GOST 22178 VT1-0 Titanium Sheet | Unalloyed Titanium (BT1-0)
What is GOST 22178 VT1-0 titanium sheet?
GOST 22178 VT1-0 titanium sheet is made to GOST 22178, the interstate standard for sheets of titanium and titanium alloys. VT1-0 (BT1-0) is the standard commercially pure titanium of the Russian system, with 0.20% maximum oxygen. It is the most common GOST titanium sheet grade for chemical, marine and general engineering use.
Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.
Its typical density of about 4.50 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Russian designations follow the original VT (BT in Cyrillic) and OT naming. VT1-00 and VT1-0 are unalloyed titanium, OT4 grades are Ti-Al-Mn alloys, and VT5-1, VT6, VT14 and VT20 are structural alloys used widely in aerospace sheet work.
SHH STEEL handles VT1-0 sheet enquiries within its range of titanium alloy plates and sheets, checking the ordered GOST 22178 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 2, ASME SB-265 Grade 2, AMS 4902 Grade 2.
Material specification for GOST 22178 VT1-0
GOST 22178 is the interstate standard for sheets of titanium and titanium alloys. It covers sheets from 0.3 to 10.5 mm thick, sets sizes, tolerances, surface quality groups and mechanical properties, and refers chemical composition to GOST 19807 or OST 1 90013. Because the standard covers sheet, this page uses the term titanium sheet.
| Ordering item | GOST 22178 basis |
|---|---|
| Standard | GOST 22178-76 with its amendments; state the revision required |
| Grade | VT1-0 (Unalloyed Titanium (BT1-0)) |
| Size range for this grade | 0.3–10.5 mm thick |
| Condition | Annealed, or annealed and lightly cold-rolled and levelled; 8.0–10.5 mm also without heat treatment |
| Surface finish | Ordinary or high surface finish; improved flatness on request |
| Designation example | Sheet VT1-0 5 × 1000 × 1500 GOST 22178-76 |
| Certificate | Quality document with chemistry and test results |
Width and length tolerances are plus-only: up to +10 mm on width for sheets up to 1500 mm long and up to +20 mm on length for sheets up to 2000 mm long. Order the grade, thickness, width, length, surface finish group and flatness class.
Many Russian aerospace orders cite OST 1 90013 for chemistry or add supplementary technical conditions to GOST 22178. If the drawing names such documents, list them on the order, because they can change impurity limits, test frequency and acceptance criteria. When sheet is bought for use outside the CIS, agree in advance whether a GOST certificate alone is acceptable or a cross-reference to another standard is required.
Chemical composition of GOST 22178 VT1-0
Composition follows GOST 19807 for the grade. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.04 max |
| Carbon (C) | 0.07 max |
| Hydrogen (H) | 0.010 max |
| Iron (Fe) | 0.25 max |
| Oxygen (O) | 0.20 max |
| Aluminium (Al) | 0.70 (permitted) |
| Silicon (Si) | 0.10 max |
| Other impurities, total | 0.30 max |
| Titanium (Ti) | Balance |
Impurity limits are tight, and the aluminium shown for the unalloyed grades is a permitted residual rather than an addition. Where an order cites both GOST and another standard, both sets of limits must be satisfied.
Mechanical properties of GOST 22178 VT1-0
The values below are the requirements for VT1-0 sheet in the annealed condition.
| Sheet thickness, mm (condition) | Tensile strength, MPa | Elongation, min, % |
|---|---|---|
| 0.3–0.4 | 375 min | 25 |
| >0.4–1.8 | 375 min | 30 |
| >1.8–6.0 | 375 min | 25 |
| 6.0–10.5 | 375 min | 20 |
| 8.0–10.5 (not heat treated) | 375 min | 20 |
GOST 22178 sets minimum tensile strength and elongation; yield strength is not specified and can be agreed separately. Tests are made on transverse specimens. The bend test is made around a mandrel, and the sheet must reach the minimum angle below without cracks.
| Sheet thickness, mm | Bend angle, min |
|---|---|
| 0.3–0.6 | 140° |
| 0.7 | 130° |
| 0.8 | 120° |
| 1.0 | 110° |
| 1.2 | 100° |
| 1.5 | 90° |
| >1.5–10.5 | 80° |
Where sheets are quenched and aged, the properties of heat-treated samples are agreed when ordering.
Delivery condition, finish and marking
GOST 22178 sheets are supplied with an ordinary or high surface finish. Light dressing of surface defects is allowed within the depth limits of the standard, and the angles of the sheet must stay within the flatness requirement for the ordered class.
- Condition: Annealed, or annealed and lightly cold-rolled and levelled; 8.0–10.5 mm also without heat treatment
- Surface: ordinary or high surface finish group, as ordered
- Flatness: normal or improved, as ordered
- Marking and packing: grade, heat, sheet size and standard number, with protection for transport
CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. Mechanical tests are made on 10% of the sheets in a lot, but not fewer than one sheet, and the lot is accepted or retested on the results.
Welding and fabrication of VT1-0 titanium sheet
VT1-0 is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.
- Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
- Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
- Use matching CP filler metal unless the design engineer specifies otherwise
- Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
- Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up
Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.
For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GOST 22178 sets thickness tolerances in Table 1 by thickness and width, and flatness and corner-gap limits in Table 5 by grade and flatness class. Width tolerance is up to +10 mm for sheets up to 1500 mm long and +15 mm above that; length tolerance is +20 mm up to 2000 mm and +25 mm above.
Order the thickness, width, length, surface finish group and flatness class. Theoretical sheet mass is based on 4.50 g/cm³ for VT1-00 and VT1-0, with conversion factors for the alloys. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of VT1-0 titanium sheet
Typical uses of VT1-0 sheet include:
- Chemical apparatus and heat exchangers
- Shipbuilding and seawater systems
- General formed sheet parts
- Electroplating and electrolysis equipment
Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.
When selecting VT1-0, compare it with VT1-00, OT4-0, OT4-1. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare VT1-0 with other GOST 22178 grades
The grades below are the closest neighbours of VT1-0 in GOST 22178. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| VT1-00 | 295 MPa min (>1.8–6.0 mm) | — | 25% | Highest-purity GOST unalloyed titanium |
| VT1-0 | 375 MPa min (>1.8–6.0 mm) | — | 25% | Standard GOST unalloyed titanium |
| OT4-0 | 470 MPa min (>1.8–6.0 mm) | — | 25% | Ti-Al-Mn, lowest-strength OT4 grade |
| OT4-1 | 590 MPa min (>1.8–6.0 mm) | — | 15% | Ti-2Al-1.5Mn, formable |
| OT4 | 685 MPa min (>1.8–6.0 mm) | — | 12% | Ti-4Al-1.5Mn, higher strength |
A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.
GOST 22178 VT1-0 equivalent grades
The designations below are commonly compared with GOST 22178 VT1-0. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GOST 22178 VT1-0 |
|---|---|---|
| ASTM B265 | Grade 2 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 2 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| AMS 4902 | CP titanium, annealed | Aerospace specification; tighter oxygen and added melting and grain-size requirements |
| JIS H4600 | Class 2 (TP340) | Close equivalent; JIS strength range and tests differ |
| GB/T 3621 | TA2G | Close equivalent; confirm grade name and limits in the ordered edition |
| ISO 5832-2 | Grade 2 | Implant-grade counterpart; medical scope and tighter controls |
| UNS | R50400 | Same unified number as ASTM Grade 2 |
| DIN / EN material number | 3.7035 (Ti 2) | Close CP equivalent; check the ordered European standard |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for VT1-0 titanium sheet
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to GOST 22178 VT1-0 sheet with the surface finish group and flatness you need
- Certificates are checked against GOST 19807 chemistry, tensile strength, elongation and bend angle
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GOST 22178 VT1-0 sheet
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GOST 22178 VT1-0, revision |
| Product form | Sheet 0.3–10.5 mm; surface finish group and flatness class |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Bend test, any quenched-and-aged tests where applicable |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Why is GOST 22178 VT1-0 called sheet rather than plate?
- GOST 22178 covers sheets from 0.3 to 10.5 mm thick. Thicker plate in Russian grades is ordered to other GOST or OST documents, so this page uses the term sheet.
-
What is the tensile strength of GOST 22178 VT1-0 titanium sheet?
- The requirement is 375 MPa minimum. Minimum elongation is 25%. Values apply to the condition and thickness range stated in the standard.
-
What is VT1-0 mainly used for?
- Typical uses include chemical apparatus and heat exchangers, shipbuilding and seawater systems and general formed sheet parts. The design engineer should confirm the grade for the actual service.
-
What thickness range applies to GOST 22178 VT1-0?
- For this grade the standard lists 0.3–10.5 mm thick. Width and length depend on thickness, so confirm the full sheet size against the standard's size table when ordering.
-
What should I send for a quotation?
- Send GOST 22178 VT1-0, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GOST 22178 VT1-0 titanium sheet
GOST 22178 VT1-0 is unalloyed titanium (BT1-0) specified for 375 MPa minimum tensile strength and 25% minimum elongation in the annealed condition. Typical uses include chemical apparatus and heat exchangers and shipbuilding and seawater systems.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GOST 22178 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com