GB/T 3621 TC1 Titanium Plate | Ti-2Al-1.5Mn

GB/T 3621 TC1 titanium plate is Ti-2Al-1.5Mn titanium alloy supplied annealed (M). It is specified for 590–735 MPa tensile strength and 25% minimum elongation. Typical uses include formed aerospace sheet parts. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
GB/T 3621 TC1 titanium plate, TC1 titanium plate, Ti-2Al-1.5Mn titanium alloy plate, GB/T 3621 titanium sheet, GB/T 3621 TC1 titanium sheet
Equivalent Grades:
GOST OT4-1 (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 3621 TC1 titanium plate?

GB/T 3621 TC1 titanium plate is made to GB/T 3621, the Chinese national standard for titanium and titanium alloy plate and sheet. TC1 is Ti-2Al-1.5Mn, a low-strength alloy of the Ti-Al-Mn family with very good formability and weldability. It corresponds in role to the Russian OT4-1.

This is an alpha or near-alpha titanium alloy. Aluminium (and in some grades tin or zirconium) strengthens the alpha phase, while only small amounts of beta stabilisers such as manganese, molybdenum or vanadium are present. Such alloys keep good weldability and creep strength at elevated temperature, are normally used annealed, and respond little to strengthening heat treatment.

Its typical density of about 4.55 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Chinese titanium designations use TA for alpha and near-alpha grades, including unalloyed titanium, TB for beta alloys and TC for alpha-beta alloys. The 2022 edition renamed the unalloyed industrial grades with a G suffix, such as TA1G and TA2G, and added or removed several alloy grades.

SHH STEEL handles TC1 plate enquiries within its range of titanium alloy plates and sheets, checking the ordered GB/T 3621 edition, product form and certificate type before confirming supply. Related designations covered on this site include GOST 22178 OT4-1, GB/T 3621 TC2.

Material specification for GB/T 3621 TC1

GB/T 3621 is the Chinese national standard for titanium and titanium alloy plate and sheet produced by rolling. The current edition, GB/T 3621-2022, replaced the 2007 edition from 1 May 2023. Chemical composition is taken from GB/T 3620.1, and product analysis tolerances from GB/T 3620.2.

Ordering item GB/T 3621 basis
Standard GB/T 3621-2022 (state the edition if an older one is required)
Grade TC1 (Ti-2Al-1.5Mn)
Condition Annealed (M)
Size range (2022) 0.3–5.0 mm thick, 400–1800 mm wide, 1000–4000 mm long; over 5.0–100.0 mm thick, 400–3000 mm wide, 1000–6000 mm long
Marking example Plate TC1 M 1.0×1000×2000 GB/T 3621
Certificate Quality certificate with chemistry, tensile results and other agreed tests

Recommended nominal thicknesses are multiples of 0.1 mm up to 5.0 mm and multiples of 0.5 mm above that. Unless the order asks for longitudinal tests, tensile properties are tested in the transverse direction. Supply route, testing and inspection are confirmed on the contract.

The 2022 edition changed more than grade names. It revised the size ranges, tightened several dimensional tolerances, updated the surface quality clauses and reorganised the property tables. Purchase orders that still cite GB/T 3621-2007 remain valid if both parties agree, but the edition, grade name and property table that govern acceptance should be written on the contract so that inspection and certification follow one document.

Chemical composition of GB/T 3621 TC1

Composition follows GB/T 3620.1, the Chinese standard for titanium and titanium alloy grades and compositions. Single values are maximums; titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.08 max
Hydrogen (H) 0.012 max
Iron (Fe) 0.3 max
Oxygen (O) 0.15 max
Aluminium (Al) 1–2.5
Manganese (Mn) 0.7–2
Other elements, each 0.1 max
Other elements, total 0.4 max
Titanium (Ti) Balance

Product analysis tolerances follow GB/T 3620.2. Other elements are not normally reported unless the contract asks for them. Grades renamed in the newer editions, such as TA1 to TA1G, keep closely related limits, but the edition named on the order governs.

Mechanical properties of GB/T 3621 TC1

The values below are the requirements for TC1 plate in the annealed (M) condition.

Thickness, mm Tensile strength Rm, MPa Proof strength Rp0.2, MPa Elongation A, min, %
0.5–1.0 590–735 — 25
>1.0–2.0 590–735 — 25
>2.0–5.0 590–735 — 20
>5.0–10.0 590–735 — 20

Values follow the GB/T 3621-2007 property table for the annealed condition. The 2022 edition revised this table, so confirm the values against the edition named on the order before acceptance.

Tensile properties are tested in the transverse direction unless the order asks for longitudinal tests. Elevated-temperature properties and bend tests are supplied only when agreed.

Delivery condition, finish and marking

GB/T 3621 plate is supplied in the condition listed for the grade. The 2022 edition revised the surface quality requirements; plate is normally pickled, ground or machined, and must be free of cracks, laps and inclusions that affect use.

  • Condition: Annealed (M)
  • Surface: pickled, ground or machined, as agreed
  • Marking: grade, condition, size, heat number and standard number
  • Packing: to GB/T 8180, or as stated on the contract

The alloy is supplied annealed; stress relieving after forming or welding is agreed with the purchaser. State whether the plate will be cold formed, welded or clad so the surface condition and flatness can be agreed.

Welding and fabrication of TC1 titanium plate

TC1 is weldable by gas tungsten arc, plasma arc, electron beam and laser processes, provided the weld zone is fully shielded from air.

  • Use trailing shields and back purging until the weld cools below about 400 °C
  • Use matching or engineer-approved filler metal and qualified procedures
  • Clean joints and filler wire; remove oil, moisture and iron contamination
  • Consider post-weld stress relief for highly restrained or precision parts, as agreed in the procedure

Room-temperature formability is lower than for CP titanium. Moderate bends can be cold formed with generous radii, but severe shapes are normally hot formed or creep formed.

Machining needs sharp carbide tools, rigid set-ups, low cutting speeds and generous coolant, because titanium alloys conduct heat poorly and the heat stays at the cutting edge. Avoid dwelling, which work-hardens the surface, and keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

GB/T 3621-2022 tightened the dimensional tolerances of the 2007 edition. Thickness tolerances depend on thickness and width, for example ±0.05 mm for 0.3–0.5 mm sheet up to 1000 mm wide and ±2.00 mm for 70–100 mm plate. Width and length tolerances are plus-only, and flatness per 1000 mm ranges from 20 mm for thin wide sheet to 8 mm or less for thick plate.

If a one-sided thickness tolerance is required, the value is twice the tabulated figure. State thickness, width, length, quantity and any cutting drawing on the order. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of TC1 titanium plate

Typical uses of TC1 plate include:

  • Formed aerospace sheet parts
  • Welded ducting
  • Low-stress structures
  • Sheet metal assemblies

As with all titanium, the alloy is not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. High-aluminium alloys can be sensitive to hot-salt stress corrosion, and maximum service temperatures depend on the alloy and design code. The design engineer must confirm suitability for the actual service.

When selecting TC1, compare it with TC2, TC3, TC4. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare TC1 with other GB/T 3621 grades

The grades below are the closest neighbours of TC1 in GB/T 3621. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
TC1 590–735 MPa — 25% Ti-2Al-1.5Mn near-alpha
TC2 685 MPa min — 25% Ti-4Al-1.5Mn near-alpha
TC3 880 MPa min — 12% Ti-5Al-4V alpha-beta
TC4 895 MPa min 830 MPa min 12% Ti-6Al-4V alpha-beta
TC4ELI 860 MPa min 795 MPa min 10% Ti-6Al-4V ELI
TC11 1030 MPa min 900 MPa min 10% Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alpha-beta
TC18 1080 MPa min 1000 MPa min 10% Ti-5Al-5Mo-5V-1Cr-1Fe near-beta

Alpha and near-alpha alloys trade formability for strength and elevated-temperature performance. Compare the full requirements, not only tensile strength, before changing grade.

GB/T 3621 TC1 equivalent grades

The designations below are commonly compared with GB/T 3621 TC1. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to GB/T 3621 TC1
GOST 22178 OT4-1 Approximate; GOST limits and sheet scope differ
GB/T 3621 TC2 Nearest by role only; composition and properties differ

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for TC1 titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the GB/T 3621 edition you name and keep old and new grade names (such as TA2 and TA2G) distinct
  • Certificates are checked against GB/T 3620.1 chemistry and the agreed tensile values
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for GB/T 3621 TC1 plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material GB/T 3621 TC1, edition
Product form Plate or sheet; condition as listed for the grade
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Which edition of GB/T 3621 applies to TC1?
GB/T 3621-2022 has applied since 1 May 2023 and replaces the 2007 edition. If a drawing still cites 2007, agree on the order which edition, grade name and property table govern acceptance.
What is the tensile strength of GB/T 3621 TC1 titanium plate?
The requirement is 590–735 MPa. The 0.2% proof or yield strength is reported as measured. Minimum elongation is 25%. Values apply to the condition and thickness range stated in the standard.
What is TC1 mainly used for?
Typical uses include formed aerospace sheet parts, welded ducting and low-stress structures. The design engineer should confirm the grade for the actual service.
What sizes does GB/T 3621-2022 cover?
Annealed plate and sheet from 0.3 to 100.0 mm thick: 400–1800 mm wide up to 5.0 mm thick, and 400–3000 mm wide above 5.0 mm. Lengths run from 1000 to 6000 mm.
What should I send for a quotation?
Send GB/T 3621 TC1, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for GB/T 3621 TC1 titanium plate

GB/T 3621 TC1 is Ti-2Al-1.5Mn titanium alloy specified for 590–735 MPa tensile strength and 25% minimum elongation in the annealed (M) condition. Typical uses include formed aerospace sheet parts and welded ducting.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GB/T 3621 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X