GB/T 3621 TA18 Titanium Plate | Ti-3Al-2.5V
What is GB/T 3621 TA18 titanium plate?
GB/T 3621 TA18 titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TA18 is Ti-3Al-2.5V, the Chinese counterpart of ASTM Grade 9. It offers medium strength with good cold formability and weldability.
This alloy sits between commercially pure titanium and Ti-6Al-4V. Its aluminium and vanadium contents are lower than Ti-6Al-4V, so it has a mostly alpha structure with a little beta phase. It gives substantially more strength than CP titanium while remaining weldable and more cold formable than Ti-6Al-4V, and it is normally used annealed.
Its typical density of about 4.48 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.
SHH STEEL handles TA18 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 9, ASME SB-265 Grade 9, JIS H4600 Class 61 TAP3250.
Material specification for GB/T 3621 TA18
GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.
| Ordering item | GB/T 3621 basis |
|---|---|
| Standard | GB/T 3621-2022 (state the edition if an older one is required) |
| Grade | TA18 (Ti-3Al-2.5V) |
| Condition | Annealed (M) |
| Size range (2022) | 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long |
| Marking example | Plate TA18 M 1.0×1000×2000 GB/T 3621 |
| Certificate | Quality certificate with chemistry, tensile results and other agreed tests |
Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.
The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.
Chemical composition of GB/T 3621 TA18
Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.
| Element | Limit, % |
|---|---|
| Nitrogen (N) | 0.05 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.015 max |
| Iron (Fe) | 0.25 max |
| Oxygen (O) | 0.12 max |
| Aluminium (Al) | 2–3.5 |
| Vanadium (V) | 1.5–3 |
| Other elements, each | 0.1 max |
| Other elements, total | 0.3 max |
| Titanium (Ti) | Balance |
Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.
Mechanical properties of GB/T 3621 TA18
The values below are the requirements for TA18 plate in the annealed (M) condition.
| Thickness, mm | Tensile strength Rm, MPa | Proof strength Rp0.2, MPa | Elongation A, min, % |
|---|---|---|---|
| 0.5–2.0 | 590–735 | — | 25 |
| >2.0–4.0 | 590–735 | — | 20 |
| >4.0–10.0 | 590–735 | — | 15 |
Values follow the GB/T 3621-2007 property table for the annealed condition. The 2022 edition revised this table, so confirm the values against the edition named on the order before acceptance.
Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.
Delivery condition, finish and marking
GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.
- Condition: Annealed (M)
- Surface: pickled, ground or machined, as agreed
- Marking: grade, condition, size, heat number and standard number
- Packing: to GB/T 8180, or as stated on the contract
The alloy is supplied annealed; it is not normally strengthened by heat treatment in plate form. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.
Welding and fabrication of TA18 titanium plate
TA18 welds readily by gas tungsten arc, plasma arc, electron beam and laser processes with full inert-gas shielding.
- Use trailing shields and back purging until the weld cools below about 400 °C
- Use matching or engineer-approved filler metal
- Clean joints and filler wire, and keep carbon steel tools away from the surface
- Use weld colour as a check of shielding quality
Cold forming is possible with larger bend radii than for CP grades. Severe shapes may need warm forming.
Machining is easier than for Ti-6Al-4V but still needs sharp tools, low cutting speeds, steady feeds and generous coolant. Heat stays at the cutting edge because titanium conducts heat poorly, so avoid dwelling and keep fine chips away from ignition sources.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.
If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of TA18 titanium plate
Typical uses of TA18 plate include:
- Lightweight sheet structures and ducting
- Pressure and hydraulic system parts made from plate
- Sporting goods and bicycle components
- Welded assemblies needing more strength than CP titanium with better formability than Ti-6Al-4V
The alloy is not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. In hot reducing brines the Pd- or Ru-bearing variants are often preferred. The design engineer must confirm suitability for the actual medium and temperature.
When selecting TA18, compare it with TA17, TA22, TA23. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare TA18 with other GB/T 3621 grades
The grades below are the closest neighbours of TA18 in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| TA17 | 685–835 MPa | — | 25% | Ti-4Al-2V near-alpha |
| TA18 | 590–735 MPa | — | 25% | Ti-3Al-2.5V, Grade 9-type |
| TA22 | 490 MPa min | — | 18% | Ti-3Al-1Mo-1Ni-1Zr |
| TA23 | 590 MPa min | — | 18% | Ti-2.5Al-2Zr-1Fe |
| TA24 | 550 MPa min | — | 13% | Ti-3Al-2Mo-2Zr |
| TA31 | 800 MPa min | 700 MPa min | 10% | Ti-6Al-3Nb-2Zr-1Mo (Ti-80) |
| TA36 | 520 MPa min | 400 MPa min | 20% | Ti-1Al-1Fe |
Grades in this group share a similar base alloy; differences come from precious-metal additions or alloy balance. Confirm the strength and corrosion needs before changing grade.
GB/T 3621 TA18 equivalent grades
The designations below are commonly compared with GB/T 3621 TA18. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to GB/T 3621 TA18 |
|---|---|---|
| ASTM B265 | Grade 9 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 9 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| JIS H4600 | Class 61 (TAP3250) | Close equivalent; JIS strength range and tests differ |
| JIS H4600 | Class 61F (TAP3250F) | Nearest by role only; composition and properties differ |
| UNS | R56320 | Same unified number as ASTM Grade 9 |
| DIN / EN material number | 3.7195 (TiAl3V2.5) | Close equivalent |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for TA18 titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
- Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for GB/T 3621 TA18 plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | GB/T 3621 TA18, edition |
| Product form | Plate or sheet; condition as listed for the grade |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Any special mechanical properties, extra analysis or reports |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Which edition of GB/T 3621 applies to TA18?
- GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
-
What is the tensile strength of GB/T 3621 TA18 titanium plate?
- The requirement is 590–735 MPa. The 0.2% proof or yield strength is reported as measured. Minimum elongation is 25%. Values apply to the condition and thickness range stated in the standard.
-
What is TA18 mainly used for?
- Typical uses include lightweight sheet structures and ducting, pressure and hydraulic system parts made from plate and sporting goods and bicycle components. The design engineer should confirm the grade for the actual service.
-
What sizes does GB/T 3621-2022 cover?
- Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
-
What should I send for a quotation?
- Send GB/T 3621 TA18, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for GB/T 3621 TA18 titanium plate
GB/T 3621 TA18 is Ti-3Al-2.5V titanium alloy specified for 590–735 MPa tensile strength and 25% minimum elongation in the annealed (M) condition. Typical uses include lightweight sheet structures and ducting and pressure and hydraulic system parts made from plate.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com