EN 10217-7 1.4307 Welded Stainless Steel Tube
What is EN 10217-7 1.4307 Welded Stainless Steel Tube
Steel name X2CrNi18-9 under steel number 1.4307 is the austenitic chemistry EN 10217-7 uses when a welded pressure-tube order must carry that analysis into the PED file. The product standard is EN 10217-7:2021 — welded stainless circular tubes for pressure and corrosion-resisting service at room, low, or elevated temperature. Writing only “304L welded tube” on a bill of materials leaves cast limits, weld route, delivery condition, and test category unspecified. Order EN 10217-7, 1.4307, TC1 or TC2, and the delivery-condition / options list so mill documentation matches the drawing. Role in practice: low-carbon 18-8 austenitic for welded pressure tubing where as-welded intergranular corrosion resistance is part of the duty story.
SHH STEEL can produce and supply EN 10217-7 1.4307 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover common cold-finished WCA/WCR bands for hygienic and utility OD, plus larger W1A/W2A descaled routes. Browse the series hub at EN 10217-7.
Buyers who want “304L welded pressure tube” under a European product standard are usually looking for 1.4307 on EN 10217-7 — not an A269 nominal-wall habit stamped onto a PED spool. Typical welded pressure duties include food process lines, pharmaceutical utilities, clean steam and condensate returns, and general PED piping where a weld seam is accepted and molybdenum is not justified. Design caution: do not treat 1.4307 as a chloride-SCC cure — when chlorides and tensile stress stack up, move to Mo-bearing austenitics or duplex rather than hoping low carbon alone will hold Commercially the grade is often called 304L; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4307 / X2CrNi18-9 on the MTC. Sister numbers on this hub include EN 10217-7 1.4301, EN 10217-7 1.4306, EN 10217-7 1.4311, EN 10217-7 1.4404.4301, 1.4306, 1.4311, 1.4404.
Remember the product-form split: this page is welded EN 10217-7 1.4307; seamless pressure stainless in the same chemistry idea belongs under EN 10216-5. Dimension preference is EN ISO 1127. Manufacturing routes stay longitudinal arc or laser per Table 1 — helical seam is outside the listed Part 7 paths used for this series. Live seamless sister: EN 10216-5 1.4307. Related live ASTM/ASME anchors: A269 TP304L, A213 TP304L, SA213 TP304L, A312 TP304L.
Chemical Composition of EN 10217-7 1.4307
Cast chemistry for 1.4307 / X2CrNi18-9 is the acceptance gate on every EN 10217-7 heat. Option 6 opens product analysis with the standard’s deviation table. SHH STEEL prints the measured cast figures on the inspection document and will not market private melt windows as EN 10217-7 limits for this austenitic grade.
Public BSSA EN 10217-7 chemistry for 1.4307 / X2CrNi18-9 is tabulated below after cross-check to the 2021 framing. Figures are maxima unless shown as ranges. Always reconcile secondary datasheets to the purchased Part 7 edition. UNCERTAIN: BSSA HTML table still shows Ni 8.0/10.0; article intro states 2021 harmonises to 8.0/10.5 — crib uses 8.0–10.5
| Element | 1.4307 cast analysis (mass %) |
|---|---|
| Carbon (C) | ≤0.030 |
| Silicon (Si) | ≤1.00 |
| Manganese (Mn) | ≤2.00 |
| Phosphorus (P) | ≤0.045 |
| Sulfur (S) | ≤0.015 |
| Nitrogen (N) | ≤0.10 |
| Chromium (Cr) | 17.5–19.5 |
| Nickel (Ni) | 8.0–10.5 |
Reference for X2CrNi18-9: public BSSA EN 10217-7 chemical compositions article, cross-checked to the 2021 grade list framing. Unlisted elements are not intentional additions without agreement, aside from finishing additions under scrap discipline that protects 1.4307 properties.
Mechanical Properties of EN 10217-7 1.4307
Solution-annealed (+AT) ambient data for steel number 1.4307 (X2CrNi18-9) are taken from the EN 10217-7 austenitic table that characterises walls up to roughly 60 mm unless the order agrees values beyond that band. Both Rp0.2 and Rp1.0 appear for austenitics. Sub-zero impact figures at −196 °C are characterisation data until Options make them certified.
The ambient numbers for X2CrNi18-9 are taken from BSSA’s BS EN 10217-7 mechanical article (2021 framing). Solution annealing temperatures are public EN cross-checks and stay UNCERTAIN versus paid Part 7 footnotes. SHH STEEL keeps 1.4307 tensile acceptance on the EN 10217-7 table — foreign standard floors are not mixed onto the MTC.
| Property | 1.4307 ambient (solution annealed +AT) |
|---|---|
| Rp0.2 min (MPa) | 180 |
| Rp1.0 min (MPa) | 215 |
| Rm (MPa) | 470–670 |
| A min % long / trans | 40 / 35 |
| IGC resistance (delivery) | Yes (method A) |
| Solution annealing (public EN band) | 1000–1100 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges |
| Cooling | water or air |
| Charpy sub-zero (transverse min J) | 60 at -196 °C (Option to verify) |
Reference trail for X2CrNi18-9: BSSA EN 10217-7 ambient mechanical article; public EN solution bands with UNCERTAIN vs paid Part 7 footnotes. Charpy values are characterisation data — verify by Option when joules must appear on the 1.4307 MTC.
Welded Tube Manufacture for EN 10217-7 1.4307
Manufacture of EN 10217-7 1.4307 (X2CrNi18-9) is longitudinal welded only: automatic arc or laser along the abutting edges of formed strip or plate. Public Table 1 sets the allowed weld-preparation and bead-work combinations; continuous forming from strip is the everyday path, while single forming from plate handles the heavier end of the band. The finished product must not include welds used only to join strip lengths prior to forming. Helical seam manufacture is outside the listed routes for this series. If the drawing demands seamless tube, change the standard to EN 10216-5.
For austenitic 1.4307 (X2CrNi18-9), mill seams are typically made without filler or with matching filler depending on route and wall; Options 3 and 4 cover inside-weld remelt or bead working when the purchaser wants a smoothed ID weld. Delivery condition symbols (Table 2) include W0, W1/W1A/W1R, W2/W2A/W2R, cold-finished WCA/WCR with recrystallized weld metal, and WG/WP ground or polished. Unless Option 5 is specified, selection is at the manufacturer’s discretion. SHH STEEL can produce and supply 1.4307 as W1A/W2A descaled or WCA/WCR cold-finished in the common pressure-tube band, and as WG/WP when roughness is agreed. 308L-type fillers and controlled heat input are typical; mill solution anneal of the tube does not replace fabricator procedures on site joints
Every 1.4307 purchase order must name TC1 or TC2 — Part 7 treats test category as mandatory order and marking data. Seam NDT follows the category; leak-tightness covers each length unless Option 15 freezes hydro versus eddy current. SHH STEEL’s paperwork for X2CrNi18-9 states the weld route and delivery-condition symbol that were really used.
Dimensions and Tolerances for EN 10217-7 1.4307
Dimensional ordering for 1.4307 / X2CrNi18-9 is OD × wall under EN ISO 1127 preferences. Stainless density, not carbon-steel 7.85, drives mass. EN 10217-7 tolerance classes apply, with Option 20 available for D4. Ovality stays within diameter tolerance; eccentricity within wall tolerance; abutting-edge radial offset at the longitudinal weld is capped by the standard’s dimensional clauses.
Option 19 covers exact lengths; Option 18 covers bevels when wall is at least 3.2 mm. For precision OD on 1.4307, WCA/WCR cold-finished delivery is often the first finish talk after descaled W1A/W2A. SHH STEEL freezes size, tolerance class, and Table 2 symbol against the order before the weld line is scheduled.
| Route / condition | Typical use | Notes |
|---|---|---|
| W1 / W1A / W1R | Hot-rolled starting flat product | Descaled or bright-annealed per symbol |
| W2 / W2A / W2R | Cold-rolled starting flat product | Smoother OD than W1 family except at weld |
| WCA / WCR | Cold finished ≥20% after weld | Recrystallized weld metal; OD often ≤168.3 mm |
| WG / WP | Ground / polished | Agree ID/OD scope and grit at enquiry |
Dimensional conformity on 1.4307 is checked against the ordered EN ISO 1127 / Part 7 class before release. Straightness and end condition for X2CrNi18-9 follow the standard’s clauses; SHH STEEL records measured OD × wall on the inspection document rather than assuming catalogue mid-tolerance. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4307 / X2CrNi18-9 on the inspection document rather than assuming mid-tolerance catalogue values.
Equivalent Grades for EN 10217-7 1.4307
The welded pressure-tube nameplate for this chemistry is EN 10217-7 1.4307 with steel name X2CrNi18-9. Commercial alias 304L may appear on ASTM/ASME tubing or pipe pages, but those standards are not automatic substitutes. Seamless EN 10216-5 is a sister product form, not a second way to accept a welded Part 7 seam.
Cross-standard shopping for 304L chemistry is common; acceptance is not. EN 10217-7 1.4307 remains the welded pressure-tube contract for X2CrNi18-9 on this page. Seamless sisters and ASTM/ASME pages are references until the order explicitly dual-certifies under each standard’s clauses.
| Reference | Designation | Note |
|---|---|---|
| EN 10217-7 | 1.4307 / X2CrNi18-9 | This product standard (welded pressure tube) |
| EN steel name | X2CrNi18-9 | EN 10027-1 designation used in body and marking |
| Commercial alias (body only) | 304L | Not a substitute for the steel number on the MTC |
| EN 10216-5 (seamless sister) | 1.4307 | Related live page — different product form (seamless) |
| A269 TP304L | A269 TP304L | Related live page — different product standard |
| A213 TP304L | A213 TP304L | Related live page — different product standard |
| SA213 TP304L | SA213 TP304L | Related live page — different product standard |
| A312 TP304L | A312 TP304L | Related live page — different product standard |
Inside this welded series, compare EN 10217-7 1.4301, EN 10217-7 1.4306, EN 10217-7 1.4311, EN 10217-7 1.4404. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4307. Live cross-standard anchors: A269 TP304L, A213 TP304L, SA213 TP304L, A312 TP304L.
Heat Treatment and Delivery Condition for EN 10217-7 1.4307
Delivery condition and heat treatment travel together on EN 10217-7 1.4307. Symbols such as W1A/W2A, WCA/WCR, and W1R/W2R imply the heat-treatment path; mechanical data assume solution-annealed (+AT) X2CrNi18-9. Uniform heating into the solution band and rapid cooling are the reference story. For X2CrNi18-9 under steel number 1.4307, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.
Public solution-annealing guidance for X2CrNi18-9 sits at 1000–1100 °C with water or air cooling. Cross-check source is public EN 10216-5 / EN 10028-7 framing — labelled UNCERTAIN versus paid Part 7:2021 footnotes. Surface (pickle, bright anneal, grind, polish) rides on Option 5 / the chosen Table 2 symbol for 1.4307.
| Item | 1.4307 |
|---|---|
| Solution annealing band (public) | 1000–1100 °C (UNCERTAIN vs paid Part 7 footnote) |
| Cooling | water or air |
| Delivery condition symbols | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify) |
| Inspection document | EN 10204 3.1 default; 3.2 under Option 21 |
No 1.4307 length leaves SHH STEEL outside the ordered delivery-condition story. Certificates for X2CrNi18-9 list the Table 2 symbol, confirm heat treatment when the symbol demands it, and call out recrystallized-weld status on WCA/WCR product so goods-in inspectors are not left reading between the lines.
Corrosion Resistance of EN 10217-7 1.4307
Corrosion-resisting austenitic 1.4307 / X2CrNi18-9 is selected for welded pressure duty where the medium and temperature need low carbon keeps the heat-affected zone out of the classic sensitisation window for many aqueous services; pitting resistance still tracks the Mo-free chromium-nickel balance. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.
IGC guideline temperatures in Part 7 are sensitisation warnings, not design stress caps. As-welded behaviour for X2CrNi18-9 tracks carbon, stabilisers, Mo/N, and duplex phase balance — compare EN 10217-7 1.4301, EN 10217-7 1.4306, EN 10217-7 1.4311, EN 10217-7 1.4404 when the medium outgrows this number. PREN/CPT marketing digits are not treated as EN 10217-7 acceptance values on 1.4307.
Applications of EN 10217-7 1.4307 Tube
EN 10217-7 1.4307 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X2CrNi18-9 the practical band is food process lines, pharmaceutical utilities, clean steam and condensate returns, and general PED piping where a weld seam is accepted and molybdenum is not justified, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.
It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4307), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4307 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit. Related live pages: A269 TP304L, A213 TP304L, SA213 TP304L, A312 TP304L.
Weldability of EN 10217-7 1.4307
1.4307 / X2CrNi18-9 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: 308L-type fillers and controlled heat input are typical; mill solution anneal of the tube does not replace fabricator procedures on site joints
Fabricator responsibility covers as-welded corrosion risk, duplex phase balance where relevant, and any PWHT the joint calculation demands on 1.4307. SHH STEEL supplies the mill product: ordered chemistry, seam route, heat treatment/delivery symbol, tensile floors, leak-tightness, and listed Options for X2CrNi18-9.
Surface Finishes for EN 10217-7 1.4307
Read the finish for steel number 1.4307 from the delivery symbol first. W1A/W2A descaled X2CrNi18-9 is the everyday pressure-tube look; W1R/W2R and WCR bright anneal serve buyers who need a cleaner outside diameter; WG/WP are written scopes, not implied catalogue grades. Packing instructions for this austenitic grade keep bare carbon steel off the tube. Free iron from foreign banding creates receiving NCRs that a PED spool does not have time to argue about on 304L material.
ID cleanliness beyond the Table 2 story — Ra caps, electropolish, solvent wipe — must be written on the 1.4307 purchase order. SHH STEEL can produce and supply descaled, bright-annealed, and polished routes for X2CrNi18-9 with measurable results, and refuses phantom surface grades that cannot be shown on the EN 10204 document for this 304L tube.
Finish upgrades on X2CrNi18-9 consume furnace and polishing capacity that descaled 1.4307 does not — schedule them explicitly. SHH STEEL confirms the Table 2 symbol against finishing slots and will say when a requested WP grit cannot be measured on the ordered OD × wall rather than shipping hopeful 304L tube.
Inspection and Testing for EN 10217-7 1.4307
Inspection on 1.4307 is specific, not statistical sampling theatre. One cast analysis per heat; tensile once per test unit under TC1 and twice from different tubes under TC2; technological tests per the D/T matrix; leak-tightness on every length (hydro or ET, Option 15 to choose); plus dimensions, visuals, and ID of X2CrNi18-9.
Under TC2 the longitudinal seam sees a tougher NDT package; laminar and edge Options appear for starting product. Order Option 13 when IGC must be tested; order impact Options when joules must appear on the certificate. SHH STEEL 3.1 documents for 1.4307 state chemistry, heat-treatment/delivery status, tensile, and leak/NDT — mandatory tests stay.
Document completeness for 1.4307 matters as much as the physical tests: cast chemistry, delivery symbol, tensile, and leak/NDT statements have to line up with marking. SHH STEEL reviews that package for X2CrNi18-9 before dispatch so the PED file is not left reconciling mismatched heats.
Packaging and Shipping for EN 10217-7 1.4307
Outbound packing for 1.4307 / X2CrNi18-9 welded pressure tube starts with protected ends, size segregation, and moisture barrier wrap on export loads. Bright-annealed and polished OD (W1R/W2R, WCR, WP) take sleeve or paper wrap against transit galling; descaled W1A/W2A utility tube still needs clean supports under the longitudinal seam. Bundle contact with carbon steel is forbidden in SHH STEEL packing instructions for this grade: rust blooms from foreign iron are visible defects on 304L OD and are treated as packing failures, not cosmetic footnotes.
Stencil content for 1.4307 normally shows maker, OD × wall, EN 10217-7, 1.4307 or X2CrNi18-9, cast, TC1/TC2, inspection mark, and correlation number. Delivery-condition letters appear when useful or when Option 5 made them contractual. SHH STEEL reconciles tags to the purchase-order marking clause before trucks leave.
Bundle IDs on the packing list point back to heats on the 1.4307 certificate. Exact-length and bevelled pieces are kept separate and end-protected. Packaging clauses in the PO are implemented before X2CrNi18-9 leaves the yard. SHH STEEL treats packing and marking for EN 10217-7 1.4307 / X2CrNi18-9 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.
Why Choose SHH STEEL
SHH STEEL can produce and supply X2CrNi18-9 under EN 10217-7 1.4307 with the heat treatment, TC1/TC2 tests, and EN 10204 3.1 paperwork the order names — not a relabelled 304L remnant. Part 7 stays separate from seamless Part 5 and from ASTM tubing/pipe standards on the certificate; wrong-table tensile paste-ups are refused.
Practical selection beats wishful stamping. Sisters worth comparing: LINKPLACE1.4301, LINKPLACE1.4306, LINKPLACE1.4311, LINKPLACE1.4404. Caution on 1.4307: do not treat 1.4307 as a chloride-SCC cure — when chlorides and tensile stress stack up, move to Mo-bearing austenitics or duplex rather than hoping low carbon alone will hold We would rather redirect the enquiry than ship the wrong EN number Linked sisters on this hub: EN 10217-7 1.4301, EN 10217-7 1.4306, EN 10217-7 1.4311, EN 10217-7 1.4404. Live ASTM/ASME anchors: A269 TP304L, A213 TP304L, SA213 TP304L, A312 TP304L.
Supply Capability
Enquiry intake for 1.4307 / X2CrNi18-9: SHH STEEL can produce and make EN 10217-7 welded tube to the edition, TC1/TC2, delivery symbol, and options you name. Use the capability table and Stock / Available sizes map as a starting size conversation. Common cold-finished wca/wcr bands for hygienic and utility od, plus larger w1a/w2a descaled routes.
| Item | SHH STEEL capability for 1.4307 |
|---|---|
| Standard | EN 10217-7 |
| Grade | 1.4307 / X2CrNi18-9 |
| Product form | Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition |
| Delivery condition | W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock) |
| Typical size band | ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement |
| Testing | TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options |
| Documents | EN 10204 3.1 (3.2 Option 21); third-party inspection on request |
Stock / Available sizes
Stock / Available sizes for 1.4307 is an enquiry map. Heats of X2CrNi18-9, forming/weld capacity, and finish route decide what can ship when. Provide OD × wall, test category, and delivery symbol rather than assuming shelf SKUs.
| OD (mm) | Typical walls (mm) | Notes |
|---|---|---|
| 12 / 14 / 16 / 19 / 21.3 / 25 | 1.0 / 1.5 / 2.0 / 2.5 | Instrument / hygienic; often WCA/WCR or W2R |
| 26.9 / 33.7 / 38 / 42.4 / 48.3 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Process and utility welded pressure tube |
| 60.3 / 76.1 / 88.9 / 114.3 | 2.0 / 3.0 / 4.0 / 5.0 / 6.0 | Utility and process; lock W1A/W2A vs WCA |
| 141.3 / 168.3 / 219.1 | 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 | Larger welded pressure tube; watch family wall ceiling |
Options 19/18/13 and dual quotes with 1.4301, 1.4306, 1.4311, 1.4404 are normal add-ons. Size bands were sense-checked against peer catalogues; contractual acceptance is still EN 10217-7 with EN ISO 1127. SHH STEEL can produce and supply 1.4307 when capacity matches the order.
FAQ
-
What is EN 10217-7 1.4307 welded stainless steel tube used for?
- EN 10217-7 1.4307 (X2CrNi18-9) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is food process lines, pharmaceutical utilities, clean steam and condensate returns, and general PED piping where a weld seam is accepted and molybdenum is not justified. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
-
Is EN 10217-7 1.4307 the same as 304L under ASTM A269 or A312?
- No. Commercial alias 304L may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP304L, A213 TP304L, SA213 TP304L, A312 TP304L.
-
Does EN 10217-7 1.4307 include seamless tube?
- No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4307. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
-
What mechanical properties does EN 10217-7 require for 1.4307?
- In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 180 MPa, Rp1.0 min 215 MPa, Rm 470–670 MPa, and elongation 40% longitudinal / 35% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
-
1.4307 vs sister grades — which EN 10217-7 number should I buy?
- Buy 1.4307 when the enquiry names this steel number or the duty matches low-carbon 18-8 austenitic for welded pressure tubing where as-welded intergranular corrosion resistance is part of the duty story. Compare EN 10217-7 1.4301, EN 10217-7 1.4306, EN 10217-7 1.4311, EN 10217-7 1.4404 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: do not treat 1.4307 as a chloride-SCC cure — when chlorides and tensile stress stack up, move to Mo-bearing austenitics or duplex rather than hoping low carbon alone will hold
-
What delivery conditions are available for EN 10217-7 1.4307?
- Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
-
What size range can SHH STEEL supply for EN 10217-7 1.4307?
- SHH STEEL can produce and supply EN 10217-7 1.4307 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Common cold-finished wca/wcr bands for hygienic and utility od, plus larger w1a/w2a descaled routes.
-
TC1 or TC2 for EN 10217-7 1.4307?
- Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
-
Is the intergranular corrosion test mandatory for 1.4307?
- No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4307.
-
What documents come with SHH STEEL EN 10217-7 1.4307?
- EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4307, size, cast, and test category.
-
How do I enquire for EN 10217-7 1.4307 with SHH STEEL?
- Send EN 10217-7, steel number 1.4307 / X2CrNi18-9, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.
Conclusion
EN 10217-7 1.4307 (X2CrNi18-9) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4307 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.