EN 10217-7 1.4539 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4539 Welded Stainless Steel Tube

EN 10217-7 1.4539 / X1CrNiMoCu25-20-5 welded stainless pressure tube (904L), austenitic, cast analysis per EN table, ambient Rp0.2 min 220 MPa, Rm 520–720, solution annealed 1060–1140 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4539 / X1CrNiMoCu25-20-5 (904L — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4539 Welded Stainless Steel Tube

When an enquiry still reads “904L welded pressure tube” without a European product standard, the PED paperwork is incomplete. EN 10217-7:2021 closes that gap for circular welded austenitic and duplex stainless tubes; within that list, 1.4539 / X1CrNiMoCu25-20-5 is the austenitic entry that matches this chemistry. SHH STEEL treats the steel number, not the shop alias, as the acceptance key on cast analysis, longitudinal arc or laser seam route, solution annealing where the delivery symbol requires it, and the TC1/TC2 inspection regime. Duty focus: high-alloy Cu-bearing austenitic (904L) welded pressure tube for sulphuric and mixed-acid PED service.

SHH STEEL can produce and supply EN 10217-7 1.4539 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover process welded OD; cold-finished and heat-treated delivery symbols common. Browse the series hub at EN 10217-7.

Commercial 904L welded tube for PED work should land as EN 10217-7 1.4539 with TC1/TC2 — not as an A269 N08904 page pasted into a European pressure file. Typical welded pressure duties include sulphuric acid handling, scrubber piping, pulp and paper chemical lines, and seawater-adjacent utilities that specify 904L. Design caution: 904L is not automatically better than duplex in warm chlorides under tensile stress — SCC and cost both deserve a design review Commercially the grade is often called 904L; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4539 / X1CrNiMoCu25-20-5 on the MTC. Sister numbers on this hub include EN 10217-7 1.4563, EN 10217-7 1.4404, EN 10217-7 1.4547, EN 10217-7 1.4462.4563, 1.4404, 1.4547, 1.4462.

Welded-only scope matters on every 1.4539 order. Seamless sisters are a different standard (EN 10216-5). Sizes prefer EN ISO 1127. Table 1 manufacture is longitudinal automatic arc or laser from strip/plate; do not specify spiral and expect automatic Part 7 acceptance without a written agreement outside the listed routes. Live seamless sister: EN 10216-5 1.4539. Related live ASTM/ASME anchors: A269 N08904.

Chemical Composition of EN 10217-7 1.4539

Ladle analysis controls 1.4539. The austenitic table entry for X1CrNiMoCu25-20-5 is what the cast must satisfy; product analysis remains Option 6. SHH STEEL’s EN 10204 paperwork shows real cast results — catalogue “typical” chemistries are not substituted for EN acceptance on 904L-class welded pressure tube.

Below is the BSSA-published EN 10217-7 cast window for X1CrNiMoCu25-20-5 (steel number 1.4539), aligned to the 2021 list. Maxima apply unless a min–max range appears. Edition confirmation beats brochure reprint.

Element 1.4539 cast analysis (mass %)
Carbon (C) ≤0.020
Silicon (Si) ≤0.70
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.030
Sulfur (S) ≤0.010
Nitrogen (N) ≤0.15
Chromium (Cr) 19.0–21.0
Nickel (Ni) 24.0–26.0
Molybdenum (Mo) 4.00–5.00
Copper (Cu) 1.20–2.00

Chemistry source for steel number 1.4539: BSSA EN 10217-7 chemical article plus public standard cross-check. Do not treat unlisted elements as free additions on X1CrNiMoCu25-20-5 without purchaser agreement (finishing additions excepted under controlled scrap practice).

Mechanical Properties of EN 10217-7 1.4539

For X1CrNiMoCu25-20-5 ordered as EN 10217-7 1.4539, room-temperature mechanical acceptance follows the austenitic ambient table in the solution-annealed (+AT) condition within about 60 mm wall unless Options extend the band. Expect Rp0.2 and Rp1.0 minima plus Rm and elongation. Cryogenic Charpy characterisation exists; tested joules require the relevant Options.

Primary ambient source for 1.4539: BSSA mechanical properties for stainless steels to BS EN 10217-7. Heat-treatment bands for X1CrNiMoCu25-20-5 are public EN stainless figures with an UNCERTAIN flag against paid EN 10217-7:2021 footnotes. Sister-standard tensile values are not silently copied onto this Part 7 document.

Property 1.4539 ambient (solution annealed +AT)
Rp0.2 min (MPa) 220
Rp1.0 min (MPa) 250
Rm (MPa) 520–720
A min % long / trans 35 / 30
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1060–1140 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Ambient mechanical citation for steel number 1.4539: BSSA EN 10217-7 article; annealing bands public EN cross-check (UNCERTAIN vs paid 2021 footnotes). Order impact Options when tested toughness for X1CrNiMoCu25-20-5 must be certified.

Welded Tube Manufacture for EN 10217-7 1.4539

For austenitic grade 1.4539, Part 7 manufacture starts with strip or plate of X1CrNiMoCu25-20-5 chemistry, forms a circular section, and closes it with a longitudinal automatic arc or laser weld per Table 1. Filler may or may not be used depending on route and wall. Outside grinding or bead working before heat treatment appear where the ordered path requires them. Commodity sizes usually run on continuous strip lines; heavier walls move to plate forming. Spiral weld is not invented here as a standard Part 7 route. Seamless product is a different standard — EN 10216-5.

High-alloy austenitic 1.4539 (X1CrNiMoCu25-20-5) is welded longitudinally under Table 1 with procedures that respect the Mo-Cu (and nitrogen where present) balance — heat input and cleanliness matter more than on commodity 18-8. Options 3/4 dress the ID weld when required; Table 2 symbols set surface/heat-treatment path with Option 5 to lock. SHH STEEL can produce and supply 1.4539 as heat-treated descaled or cold-finished product when strip chemistry and weld slots align. Filler guidance for this page: 904L-matching fillers; control heat input; avoid carbon-steel contamination on the weld prep

Declare TC1 or TC2 when buying 1.4539 welded pressure tube. Inspection planning, marking, and NDT scope all read that field. Leak-tightness covers the full quantity; Option 15 chooses hydrostatic versus eddy current. SHH STEEL ties X1CrNiMoCu25-20-5 certificates to the manufacturing route and delivery condition that left the mill.

Dimensions and Tolerances for EN 10217-7 1.4539

Specify D and T when buying EN 10217-7 1.4539 (X1CrNiMoCu25-20-5). EN ISO 1127 preferred sizes are the usual starting list; mass uses stainless density tables. Diameter/wall classes follow Part 7 with EN ISO 1127, including Option 20 D4. Out-of-roundness and eccentricity are absorbed inside those tolerances; weld-edge radial mismatch is separately limited.

Cut-to-length (Option 19) and bevelled ends (Option 18, wall ≥ 3.2 mm) are everyday extras on X1CrNiMoCu25-20-5 welded tube. Tighter OD conversations usually move toward WCA/WCR. SHH STEEL matches the ordered D × T, tolerance class, and delivery symbol before committing 1.4539 weld capacity.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

For X1CrNiMoCu25-20-5 welded tube, SHH STEEL verifies OD, wall, and the selected tolerance class on EN 10217-7 1.4539 before marking. Straightness and end-finish rules in the dimensional clauses still apply — they are not waived by a tight delivery promise. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4539 / X1CrNiMoCu25-20-5 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4539

Designation discipline: EN 10217-7 writes 1.4539 / X1CrNiMoCu25-20-5; shops say 904L. Related ASTM/ASME product pages are cross-references only — wall basis, tensile tables, and inspection differ. EN 10216-5 seamless pages are chemistry cousins with a different manufacture and acceptance route.

Bill-of-materials writers sometimes list 904L next to EN and ASTM numbers interchangeably. For this product, steel number 1.4539 with name X1CrNiMoCu25-20-5 under EN 10217-7 is the welded acceptance path; confirm any dual mark against both mechanical tables before release to fabrication.

Reference Designation Note
EN 10217-7 1.4539 / X1CrNiMoCu25-20-5 This product standard (welded pressure tube)
EN steel name X1CrNiMoCu25-20-5 EN 10027-1 designation used in body and marking
Commercial alias (body only) 904L Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4539 Related live page — different product form (seamless)
A269 N08904 A269 N08904 Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4563, EN 10217-7 1.4404, EN 10217-7 1.4547, EN 10217-7 1.4462. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4539. Live cross-standard anchors: A269 N08904.

Heat Treatment and Delivery Condition for EN 10217-7 1.4539

For X1CrNiMoCu25-20-5 ordered as 1.4539, pick a Table 2 symbol that encodes the required heat treatment and surface. Solution annealing (+AT) underpins the ambient mechanical table: bring the tube into the solution-temperature window and cool quickly enough to satisfy strength and corrosion notes. For X1CrNiMoCu25-20-5 under steel number 1.4539, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Solution band used on this page for 1.4539: 1060–1140 °C, cool by water or air (public EN stainless cross-check; UNCERTAIN vs paid EN 10217-7:2021 footnotes). Lock the delivery-condition symbol with Option 5 when pickle versus bright anneal versus WG/WP must be contractual for X1CrNiMoCu25-20-5.

Item 1.4539
Solution annealing band (public) 1060–1140 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Heat-treatment honesty is part of the X1CrNiMoCu25-20-5 supply package: SHH STEEL documents the delivery-condition symbol actually run on EN 10217-7 1.4539, including whether the longitudinal weld was recrystallized on cold-finished routes, rather than implying a generic “annealed” stamp without Table 2 language. For X1CrNiMoCu25-20-5 under steel number 1.4539, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4539

Choose 1.4539 (X1CrNiMoCu25-20-5) when welded PED tubing must carry this corrosion story: high Ni-Mo-Cu for reducing acids and improved localised corrosion versus 316L; still an austenitic SCC profile in hot chlorides. Delivery-condition IGC resistance is characterised to EN ISO 3651-2 methods in the Part 7 tables, but a tested IGC result still requires Option 13 on the order.

When a specification cites PREN for 1.4539, treat it as project language, not as an EN 10217-7 table value. Ambient acceptance for X1CrNiMoCu25-20-5 stays on the Part 7 mechanical/chemical path; sister numbers EN 10217-7 1.4563, EN 10217-7 1.4404, EN 10217-7 1.4547, EN 10217-7 1.4462 cover step-ups in Mo, N, or duplex balance.

Applications of EN 10217-7 1.4539 Tube

Applications for steel number 1.4539 / X1CrNiMoCu25-20-5 cluster around welded PED service that tolerates a mill seam: sulphuric acid handling, scrubber piping, pulp and paper chemical lines, and seawater-adjacent utilities that specify 904L. Delivery condition and test category on the order decide how that tube is finished and inspected before it reaches the spool.

Skip 1.4539 when the specification locks seamless product (EN 10216-5 — see EN 10216-5 1.4539), when ASTM A269/A312 text is the only acceptance language, or when corrosion/strength clearly points at another family. SHH STEEL can produce and supply X1CrNiMoCu25-20-5 welded tube in the enquiry band and will redirect to a sister or live ASTM/ASME page when that is wiser. Related live pages: A269 N08904.

Weldability of EN 10217-7 1.4539

Mill welding of EN 10217-7 1.4539 is the longitudinal arc/laser seam on the ordered Table 1 route; field or shop welding is a separate PED joint design. Filler and procedure choices track the austenitic chemistry of X1CrNiMoCu25-20-5. Practical note: 904L-matching fillers; control heat input; avoid carbon-steel contamination on the weld prep

PED joint design — including whether X1CrNiMoCu25-20-5 can remain as-welded in corrosive service — is outside mill scope. SHH STEEL’s deliverable for 1.4539 is compliant welded tube with documented chemistry, route, delivery condition, mechanical results, and leak/NDT statements.

Surface Finishes for EN 10217-7 1.4539

For X1CrNiMoCu25-20-5 welded under EN 10217-7 1.4539, finish language equals Table 2 language: descaled for utility, bright-annealed for cleaner OD, ground or polished when roughness is contractual. Agree WP/WG at enquiry with inspectable criteria. Transit contact with carbon steel is forbidden because free-iron rust blooms on 904L OD fail goods-in visual checks and contaminate stainless systems downstream of the weld seam.

Special ID finishes are order lines. When measurement is possible, SHH STEEL can produce and supply pickled, bright-annealed, and polished 1.4539; we will not invent an Ra number for 904L or imply electropolish that was never run on X1CrNiMoCu25-20-5. Exterior polish without an agreed grit is equally unacceptable as certificate language.

When 904L welded tube must look like instrumentation stock, bright anneal or polish belongs on the order with 1.4539. Descaled W1A/W2A remains correct for many lagged utility runs. SHH STEEL can produce and supply only the finish path X1CrNiMoCu25-20-5 can actually certify under EN 10217-7 on the promised date.

Inspection and Testing for EN 10217-7 1.4539

For EN 10217-7 1.4539 / X1CrNiMoCu25-20-5, expect cast chemistry per heat, ambient tensile at TC1/TC2 frequency, technological tests from the standard’s table, and 100% leak-tightness (hydrostatic or eddy current). Dimensional, visual, and material-identification checks close the baseline regime. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4539 purchase order so X1CrNiMoCu25-20-5 inspection planning matches the PED file before weld slots are locked.

Heavier weld-seam NDT is the TC2 differentiator on 1.4539. Laminar/edge NDT Options, IGC Option 13, and Charpy Options are purchaser choices. SHH STEEL’s EN 10204 3.1 file records what was melted, how X1CrNiMoCu25-20-5 was heat-treated, what tensile was achieved, and which leak/NDT path ran — without skipping required tests for speed.

Option 13 IGC for 1.4539 should be named when the end user expects a tested EN ISO 3651-2 result on the MTC. Table “resists IGC as delivered” language for X1CrNiMoCu25-20-5 is not the same as a witnessed test report.

Packaging and Shipping for EN 10217-7 1.4539

SHH STEEL ships EN 10217-7 1.4539 in end-protected, size-sorted bundles or wooden crates with waterproof wrapping for sea freight. High-alloy 904L bright-annealed or polished OD is sleeved against transit galling; descaled chemical-service tube still ships on non-contaminating supports with capped ends. Because X1CrNiMoCu25-20-5 is stainless, packing deliberately keeps carbon-steel strapping and rusty fixtures off the tube surface — free-iron transfer is a common transit complaint on 904L and is prevented at the dock, not debated later.

Traceability marking on X1CrNiMoCu25-20-5 welded tube carries EN 10217-7, steel number 1.4539, size, cast, test category, and inspection/correlation marks. Delivery symbols are added when ordered or when clarity helps receiving. SHH STEEL aligns stencil language with the PO before dispatch. SHH STEEL treats packing and marking for EN 10217-7 1.4539 / X1CrNiMoCu25-20-5 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Heat-to-bundle correlation on export documents saves receiving time for 904L welded tube. Cut-to-length and bevelled lots are packed apart with caps fitted. SHH STEEL applies the agreed packing note on every 1.4539 shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4539 / X1CrNiMoCu25-20-5 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and make EN 10217-7 1.4539 welded pressure tube for buyers who need documented X1CrNiMoCu25-20-5 chemistry, delivery-condition heat treatment, and leak-tightness — not a shop-floor 904L stamp. We refuse to blur this page into EN 10216-5 seamless acceptance or to decorate MTCs with foreign tensile floors.

When 904L is the wrong tool, SHH STEEL steers toward EN 10217-7 LINKPLACE1.4563, EN 10217-7 LINKPLACE1.4404, EN 10217-7 LINKPLACE1.4547, EN 10217-7 LINKPLACE1.4462. Keep this caution in view: 904L is not automatically better than duplex in warm chlorides under tensile stress — SCC and cost both deserve a design review A mis-selected steel number helps no PED dossier. Live ASTM/ASME anchors: A269 N08904.

Supply Capability

SHH STEEL can produce and supply welded EN 10217-7 1.4539 when your enquiry states standard edition, test category, delivery condition, and options. Capability and Stock / Available sizes tables below support first sizing for this 904L pressure grade. Process welded od; cold-finished and heat-treated delivery symbols common.

Item SHH STEEL capability for 1.4539
Standard EN 10217-7
Grade 1.4539 / X1CrNiMoCu25-20-5
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

Treat the size map as availability language for 904L welded pressure tube, not a tonnage inventory. 1.4539 depends on X1CrNiMoCu25-20-5 flat-product supply and weld finishing. Confirm against your OD × wall and TC1/TC2 list.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Exact length, bevel, IGC, and sister-grade duals (1.4563, 1.4404, 1.4547, 1.4462) can share one enquiry. Catalogue size patterns are indicative; EN 10217-7 governs. SHH STEEL can produce and supply X1CrNiMoCu25-20-5 welded tube in this map when the mill path fits.

FAQ

What is EN 10217-7 1.4539 welded stainless steel tube used for?
EN 10217-7 1.4539 (X1CrNiMoCu25-20-5) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is sulphuric acid handling, scrubber piping, pulp and paper chemical lines, and seawater-adjacent utilities that specify 904L. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4539 the same as 904L under ASTM A269 or A312?
No. Commercial alias 904L may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 N08904.
Does EN 10217-7 1.4539 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4539. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4539?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 220 MPa, Rp1.0 min 250 MPa, Rm 520–720 MPa, and elongation 35% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4539 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4539 when the enquiry names this steel number or the duty matches high-alloy Cu-bearing austenitic (904L) welded pressure tube for sulphuric and mixed-acid PED service. Compare EN 10217-7 1.4563, EN 10217-7 1.4404, EN 10217-7 1.4547, EN 10217-7 1.4462 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: 904L is not automatically better than duplex in warm chlorides under tensile stress — SCC and cost both deserve a design review
What delivery conditions are available for EN 10217-7 1.4539?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4539?
SHH STEEL can produce and supply EN 10217-7 1.4539 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Process welded od; cold-finished and heat-treated delivery symbols common.
TC1 or TC2 for EN 10217-7 1.4539?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4539?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4539.
What documents come with SHH STEEL EN 10217-7 1.4539?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4539, size, cast, and test category.
How do I enquire for EN 10217-7 1.4539 with SHH STEEL?
Send EN 10217-7, steel number 1.4539 / X1CrNiMoCu25-20-5, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4539 (X1CrNiMoCu25-20-5) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4539 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X