified number
DIN / EN material number 3.7035 (Ti 2) Close CP equivalent; check the ordered European standard
JIS H4600 Class 2 (TP340) Close equivalent; JIS strength range differs
GB/T 3621 TA2 (TA2G in the 2022 edition) Close equivalent; confirm grade name and limits in the ordered edition
GOST 22178 VT1-0 Approximate; GOST limits and sheet scope differ
ISO 5832-2 Grade 2 Surgical implant material; not an industrial plate substitute

For dual certification, for example ASTM B265 and ASME SB-265 Grade 2 on the same plate, request it at enquiry so the certificate shows both.

Why choose SHH STEEL for Grade 2 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate.

  • We quote to the ASTM B265 edition, grade and product form you name, and keep B265 and SB-265 requirements distinct
  • Certificates are checked against the Grade 2 chemistry and tensile limits, including the yield upper limit
  • Finish, marking and packing are agreed before production
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed

How to enquire for ASTM B265 Grade 2 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASTM B265 Grade 2 (UNS R50400), edition; add ASME SB-265 if Code use
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted or ground
Testing Any special mechanical properties, lower hydrogen limit or extra reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Is ASTM B265 Grade 2 the same as ASME SB-265 Grade 2?
SB-265 is the ASME Code adoption of B265, so Grade 2 requirements normally match. They are separate documents, and ASME may adopt a different edition. For Code work, order SB-265 Grade 2 or dual certification.
What is the yield strength of Grade 2 titanium plate?
The 0.2% offset yield must be 40–65 ksi (275–450 MPa). Tensile strength is 50 ksi (345 MPa) minimum and elongation is 20% minimum in 2 in or 50 mm.
What is the difference between Grade 2 and Grade 2H?
The chemistry is the same. Grade 2H guarantees a 58 ksi (400 MPa) minimum tensile strength instead of 50 ksi (345 MPa), and it may also be certified as Grade 2.
When is a titanium product classed as plate under B265?
Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide. Thinner product is sheet if 24 in (610 mm) wide or more, otherwise strip.
What should I send for a quotation?
Send ASTM B265 Grade 2, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination. Add ASME SB-265 if the plate is for Code construction.

Request a quotation for ASTM B265 Grade 2 titanium plate

ASTM B265 Grade 2 is unalloyed titanium, UNS R50400, with 0.25% maximum oxygen, 50 ksi (345 MPa) minimum tensile strength, 40–65 ksi (275–450 MPa) yield and 20% minimum elongation in the annealed condition.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASTM B265 page. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X